IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 211 documents. Displaying 25 entries per page.


Laboratory evaluation of copper naphthenate pressure treatments against the Formosan subterranean termite
1993 - IRG/WP 93-10005
Southern pine wafers and Douglas-fir cubes pressure treated with copper naphthenate in AWPA P9 Type A oil or in toluene were evaluated for resistance to attack by the Formosan subterranean termite, Coptotermes formosanus Shiraki (Isoptera: Rhinotermitidae). Wood samples were pressure treated to target copper retentions of 0.040, 0.075, 0.095, or 0.150 pcf, conditioned to simulate field exposure, a...
J K Grace, R T Yamamoto, P E Laks


Efficacy of Didecyl Dimethyl Ammonium Chloride (DDAC), Disodium Octaborate Tetrahydrate (DOT), and Chlorothalonil (CTL) against Common Mold Fungi
2004 - IRG/WP 04-30338
The fungitoxic properties of four fungicides, alone and in combination, against four different mold fungi commonly associated with indoor air quality problems were evaluated on two different wood species and sheetrock. The fungicides were chlorothalonil (2,4,5,6-tetrachloroisophthalonitrile) (CTL) in a 40.4% aqueous dispersion, disodium octaborate tetrahydrate (DOT) in two different forms - a ...
J A Micales-Glaeser, J D Lloyd, T L Woods


The difficult choice of the preservation industry when changing to more environmentally acceptable products
2000 - IRG/WP 00-50156
Until recent years the preservation industry in Norway had no problems with the environmental authorities. However, during the last three years the pressure has increased, and the authorities' solution to restrict hazardous chemicals is to introduce green (environmental) taxes for the products containing these chemicals, and also for the pressure-treated wood. The preservation industry ac...
F G Evans


Tributyltin compounds in wood preservation: Health and safety aspects
1986 - IRG/WP 3396
The toxicity of organotin compounds of the general formula RnSnX(4-n) depends strongly on the type of organic substituent R and on the degree of substitution n. The residues X, not bound through a tin-carbon bond, are however of much smaller influence. Furthermore, there is evidence that hydrolysis of tributyltin esters will occur under environmental as well as under physiological conditions to TB...
H Schweinfurth, P Günzel, H A B Landsiedel, R Lang, R Reimann, C Schöbel, F Siegmund


Temperature and pressure inside wood during creosote impregnation
1991 - IRG/WP 3649
Creosote gives the best protection against decay for sleepers and poles. However, it has a major drawback - bleeding. Modified impregnation processes to reduce bleeding have been tried. For developing such processes it is important to know the actual temperature and pressure inside the wood. This paper describes measurement of temperature and pressure inside wood during creosote impregnation. The ...
Ö Bergman


Comparison of variable, constant and fluctuating pressure methods
2001 - IRG/WP 01-40212
The objective of this work was to evaluate potential improvements in pressure treatment arising from the use of a control valve. A constant pressure of 1035 kPa was compared to the conventional variable pressure method where the pressure is allowed to drop to 860 kPa as the solution is absorbed by the wood. A fluctuating pressure method (FPM) where the pressure cycles between 1000 and 1070 kPa was...
S M McFarling, P I Morris


The effect of rate of pressure application on preservative uptake along and across the grain of fir (Abies bornmulleriana Mattf.) at different ramp and constant pressure times
2004 - IRG/WP 04-20292
This study was particularly design to determine the preservative uptake at different ramp (rate of increase in pressure) and constant pressure times on longitudinal, tangential and radial penetrations of fir (Abies bornmulleriana Mattf.) which grown indigeneously in Turkey. The samples of 2 cm cubes of kiln-dried wood (nominated to 12% moisture content) were treated at different ramp times varied ...
I Usta


Standardization of preservative treated timber species for conductor, insulator and transformer packing of REB
1996 - IRG/WP 96-40071
In order to resolve the post landing failure problem of wooden packing for conductor, insulator, transformer of REB, the names of the suitable timber species from different parts of the world, irrespective of countries of origin have been standardized along with their strength and treatability grades. The CCA treatability of some Pakistani timber species have been presented for example which was t...
A K Lahiry


Persistance of active ingredients in treated wood
1993 - IRG/WP 93-50001-20
Disposing of chemically protected waste wood implies the distinction between surface and pressure treatment. Considering that barked round-wood merely contains, after 7 months open storage, less than 30 g per ton of bark or 25 mg per ton of sapwood, depending on the type of insecticide, the bark or sapwood shavings may be incinerated normally, according to less severe legal prescriptions than for ...
E Graf, P Manser, S Rezzonico, B Zgraggen


Strategies for enhancing usage of treated wood in Indian context
2005 - IRG/WP 05-40305
India constitutes 2% of the world’s forest area but it has to support over 15% of the human and nearly 14% of the cattle population and therefore forests in India are under immense biotic pressure. The main concern today is the rate at which avoidable factors or man made threats accelerate the process of forest degradation and to evolve measures to check the same. Man made threats include expl...
P K Aggarwal, S C Gairola


Adequate preservative treatment of kiln dried Eucalyptus camaldulensis and Acacia mangium for tropical and subtropical wood poles
1996 - IRG/WP 96-40075
The Eucalyptus camaldulensis and Acacia mangium round timbers kiln-dried at EMC and full cell pressure treated with CCA-C ensured requisite penetration and adequate dry retention (30 kg/m³ or 4% w/w). The sufficient inherent strength, seasoning property, treatability of sapwood and heartwood equivalent to 44% of radius, natural durability of heartwood, and field investigation on service performan...
A K Lahiry


Tebuconazole - A new triazole fungicide for wood preservation
1990 - IRG/WP 3629
The main cause of economic damage to timber and millwork worldwide are Basidiomycetes (brown and white rot). After testing a wide range of triazole derivatives for their effectiveness against decay fungi, Tebuconazole, a triazole compound, was selected. The physico-chemical, toxicological and ecotoxicological data of this substance are described. Tebuconazole is unleachable, light-stable, heat-sta...
R Gründlinger, O Exner


Some aspects of testing water repellents
1998 - IRG/WP 98-40113
Several test methods are used to determine the efficiency of water repellent treatments on wood. The most common are: contact angle measurement, swelling rate of samples immersed under water and, the increase in mass of wood samples with time or after a fixed period of time either fully immersed under, or partially immersed in or floating on water. In this paper, some fundamental aspects of the l...
D Lukowsky, M Farnow, T Rypstra


Evaluation of the biocide diffusion from treated wood in indoor air. Bibliographic study
1990 - IRG/WP 3584
Within the frame of the risk assessment of the wood preservation products for the Health, the treated wood risk particularly when it is installed in dwellings becomes most important. The European directive "Building materials" (89/106/CEE) mentions the basic requirements with the buildings must comply. Annexe l states in particular that "the building must be conceived and built in order not to bec...
A Pichard


Clean creosote - its development, and comparison with conventional high temperature creosote
1983 - IRG/WP 3235
Pigment emulsified creosote (PEC) is presently being tested and shows considerable stability in terms of water content, pigment level, pH, viscosity, rheological behaviour and microscopy. Timber samples from several eucalypt species have been treated with PEC and side matched samples treated with conventional high temperature creosote (HTC). The PEC treated specimens showed higher weight retention...
C W Chin, J B Watkins, H Greaves


Sawn timber of fir (Abies alba Mill.) - Treatability and usability for the Hazard Classes 3 and 4
1999 - IRG/WP 99-40147
Within a national research project, tests on the treatability on sawn timber of fir (Abies alba Mill.) in oscillation pressure, vacuum pressure and double-vacuum processes have been worked out with 95 trunks taken from 3 different altitude levels (up to a height of 590 metres, 600 to 990 metres and over 1000 metres) and from 4 different regions of Switzerland. As the treatability of round wood can...
E Graf, T Bör


Utilization of coconut timber from north Sulawesi, Indonesia. Part 2: Treatability
1994 - IRG/WP 94-40025
Under tropical conditions coconut wood is quickly degraded by mold and blue stain fungi. Low density wood in ground contact is commonly decomposed by wood destroying fungi within a period of only a few months, higher density wood from the outer stem regions within 24 to 30 months (MOSTEIRO, CASIN, SERIBAN 1976; McQUIRE 1975). Moreover, according to McQUIRE (1975) green wood of lower density is hig...
R-D Peek


Simulation test of subchronic inhalation toxicity of TBTO vapours in the air
1987 - IRG/WP 3454
The test was carried out in a wainscotted room of a normal size. Wooden panelling had been treated with one coat of basic preserving agent and, after the installation, with 2 coats of stain. Laboratory animals (rats) were kept in this room for 90 days. For the same period a control group of test animals was kept in a room of equal size where there was no panelling. During the test, concentration o...
V Skubic, S Kobal, J Stupar, R Ajlec, J Korošin, G R Pecenko


Pretreatment decay in air-seasoning Scots and Corsican pine poles in England
1989 - IRG/WP 1390
British grown Scots and Corsican pine poles were sampled for colonization by basidiomycetes after air-seasoning for 6 to 9, or 16 to 20 months. The amount of infection present in these poles was compared with that in poles which were imported from Finland. After 6 to 9 months seasoning, the British grown pine poles were heavily infected with Peniophora gigantea, Cylindrobasidium evolvens, Stereum ...
A R Zahora, D J Dickinson


Environmental consequences of various materials in utility poles - A life cycle analysis
1992 - IRG/WP 92-3726
A model for environmental life cycle analysis, LCA, has been created to compare environmental impact from transmission poles, made alternatively of concrete, steel, aluminium and pine wood treated with CCA type B or creosote. The main pollution sources and energy use are included in the LCA. One pole size, 12 meters long, is presented in the study, a so called "45 kV" pole. Poles of different mate...
M Erlandsson, K Ödeen, M-L Edlund


Inhibitory effects of leachates from Scots pine wood on germination of some wood rotting fungi
1986 - IRG/WP 1282
Leachates from sapwood of Pinus sylvestris inhibited or reduced the germination of basidiospores of the wood decay fungi tested. The fungi were selected among those preferentially colonizing hardwood or softwood, representatives for brown rot and white rot fungi, early basidiomycete colonizers and late basidiomycete colonizers in above-ground parts of pine as well as fungi found in high frequencie...
J Bjurman


Mould growth at lumber surfaces of pine after kiln and air drying
1994 - IRG/WP 94-40033
Distribution of water soluble substances in green wood and later redistribution during drying is of importance for the colonisation of wood by microorganisms. According to literature the availability of nitrogenous materials is probably a major limiting factor to the microbial colonisation of wood. King et al. (1974) and Oxley et al. (1976) have shown correlation between surface nutrient concentra...
N Terziev, J Bjurman, J B Boutelje


Protection of rubberwood timber. Part 1: Impregnation with boron preservatives
1989 - IRG/WP 3551
Rubberwood (Hevea brasiliensis) were treated with a 3% proprietary mixture of borax/boric acid using three different treatment schedules i.e. full-cell, full-cell to refusal and full-cell with 12 cycles of vacuum/pressure. Freshly cut samples had mean preservative retentions of 187 kg/m³, 214 kg/m³ and 178 kg/m³ respectively. Pre-air dried samples for one week had retentions of 252 kg/m³, 308 ...
L T Hong, C C K Liew


Step-wise pressure process for reducing surface roughness in Japanese cedar timber
2003 - IRG/WP 03-40256
Sixteen dried sawn-timber (10.5 x 10.5 x 360 cm) were cut into half. The half of them was treated by step-wise pressure process with 2.5 MPa maximum, and the other half was treated by conventional pressure process with 2.5 MPa maximum. Average DDAC preservative absorption was 461 kg/m3 in the former and 525 kg/m3 in the later. Surface roughness was expressed as the profile element height of collap...
K Yamamoto, M Nozoki


Detection of dry rot by air analysis
1992 - IRG/WP 92-2399
Detection of dry rot (Serpula lacrymans) at an early stage appears to be very difficult in practice. Also control inspections in buildings, after remedial treatment of dry rot, have a limited accuracy. The use of trained dogs in Denmark initiated the idea for this research on the possible use of air analysis as a detection method. The Centre for Timber Research-TNO (TNO-CHT) and the Institute for ...
P Esser, A C Tas


Previous Page | Next Page