IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 371 documents. Displaying 25 entries per page.


4th Report on condition of panels at Sekondi, Ghana
1978 - IRG/WP 445
F F K Ampong


Germination of basidiospores on preservative treated wood after leaching or natural weathering
1981 - IRG/WP 2150
In tests of residual toxic efficacy after leaching or natural weathering, spore germination with Gloeophyllum trabeum has proved to be a less reliable criterion of attack than when used with unaged preservative treatments. Since spores sometimes prove more tolerant than their parent mycelium, their use should be continued....
J K Carey


Assessment of the natural durability of four Ghanaian hardwoods against the white-rot fungus Coriolus versicolor and soft-rot using laboratory tests
2003 - IRG/WP 03-10498
The natural durability of two lesser-utilized species (LUS) (Corynanthe pachyceras Welw. (pamprana) and Glyphaea brevis (Sprengel) Monachino) (foto) from three forest districts, and two related primary species (Nauclea diderrichii (de Wild.) Merr. (opepe) and Nesogodornia papaverifera (A. Chev.) R. Capuron.) (danta) from one district in Ghana is assessed against Coriolus versicolor Linnaeus Quelet...
C Antwi-Boasiako, A J Pitman, J R Barnett


Adequate preservative treatment of tropical and subtropical hardwoods for electric anchor logs
1997 - IRG/WP 97-40101
Most available 27 different hardwood species grown in Bangladesh was investigated regarding suitability as CCA-C (chromated copper arsenate type-C) impregnated anchor logs for rural electrification programme. The kiln-drying properties, sapwood thicknesses, CCA treatability grades of sapwood and heartwood, natural durability of heartwood and CCA retainability at specific assay zone separated 27 ha...
A K Lahiry


A natural exposure weathering test for the evaluation of preservative performance
1992 - IRG/WP 92-2400
Natural exposure weathering tests were carried out by externally exposing treated wood samples for varying periodes of time up to 36 months. In the laboratory these samples were assayed for residual preservative effeciveness using Coniophora puteana FPRL 11E. The results indicated a loss in efficacy over and above that determined using artificial ageing procedures such as EN73 (evaporative ageing)...
J Brown, G R Williams


The potential for accelerated ageing to determine the persistence of active ingredients in timber
2006 - IRG/WP 06-20323
Fast screening methods for evaluating the persistence of active ingredients in timber are proposed. This is an outline proposal which is intended to provoke discussion and further development of the methods. Reliable and accurate analytical methods are key to these tests....
L D A Saunders, M R Powell


Flow charts for termite and decay tests to determine the natural durability of Japanese cedar (Cryptomeria japonica D. Don)
2008 - IRG/WP 08-20385
This paper deals with the experimental flow charts that were used for determination the effects of fungal decay and termite attack on Sugi heartwood during the course of the study of “Comparative studies of natural durability of Japanese cedar (Cryptomeria japonica D. Don) among the geographic cultivate”, which was carried out by Usta et al (2006)....
I Usta, S Doi


Natural Durability Classification Systems Used Around the World
2009 - IRG/WP 09-10694
Around the world natural durability is classified in different ways. The nature and rigor of the tests used to measure durability, the method of classification based on these data, and use of these classifications to specify end uses or predict service life all vary. This can lead to confusion among people not familiar with the various systems used. This review describes the methods used to classi...
R Stirling


Natural durability of some commercial timbers of Sarawak, Malaysia in tropical marine environment
2005 - IRG/WP 05-10561
The abundant supply of timber resources in Sarawak makes timber an ideal choice to be used for marine construction. The natural durability of the main commercial timber species of Sarawak in ground contact is well established but the same is not available for marine environment. This study was conducted to assess the natural durability of 28 commercial timber species in tropical marine environmen...
K Jenang, Wang Choon Ling


Natural durability of some common Indian timbers and marine plywood against biodeterioration in Kochi waters (India)
1992 - IRG/WP 92-4177
Panels of thirty-eight timber species and marine plywood were tested in Kochi harbour (South-west India) for periods ranging from 3 to 21 months, so as to evaluate their natural resistance against marine borers. Results indicate that all the timber species studied are non-durable, 6 of them having undergone more than 50% internal destruction within 3 months; 14 species in 6 months, 13 species and ...
L N Santhakumaran, M V Rao


Criteria for basidiomycetes testing and ways of defining natural durability classes
1998 - IRG/WP 98-20144
Within the framework of a European research project several laboratories have tested a series of 17 wood species covering the total range of natural durability. Basidiomycete tests are part of the total set up. Although generally based upon standard methods some minor differences in execution of the tests were evaluated for their impact on the results. This variation was superimposed with the fac...
J Van Acker, M Stevens, J K Carey, R Sierra-Alvarez, H Militz, I Le Bayon, G Kleist, R-D Peek


Natural durability of eight tropical hardwoods species from Africa
2005 - IRG/WP 05-10563
Current forest inventory results reveal that there are more than 700 hundred-hardwood species in tropical forests, of which less than 10 percent are harvested and used for commercial purposes. The increased use of lesser-known species can decrease the pressure on current commercial species, increase the value of the forest and lead to better management practices. However basic information on physi...
P Nzokou, K Wehner, D P Kamdem


Evaluating the natural durability of a number of lesser known species of Ghanaian hardwoods using a short term laboratory assay
2004 - IRG/WP 04-10540
Resistance of a number of Ghanaian hardwoods to attack by the crustacean Limnoria quadripunctata was assessed by measuring the production of faecal pellets under forced feeding conditions over a two week period. Small sticks of commercially available, lesser known timber species, were leached in seawater for one week then placed in a cell culture chamber with one animal and 4 ml of seawater. At in...
J R Williams, S M Cragg, L M S Borges, B Shayler


Sustainability Through New Technologies for Enhanced Wood Durability. COST Action E37 – A New Action in the Forestry Domain
2004 - IRG/WP 04-40293
The main overall objective of the action is to concentrate on the contribution of wood durability on the sustainability through the development of systems for quality assurance and perfoamance of modified wood and wood products as alternatives to wood treated with traditional preservatives. By this means it seeks to improve and consequently increase the cost-effective use of sustainably produced E...
R-D Peek


Natural durability of wood in ground contact - A correlation between field and laboratory tests
1985 - IRG/WP 2182
A field test is being carried out to evaluate the natural durability of 20 hardwoods. The resistance to decay and termite attack was evaluated in accelerated laboratory tests. The results of the field test after 6 years and 8 months indicate that there is not necessarily agreement between results from laboratory and field tests. It is pointed out that apart from the artificiality of the laboratory...
M S Cavalcante, G A C Lopez, R G Montagna, M E S Fosco Mucci


Natural resistance of different species of timber to marine borer attack in the Trondheimsfjord (Western Norway)
1978 - IRG/WP 435
Natural resistance of 34 timber species to marine wood-borers has been discussed, based on data collected from panels immersed in selected localities in the Trondheimsfjord during 1977-78. The wood-borers encountered on the panels were Psiloteredo megotara, Xylophaga dorsalis, Xylophaga praestans and Limnoria lignorum. The number of borers present and their growth were taken as the criterion for a...
L N Santhakumaran, J A Sneli


Durability of wood in the area of wood-inhabiting termites in Slovenia
1981 - IRG/WP 1139
This report describes a research dealing with resistance and durability of five different species of wood. The experiment was made in natural conditions in the Slovene area of wood-inhabiting termites. The results of our experimental field, which correspond to the results of the former laboratory experiments, show a very weak resistance of spruce-wood, fir-wood, and beech-wood. They also show thei...
L Kervina


Laboratory determination of the natural decay resistance of some lesser-utilized timbers from Tanzania against wood decay fungi
2004 - IRG/WP 04-10517
Four lesser known/utilized timber species (sap and heartwoods) from Tanzania, namely Albizia lebbeck, Zanthoxylum gilletii, Faurea saligna and Parinari curatellifolia were exposed to the brown rot fungi (Gloeophyllum trabeum and Coniophora puteana) and the white rot fungus (Coriolus versicolor) to determine their natural decay resistance according to the EN 113 standard procedure. The timbers were...
P R Gillah, R C Ishengoma, E Julias, S A Amartey, D H Kitojo


A summary of work carried out to compare natural and artificial weathering for preconditioning test specimens in testing anti-stain chemicals for wood in service
1976 - IRG/WP 266
Since 1972 work has been in progress within CEN to establish a European standard for the testing of wood preservatives designed to prevent blue-staining of wood in service. The method is based on the Butin test and involves pre-weathering of the samples prior to biological testing. The weathering regime employed is 6 months outside exposure from March to October. This imposes severe limitations on...
D J Dickinson, A F Bravery


Natural durability of European wood species for exterior use above ground
2003 - IRG/WP 03-10499
The main interest in using more timber for exterior constructions is to protect the environment, where wood is considered an environmentally friendly material. However, chemicals for wood protection are getting more and more restricted, consequently, the focus on the natural durability of wood is increased. Good, well-documented data on the durability of wood species in ground contact exist, which...
B Lindegaard, N Morsing


The chemical analysis and biological evaluation of wood extractives as potential timber preservatives
1995 - IRG/WP 95-30090
Work involved the biological performance of water and organic solvent soluble extractives of four naturally durable wood species, namely; Matumi, Tamboti, Sneezewood and the Turpentine tree. These timber species are known to be naturally durable against termites and fungi (±25 to 35 years). The extractives were evaluated against termites and fungi using impregnated pine pencil stakes in field tes...
P Turner, D Conradie


Natural durability of Iranian saxual wood (Haloxylon persicum) against the fungal decay
1991 - IRG/WP 1515
Haloxylon persicum is vidly planted in the deserfic region of Iran. At the present time, in the age of 30, these small trees are ready for cutting for the different uses, specially for rural buildings. But there's any knowledge about its durability. In this study the laboratory tests were carried out in accordance to European Standard. 5 fungi were used as: Trametes versicolor, Coniophora...
D Parsapajouh, F H Schweingruber, K Richter


Study of the degradation of retified wood through ultrasonic and gravimetric techniques
1994 - IRG/WP 94-40030
One of the non-polluting processes that increase the natural durability of wood is a thermal treatment in an atmosphere poor in oxygen, producing what is normally denominated "retified wood". In this study the validity of a non-destructive technique (ultrasound) in order to determine the biodegradation suffered by wood across time has been studied. For this reason, the behavior of a wood species (...
D T De Troya, A M Navarrete


An in-ground natural durability field test of Australian timbers and exotic reference species. Part 5: Extensive data from a site where both decay and termites are active. Results from a full-replicated set of heartwood specimens from each of ten myrtaceous hardwoods after 18, 19 and 20 years' exposure - A discussion paper
1988 - IRG/WP 2324
Extensive data are presented on the decay situation, the termite situation and the decay-termite associations; all gathered from a fully-replicated set of heartwood specimens of 10 hardwood timbers after 18, 19 and 20 years' exposure in the ground at a single test site, i.e. a semi-arid steppe site. Sixteen tables are presented in addition to the one table providing the rating data; the l...
J D Thornton, G C Johnson, J W Creffield


UV-microspectrophotometry of lignin and accessory compounds in wood cell walls of conifers
1999 - IRG/WP 99-20171
The distribution of lignin in the cell wall of conifer tracheids was determined by UV-VIS microspectro-photometer. Wood sections of one micron thickness were measured between the wavelength 240 and 700 nm. Spectral analyses revealed that the conifer lignin associated with the tracheid secondary wall and middle lamella is composed of guiacylpropane units which exhibit a characteristic UV absorption...
G Kleist, G Koch, J Bauch


Previous Page | Next Page