An engineering model for the decay of timber in ground contact
2003 - IRG/WP 03-20260
To predict the residual strength of an engineered structure, it is first necessary to predict the effect of decay. A model was developed in which the effective area of structural decay in large section timbers was defined as that area that could be picked out with a pen-knife. Some limited studies indicated that for practical purposes the remaining wood could be assumed to have its full residual s...
R H Leicester, C-H Wang, M N Nguyen, J D Thornton, G Johnson, D Gardner, G C Foliente, C MacKenzie


A summary of work carried out to compare natural and artificial weathering for preconditioning test specimens in testing anti-stain chemicals for wood in service
1976 - IRG/WP 266
Since 1972 work has been in progress within CEN to establish a European standard for the testing of wood preservatives designed to prevent blue-staining of wood in service. The method is based on the Butin test and involves pre-weathering of the samples prior to biological testing. The weathering regime employed is 6 months outside exposure from March to October. This imposes severe limitations on...
D J Dickinson, A F Bravery


Serviceability modeling-Predicting and extending the useful service life of FRT-plywood roof sheathing
2000 - IRG/WP 00-20210
One of the most, if not the most, efficient methods of extending our existing forest resource is to prolong the service life of wood currently in-service by using those existing structures to meet our future needs (Hamilton and Winandy 1998). It is currently estimated that over 7 x 109 m3 (3 trillion bd. ft) of wood is currently in service within the United States of America (PATH 1999). Research ...
J E Winandy


Resolution from IRG Working Group II Sub-group 4 'Stain in timber in service'
1984 - IRG/WP 2230
Sub-group 4 of IRG Working Group II has completed a series of studies of artificial weathering as an alternative to natural weathering in relation to testing the efficacy of chemicals in preventing blue stain in service. The Sub-group reports that within the limits of the equipments studied and described in its report Document No: IRG/WP/2215 the extent of blue stain varied little as a direct cons...
D J Dickinson


Appearance of PEC-treated poles in service
1985 - IRG/WP 3323
Poles treated with conventional high temperature creosote (HTC) are banned for use in Australia by the major union handling them. Pigment emulsified creosote (PEC) is an acceptable alternative because it provides much dryer and cleaner commodities than does HTC. More than 5000 poles have so far been treated with PEC and many are being installed into service. The brown pigmented PEC 30 B has given ...
H Greaves, C-W Chin, K J McCarthy, J B Watkins


Fungus cellar testing as an evaluation method for performance of treated timber in ground contact
2001 - IRG/WP 01-20227
A fungus cellar method for the accelerated evaluation of performance of treated wood in ground contact is described. The test soil comprised of sandy loam, vermiculite and Japanese horticulture soil "Kanumatsuchi" in a ratio of 6:2:2 by volume. The soil was inoculated with the dominant test fungus isolated with selective medium from decayed wood samples. Pairs of treated and untreated wood specime...
Y Nagano


Butt-end incising to improve penetration and retention of creosote in Eucalyptus saligna power transmission poles in Kenya. Preliminary results
2002 - IRG/WP 02-40249
Incising as a possible technique to improve penetration and retention of creosote in the butt end of Eucalyptus saligna power transmission poles in Kenya was investigated. Debarked, butt-end samples from whole poles were seasoned (15% MC), incised using four patterns of incisions, sealed at the top or small diameter end, and pressure treated with a mixture of creosote-furnace oil (60/40 mix) at a...
R Venkatasamy


Service life of pressure treated deckings of spruce in direct contact with the ground
1988 - IRG/WP 3463
For decking outdoors in Sweden, pressure treated Scots pine (Pinus sylvestris L.) is used, on account of its treatability. The feasibility of using instead the refractory Norway spruce (Picea abies Karst.) is tested in a field trial. The spruce decks were treated together with pine decks with an ordinary Bethell process. As yet, after more than four years of exposure, neither in the battens nor in...
J B Boutelje, T Sebring


Butt-end incising to improve penetration and retention of CCA in Eucalyptus saligna telegraph poles in Kenya: Preliminary results
2002 - IRG/WP 02-40243
Incising to improve penetration and retention of Copper Chrome Arsenate (CCA) in the butt end of Eucalyptus saligna telegraph poles was investigated. Debarked, seasoned (15% MC) butt-end samples from full size telegraph poles were incised using four patterns of incisions, sealed at the top or small diameter end, and pressure treated, together with un-incised samples, with CCA-C (3.0% oxide typ...
R Venkatasamy


A serial exposure technique for estimating probable service life of treated timber
1978 - IRG/WP 2111
This paper briefly describes part of our preliminary work aimed at developing a test procedure that culd be adopted as a standard method. A detailed version of the work has been submitted for formal publication. In both papers, the aim is to promote interest in extended laboratory testing of wood preservatives. It is believed that this work may provide the basis of a laboratory test procedure from...
J A Butcher


Alternatives to CCA for ground contact protection of timber: a perspective from UK on performance and service life expectations
2002 - IRG/WP 02-30289
The proposed amendment to the European Union's Marketing and Use Directive (1976/769/EEC) in respect of arsenic in CCA wood preservatives seeks to restrict the use of CCA across the European Union. CCA is an extremely important wood preservative in the UK from the manufacturing of the product to the extent of use of CCA-treated timber. Based on our experience and judgement on the use of ...
E D Suttie, A F Bravery, T B Dearling


Natural durability, density and extractive contents of 42 wood species of Bangladesh.
2003 - IRG/WP 03-10490
Natural durability, density and major extractive contents of 42 lesser used or unused wood species of Bangladesh have been studied. Correlation analysis between these properties has been performed. It has been shown that natural durability of these species neither explained by water soluble nor by alcohol benzene extractive contents. Density has a weak but significant positive correlation with dur...
S Akhter, K Akhter, S C Das


Field test design for service life prediction of wooden components
2005 - IRG/WP 05-20308
Wood is predominantly degraded by organisms. Thus, compared to other building materials, service life of wooden material is influenced by many more factors, which are divided into direct and indirect factors. Climate, geographical position, and construction criteria count to the indirect decay factors. Besides material inherent properties (natural durability, wood preservatives), wood temperature...
A O Rapp, C Brischke


Effect of kerfing on performance of Douglas-fir utility poles in the Pacific Northwest
1990 - IRG/WP 3604
Preservative treatment produces an external layer of protection in Douglas-fir poles, but the development of deep checks as the wood dries after treatment can permit entry by fungi and insects. A variety of remedial treatments can arrest this decay; however, it is far more efficient to prevent checking. Kerfing represents one potential method for limiting the development of deep checks. In previou...
J J Morrell


Blue stain in timber in service. Results of further IRG collaborative tests to compare different artificial weathering systems
1981 - IRG/WP 2146
The previous work described in Document No IRG/WP/286 examined 3 preservatives (1% phenyl mercury succinate - PMS, 5% pentachlorophenol - PCP and 1.5% Preventol A4 - PA4) subjected to 5 different artificial weathering systems (BAM Xenotest, Cuprinol Marr, EMPA Xenotest, Gori Atlas and PRL Marr) and after natural weathering at 5 sites (BAM, Cuprinol, EMPA, Gori and PRL). Results showed good correla...
A F Bravery, D J Dickinson


Service life of outdoor wooden constructions. Expectations of private house owners in Sweden
2001 - IRG/WP 01-10401
Wood is traditionally used in indoor as well as outdoor applications. However, if not kept dry, wood is easily attacked by wood degrading micro-organisms. Thus the service life is heavily affected by construction design, choice of wood and wood treatment. For most constructions there is an expected service life. The expectations concerning wooden constructions and what kind of wood is chosen to fu...
M-L Edlund, J Jermer


Quality assured wooden sidings - Criteria, performance evaluations and current status
2000 - IRG/WP 00-20216
Quality assured wooden sidings were brought to the Swedish market in 1998. The system was worked out during a six year period in a close cooperation between the sawmill industry and several research institutes. Centuries of use have given a wealth of experience of spruce boards as a siding material, showing that it works well in most cases but also that its longevity is highly variable, depending ...
F Englund, I Johansson, J Ekstedt, R Nussbaum


Artificial weathering as an aid to assessing the effectiveness of chemicals for preventing blue stain in service - a co-operative study
1984 - IRG/WP 2215
The paper reports co-operative studies carried out within Working Group II of the International Research Group on Wood Preservation to assess the effects of different artificial weathering systems on the performance of fungicides to control blue-stain in service. It has been shown that Atlas, Xenotest and Marr equipments operated according to particular standard schedules can give essentially the ...
A F Bravery, D J Dickinson


Preservative treatment of rubber wood (Hevea brasiliensis) to increase its service life
2005 - IRG/WP 05-40320
Rubber wood (Hevea brasiliensis) possess excellent properties for interior designing, wood working and furniture making. But it is very much susceptible to sap stain and mould fungi which decreases the service life. For profitable uses , it is necessary to increase the service life of rubber wood. To protect the rubber wood from wood degrading agents, the sawn timber were treated with Borax – b...
K Akhter


Deterioration of wood viewed from iron nail
1991 - IRG/WP 2368
Deterioration of nail was graded by a five - rank numerical - rating. The rating of nail moisture content and decay of wood were inspected in a mortal-wall of 34-year-old house. The wood was mostly in decay, when the rating of the nail was above about 4, and the moisture content was above about 20%. Nailed wood specimens kept in several humidity room of 20°C for 4 years showed that the rating of ...
H Imamura


Service Life Prediction of Wood Claddings by in-situ Measurement of Wood Moisture Content
2004 - IRG/WP 04-20304
The Danish Technological Institute is in co-operation with industry partners running a project aiming at predicting the service life of different wood protecting systems. The project focuses on examining the moisture reducing effect of different wood claddings and the ability to maintain the appearance of the surfaces, when the wood is used in service class 3. A façade construction is exposed t...
B Lindegaard, N Morsing


Suitability of propiconazole (R 49362) as a new-generation fungicide
1989 - IRG/WP 3529
Propiconazole (R 49362), an anti-fungal triazole-compound of Janssen Pharmaceutica, has been extensively tested to determine its potential use as a wood preserving fungicide. Various tests in both private laboratories and official institutes indicate a good activity against Basidiomycetes (brown and white rot) and Ascomycetes (blue stain-in-service). The active ingredient seems very resistant to w...
A R Valcke


Comparison of the anti-fungal efficacy of Cobra with drill perforation on oscillating pressure treated spruce transmission poles -Laboratory test
1988 - IRG/WP 3469
A laboratory method for measuring the depth of penetration of the fungicidal concentrations effective against basidiomycetes (brown rot) was developed. The tests on CCB oscillating pressure treated spruce transmission poles have shown that the depth of salt penetration can be increased by about 10 mm by a drill perforation before the impregnation. An even better penetration is reached, however, if...
E Graf, B Zgraggen


Some fundamental thoughts on the prediction of field performance from lab-testing based on comparison of lab and field test results of some copper-free materials
2003 - IRG/WP 03-20269
In the paper results from lab testing (ENV 807 and EN 113) are compared with field results (EN 252) of differently treated wood. Depending on the type of the organic biocide containing material and depending on type of soil and type of decay differences were found in suitability of the lab methods to predict field performance. The attempt is made to interpret the found differences. Furthermore it ...
A O Rapp, U Augusta


Blue stain in timber in service. Preliminary results of the IRG collaborative tests to compare natural and artificial weathering
1978 - IRG/WP 286
The collaborative programme was initiated at IRG Meetings in Wildhaus, 1976. The six collaborators were BAM (Berlin), Cuprinol Ltd (UK), EMPA (Switzerland), GORI (Denmark), PRL (UK) and Imperial College (UK). Experimental plans were finalised in December 1976 and panels treated by Cuprinol Ltd early in 1977. Natural weathering was carried out by BAM, Cuprinol, EMPA, GORI and PRL during April-Septe...
A F Bravery, D J Dickinson