Wood preservation in East European countries
1989 - IRG/WP 3527
The paper discusses the main problems of wood preservation in Bulgaria, Czechoslovakia, German DR, Hungary, Poland, Rumania and the USSR. The main types of wood preservatives produced have been presented, as well as the state of standarization to test their properties. There have been considered methods of wood treatment in use and application range of treated wood....
J Wazny


An investigation to assess the feasibility of developing an accelerated laboratory test to determine the abrasion resistance of lesser-used timber species for use in marine constructio
2005 - IRG/WP 05-20317
The paper describes the evaluation of a laboratory-accelerated test to compare the shingle abrasion resistance of current and potential timbers for use in marine construction. Useful results were achieved in 47.5 hours, but identified a number of issues to be resolved for the test to be refined and the subsequent results to be interpreted correctly....
G S Sawyer, J R Williams


IRG/COIPM INTERNATIONAL MARINE TEST - to determine the effect of timber substrate on the effectiveness of water-borne salt preservatives in sea-water: Final report
1987 - IRG/WP 4133
Three timbers chosen as reference species were treated with 3, 6 and 10% solutions of CCA and CCB preservatives and exposed for up to 93 months at 8 tropical and temperate marine sites. Eleven local species treated in the same way were exposed at 4 of the 8 sites. There was no apparent difference in performance between CCA and CCB treated specimens. The severest test site was Panama Canal but mari...
R A Eaton


The biological natural durability of timber in ground contact
1994 - IRG/WP 94-20051
The BRE ground contact field trials for the determination of the biological natural durability of different timber species have recently been reviewed. The data obtained from these trials have been used to appraise the different ways in which natural durability may be expressed. It is concluded that the use of the mean as a method of assigning the timber to one of five durability classes may be ac...
G A Smith, R J Orsler


Estimation of service life of durable timber species by accelerated decay test and fungal cellar test
2002 - IRG/WP 02-20249
Many kinds of durable wood species for outdoor uses has been imported from all over the world to Japan. However information on the natural durability of these species is not sufficient to estimate the service life of them in the climate of Japan. Highly durable species such as Jarrh, Teak, Ipe, Ekki, Selangan batu, Red wood, Western red cedar showed no significant percent mass losses by accelerate...
K Yamamoto, I Momohara


Regulatory and Consumer Challenges Facing Timber Preservation and Durability Interests in New Zealand and Australia
2003 - IRG/WP 03-20282
Timber preservation and durability interests in Australia and New Zealand are facing many challenges and threats arising from regulation and standards changes, to direct competition from competitive materials producers. Industry can address these challenges by pro-active initiation of sound, holistic, research, that addresses the performance needs of the regulators and specifiers and the expectati...
C MacKenzie


Inventaire des "déchets" ou produits connexes de la filière bois
1993 - IRG/WP 93-50001-33
G Marcotte


Some biological observations on the management of preservativion experiments with submerged timber in the marine environment
1976 - IRG/WP 421 E
P Deschamps


The benefits to New Zealand of boron salt treatment of Pinus radiata
1992 - IRG/WP 92-3692
The historical reasons for New Zealand adopting boric salt diffusion of Pinus radiata are summarised, and present day processes and their associated costs are given. The biological hazards of using Pinus radiata untreated are then argued, using endemic fungal and insect species as examples, as well as a discussion of the risks from species that may yet be accidentally introduced into the country....
D J Cross


Weather testing of timber - discoloration
2001 - IRG/WP 01-20221
The brightness and color saturation of the timber were reduced over time. The perception of an increasingly dark color in the timber over time is due to the gradual reduction in brightness. The period from May to September was characterized by the greatest discoloration of all three periods of the year. Because this period has the largest number of sunlight hours, and the timber is subjected to a ...
T Toyoda, M Azuma, Y Hikita


Protection of Ochroma pyramidale from fungal decay with N,N-napthaloylhyroxylamine
1998 - IRG/WP 98-30182
Fungal decay of wood in service results in billions of dollars (U.S.) in losses annually. Recent environmental restrictions, both U.S. and international, are limiting and eliminating the use of broad-spectrum, heavy metal biocides for wood preservation. Restrictions result primarily from problems with disposal. New wood preservatives need to be developed and tested which specifically target key el...
F Green III, T L Highley


Thirty-four year test of on-site preservative treatments to control decay in wood above ground
1993 - IRG/WP 93-30015
This research was initiated in 1958 to investigate efficacy of various preservatives and treating methods for new lumber going into exterior structures of buildings. Post-rail units (2x4 inches) constructed of Southern Pine sapwood, Douglas-fir heartwood, and mill run western hemlock were dip- or brush-treated before or after assembly. Units were trested with pentachlorophenol in various petroleum...
T L Highley, T C Scheffer


Physical and mechanical properties of a suitable constructional timber of Bangladesh
1997 - IRG/WP 97-40102
The study of physical and mechanical properties of lohasirish timber (Derris robusta Roxb.) grown in Bangladesh revealed that the sapwood is whitish to yellowish white, heartwood is dark grey to blackish in colour; the texture is moderately fine, the grain in mostly straight and coarse with whitish rings of parenchyma; shrinkage is moderate; the EMC ranges from 12% to 16%; fuelwood colorific value...
A K Lahiry


Maintaining the adoption of the equilibrium moisture content in timber by bifluorides under outdoor circumstance
1989 - IRG/WP 3541
A description is given of the practical application of bifluorides, f. ex. Diffusec in maintaining the adaption of the equilibrium moisture content in timber, as a result of a many years observation of treated timber under outdoor circumstances....
H F M Nijman


Co-operative Field Experiment: Performance of preservative-treated timber: Report on condition of specimens after seven years installed in New South Wales - Australia
1986 - IRG/WP 3362
R S Johnstone


Work program of CEN/TC 38 (April 1993). Durability of wood and wood-based products
1993 - IRG/WP 93-20012
R Hüe


A risk model for termite attack in Australia
2003 - IRG/WP 03-10468
This paper describes a model to predict the risk of termite attack on a house in Australia. It is based on a survey of expert opinion and data from 5000 houses. The model gives a quantitative estimate of risk, and as such is useful for the development of risk management systems. An example of the application of such a system is given....
R H Leicester, C-H Wang, L J Cookson


Field trials on preserved timber out of ground contact
1978 - IRG/WP 3154
This report describes two different field trials studying the performance of preservative treatments on timber exposed to the weather, but above the ground. Results are presented on the protection afforded against decay, and on the efficiency of water-repellent preservative treatments in controlling the uptake of moisture by the timber. Proposals for a standard field test system are briefly discus...
D F Purslow, N A Williams


A field test with anti-sapstain chemicals on sawn pine timber in Finland
1986 - IRG/WP 3368
Fourteen formulations, each in two concentrations, were tested for effectiveness against sapstain, mould and decay on Scots pine (Pinus sylvestris L.) in a field test in South-Finland. The trial was commenced in June 1985 and finished in October 1985. During the test the boards were infected mainly by mould fungi. In kiln dried boards the protective effects of nine and in green boards of four trea...
L Paajanen


Oxalic acid production of fifteen brown-rot fungi in copper citrate- treated southern yellow pine
2001 - IRG/WP 01-10388
Non-arsenical copper-based wood preservatives have grown in number since the 1980's as a response to environmental concerns posed by arsenicals. Interest in copper tolerant decay fungi has increased accordingly. Oxalic acid (OA) production by brown-rot fungi has been proposed as one mechanism of copper tolerance. Fifteen brown-rot fungi representing the genera Postia, Wolfiporia, Serpula,...
F Green III, C A Clausen


Effect of leaching temperature and water acidity on the loss of metal elements from CCA treated timber in aquatic conditions. Part 2: Semi-industrial investigation
1995 - IRG/WP 95-50040-13
In continuation of previous leaching research on the quantification and modelling of metal elements released from CCA treated timber, a series of experiments has been carried out dealing with the influence of temperature and pH of the relative aquatic environment. The leaching method used is the Dutch prestandard for building materials, a long term static leaching test simulating practical bank-sh...
G M F Van Eetvelde, W J Homan, H Militz, M Stevens


Timber Preservation and Sustainable Construction in Australia
2005 - IRG/WP 05-50224-14
Sustainable development has been described as meeting the needs of the present without compromising the ability of future generations to meeting their own needs. (Bruntland 1987) To achieve the sustainable development goal therefore, the maximum performance has to be obtained from existing resources (timber) so that the remaining resource is protected from over-exploitation. Clearly, wood preserva...
J Norton


Results of field tests on the natural durability of timber (1932-1975)
1976 - IRG/WP 3105
This paper describes a continuing field stake trial to determine the natural resistance of different species of timber to decay. Data are presented for about 180 timbers, covering over 6000 stakes, and the results are discussed in terms of a natural durability classification....
D W Purslow


Recycling of impregnated timber: Part 2: Combustion trial
1999 - IRG/WP 99-50132
Totally 270 m3 (61,3 t) of CCA impregnated wood was chipped and incinerated at the combustion plant of Jalasjärvi. After the normal gas cleaning venture scrubbers were tested. After the trial a metal balance was calculated. Ash was treated at the copper smelter of Outokumpu Harjavalta Metals Oy. Condensate waters were transfered to the Outokumpu's CCA production plant and utilized by the...
L Lindroos


A laboratory evaluation of the susceptibility to biological attack of glued laminated pine timber
1991 - IRG/WP 2387
In the scope of a research programme concerning the use of maritime pine (Pinus pinaster) to produce glued laminated timber structures in Portugal, the natural durability of this material was checked by using laboratory test methods. An European standard, EN 113, was used to test durability against basidiomycetes and a test method developed at LNEC for termites was adapted for this purpose. From t...
L Nunes, H Cruz