Questionnaire on alternative prophylactic chemicals
1982 - IRG/WP 3189
IRG Secretariat


An evaluation of anti-apstain chemicals in Queensland, Australia
1986 - IRG/WP 3374
Five formulations were evaluated for potential use as antisapstain chemicals. Tolcide FSM (0.01, 0.02, 0.04%), Koppers N.P.-1 (0.70, 0.35, 0.25%), Kathon WT (0.10, 0.25, 0.40%) and Sinesto B (2.5, 5.0 and 7.5%) offer potential as antisapstain treatments. An incorrect stock of Busan 1009 was used resulting in unacceptable results....
L E Leightley


Seasonal effects of the field evaluation on wood preservatives against mold fungi
1996 - IRG/WP 96-20087
For the purpose of the amelioration of field test methods, commercial preservatives against mold fungi were tested under two different seasons, in winter and in summer. The specimens were bundled and set over the water bath and all these systems were covered with plastic film. At top of the system under film, black films for regeneration of sunlight were put in, and windows for changing air were r...
K Suzuki, Y Sugai, K Ryugo, D Watanabe


A field test with anti-sapstain chemicals on sawn pine timber in Finland
1986 - IRG/WP 3368
Fourteen formulations, each in two concentrations, were tested for effectiveness against sapstain, mould and decay on Scots pine (Pinus sylvestris L.) in a field test in South-Finland. The trial was commenced in June 1985 and finished in October 1985. During the test the boards were infected mainly by mould fungi. In kiln dried boards the protective effects of nine and in green boards of four trea...
L Paajanen


The use of chlorothalonil for protection against mold and sapstain fungi. Part 1: Laboratory evaluation
1989 - IRG/WP 3515
Laboratory screening of chlorothalonil alone and in combination with other fungicides was conducted against six mold and sapstain fungi. The most promising treatments appear to be chlorothalonil supplemented with CCA or copper-8-quinolinolate. Field tests have been implemented....
J A Micales, T L Highley, A L Richter


The preliminary evaluation of selected sulfonium salts for use in wood preservation
1984 - IRG/WP 3278
Five sulfonium compounds, including two sulfonium methosulfates, one sulfonium bromide and two amphoteric sulfonium propanesulfonates, were prepared in crude form and subjected to various biocidal screening tests. A rapid screening test in which treated Pinus radiata pulp pellets were exposed to one of three wood-decaying fungi growing on malt agar revealed that dodecyl dimethyl sulfonium methosul...
D V Plackett


Thermotolerant mould growth in dehumidifier kilns in New Zealand
1996 - IRG/WP 96-10169
Growth of Aspergillus fumigatus and Paecilomyces variottii is common on wood dried in dehumidifier kilns that operate within a temperature range of 35-55°C. Aspergillus fumigatus causes an unacceptable blue / grey discolouration of the woods surface and prolonged exposure to spores during handling of mouldy wood can cause health problems amongst timber workers. A survey of dehumidifier kiln opera...
R N Wakeling, J G Van der Waals


Some tests on ES - AS 11, a novel anti-sapstain formulation, and its properties
1987 - IRG/WP 3399
The results of some tests with the formulation ES - AS 11 are given. The formulation is an attempt to improve the performance of an anti-sapstain chemical by: 1) increasing its penetrability 2) uniquely combining its active ingredients. Very short times of treatment (dipping not longer than 5 seconds), low concentrations of active ingredients, and lower toxicological and environmental risks may be...
U Straetmans


Production of preservative-treated wood in some countries
1990 - IRG/WP 3598
This report presents figures of the production of preservative-treated wood and wood treated with anti-stain chemicals in 26 and 20 countries respectively from all over the world....
J Jermer


Field and laboratory studies on anti-sapstain preservatives
1982 - IRG/WP 3205
The field tests included 11 different anti-sapstain preservatives and were carried out at different sawmills in southern Sweden. Drying conditions, climate and the local fungus flora were not identical for the different preservatives and comparisons between the preservatives should therefore be made with caution. Results obtained in the field tests are, however, in relatively good agreement with t...
M-L Edlund, B Henningsson


Wood preservation in Kenya
2000 - IRG/WP 00-40191
Current research on wood preservation in Kenya is mainly on the development of biological control of wood-destroying termite species, using mycoinsecticides. The major research institutions include the Kenya Agricultural Research Institute (KARI), Kenya Forestry Research Institute (KEFRI), Moi University and the International Centre for Insect Physiology (ICIPE). Training institutions include Fore...
G Ochiel


Programme Section 3 Wood protecting chemicals
1999 - IRG/WP 99-30210
IRG Secretariat


Preliminary note on the fungal problem of rubber wood
1983 - IRG/WP 3246
Susceptibility of rubber wood to fungal attack limits its wider utilisation. Fungal problems encountered in treating rubber wood with boron compounds by diffusion process have been discussed. Sodium pentachlorophenoxide and 2-thiocyanomethylthio benzothioazole (TCMTB) were investigated for possible control of fungal growth during diffusion storage and their performance has been reported....
R Gnanaharan


Monographic information on Serpula incrassata (Berk. and Curt.) Donk
1980 - IRG/WP 1128
J G Palmer, W E Eslyn


Monographic information on Lentinus lepideus.markup
1973 - IRG/WP 115
W Liese, G Seehann


First draft of a monographic card for Gloeophyllum abietinum (Bull. ex Fr.) Karst
1973 - IRG/WP 116
T Hof


Protection of beech veneer for fruit and vegetable boxes
1981 - IRG/WP 3176
In Yugoslavia about 50,000 m³ of low quality beech logs annually are rotary cut into veneer from which boxes are made for transporting fruit and vegetables. Because of steaming before rotary cutting, beech veneer becomes extremely sensitive to mould attack which decreases the quality and commercial value of the final product. To avoid mould attack, veneer sheets are dried to 16% moisture content ...
N Vidovic


Generic code of good practices for wood protection facilities. Part 1: Wood protection (antisapstain) facilities
1993 - IRG/WP 93-50003
In general, the potential of high toxicity (aquatic and human) of wood protection (antisapstain) chemicals dictates the need to protect the environment and humans from its harmful effects. This document is a compendium of recommendations for the design and operating practices of wood protection facilities. The suggested recommendations focus on achieving the objectives of protecting the environmen...
G Das, V N P Mathur


A summary of work carried out to compare natural and artificial weathering for preconditioning test specimens in testing anti-stain chemicals for wood in service
1976 - IRG/WP 266
Since 1972 work has been in progress within CEN to establish a European standard for the testing of wood preservatives designed to prevent blue-staining of wood in service. The method is based on the Butin test and involves pre-weathering of the samples prior to biological testing. The weathering regime employed is 6 months outside exposure from March to October. This imposes severe limitations on...
D J Dickinson, A F Bravery


A potential anti-sapstain chemical for sawmills
1984 - IRG/WP 3300
Several biocidal formulations were tested under laboratory conditions in order to discover an alternative antisapstain chemical to chlorophenoxides. The formulations tested were experimental water solutions containing a quaternary ammonium chloride, a commercial fungicide and/or a sodium salt of some carboxylic acids. The effect of sodium carbonate and borax decahydrate in mixture with a quaternar...
I A Linderborg


Long-term protection of stored lumber against mould, stain, and specifically decay: A comparative field test of fungicidal formulations
1984 - IRG/WP 3281
The problem of decay in packaged, unseasoned lumber stored for many months has become of major importance in recent years. Large financial claims have resulted from decay in Canadian lumber stored at length in seaports and storage yards of distributors. For decades acceptable protection from moulds and sapstain was readily achieved with chlorinated phenols applied at appropriate treating levels. H...
A J Cserjesi, A Byrne, E L Johnson


Evaluation of an alkyl ammonium compound as a fungicide to control sapstain and mould during diffusion storage
1984 - IRG/WP 3282
An alkyl ammonium compound ('Akzo' ES 255) was evaluated for its effectiveness against mould and sapstain during diffusion storage of boron-treated rubber wood. Though ES 255 at 1.0% concentration was effective against mould (71%) and sapstain (89%) it is less satisfactory compared to 0.5% sodium pentachlorophenoxide against mould (92%) and sapstain (98%)....
R Gnanaharan


Tebuconazole - a new triazole fungicide for wood preservation
1991 - IRG/WP 3680
The great potential of Tebuconazole for wood preservation is demonstrated. Test carried out by official institutes shown that Tebuconazole is particularly effective against wood-rotting basidiomycetes strains. The efficacy of Tebuconazole against the brown rot Gloeophyllum trabeum is outstanding: the toxic value measured in accordane with EN 113, without·ageing, after leaching (EN 84) and after e...
O Exner


Efficacy of linear chain carboxylic acid anhydrides as wood protection chemicals
2002 - IRG/WP 02-30295
This paper presents an assessment of the effectiveness of linear chain carboxylic acid anhydrides namely, acetic, propionic, butyric, valeric and hexanoic anhydride, in improving the decay resistance of Corsican pine (Pinus nigra Schneid) sapwood. Wood-anhydride bond formation was verified by the increase in sample weight and volume. A brown rot fungus [Coniophora puteana (Schum.:Fr)] was selec...
A N Papadopoulos, M D C Hale, C A S Hill


Agenda Special Seminar: Screening techniques for potential wood preservative chemicals
1978 - IRG/WP 2115
IRG Secretariat