The Influence of Wood Included Salinity on Nail
2019 - IRG/WP 19-40863
In the Great East Japan Earthquake that occurred on March 11, 2011, many buildings suffered from natural seawater dipping due to the tsunami. It has become clear that corrosion progresses in nail that had submerged in natural seawater compared to nail that had not submerged in natural seawater. However, processing for this has not been developed. Therefore, in this research, we experimentally expl...
R Nakano, H Ishiyama, K Sakano
Color change of timber exposed outdoors - Influence of season exposure test starts
2019 - IRG/WP 19-40865
For the client the material and color of the exterior wall are important, because they affect the impression of the building [1]. However, discoloration of the exterior wall begins as soon as the building is completed, by various factors such as rainfall. We tried to quantitatively evaluate the changes of the exterior wood, and to organize the influences of climate conditions, in order to use the ...
K Usami, H Ishiyama
Influence of Drying Condition of Wood on Rusting of Nail
2019 - IRG/WP 19-40887
Recently in Japan, the durability of metal joint in wooden structures become important. Revised Building Standard Law was enacted in 2000 and Act on the Promotion of Popularization of Long-life Quality Housing was enacted in 2008 in Japan. Since then, the durability of the metal joints in the wooden houses becomes important. But there are not any detailed regulation for the durability of the metal...
H Ishiyama, N Wada, T Nishimura, T Mori
The influence of chemical compounds on wood cell wall to surface cracks
2020 - IRG/WP 20-40908
Degradation due to cracking and dimensional changes caused by drying, have a significantly negative impact on the preservation and durability of wood. Therefore, the prevention of surface cracking, which tends to occur during the drying process, is vital. High temperature set drying is one of the most effective methods for preventing wood surface cracking. It begins with softening the wood at a hi...
R Suzuki, Y Mori, K Yoshihiro, K Yamashita, M Kiguchi
Influence of weathering on surface roughness of thermally modified wood
2021 - IRG/WP 21-40915
Thermally modified wood is exposed to weathering similarly as other wood-based building materials. It has been reported that if thermally modified wood is exposed to weathering, its moisture performance might decrease fairly fast. The aim of this study was to determine whether this phenomenon is associated with crack formations or roughness. Norway spruce, thermally modified spruce, wax-treated th...
E Kerzic, B Lesar, M Humar
Premature adhesion failure of exterior wood coatings – The influence of substrate temperature at coating application and moisture accumulation during storage
2022 - IRG/WP 22-40937
The present study aimed at extending the knowledge about premature coating failures of industrially finished wood cladding. Two potential factors were studied: the influence of substrate temperature at coating application and moisture accumulation during storage on the adhesion of waterborne coating systems. In the first experiment, 4 batches of wood specimens were submitted to 4 different tempera...
U Hundhausen
The influence of thermal modification and surface charring to different levels on wettability of Norway spruce wood
2022 - IRG/WP 22-40942
The wood can alternatively be protected from water absorption by thermal modification and charring. Both techniques cause certain chemical and physical changes in the wood, the extent of which depends on the level of temperature applied. The objective of this study was to determine how the combination of charring to different levels and thermal modification affects the chemical, morphological, and...
J Žigon, C Gerardin, M E P Wålinder, P Gerardin
Joints design considerations in indoor high humidity conditions
2022 - IRG/WP 22-40950
In recent years, a number of cases of degradation by wood destroying fungi have been detected in covered timber structures such as pools, wineries, bathrooms, etc. – in fact, any building where indoor air may reach high humidity values during certain periods of time.
The origin of this kind of decay was not related to water leaks, but to the condensation of the water vapor over the steel connec...
A Lozano, D Lorenzo, M Alonso, F Álvarez, J E Martínez
Influence of weathering on the mechanical properties and performance of exterior wood coatings
2022 - IRG/WP 22-40951
Three commercial coatings were exposed to artificial (EN 927-6) and natural weathering (EN 927-3) on wood samples. Cracking was visually assessed as well as Persoz hardness. Free films of the same coatings were also exposed to the same weathering tests before their tensile properties were measured. Results show that artificial and natural weathering modified the overall mechanical properties of wo...
L Podgorski, J-D Lanvin
The influence of climate changes on Central European forests with an emphasis on Slovenia
2022 - IRG/WP 22-50368
When forests are managed sustainably, they play an essential role in protecting climate and biodiversity. They protect soils and water resources, provide livelihoods, and contribute to the well-being of rural and urban communities. European forests are multifunctional and provide a range of ecosystem services. These include the production of renewable materials that can replace materials with a la...
J Gričar, L Krajnc, M Westergren, S Rus, H Kraigher
Influence of weathering of wood surfaces before and after treatment with iron(II) sulphate
2023 - IRG/WP 23-30786
Outdoor wood is exposed to various factors that cause the wood to grey or age. The ageing processes can vary greatly depending on the exposure. Parts of the wood that are not exposed to external factors, e.g. under the eaves, are less exposed and the ageing process is therefore slower. This can be accelerated by solutions based on iron ions. In this way, the wood greys quickly and evenly. However,...
B Lesar, M Humar, F Osvald
The influence of chemical and thermal modification on homogeneity between sapwood, heartwood, and transition wood of short rotation teak
2023 - IRG/WP 23-40961
Short rotation teak wood has low quality especially in durability. Heartwood presents sufficient natural durability and poor impregnability; meanwhile, most sapwood requires special treatment to increase its durability. The objective of this work was to investigate the effect of thermal or chemical treatment on homogenization between sapwood, heartwood, and transition wood for some selected proper...
R Martha, B George, W Darmawan, P Gerardin
Eradication of beetles attacking wooden historical buildings by humidity-controlled warm-air treatment
2023 - IRG/WP 23-11028
Humidity-controlled warm-air treatment is a method that kills mainly beetles that are damaging the wood. In this process, a heat-insulating and airtight covering is placed around the object building, and the temperature inside the covering is gradually raised to about 60°C, held for a certain period of time, and then gradually lowered. While maintained at 60°C, all forms of damaging insects - ad...
Y Fujii, Y Fujiwara, M Harada, H Kitahara, M Shimada, S Kondo, Y Sato, M Shimada, R Kigawa, H Watanabe, Y Komine, S Hidaka, D Ogura
Influence of the substitution of phenol with lignin cleavage products in phenol-formaldehyde impregnation resins for wood modification on the fungal decay resistance and impregnation depth
2024 - IRG/WP 24-30805
The impregnation modification of wood with phenol-formaldehyde (PF) resins increases the woods dimensional stability and resistance against fungal decay. However, to decrease the usage of non-renewable resources, the substitution of phenol has been a topic of scientific interest. Lignin is a currently underutilized resource with a chemical structure that contains phenolic units. For adhesive appli...
J Karthäuser, L Tarentino, A Treu, H Militz, G Alfredsen
How personality traits influence the perception of fungal decay in a wooden cladding – A survey in three Modelling wood moisture content in outdoor conditions from measured data
2024 - IRG/WP 24-41002
This study examined perceptions of fungal decay damage on wooden cladding across Norway, Sweden, and Germany. The majority of respondents across all countries did not find the fungal decay damage in question acceptable, with the least acceptance in Norway. This could be due to Norway having the highest frequency of wooden residential buildings and the most experience with maintaining wooden claddi...
G W Gustavsen, G Alfredsen, P B van Niekerk, J Niklewski, C Brischke
Performance of Douglas-fir cross laminated timber (CLT) subjected to elevated humidity in a ground proximity field test for 6 years
2024 - IRG/WP 24-41010
The ability of insecticidal soil drenches or spray-on insecticide/fungicide treatments to protect mass timber elements exposed in a high moisture environment but out of direct soil contact was assessed using a modified AWPA ground proximity test established in 2017. Three-ply Douglas-fir CLT pieces measuring 305 x 355 x 105 mm (L x H x W) were installed at the Harrison Experimental Forest (HEF) (S...
M E Mankowski, J J Morrell, T G Shelton, G T Kirker
Influence of incising methods and wood moisture content on ‘deep penetration treatment’ in Japanese cedar and larch
2025 - IRG/WP 25-20749
To expand applicability of ‘deep penetration treatment’, a solvent-borne and non-pressure treatment that is commonly coupled with roller-type incising using a flat blade, we investigated drill and laser machining as alternative incising methods and examined the influence of wood moisture content on the preservative penetration. Various incising methods were applied to heartwood of Japanese ced...
S Taira, T Miyauchi, S Isaji, H Matsunaga
Chestnut tannin-furfurylic resins for wood preservation: influence of the proportion of tannins as a copolymer
2025 - IRG/WP 25-30816
Tannin, which is present in all plants, is the most abundant polyphenol globally and can be extracted using water or organic solvents such as acetone, ethanol and methanol. Tannins are classified into two categories: condensed tannins (catechin-based polymers) and hydrolysable tannins (sugar esters with galloyl units). Previous studies have demonstrated its potential as a raw material for modifyin...
J V Dorini-Falavinha, C Gerardin-Charbonnier, P Cademartori
Process Development in Continuous Wood Densification and the Influence of Ionic Liquids on Set-Recovery and Mechanical Properties
2025 - IRG/WP 25-30827
The densification of wood significantly enhances its mechanical properties, making low-density species more viable for high-performance applications. However, challenges such as set-recovery (SR) and production speed hinder large-scale adoption. This study investigates continuous surface densification using a custom-built belt press and examines the effect of chemical pre-treatment with ionic liqu...
D Jones, A Scharf, B Neyses, D Sandberg
Influence of plasma treatment on the coatability of wood primer with a topcoat for exterior use
2025 - IRG/WP 25-30828
The coatability of oil, or of solvent-borne alkyd resin wood primers with waterborne acrylic finish is the subject of much debate, but not much information can be found in the scientific literature on this topic. The aim of our study was therefore to evaluate the adhesion strength of the waterborne acrylic coating on oiled wood or wood with a solvent-based alkyd primer and to test the recoatabilit...
M Petrič, L Albreht, N B Štrus, E Keržič, M Pavlič, J Žigon, S Dahle
Preservation conditions of wooden roofs of two historical churches in middle-Sweden
2025 - IRG/WP 25-41016
Assessment of biodegradation by the rot of shingles from the roofs of churches of Hammarby and Tångeråsa in mid-Sweden was done by studies with X-ray computer tomography. The study suggests that inner rot could be detected with CT, which was not always easily detected by visual inspection. In some cases, erosion from the weathered side was fairly large, but the inner wood part was found not to b...
O Karlsson, Y Huang, A Postovoitova, C-F Lin, O Myronycheva
Relationship between changes inside moisture content of wood measured using temperature and humidity sensors and swelling and shrinkage
2025 - IRG/WP 25-41030
With the spread of mid and high-rise timber buildings, the long-term use of timber buildings is getting required more than ever. It is considered that measurement of the local inside moisture content of a wooden member is one of the useful methods for periodic health assessment of timber buildings. The aim of this research is to establish an easy estimation method of the local inside moisture cont...
Y Sadakane, T Mori
Towards Sustainable Wood Protection: PF resins-impregnated Paper Honeycombs and the role of Processing Parameters analysis by Response Surface Methodology
2025 - IRG/WP 25-41045
Honeycomb paperboard is an important wood-derived product and also an emerging new material to combine with wood panels. It is commonly applied as cushioning materials with excellent mechanical performance, and high demands in packaging market. The aims of this study were to enhance the durability of honeycomb paperboard using PF resins of various molecular weights (Mw 200, Mw 500, Mw 700), partic...
Y-C Wu, P-Y Kuo