Preliminary field and laboratory findings regarding the efficacy of a novel anti-marine wood borer agent
2000 - IRG/WP 00-10380
Blocks of sapwood of Pinus nigra were treated by vacuum impregnation with Biocide A to retentions of 0.5, 1 and 2 kg m-3. Similar blocks were vacuum-pressure impregnated with CCA to retentions of 2, 24 and 38kg m-3. The blocks were exposed subtidally in Mourilyan Harbour (Queensland, Australia). After 5 and 10 months exposure, blocks were removed, examined for superficial signs of attack by wood b...
A Praël, S M Cragg, R A Eaton


Long-term protection of stored lumber against mould, stain, and specifically decay: A comparative field test of fungicidal formulations
1984 - IRG/WP 3281
The problem of decay in packaged, unseasoned lumber stored for many months has become of major importance in recent years. Large financial claims have resulted from decay in Canadian lumber stored at length in seaports and storage yards of distributors. For decades acceptable protection from moulds and sapstain was readily achieved with chlorinated phenols applied at appropriate treating levels. H...
A J Cserjesi, A Byrne, E L Johnson


Effects of heat treatment on water repellence and anti-swelling efficiency of beech wood
2002 - IRG/WP 02-40223
The heating of solid wood to higher temperatures is the simplest and the cheapest means for stabilizing its dimensions. For the investigation of the effect of thermal treatment on water repellency effectiveness and anti-swelling efficiency of beech wood (Fagus orientalis Lipsky), air-seasoned samples of beech wood were heated in presence of air at temperatures of 130 C, 150 C, 180 C and 200 C for ...
S Yildiz


A status report on code of good practices
1991 - IRG/WP 3679
Code of Good Practices - Anti Sapstain documents, presented to IRG meetings in the past, are the basic documents for health and safety of the workers and the environment in Canada. The BC Ministry of Environnment has now issued regulations in the area of effluent discharge. While Pentachlorophenols (PCP) are not used by the industry, the documents are still used as a guideline document for the oth...
V N P Mathur, G Das


Standardisation of sapstain tests - A challenge
1992 - IRG/WP 92-2403
In the last decade many new anti-sapstain products have been tested world-wide under laboratory and field conditions. Several extensive test programmes have been executed with different non-standardized test methods and procedures, with the result that the biological findings cannot be compared with each other. In this paper, gathered recommendations will be given in order to standardize test meth...
G Rustenburg, C J Klaver


International comparison of three field methods for assessing the in-ground termite resistance of materials - highlights after two years
1999 - IRG/WP 99-20157
First-year results of a comparative study, evaluating the in-ground termite resistance of a range of materials, including CCA and ACQ-treated timbers, using the below-ground exposure, ground contact and graveyard methods against diverse termite faunas were provided in IRG/WP/98-20132. Further annual inspections have confirmed early trends and identified notable differences between sites and method...
M Lenz, J W Creffield, A F Preston, B M Kard, C Vongkaluang, Y Sornnuwat


An evaluation of chemical treatments for the protection of radiata pine logs from fungal degrade
1986 - IRG/WP 3377
Busan 30, Busan 1009, Mitrol PQ375. and sodium pentachlorophenoxide (NaPCP) plus have been evaluated as antisapstain treatments for the long-term protection of debarked radiata pine logs. After 3 months' winter-spring storage, treated debarked logs had less surface and internal sapstain than 'control' logs. After 6 months' storage all logs had internal sapstain ...
J A Drysdale, M E Hedley, J A Butcher


Durability of Wood Plastic Composites Relative to Natural Weathering and Preservative Treatment With Zinc Borate
2005 - IRG/WP 05-40316
Wood-Plastic Composites (WPCs) used for decking have experienced dramatic increases in North America, averaging 25% growth per annum since 1998. A key factor contributing to this growth has been the successfully communicated message that they are "virtually maintenance free". The common perception being that the wood fiber is completely encapsulated by the thermoplastic resin, minimizing the pot...
M E Mankowski, F M Ascherl, M J Manning


Properties of hot oil treated wood and the possible chemical reactions between wood and soybean oil during heat treatment
2005 - IRG/WP 05-40304
Thermal treatment with hot oil as the heating media based on the original idea from oil-heat treatment in Germany was investigated. The treatment was mainly carried out at 200ºC and 220ºC for 2 hours and 4 hours, and the wood species were mainly spruce and fir. This paper focuses on the difference between soybean oil and palm oil and the possible chemical reactions between wood and soybean oil. ...
Jieying Wang, P A Cooper


Comparison of three methods for assessing the in-ground termite resistance of treated timber, durable timber and plastics at sites in Australia, USA and Thailand - First results
1998 - IRG/WP 98-20132
The in-ground resistance of materials to attack by subterranean termites is most commonly assessed with one form or another of the conventional graveyard method, despite the significant shortcomings of this method. In Australia, an alternative method, in which all samples of test materials are placed below-ground, has been in use for more than 10 years. The method provides reliable exposure of sam...
M Lenz, A F Preston, J W Creffield, K J Archer, B M Kard, C Vongkaluang, Y Sornnuwat


Which fungi should be included in the laboratory evaluation of anti-stain chemicals?
2001 - IRG/WP 01-20236
Test fungi for efficacy tests of anti-stain formulations were selected based on the assumptions that test fungi should be fungicide-tolerant antagonists and fungi resistant to both fungicides and fungicide- tolerant antagonists, and such fungi should be re-isolated from treated samples with the highest fungicidal concentration used for laboratory evaluation of fungicides. This paper discusses the ...
Hyung-Jun Kim, Jae-Jin Kim, Gyu-Hyeok Kim


Screening results of fungicides for sapstain control on Pinus radiata
1983 - IRG/WP 3236
Thirty-two compounds were tested to determine their ability to contain the growth of stain, mould and rot organisms on fresh Pinus radiata D Don. A screening technique was employed using 35 to 50 mm diameter biscuits of Pinus radiata stemwood 10 mm thick. No compound was found to be cost effective when compared against the standard treatments of NaPCP (0.5% a.i.) plus borax (1.5%) and Captafol (0....
P J Hayward, J Duff, W Rae


Risk assessment of energetic valorization of treated wood - wooden recycling
1996 - IRG/WP 96-50072
The most useful method for the valorization of wood wastes and wooden wastes is energetic valorization. In France the percentage of wood treated by antisaptain products is around 30%. Currently with the growing regulation, there is a need for cleaner methods and technology to allow sustainable valorization. The preservatives concerned are common organochlorine compounds (NaPCP) less used nowadays ...
G Deroubaix, P Marchal, G Labat


A field test with anti-sapstain chemicals on sawn pine timber stored and seasoned under different conditions
1984 - IRG/WP 3245
Newly sawn timber of European redwood (Pinus sylvestris L.) was dip treated in four different anti-sapstain chemicals. The protectife effect against sapstain, mould and decay was examined after 10 weeks' and 10 months' storage in open and closed stacks. The results showed that the performance of individual chemicals was different in open and close stacks, although the wood as wel...
D J Dickinson, B Henningsson


Laboratory evaluation of potential antisapstain treatments for Pinus radiata
1983 - IRG/WP 3237
Twelve formulations were tested in the laboratory using a 'mini' board test for effectiveness on Pinus radiata (D. Don) against sapstain, mould and decay fungi. Three formulations, sodium pentachlorophenoxide (NaPCP) plus borax, Haipen 50 WP, and Mitrol 375, are used commercially in New Zealand. Busan 1009 (0.5% product), IWD Product A (0.2% ai), IWD Product B (0.3% ai), Fennotox...
J A Drysdale


Laboratory and field evaluations of a novel formulation, BAM as an anti-sapstain agent
1991 - IRG/WP 3639
A novel anti-sapstain formulation, BAM, consisting of 2-(thiocyanomethylthio) benzothiazole (TCMTB) and methylene bis thiocyanate (MBT) was evaluated for ist anti-sapstain performance in the laboratory and in the field as well. BAM proved effective in controlling the growth of molds and a sapstaining fungus in the standardized Japan Wood Preserving Association (JWPA) tests. All the test fungi coul...
Y Nomura


The degradation of wood by metal fastenings and fittings
1972 - IRG/WP 302
As well as the hazards of biological decay, timber used in boat building is subject to the effects of chemical decay associated with the corrosion of metallic fastenings. The title has been deliberately chosen to emphasize that in wooden construction the troubles are not just those of corrosion of the fastenings, but also the destructive secondary effects on the wood caused by the products of the ...
L C Pinion


Mixtures of fungicides screened for the control of sapstain on Pinus radiata
1984 - IRG/WP 3307
Fourty nine mixtures of fungicides were evaluated in a rapid laboratory screen for the control of stain, mould and decay fungi on Pinus radiata (D.Don). The most effective mixture was thiophanate methyl plus chlorothalonil closely followed by the mixtures of thiophanate methyl plus benzisothiazolone and thiophanate methyl plus dithio-bis (benzmethylamide). Benzalkonium chloride, thiram and ziram, ...
P J Hayward, W Rae, J Duff


Oxine copper (NYTEK® GD) for the control of mould and sapstain on lumber in North America
1989 - IRG/WP 3517
NYTEK® GD is a new, water-based, micro-dispersible formulation of oxine copper registered in the United States and Canada for control of mold and sapstain-causing fungi. NYTEK GD is noncorrosive and of low hazard to applicators and people handling treated lumber, when used according to the label. The product is an effective wood protectant applied as a dip or spray treatment at concentrations of ...
D F Myers, J M Fyler, C H Palmer, G D Rosebery


Field trials of Sinesto B at some sawmills in Portugal
1989 - IRG/WP 3512
The efficacy of SINESTO B as antistain chemical for use in Portugal has been studied. The studies were done during the years 1987-1988 at several Portuguese sawmills in co-operation with the Instituto dos Produtos Florestais and the APCIM (Associacao Portuguesa de Comercio e Industria de Madeiras). SINESTO B was used in 5% and 8% concentrations. The storage time varied from 10 weeks to 6 months. I...
I A Linderborg


Anti-feedant activity of stilbenic components from bark of Picea glehnii against a subterranean termite, Reticulitermes speratus
2002 - IRG/WP 02-10447
Stilbenic components, one of polyphenolic groups, widely distributed in plant bodies have been known as anti-microbial agents, but not known whether to have anti-termite activities. A stilbene glucoside, isorhapontin, from the bark of Picea glehnii was examined on the anti-feedant activity against a subterranean Reticulitermes speratus. Isorhapontigenin, the aglycone of isorhapontin, induced from ...
S Shibutani, M Samejima, S Doi


Evaluation of a new anti-sapstain formulation
1994 - IRG/WP 94-30035
A new anti-sapstain mixture, which consists of 2% IPBC (3-iodo-2-propynylbutyl carbamate) and 1.5% DCOI (4,5-dichloro-2-n-octylisothiazolin-3-one), was evaluated by three methods in the laboratory. A standardized test (JWPA standard 2) demonstrated that the new anti-sapstain formulation was highly effective in controlling growth of monocultures of five test fungi on wood substrate. When exposed to...
K Tsunoda, H Kumagai, M Sakurai


A shower test protocol for measuring antisapstain wash-off from small individual log billets
1996 - IRG/WP 96-50069
According to New Zealand Timber Industry Federation statistics New Zealand exported 4,835,000 m³ of logs in 1994 and it is estimated that c. 20% were anti-sapstain treated. Loss of preservative from logs as a result of rain impact after application is of considerable concern both with respect to potential loss of efficacy and environmental contamination. Whilst Environment Canada have a proposed ...
A J Pendlebury, H Pearson


Comparison between two laboratory test methods for determining the effectiveness on wood preservatives against blue stain in fresh wood
1987 - IRG/WP 2289
Most of the work done on determination of the effectiveness of new formulae for treating fresh wood against blue stain have been focussed on their use in the manufacture of saw timber. This work explains two laboratory methods, one which simulates the working and climatological conditions of factories making packages for fruit and vegetables in the Spanish Levante, showing that contamination of wo...
A M Navarrete, M T De Troya


The use of preservative containing waste wood as substrate for growing greenhouse crops
1993 - IRG/WP 93-50011
In the Netherlands a large amount of waste wood and wood waste is produced every year. An important part of this amount comes from the pallet and packaging industries. One of the possibilities to re-use this relatively clean material is to convert it into substrates for growing crops in glass houses instead of the commonly used materials such as rock wool and glass wool. In this research, the infl...