Reliability-based service life prediction methodology for assessment of water protection efficiency for coatings on wood
2003 - IRG/WP 03-20268
Assessment of water protection efficiency according to EN 927-5 has been shown to give significant differences in water absorption values for different types of coatings on wood. It is shown that the combination of EN 927-5 and an artificial weathering procedure gives more information regarding expected durability and long-term performance than a single measurement of water absorption on fresh, un...
J Ekstedt


Some biological observations on the management of preservativion experiments with submerged timber in the marine environment
1976 - IRG/WP 421 E
P Deschamps


Safety technique in wood preservation
1974 - IRG/WP 54
S N Gorshin, I G Krapivina, B I Telryatnikova


Trends in environmental management in industry. Implications for wood preservation activities
1993 - IRG/WP 93-50001-34
J A De Larderel


Cleaner prodiction and the wood preserving industry
1995 - IRG/WP 95-50040-29
H Carr-Harris, C R Coggins


Wood preservation in China
1989 - IRG/WP 3546
Huiming Zhou, Zhongwei Jin


Chlorodioxins in pentachlorophenol
1975 - IRG/WP 346 E
At the 6th meeting of the IRG/WP plenary group held on 20 June, 1974, in Vienna, Mr Richardson expressed some concern about dioxins which might be contained as impurities in pentachlorophenol and in sodium pentachlorophenoxide or which might be formed during the combustion of treated wood. He mentioned the malformations that have been noted in Vietnam due to the teratogenic action of the 2, 3, 7, ...
H Alliot


Marine borers as wood degraders in Bangladesh and their protection
1996 - IRG/WP 96-10186
Field study on timber piles used in Bangladeshi brackish waters revealed that untreated and pentachlorophenol treated piles drastically degraded by the attack of molluscs and pholads (marine borers). Adequately CCA-C impregnated (30 kg/m³ or 6% W/W dry oxide retention) timber piles can protect the attack of molluscs. It is very difficult to protect pholads which can invade naturally very durable ...
A K Lahiry


Migration of active ingredients from treated timber into fresh water
1991 - IRG/WP 3669
Spruce roundwoods and segments were treated with three different wood preservatives. Two of them containing copper and chromium the other one free of chromium. After fixation (3 weeks, 20°C) the specimens were leached by using artifical rain or by shaking the segments for one hour in contact with demineralized water. The water was analysed for the relevant elements of the preservative tested. Lea...
H Klipp, H Willeitner, K Brandt, A Müller-Grimm


Chlorodioxines dans le pentachlorophénol
1975 - IRG/WP 346
H Alliot


Investigation of the fixation in wood of chromated zinc chloride and copperised chromated zinc chloride preservatives
1976 - IRG/WP 372
A biological method of evaluating the extent to which CZC and CCZC preparations are retained in wood in terms of the potential protection which they afford against destruction by Merulius lacrymans (dry rot) is given. CCZC is recommended for protection of wood under moderate leaching conditions, while the use of CZC under such conditions is not recommended....
V N Sozonova, D A Belenkov


Production of preservative-treated wood in some countries
1990 - IRG/WP 3598
This report presents figures of the production of preservative-treated wood and wood treated with anti-stain chemicals in 26 and 20 countries respectively from all over the world....
J Jermer


Status of the Working Group on Preservation of Wood in the Marine Environment - Questionnaire results
1977 - IRG/WP 434
At the joint meeting of the IRG and COIPM dealing with preservation of wood in the marine environment, it was suggested that a Marine Group should be formally recognised within IRG. It was agreed that a questionnaire (Document No: IRG/WP/424) should be circulated to determine the views of the membership on the future status of this group. The results of this questionnaire are presented....
R A Eaton


Efficacy of some extractives from Pinus heartwood for protection of Pinus radiata sapwood against biodeterioration. Part 1: Fungal decay
1995 - IRG/WP 95-30072
Chemical compounds thought to contribute to the natural durability of heartwood of Pinus spp. were either chemically synthesised in the laboratory or extracted from the heartwood of Pinus elliottii or Pinus caribaea. These compounds included the stilbenes, pinosylvin and its mono- and di-methyl ethers, and the flavonoids, pinobanksin and pinocembrin. Small blocks of Pinus radiata sapwood were impr...
M J Kennedy, J A Drysdale, J Brown


An introduction to environmental aspects of groundwater arsenic and CCA treated wood poles in Bangladesh
1997 - IRG/WP 97-50081
The environment comprises biosphere, lithosphere, atmosphere and hydrosphere. Therefore, environmental science is a multi-disciplinary study, includes life sciences, physical sciences, chemical sciences, geology, geography, meteorology, forestry, agriculture, soil science, hydrology, ecology, public health, engineering etc. Tremendous industrial and mining activities, deforestation and population ...
A K Lahiry


Surface Barriers for Protection of Culture and Heritage Wooden Objects from Insect Attack
2004 - IRG/WP 04-40286
Anoxic treatment is an environment friendly procedure for eradication of wood boring insects in wooden objects of cultural and historical heritage. However, after the anoxic treatment, wooden antiques remain susceptible to further insect attacks. Possible protection against insects could be provided by the so-called post-repression protective barriers. Potential coating materials for such barriers...
M Petric, M Pavlic, B Kricej, M Humar, F Pohleven


Framework document for an international code of good practices for wood preservation and wood protection (anti-sapstain) facilities
1992 - IRG/WP 92-3683
At the Kyoto meeting, the Health & Safety committee agreed to form a task force to prepare a global plan for writing a code of good practices (Code) for wood protection and preservation facilities (Doc. No. IRG/WP/3681). The Canadian document had been presented to the IRG group earlier (Doc. No. IRG/WP/3447) and similar documents were solicited from other countries for preparing a framework do...
V N P Mathur, G Das


Copper based water-borne preservatives: The use of a thin section technique to compare the protection of wood by copper based preservatives against soft-rot and bacterial decay
1987 - IRG/WP 2286
This paper describes the techniques developed and gives examples of results obtained for the performance of copper based wood preservatives against both the bacterial and fungal hazards....
A M Wyles, D J Dickinson


Proposal for further work on environmental questions
1988 - IRG/WP 3494
Although very much is known about the environmental and health and safety aspects on various wood preservatives and treated wood knowledge is still lacking on some important issues. Some examples are: - The fate of wood preservatives in the environment, eg by leaching from treated wood and contaminated soil; - How big is the "problem" of pollution, etc from the wood preserving industry in comparis...
J Jermer, M-L Edlund


Wood preservation and the environment: A Canadian perspective
1990 - IRG/WP 3577
The non-pressure (surface) and pressure treatment of wood impacts on the environment in four ways. These are: through the production of treated wood at sawmills and pressure treating facilities; during the storage of treated wood prior to use; when the pressure treated wood is placed in service; and finally, when the treated product reaches the end of its useful life and must be disposed. By refer...
J N R Ruddick


Protection of Ochroma pyramidale from fungal decay with N,N-napthaloylhyroxylamine
1998 - IRG/WP 98-30182
Fungal decay of wood in service results in billions of dollars (U.S.) in losses annually. Recent environmental restrictions, both U.S. and international, are limiting and eliminating the use of broad-spectrum, heavy metal biocides for wood preservation. Restrictions result primarily from problems with disposal. New wood preservatives need to be developed and tested which specifically target key el...
F Green III, T L Highley


Safety clearance of wood preservatives in United Kingdom
1977 - IRG/WP 398
In the United Kingdom the principal route of control of pesticides is through the Pesticides Safety Precautions Scheme (PSPS) which is a non-statutory scheme agreed between government ministries and departments (referred to as "Departments") and associations representing the pesticide industries. The scheme formally began in 1957 covering those pesticides and related substances used in agriculture...
J M Baker


Environmentally more acceptable solvents
1979 - IRG/WP 3131
The subject of this paper is hydrocarbon solvents with particular reference to the cyclo-aliphatic or naphthene-rich, grades which are now available. The specialised low aromatic high boiling petroleum fractions are also discussed....
A M Cumbers


Traitement curatif des bois en place. Hygiène et sécurité
1990 - IRG/WP 3585
P Huré


Questionnaire on the state of pollution control in the field of wood preservation
1974 - IRG/WP 52
H Willeitner