Performance of borate-treated lumber in a protected, above-ground field test in Japan
2006 - IRG/WP 06-30395
This document is supplemental to the previous IRG document (Tsunoda et al. 2004). An experiment to simulate the sill plate (dodai) of the Japanese houses was conducted at the termite field test site of the Research Institute for Sustainable Humanosphere of Kyoto University in Kagoshima Pref., Japan where two economically important subterranean termite species [Coptotermes formosanus Shiraki and R...
K Tsunoda, A Byrne, P I Morris, J K Grace


Interaction between Aspergillus niger fungus and other filamentous fungi on salt-agar medium and their growth on natural wood and wood treated with fungicide
2015 - IRG/WP 15-20569
Aspergillus niger (An) is very often used alone or in mixture with other filamentous fungi of the genus in testing biocides in disinfection procedures, safety, hygiene, medical fields as well as for testing resistance of wood and wood-based materials to moulds. Softwood species as well as hardwood are overgrown with An fungus very easily, causing drop of mainly the aesthetic value of wood product....
A Fojutowski, A Kropacz, A Koziróg


Agar block durability test of plywood made of neem (Azadiracta indica) leaves treated veneer using two white rot fungi
2017 - IRG/WP 17-40782
This study has been undertaken to investigate the durability of plywood made from non-durable wood (simul, Bombax ceiba) veneer treated by neem (Azadiracta indica, A. Juss.) leaves. The veneers were treated with cold and hot water solution of neem leaves of different concentrations (10%, 5%, 2.5%) and treatment durations (1, 2, 3 days) for cold water and 20, 40 and 60 minutes for hot water. The pl...
K Akhter, M A Hashem, S Akhter


Development of accelerated decay test for CLT using a fungus grown on agar medium
2019 - IRG/WP 19-20664
CLT is a large-scale wooden board which consists of several layers of sawn lumber stacked in altering directions. Therefore, a lot of large cross sections appear on all narrow faces of CLT. As water penetrates easily into timber from cross section, wooden material whose cross section is exposed to water in in a usage environment is susceptible to deterioration by organisms. Wood deterioration orga...
T Miyauchi, K Kambara, W Ohmura, T Mori, H Matsunaga, N Hattori


Studying amount, location and state of water in modified wood at moisture levels relevant for fungal degradation
2020 - IRG/WP 20-40889
Water is an essential parameter for fungal degradation of wood, but degradation primarily occurs at high moisture levels at water potential in the range of -4 to -0.1 MPa, which corresponds to 97-99.9% relative humidity. At these moisture levels, water is present in the wood structure both in and outside of cell walls. The majority of previous studies on the interaction between wood and water for ...
M Fredriksson, E Engelund Thybring, Ramunas Digaitis


Cellulose nanomaterials in growth media for wood decay fungi
2024 - IRG/WP 24-11035
Cellulose nanofibrils (CNFs) were investigated as a partial substitution for agar in growth media for wood decay fungi. Radial growth measurements of eight basidiomycete fungi were taken on solid growth media with and without CNFs. Additionally, fungal strain virulence was evaluated using the European CSN Standard EN 113-2 wood decay durability test. The inclusion of CNFs did not significantly aff...
K M Ohno, R A Arango, R Sabo, C M Clemons, G T Kirker, A B Bishell


Cellulose nanomaterials in growth media for wood decay fungi
2024 - IRG/WP 24-11035
Cellulose nanofibrils (CNFs) were investigated as a partial substitution for agar in growth media for wood decay fungi. Radial growth measurements of eight basidiomycete fungi were taken on solid growth media with and without CNFs. Additionally, fungal strain virulence was evaluated using the European CSN Standard EN 113-2 wood decay durability test. The inclusion of CNFs did not significantly aff...
K M Ohno, R A Arango, R Sabo, C M Clemons, G T Kirker, A B Bishell