IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 735 documents. Displaying 25 entries per page.


The use of pyrethroids against Limnoria spp
1981 - IRG/WP 473
Synthetic pyrethroid insecticides discovered in the last fifteen years have been developed as crop sprays and used in aerosol formulations for the control of household pests. High toxicity to a wide range of arthropod pests, combined with reasonably low mammalian toxicity, confers an advantage over many other control agents. Some of the more recent pyrethroids are photostable and display residual ...
D Rutherford, R C Reay, M G Ford


N-tritylmorpholine as a potential marine wood protectant against teredinids and pholads - A preliminary evaluation
1983 - IRG/WP 497
The molluscicide, N-tritylmorpholine, is effective in eradicating certain fresh water snails, the intermediate hosts in the transmission of schistosomiasis in man. This preliminary study shows that N-tritylmorpholine is also active against wood-boring marine mollusks. Fine sapwood impregnated with this morpholino compound was not damaged by teredinids or pholads while exposed at two marine sites i...
J D Bultman, K K Parrish


An interim report on trials with 'Boliden K33' and 'Celcure A' in water of different salinities in the Baltic Sea and in the UK
1974 - IRG/WP 406
It was felt necessary to undertake field trials using large test samples exposed in natural water of different salinity in order to determine preservative leaching and to assess the degree of biological attack....
R A Eaton, D J Dickinson


Rapport sur l'activité du CEN/TC 38 "Méthodes d'essais des produits de préservation du bois"
1982 - IRG/WP 2188
M Pottevin


Leaching of CCA from Pinus patula during marine trials in the southern hemisphere
1991 - IRG/WP 4167
Pinus patula stakes were treated with CCA to retentions of 31 kg/m³ salts, and were sited in the sea of Port Alfred, South Africa, for two years. Samples were then removed to the laboratory and analysed as before for copper and arsenic. Prelimiary data showing CAA losses from these stakes in the marine environment showed that CCA was longitudinally leached from them, and was also transversly redi...
G D Shelver, C D McQuaid, A W W Baecker


Initial microbial colonisation of CCA-treated, creosote-treated and untreated Pinus sylvestris L. blocks in seawater
1996 - IRG/WP 96-10171
CCA-treated, creosote-treated and untreated Pinus sylvestris sample blocks were immersed in a seawater through-flow system for periods of between 1 and 265 hours. Samples were fixed immediately on removal and examined both qualitatively and quantitatively using the scanning electron microscope. This study of primary microbial colonisation showed differences between treatments in the diversity of m...
K Sturgess, A J Pitman


Test of N-tritylmorpholine in combination with synthetic pyrethroids against marine borers in tropical Australia and Panama
1991 - IRG/WP 4168
Test blocks ol Pinus sylvestris sapwood were pressure impregnated with white spirit solutions of N-tritylmorpholine, either alone or in combination with permethrin, deltamethrin or cypermethrin. They were exposed in the intertidal zone at Mourilyan Harbour, North Queensland, Australia and subtidally at either end of the Panama Canal. After 5 months' exposure at Naos Island at the Pacific ...
S M Cragg, J D Bultman


Description of a trial with wood preservatives against marine wood boring organisms
1975 - IRG/WP 412
Wood situated in sea water along the Atlantic coasts of the Nordic countries is attacked by marine wood boring organisms. Timber constructions in these waters therefore must be preservative treated. In order to evaluate the effect of various preservatives against marine wood borers, the Nordic Wood Preservation Council (NWPC) organized a rather extensive trial in 1972. In the absence of and while ...
E Norman, B Henningsson


Marine trials with ammoniacal wood preservatives
1980 - IRG/WP 423
Ammoniacal wood preservatives have been known for many years and are considered among the best water-borne systems for protecting wood in ground contact. In recent years attention has been increasingly focussed on these preservatives because of their ability to penetrate difficult-to-treat species better than most other fixed water-borne preservatives. This is particularly important for example, i...
M A Hulme, D P Ostaff


A marine borer test with water-borne preservatives
1980 - IRG/WP 452
The use of preservative treated timber in sea-water where marine borers are active is of great economic importance, since untreated wood immediately will be damaged. Vacuum/pressure treated timber has been tested in several marine exposure trials on the Swedish west coast since the 1930s (Hager 1941, Hultman 1949, Sandstrom 1951, Nylinder-Norman et al. 1974). Since new interesting materials or pre...
B Henningsson, E Norman


Marine trial progress report
1980 - IRG/WP 453
In May 1977 and May 1978, tests of new chemical formulations for the protection of timber in the sea were installed in Mt. Maunganui Harbour. Investigation into new preservatives for such usage was urgently required since it had been found that there was progressive leaching of copper from copper-chrome-arsenate treated marine piles which could lead to a reduction in their service life. Hochmann (...
A F Preston, C M Chittenden


Natural resistance of timbers to marine borer attack. A laboratory test with Limnoria tripunctata
1977 - IRG/WP 430
Attack of the timber specimens was much less severe in the laboratory than in some marine localities. This is not surprising. One reason is certainly that wood-boring molluscs (Teredinidae and Pholodidae) which were missing in the laboratory are the most important wood-destroying organisms in the open sea. Another reason is that it is not possible to offer the gribbles optimal environmental condit...
H Kühne


Natural durability of fifty species of Indian timber in Goa waters against marine wood-borers
1989 - IRG/WP 4150
Results of the investigations on the natural durabilitv of fifty species of Indian timber, based on data collected bv exposing test panels at Betim near Panaji (Goa) continuously for a period of 11 months are presented. The study revealed that none of the timber species tested has any natural resistance at this locality and all the panels were completely destroyed within 11 months. Details on the ...
L N Santhakumaran, S Udaya Bhaskar, J C Jain


Microbial fouling of 10-40% naphthalene in creosote treated and untreated wooden pilings in the marine environment - A progress report
1980 - IRG/WP 455
In June 1978, Document No: IRG/WP/442 entitled 'Microbial Biofouling of 10-40% Naphthalene in Creosote Treated and Untreated Wooden Pilings in the Marine Environment" was released to the IRG members as a report on the early results of a long term (about 5 years) study of whether the naphthalene content of creosote was importart in protecting wood pilings in the marine environment from bor...
R R Colwell, A J Emery


Performance of preservative-treated timber against biodeterioration in Indian waters
1984 - IRG/WP 4106
Results on the investigation on the durability of panels of 32 timber species, pressure-treated with various preservatives and exposed along the Indian coast for varying periods upto a maximum of 15 years, are summarised. Panels of even non-durable timber gave excellent results against biodeterioration after treatment. Their life was comparable to that of treated durable timber. The preservative t...
L N Santhakumaran, J C Jain, M C Tewari


Marine trials with water-borne salts and organotin compound
1986 - IRG/WP 4128
Pinus sylvestris blocks treated with water-borne salts (CCA, CCB, CCF) and organotin compounds (TBTO, TBTCl) were submerged in the sea at Follonica station. The results obtained after 12 years of immersion are presented. The samples treated with CCA, CCB and CCF at the lowest concentration (2%) were destroyed after 7-9 years and the samples treated with CCB and CCF at the highest concentrations (4...
A Gambetta, E Orlandi


Surface accumulation of copper on CCA-impregnated Pinus patula stakes during marine preservative trials in the southern hemisphere
1992 - IRG/WP 92-4181
Pinus patula stakes treated with CCA to target retentions of 30 kg/m³ salts were exposed to sea water in marine and estuarine ecosystems off the coast of Southern Africa for two years. Samples were then analysed for copper and arsenic. Analysis of samples from the marine ecosystem showed (IRG/WP/4167) that arsenic was longitudinally and transversely leached from the wood, whereas the copper was r...
G D Shelver, C D McQuaid, M Tarin, A A W Baecker


Screening techniques for potential wood preservative chemicals. Proceedings of a special seminar held in association with the 10th Annual Meeting of the IRG, Peebles 1978. Report No 136, 1979
1980 - IRG/WP 2138
This paper continues following issues: I. SCREENING INSECTICIDES 1) R W Berry (BRE/PRL, UK): Screen testing of insecticides for use in remedial wood preservatives. 2) D J Cross (FRI, New Zealand): Rapid screening of contact insecticides for use on forest products. 3) C R Coggins; A Forsyth; A E Glaser (Rentokil, UK): Experience in the use of indicative screening techniques for termiticides. ...
Anonymous


Ability of chloropicrin, Vorlex, or methylisothiocyante to prevent marine borer attack of Douglas fir piling
1989 - IRG/WP 4153
The preservative-treated shell around Douglas-fir piling is an excellent barrier to attack by marine borers; however, damage to this shell can permit marine borer attack. The feasibility of using fumigants to enhance piling performance was examined by exposing fumigant-treated Douglas-fir sections in marine waters off Newport, OR, or Port Hueneme, CA. The piling were inspected annually and increme...
M A Newbill, J J Morrell


Relative tolerance of CCA by larvae and adults of the common shipworm, Bankia gouldi
1992 - IRG/WP 92-4174
Southern pine sapwood "2 x 4´s" were created by bolting together four panels 13 mm thick by 89 mm wide by 457 mm long. The two outer laminates were untreated and the two inner laminates were each treated to different CCA retentions, ranging from 8.0 to 43.2 kg/m³. Test specimens were exposed from May to October in a tributary of the Chesapeake Bay. Larvae were unable to settle on and burrow into...
B R Johnson


Lab and field test results for wood treated with polymeric alkylphenol polysulfide
2001 - IRG/WP 01-30268
A new wood preservative based on polymeric alkyphenol polysulfide (PXTS-A) is being evaluated in a series of laboratory and field tests and the results continue to show promise. A modified formulation (PXTS-B), which contains additives to reduce the viscosity, is being evaluated along with the original formulation. Soil block decay tests comparing PXTS-B with CCA-C indicate that PXTS-B is equally ...
J Goswami, A Abramson, R Buff, D D Nicholas, T Schultz


Occurrence of wood-boring pholads in Kochi harbour waters (south-west coast of India)
1992 - IRG/WP 92-4175
The paper reports the occurrence of four species of wood-boring pholads (Pholadidae: Martesiinae), namely Martesia (Martesia) striata (Linnaeus), Martesia (Martesia) fragilis Verrill and Bush. Martesia (Particoma) nairi Turner and Santhakumaran and Lignopholas fluminalis (Blanford), in the Kochi back-waters, south-west coast of India. Of these Martesia nairi and Lignopholas fluminalis are now reco...
L N Santhakumaran, M V Rao


Wood decay of Pinus sylvestris L. and Fagus sylvatica L. by marine fungi. Part 2
1991 - IRG/WP 1471
The water-logged wood conservation requires a good knowledge of the wood decay organims which produce the degradation. Previous conducted studies (ESCORIAL, TROYA, GARCIA DE LOS RIOS, 1990) have shown that the incubation times normally used for in vitro laboratory tests are not sufficients for a significant wood degradation. This has been the reason why the aim of this work was the study of such d...
M T De Troya, A M Navarrete, M C Escorial


Leaching from CCA-treated wood submerged in seawater: Effect of high loadings, and a comparison between laboratory and marine conditions
1996 - IRG/WP 96-50080
This study of leaching examined the following variables: CCA loading; marine versus laboratory exposure and length of submergence. Blocks of Pinus sylvestris were treated to a range of nominal retentions from 15 to 50 kg/m³. Each block was then divided into three cubes and all transverse faces were sealed. All cubes were allowed to fix at ambient temperature for a minimum of one week. One set of ...
R M Albuquerque, S M Cragg, J D Icely


Special seminar on screening techniques for potential wood preservative chemicals
1978 - IRG/WP 2113
This paper continues following issues: I. SCREENING INSECTICIDES 1) R W Berry (BRE/PRL, UK): Screen testing of insecticides for use in remedial wood preservatives. 2) D J Cross (FRI, New Zealand): Rapid screening of contact insecticides for use on forest products. 3) C R Coggins; A Forsyth; A E Glaser (Rentokil, UK): Experience in the use of indicative screening techniques for termiticides. ...
Anonymous


Previous Page | Next Page