Proposed standard laboratory method for testing fungicides for controlling sapstain and mould on unseasoned lumber
1977 - IRG/WP 292
This laboratory method is for determining the effective concentration, or concentration for zero growth (CGo), for fungicides or preparations of fungicides which are potentially useful in protecting packaged or unseasoned lumber in storage and shipment from biodeterioration by sapstain fungi and moulds. The test is rapid and may be completed in three weeks and gives a good indication of the toxici...
A J Cserjesi


Conforming to european standards for preservative-treated timber: Specifying with confidence
2000 - IRG/WP 00-20194
A four-year collaborative study between four industrial partners and BRE has assessed timber treated by current UK industrial practices in the light of current European Standards. Data were collected for CCA and creosote treated timber components, and compared with the requirements laid out in EN351-1 and -2. A number of difficulties were encountered that have been described in previous IRG papers...
E D Suttie, R J Orsler


Local preservation with difluoride pills: Life-time of preservative
1998 - IRG/WP 98-40127
A brief history of the situation in the Netherlands with respect to the preservation of joinery is given. Already in the eighties in the Netherlands many spruce window frames were treated with difluoride pills. One of the possible disadvantages of this kind of diffusing preservatives is the high leaching rate found in laboratory situations. The leaching rate in practice is influenced by many facto...
W J Homan, C Blom, B W Holleboom


Mould resistance of lignocellulosic material treated with some protective chemicals
1984 - IRG/WP 3294
Effectiveness of preserving lignocellulosic material against moulding by treatement with water solutions of commercial wood preservatives and mixtures of various inorganic salts was investigated and compared with the effectivenes of sodium pentachlorophenoxide and boric acid....
K Lutomski


IRG test of preservative-treated hardwoods with particular reference to soft rot. Report on condition of specimens installed in Victoria, Australia
1982 - IRG/WP 3207
J Beesley


Field trials of anti-sapstain products. Part 1
1991 - IRG/WP 3675
The results obtained in two field tests of anti-sapatain products, carried out in four locations in Portugal, are presented. Boards from freshly cut logs were hand-dipped, close staked and left to dry for periods from four to six months. The results obtained seem to indicate that some of the products tested performed at least as well and sometimes better, than a 3% NaPCP solution which was used as...
L Nunes, F Peixoto, M M Pedroso, J A Santos


Inventory of the use of preservative-treated wood and wood preservatives in Sweden 1900-1997
1999 - IRG/WP 99-50137
The objective of this study was to present an overview of the use of wood preservatives and their active ingredients and industrially preservative-treated wood in Sweden since the beginning of the 20th century. The data presented in the report could for example be used as a basis for different waste management scenarios for preservative-treated wood. Before 1960 railway sleepers and utility poles ...
J Jermer, K Nilsson


Preservative treatment of Eucalyptus saligna fence posts by the double-diffusion method
1982 - IRG/WP 3196
Eucalyptus saligna fence posts treated by the double-diffusion method with two chemical combinations showed average lives of 11.2 years (copper sulphate and potassium dichromate at 10.5 kg/m³ retention)and of 14.3 years (copper sulphate and sodium mono-H arsenate at 7.1 kg/m³ retention), as determined in five test sites in the State of Sao Paulo, Brazil. The exponential model was the best fit wh...
E S Lepage, A R De Freitas


Selective adsorption of antisapstain actives from two aqueous suspensions, and movement of actives into wood
1996 - IRG/WP 96-30103
Green-off-saw rough sawn Pinus elliottii (slash pine) boards were dipped in aqueous suspensions of two antisapstain formulations, NeXgenâ and Busanâ Sap Stain Preventative (Busan 1009), at three product concentration levels. Concentrations of active ingredients (NeXgen: CTL (chloro-thalonil) and MTC (methylene bisthiocyanate); Busan 1009: TCMTB (2(thiocyanomethylthio)-benzothiazole) and MTC) wer...
M J Kennedy, T L Woods


Rates of emission from CCA-treated wood in the marine environment: measurement, modelling and requirements for further research
2001 - IRG/WP 01-50166-12
Accurate estimates of rates of emission of leachate from preservative treated wood are crucial for realistic predictions of the environmental impact of its use in maritime construction. Estimates are available for some commonly used preservatives, but these vary widely. Though variable, these measurements suggest that emission generally decreases exponentially with time. Part of the variation is d...
S M Cragg, C J Brown, R A Albuquerque, R A Eaton


Point sur la réglementation et contraintes administratives
1990 - IRG/WP 3575
J H Moneger


Evaluation of the effectiveness of three microbiocides in the control of sapstains
1982 - IRG/WP 3212
Results of field test on the effectiveness of BUSAN 30, CAPTAN, FOLPET against mould and sapstain in Pinus elliottii are presented. The viability of use of FOLPET in Brazil as an alternative to sodium pentachlorophenate is also discussed....
S Milano, J A A Vianna Neto


Collaborative soft rot tests: Interim report on PRL tests of Cu/Cr/As preservative using method of Document No: IRG/WP/208
1972 - IRG/WP 211
Preservative: Tanalith CT.106 - Results obtained with beech are given in the table and indicate a toxic limit of 16.7-19.2 kg/m³ - The initial soil moisture content was adjusted to 27.8% (the water holding capacity). Noticeable drying out has occurred in some of the test bottles....
J G Savory


Factors affecting leaching of preservatives in practice
1978 - IRG/WP 3113
At the 7th Meeting of the IRG in Poland in May 1975, the findings of collaborative laboratory leaching techniques were discussed, and the dangers inherent in using such results to predict the behaviour of preservative-treated components in service were emphasised. In order to improve our understanding of the factors governing leaching of preservatives in practice, and to identify areas where furth...
R Cockcroft, R A Laidlaw


Efficacy of anhydrides as wood protection chemicals - II. Performance against soft rot fungi
1998 - IRG/WP 98-30174
Pine sapwood modified with various anhydrides and with butyl isocyanate was tested for its resistance to soft rot decay. Small stakes were exposed for 20 months in unsterile soil in a fungal cellar test. Wood modified with butyl isocyanate performed better than any of the anhydrides tested, with a threshold level of protection (less than 3% weight loss) at 12% weight percent gain (WPG). Stakes ac...
S C Forster, M D C Hale, G R Williams


The identification and preservative tolerance of species aggregates of Trichoderma isolated from freshly felled timber
1992 - IRG/WP 92-1553
The surface disfigurement of antisapstain treated timber by preservative-tolerant fungi remains a major problem in stored timber. Identification of a range of isolates of Trichoderma based on microscopic morphological characteristics was found to be imprecise due to the variable nature of this organism. In addition, studies to compare visual (morphological) characteristics of these isolates with t...
R J Wallace, R A Eaton, M A Carter, G R Williams


New technique for inoculation of wood wafers with fungi
1997 - IRG/WP 97-20113
A pilot study is described for determining the best possible method for inoculating fungi onto the surface of wood wafers for sapstain control studies. Direct inoculation and spray inoculation are compared on water soaked and malt extract broth soaked wood wafers. The best growth of fungal hyphae across the surface of the wood wafers was achieved following spray inoculation onto malt extract broth...
J Snow, P Vinden


Light organic solvent preservative treatment of glue-laminated radiata pine
1986 - IRG/WP 3380
The high permeability of radiata pine (Pinus radiata D. Don) is associated with ray-tissue and in particular the cross-field pits linking ray-tissue to tracheids. This pathway is absent in the tangential grain direction, leading to poor preservative penetration when treatment is restricted to the radial face - for example, timber fabricated into glue-laminated beams....
P Vinden


A new ground-contact wide-spectrum organic wood preservative: DNBP
1986 - IRG/WP 3358
A new organic wood preservative, which 25 years field tests have proved to be of efficiency and effectiveness comparable to CCA wood preservatives for ground-contact applications, is presented. Physical and chemical tests, supporting the long term field test results as well as indicating the characteristics of this preservative, are also presented....
W E Conradie, A Pizzi


Soft rot and bacterial decay in preservative treated eucalypt power transmission poles
1982 - IRG/WP 1155
Bacterial type decay was observed in CCA and PCP treated eucalypt power transmission poles. Detailed observations made with the SEM revealed bacterial colonisation and decay, especially in fibres. Plug samples taken from poles throughout Queensland were examined for preservative retention and presence of soft-rot decay. The severity of decay was different according to location, retention and speci...
L E Leightley


Some observations on causes of failure of preservative treated natural round transmission poles in Nigeria
1977 - IRG/WP 291
Treated natural round transmission poles in Nigeria have been discovered to be attacked underground as early as two years after planting. Termites and rot fungi attack the inner tissues and leave a pattern characteristic for the species of the pole. Tectona grandis, Nauclea diderrichii and Wide Pore pine, the major species for transmission poles in Nigeria show these attacks. A form of termite shi...
M A Odeyinde


The effectiveness test of chemicals against Serpula lacrymans
1984 - IRG/WP 2222
The effectiveness tests of wood preservatives against Serpula lacrymans were conducted in accordance with Japan Industrial Standard A 9302 and Japanese Wood Preserving Association Standard No. 1. Also, the soil treatment test against this fungus was carried out with two chemicals. The preservatives tested without Creosote oil (out of JIS) had sufficient preservative effect against Serpula lacryman...
S Doi


Laboratory investigations about the mobility of some inorganic wood preservatives in soils
1998 - IRG/WP 98-50101-22
Wood preservatives and components of wood preservatives leached from impregnated wood can enter the soil and thus contribute to the pollution of the groundwater. However, there is lack of understanding concerning the interacting parameters of wood preservative, leachate, soil and soil solution. To characterise of the behaviour of active ingredients and for the assessment of their environmental imp...
E Melcher, R-D Peek


Fire resistance of Alder wood treated with some chemicals. Part II. Effect of Other Chemicals on the Combustion Properties
2002 - IRG/WP 02-40235
Samples from alder wood (Alnus glutinosa (L.) Gaertn. subsp. barbata (C.A.Mey) Yalt.) were impregnated according to ASTM D 1413-88 with boron compounds (boric acid, borax, sodium perborate), vinyl monomers (styrene, methyl methacrylate), Tanalith-CBC, Phosphoric acid, Vacsol, Immersol, Polyethylene glycole (PEG-400) and their mixed solutions of chemicals in order to determine their combustion pro...
A Temiz, Ü C Yildiz


Leaching of Active Components from Preservative Treated Timber. Stage 1: Semi-Field Testing
2004 - IRG/WP 04-20302
The project is aiming at finding realistic leaching rates from preservative-treated wood in use class 3 (above ground). The project focuses on developing a field trial method for investigating leaching. Panels are subjected to outdoor exposure under natural weather conditions at a test field at the Danish Technological Institute. The leachate is collected and monitored by chemical analysis of the...
N Morsing, B Lindegaard