Your search resulted in 13 documents.


Iron promotes decay capacity of Serpula lacrymans
1993 - IRG/WP 93-10008
The influence of iron and iron compounds on the decay capacity of Serpula lacrymans was studied. Mass losses of pine wood caused by dry rot fungus were increased when FeSO4 was added into the culture medium or when there were iron nails or stone wool on the culture medium. This supports the hypothesis that iron in stone-based building materials is one reason for the increased decay capacity of Ser...
L Paajanen


Effect of mineral wools on growth and decay capacities of Serpula lacrymans and some other brown-rot fungi
1991 - IRG/WP 1481
The influence of stone wool and glass wool on growth and decay capacities of Serpula lacrymans and some other brown-rot fungi was studied. Mass losses of pine wood caused by Serpula lacrymans and Gloeophyllum trabeum were increased when stone wool was present. Glass wool had no influence on mass losses. Coniophora puteana, Serpula lacrymans and Gloeophyllum trabeum grew into stone wool and destroy...
L Paajanen, A-C Ritschkoff


Iron in stone wool - one reason for the increased growth and decay capacity of Serpula lacrymans
1992 - IRG/WP 92-1537
The chemical compositions of stone wool and glass wool were analysed. There was more iron in the stone wool than in the glass wool. It was found that iron present in stone wool was easily dissolved by oxalic acid that Serpula lacrymans is able to produce. The stone wool promoted the decay of pine wood by Serpula lacrymans. The glass wool had no effect on the decay capacity of Serpula Iacrymans. Th...
L Paajanen, A-C Ritschkoff


The effect of temperature on the rate of fixation of an alkyl ammonium compound (AAC) wood preservative
1984 - IRG/WP 3293
The rate of fixation of an alkyl ammonium compound wood preservative was measured by soaking samples of wood wool in various preparations of the preservative for arbitrary times followed by immediate leaching in water. The wood wool was then analysed for residual preservative. The results indicated that fixation was very rapid and increased at higher temperatures....
P Vinden


The use of plastic meshes in soft rot monoculture testing
1990 - IRG/WP 2353
Plastic meshes were introduced between the wood blocks and agar medium in a miniaturised soft rot monoculture test in order to minimise transfer of the preservative from the wood and mineral salts from the agar. Although several different sizes and types of mesh were used and the blocks were wetted up to an appropriate moisture content for soft rot attack the amount of decay was substantially redu...
S M Gray


Conditions and possibility of nanobiocides formulation for wood protection
2008 - IRG/WP 08-30467
During development of nanobiocides for wood protection the need to identify mineral composition of wood in respect of trace elements and nourishing conditions of wood destroying fungi in relation to these elements was discussed....
J Wazny, A Kundzewicz


Preservative effect of cellulose insulation material against some mould fungi and brown rot fungus Coniophora puteana in pine sapwood
1991 - IRG/WP 1484
The influence of mineral wool and loose-fill cellulose wool on biodeterioration of pine sapwood was studied. The test fungi were mould fungi Aspergillus versicolor, Cladosporium sphaerospermum, Penicillium sp. and Aureobasidium pullullans and brown rot fungus Coniophora puteana. Cellulose wool inhibited the growth of mould fungi on the face of wood contacted with insulation material at RH of 97 an...
H Viitanen


The effect of brighteners on wood surface aesthetics – exploring the use of various organo-phosphonates based precursors
2007 - IRG/WP 07-30441
Freshly cut hardwood lumber such as white oak, red oak, beech, or redwood are rich in mineral stain (mostly iron and calcium), which provides a strong discoloration of the wood surface significantly influencing the aesthetic of the wood surface and strongly affecting the cost of this lumber. The influence of mineral stain on soft wood discoloration (Southern Yellow Pine, Douglas fir, etc.) is les...
R Craciun, P Mitchell


Efficiency of the Amazon Forest Oils as Preservatives to the Attack of cellulolytic fungi in Pine Wood
2012 - IRG/WP 12-30599
The bobbins of wood are used for storage and field installation of cables from the electricity and telecommunications sectors. There are legal requirements governing the Brazilian ways of treating the wood used in these sectors, aimed at preventing pollution and protecting nature. When exposed to severe environmental conditions in Brazil these products are degraded and occurs many operational prob...
S Silveira, I M S Mendes, R S Paiva, J E Volponi, R C G Comar, R S Cruz


Fungal decay of archaeological waterlogged oak timber: role of the mineral content
2016 - IRG/WP 16-10873
In service, wood foundation poles are subjected to water level fluctuation in soil. While wood is saturated by water only bacterial decay occurs. When oxygen content increases and moisture content decreases, severe fungal attack may occur. To evaluate the long term fungal durability of wood foundation pole in the context of service, 300 years waterlogged archaeological wood poles were used. The oa...
A Besserer, M Letellier, E Fredon, Q Kleindienst, M-L Antoine, C Perrin, J Lallemand, C Rose, M-C Trouy


Effects of wollastonite nanofibers on biological resistance of historical paper against Aspergillus niger
2017 - IRG/WP 17-10878
Effect of wollastonite nanofibers on biological resistance of historical paper against Aspergillus niger was studied. Specimens from A4 papers were also prepared for comparison purposes. Paper specimens were dipped in aqueous nanowollastonite (NW) with 10, 20, 30, and 40% concentrations and compared with control specimens. In order the nanofibers be fixed on paper specimens, 5% of polyvinyl acetat...
H R Taghiyari, A Kalantari, A Ershad-Langroudi, A Kalantari


Effects of Nano-Wollastonite Impregnation on Fire Properties of Some Thermally-Treated Solid Wood Species
2017 - IRG/WP 17-40771
The effects of nano-wollastonite (NW) suspension impregnation on the fire-retarding properties of heat-treated solid wood of three species (beech, poplar, fir) were studied. Heat treatment was performed at two temperatures of 180 °C and 200 °C. Impregnation was carried out at a pressure of 3 bars for 30 min. The fire properties included ignition time, glowing time, back-darkening, back-splitting...
H R Taghiyari, R Hossinpourpia, S Adamopoulos, A Jahangiri, D Rabie


Comparative study of the properties of silicate coatings with different mineral pigments (titanium dioxide, iron (III) oxide, copper (II) oxide) on the surface of wood
2022 - IRG/WP 22-40936
Silicate coatings are attractive alternatives to conventional organic-based coatings for wood protection. In this work, silicate coatings were prepared with a potassium silicate binder modified with a methyl siliconate solution, and three types of mineral pigments titanium dioxide, iron (III) oxide and copper (II) oxide. The coatings were applied on beech wood and cured under ambient conditions. T...
A M Cheumani Yona, M Petrič