Water repellency of wood treated with alkylammonium compounds and chromated copper arsenate
2000 - IRG/WP 00-30231
The comparative water sorption properties of southern pine treated with CCA and several alkylammonium compounds was evaluated for freshly treated wood and for wood after exposure in a fungus cellar. It was found that CCA imparts considerable water repellency to wood which is reduced somewhat after exposure to wet soil. With the exception of a long chain (C20 -C22) compound, the alkylammonium compo...
D D Nicholas, A Kabir, A D Williams, A F Preston


Investigations of the treatability of various commercially significant Turkish timbers
1976 - IRG/WP 370 E
Timbers which naturally deteriorate quickly can only be used commercially when their life is increased by the use of chemical treatments. The treatment of the timber can only be planned on a regular basis when the treatability of the wood is known. The purpose of the experiments was therefore to determine to what extent the various types of wood could be sufficiently impregnated. The question of t...
R Ilhan


Strategies for enhancing usage of treated wood in Indian context
2005 - IRG/WP 05-40305
India constitutes 2% of the world’s forest area but it has to support over 15% of the human and nearly 14% of the cattle population and therefore forests in India are under immense biotic pressure. The main concern today is the rate at which avoidable factors or man made threats accelerate the process of forest degradation and to evolve measures to check the same. Man made threats include expl...
P K Aggarwal, S C Gairola


Influences of the hydro-thermal treatment on physical properties of beech wood (Fagus orientalis)
2005 - IRG/WP 05-40303
Influences of the hydro-thermal treatment on physical properties of beech wood were studied. Wood specimens (2×2×2cm) were treated in two steps. At first step, samples were treated at 160,180 & 200ºC for 4, 5 & 6 hours. At second step, treated samples were cured based on their first step treatment temperatures (160,180 & 200ºC) for 16 hours. The treated samples were soaked in water...
B Mohebby, I Sanaei


Färbeverfahren zur Unterscheidung von Holzzonen mit unterschiedlichem Absorptionsvermögen, insbesondere bei Fichtenholz (Picea abies Karst.). [Staining method for distinguishing zones of wood with different absorption behaviour, particularly in spruce (Picea abies Karst.)]
1980 - IRG/WP 3163
A simple regressive staining method for crosscut wood surfaces is described. Phloroglucinol-hydrochloric acid serves as stain; flowing water and a solution of sodium carbonate are used for development and fixation of a picture showing the differences of absorption. Hydrophobic zones and, contrary to this, zones with a high water content can also be shown. Comparing green spruce wood before and dur...
S Cymorek


Estimates of wood-consumption rates by termites
1983 - IRG/WP 1201
Effects of 2 components; termite-biomass and experiment duration on estimates of wood-consumption rates (mg wood/g termite/day), were examined. Three models; (1) no mortality, (2) linear mortality and (3) nonlinear mortality were used to calculate mean standing-crop biomass of termites. Model (1) predicted a significantly lower wood-consumption rate than those based on models (2) and (3). No signi...
N-Y Su, J P La Fage


The relationship between basic density and liquid absorption in fast, plantation grown 8 Year Old Eucalyptus pellita and E. Urophylla
2002 - IRG/WP 02-40220
The liquid absorption characteristics of 8 year old Eucalyptus pellita and E. urophylla were studied in order to gain insight into the treatability of this young, fast grown eucalypt plantation resource. The trees were grown in an experimental plantation trial near Innisfail in northeast Queensland. The study demonstrated that average sapwood basic density in young plantation grown E. pellita a...
J Norton, A Muneri


Wood structure in relation to excessive absorption - a literature survey
1971 - IRG/WP 300
This literature study, composed in connection with 'the structure of wood in relation to the excessive absorption', started from the idea that the subject only could be dealt with successfully if the structure was taken into account in relation to a normal absorption pattern in so far as this knowledge can enlighten the understanding of the abnormal situation. The normal penetrat...
S M Jutte


A technical note on the limitations of atomic absorption spectrophotometric analysis of copper/chrome/arsenic solutions according to BS 4072 (1974) and BS 5666: Part 3 (1979)
1988 - IRG/WP 2320
British Standards BS 4072 (1974) and BS 5666: Part 3 (1979) detail an atomic absorption spectrophotometric method for the quantitative determination of copper, chrome and arsenic in both preservative solutions and treated timber. Use of this technique during a research programme at Aberdeen has highlighted some potential inaccuracies with this method if these standard specifications are adhered to...
A J Pendlebury, J A Petty


The natural history of teredinid molluscs and other marine wood borers in Papua New Guinea
1975 - IRG/WP 410
The teredinids, commonly known as teredos or shipworms, are bivalve molluscs adapted to boring into wood. They are most closely related to the Family Pholadidae, or piddocks, which bore into mud, stone and coral. The teredinids have a relatively small, hemi-spherically shaped shell, the elongated body extending beyond the posterior end of the shell valves. The soft body, protected by the wood and ...
S M Rayner


In vivo growth study on two gymnosperms and four angiosperms for REB wood poles
1998 - IRG/WP 98-10246
Revealed that the highest growth rates and pole yield in two plantation sites in Bangladesh are significant with 2.06 cm/y in diameter, 0.97 m/y in height and 90% pole yield within 19y in Pinus caribaea; 1.96 cm/y, 0.91 m/y and 100% pole yield within 15y in Xylia dolabriformis; 1.88 cm/y, 0.91 m/y and 22% pole yield within 13y in Dipterocarpus turbinatus; 1.64 cm/y, 0.82 m/y and 28.75% pole within...
A K Lahiry


Uptake of copper by mycelium of wood decay fungi growing on copper S-substituted thioglycolate containing nutrient media
1998 - IRG/WP 98-10291
Mycelia of Trametes versicolor, Coniophora puteana and Poria monticola were grown on potato dextrose agar (PDA) media, containing various concentrations of copper N,N-dimethyldithiocarbamoylacetate (which may be regarded as a copper S-substituted thioglycolate). The tested copper compound revealed relatively low fungicidal activity. After 13-18 day growing period, we determined concentrations of a...
M Humar, M Petric, F Pohleven, P Kalan


Laboratory evaluation of water repellents as antisapstain treatment additives
1986 - IRG/WP 3382
Water repellent formulations consisting of five paraffin wax emulsions, three polyethylene wax emulsions, two polybutadiene resin emulsions, a polyester emulsion, and a ß-pinene polymer emulsion were subjected to water repellency tests on radiata pine sapwood. With one exception, the parafin wax emulsions were more effective water repellents than the alternative formulations and one of the paraff...
D V Plackett, C M Chittenden


Creosote immersion treatments of fence-posts of different pines
1986 - IRG/WP 3386
This paper describes the preservation with creosote by immersion of fence-post of Pinus sylvestris, Pinus pinea and Pinus radiata. Taking into account the rural use of the fence-post, an easy method available in the field to the agriculturalists. A regressions analysis has been carried out, dealing with the absorption, retentions and penetrations shown after 1, 3 and 7 days of treatment. The great...
C De Arana Moncada


Permeability measurements on surface layers for detecting wood with abnormally high permeability
1988 - IRG/WP 2298
Wet storage of timber during the warm period of the year may lead to an increased permeability of the wood, an undesirable phenomenon for several wood industries and also for many end-uses. Neither before nor after drying, such wood with "wet storage damage" can be visually distinguished from wood with a normal permeability. A non-destructive method for inspecting the permeability of surface layer...
J B Boutelje, G Hägglund


Penetration and absorption of water-borne preservatives in conifers from the Western United States: A preliminary report
1988 - IRG/WP 3475
The treatment of most softwoods from the western United States with waterborne chemicals poses a major challenge. Although many of these species are commercially treated with waterbornes, there is considerable debate about their treatability. At present, there is little or no information on the treatability of western wood species with waterborne chemicals. The lack of accurate treatability inform...
S Kumar, J J Morrell


Factors affecting decay rates in a fungus cellar
1985 - IRG/WP 2242
Birch and pine stakes treated with chromated copper arsenate and didecyldimethylammonium chloride were incubated in two soils in a "Fungus Cellar" test. At three month intervals, sets of stakes were inspected and assigned visual ratings or removed from the soil beds for weight loss determination. Preliminary results after nine months exposure have shown differences in the decay rates between birch...
P A McKaig


Wood cement composites using spent CCA treated wood
1999 - IRG/WP 99-50126
The feasibility of using spent or out-of-service CCA treated wood as a component of wood/cement composites was evaluated. Cold pressed wood particle cement boards were made using CCA treated particles from a red pine (Pinus resinosa Ait.) pole removed from service and from untreated red pine wood from a new pole. Boards were manufactured using a range of wood to cement ratios and water to cement r...
Chen Huang, P A Cooper


Decay rates and strength and stiffness loss in foundation beams
1992 - IRG/WP 92-1563
The TNO Centre for Timber Research has executed an extensive research programme into the rate of decay in foundation beams, as a result of lowering of ground water tables. The aim of the research was to develop a method, predicting the decrease in strength and stiffness in beams, due to wood decay during drytime of foundation beams. With the calculated extremes in decay, the damage caused by local...
P Esser, H S Buitenkamp


Preservative treatment of round bamboos by a new technique - Some further studies. Part 1
1990 - IRG/WP 3607
In general, the easy susceptibility of bamboos to wood destroying agencies is a major constraint in its rational utilisation. This is more so in tropical countries like India where wood destroying agencies are quite active. In an earlier publication, it was reported that round bamboo specimens of Bambusa balcooa, having three nodes, could be satisfactorily treated by CCA by a new technique develop...
V R Sonti, B Chatterjee


Effects of the delay in the beginning of treatment on absorption and distribution of water-soluble salts in posts treated by sap-replacement method
1992 - IRG/WP 92-3719
One of the most important matters in green wood treatments, such as sap-replacement method, is knowing the longest time available for beginning treatment without losing efficacy. In this paper, the influence of this factor on absorptions and distribution of the preservative into the wood is analized. Tree start-up times were first chosen: 3-6 hours, 48 h and 120 h after being cut down. The treatme...
M V Baonza Merino


Hot and cold treatment in fence posts of Eucalyptus globulus, Castanea sativa, Pinus nigra and Pinus pinaster
1988 - IRG/WP 3489
An analysis is made of the treatment of fence-posts of Eucalyptus globulus, Castanea sativa, Pinus nigra and Pinus pinaster by hot and cold immersion in creosote. The temperatures of the different treatments were 60, 70 and 90°C. The posts were heated for one hour and then allowed to cool for 21 hours 30 min., and finally reheated for 1 hour 30 min. The greatest absorption rates were recorded in ...
C De Arana Moncada, A M Navarrete


Resistance of pine and spruce heartwood against decay - The effect of wood chemical composition and coating with water-borne wood oil product
2006 - IRG/WP 06-10597
Natural durability of wood has been widely studied, but the combination of the natural durability and different treatments has not been the focus of many studies. The durability of wooden products is mainly based on the water permeability and the resistance against organisms. In this study, the water absorption and decay resistance of sapwood and heartwood of Scots pine and Norway spruce were exam...
H Viitanen, S Metsä-Kortelainen, T Laakso


Comparing microbial colonisation and Decay Rates of Wood from Sound and Aphid-Killed Kenyan-Grown Mexican Cypress (Cupressus lusitanica)
2006 - IRG/WP 06-10599
Samples of wood from 10, 15, and 30-year old trees attacked and killed by the cypress aphid (Cinara cupressi) and sound Kenyan-grown Cupressus lusitanica trees were investigated for variations in moisture content, density and susceptibility to microbial decay. MC varied with tree age, a normal trend, and between samples from aphid-killed and sound trees. In samples from 10, 15 and 20-year old so...
R Venkatasamy


Wood-Plastic Composites and the Durability Dilemma: Observations from the Field
2006 - IRG/WP 06-40351
Wood-Plastic Composites (WPCs) used for decking, window & door moldings have experienced dramatic growth in North America over the last several years, with annual production increasing at rates greater than 20% per annum since 1998. A key factor contributing to this growth has been the successfully communicated message that they are "virtually maintenance free". The common perception being t...