Your search resulted in 3187 documents. Displaying 25 entries per page.
Current models used by the European Health Authorities to evaluate the volatilization of active ingredients from treated wood used inside dwellings. A case study: Volatilization of azaconazole and propiconazole from treated wood
1990 - IRG/WP 3565
The use of wood preservatives inside houses may result in measurable aerial concentrations of active ingredients. These airborne contaminants may be inhaled by the inhabitants over periods lasting from a couple of days to several months. To assess the potential health hazard of preservative residues in the air, various risk-assessment models have been worked out. Three schemes, currently used by t...
A R Valcke, L Van Leemput
Electronic noses for detection of rot in wood
1996 - IRG/WP 96-20098
In an ongoing project an electronic nose is being studied and developed for detection of volatile organic compounds (VOC) emitted from wood colonised and decayed by fungi. The electronic nose consists of an array of gas sensors with different selectivity patterns for different groups of volatile organic compounds (VOC). The use of pattern recognition routines implemented by artificial neural netwo...
K Nilsson
Copper based water-borne preservatives: The use of a thin section technique to compare the protection of wood by copper based preservatives against soft-rot and bacterial decay
1987 - IRG/WP 2286
This paper describes the techniques developed and gives examples of results obtained for the performance of copper based wood preservatives against both the bacterial and fungal hazards....
A M Wyles, D J Dickinson
Available iron promotes brown rot of treated wood
1992 - IRG/WP 92-1526
Exposure of treated wood blocks to rusting iron increased the toxic threshold of chromated copper arsenate and ammoniacal copper arsenate to a brown-rot fungus Leucogyrophana sp. This supports the hypothesis that the movement of iron ions into wood contributes to the unexpectedly high decay rate of treated wood at the stake test site at Westham Island BC. To what extent this phenomenon may occur e...
P I Morris
Leaching of chromium and other cca components from wood-cement composites made with spent CCA treated wood
2000 - IRG/WP 00-50153
Wood cement composites are an attractive option for recycling spent treated wood, since the CCA treatment enhances the physical, mechanical and biological resistance properties of the composite. However, we have noted a higher than normal leaching of chromium from these products and this appears to result from conversion of some of the trivalent chromium to the more leachable and toxic hexavalent ...
D Qi, P A Cooper
Autoxidation of beech condensate
2003 - IRG/WP 03-40261
Liquid effluent from steaming beech wood was studied. The effluent contains many phenolic compounds which can present a significant toxicity. The effluent was treated by oxidation was carried out at 250 rpm for 30 min with NaOH. This was followed flocculation with CaCl2 for 30 min. The influence of parameters such as pH, time of autoxidation were studied. Experimental results reveal the electrosta...
M Irmouli, J P Haluk
Experience with an industrial scale-up for the biological purification of CCA-treated wood waste
1997 - IRG/WP 97-50095
The biological purification of CCA-treated wood waste was tested in co-operation of the BFH and the Italian impregnation plant SoFoMe. Chipped poles were infested with the chromium and arsenic tolerant brown-rot fungus Antrodia vaillantii which can transform in the laboratory ca. 90% of the chromium and arsenic into watersoluble salts. These can be leached to 100-200 ppm residual metal content. Th...
H Leithoff, R-D Peek
Nomination procedure for the offices of President, Vice-President and members of the Executive council of IRG
2003 - IRG/WP 03-60180
IRG Secretariat
Preliminary note on the fungal problem of rubber wood
1983 - IRG/WP 3246
Susceptibility of rubber wood to fungal attack limits its wider utilisation. Fungal problems encountered in treating rubber wood with boron compounds by diffusion process have been discussed. Sodium pentachlorophenoxide and 2-thiocyanomethylthio benzothioazole (TCMTB) were investigated for possible control of fungal growth during diffusion storage and their performance has been reported....
R Gnanaharan
Production of treated wood in Brazil in 1984
1986 - IRG/WP 3357
The data of the Brazilian production of sleepers, poles, crossarms, fence posts and other commodities are given for the year of 1984....
M S Cavalcante
The development of a screening method for the activity of pyrethroids against wood boring marine crustaceans, Limnoria spp
1978 - IRG/WP 443
The present work is concerned with the develepment of a suitable bio-assay technique to determine the biological activity (contact action) of pyrethroids against Limnoria spp. Estimates of the toxicity of three pyrethroids, permethrin, cypermethrin and decamethrin (the structures of which are shown in Fig. 1.) to the marine borer have been obtained....
D Rutherford, R C Reay, M G Ford
Incorporating insect behaviour in standard tests of wood preservatives - A possible way to reduce pesticide loadings
2000 - IRG/WP 00-20190
The application of wood preservatives to protect timber against insect infestation is common practice world wide. The effectiveness of wood protecting insecticides is usually determined in various standard tests. Depending on the target pest species and the test method, larvae of different developmental stages and sizes or adult insects are exposed artificially to the insecticide-treated commodity...
H Hertel, R Plarre
Germination of basidiospores on preservative treated wood after leaching or natural weathering
1981 - IRG/WP 2150
In tests of residual toxic efficacy after leaching or natural weathering, spore germination with Gloeophyllum trabeum has proved to be a less reliable criterion of attack than when used with unaged preservative treatments. Since spores sometimes prove more tolerant than their parent mycelium, their use should be continued....
J K Carey
Report of activity of CEN/TC 38: Test Methods for Wood Preservatives
1987 - IRG/WP 2287
G Castan
A collaborative test to determine the efficacy of poyurethane coatings on wood samples exposed in the marine environment. 1st Interim Report
1988 - IRG/WP 4145
Wood samples coated with elastomeric polyurethane (ca. 50 mils thick) were exposed for up to 2 years in 12 tropical and temperate marine test sites with known teredinid, pholad and/or crustacean infestations. All uncoated control samples were destroyed or partially destroyed. Polyurethane-coated samples were not attacked, the surfaces of the coating were sound and the polyurethane adhered well to ...
R A Eaton
Antifungal properties of new quaternary ammonium and imidazolium salts against wood decay, staining and mould fungi
2004 - IRG/WP 04-30347
The biological activity of twenty-four potential wood preservatives – imidazolium and quaternary ammonium salts with a modified anion structure was determined employing screening agar-plate and agar-block methods. Experiments were carried out on Scots pine (Pinus sylvestris L.) wood. The aim of the performed studies was to investigate the effect of structure modification of IC and QAC with organ...
J Zabielska-Matejuk, W Wieczorek
Environmental behaviour of treated wood in (semi-)permanent contact with fresh or seawater
1998 - IRG/WP 98-50101-20
This study presents a strategy for the environmental toxicity evaluation of treated wood towards the aquatic compartment, using non target water organisms toxicity tests. A lixiviation process is applied on wood (Pinus sylvestris) treated with several wood preservatives formulations. The lixiviation process is carried out in the laboratory with ultrapure water or synthetic seawater.
After chemica...
P Marchal, C Martin
An experimental method to simulate incipient decay of wood by basidiomycete fungi
2000 - IRG/WP 00-20200
At very early stages of decay of wood by basidiomycete fungi, strength loss can be measured from wood before any measurable weight loss. Therefore, strength loss is a more efficient measure of incipient decay than weight loss. However, common standard decay tests (e.g. EN 113 or ASTM D2017) use weight loss as the measure of decay. A method was developed that allowed progressive removal of samples ...
S F Curling, J E Winandy, C A Clausen
The proposal for optimalization of the agar-block method for wood preservatives fungitoxic evaluation
1995 - IRG/WP 95-20065
On the base of own research and other scientists results the proposal for optimalization of agar-block method was presented by:
- selection of test fungal species and strains and central distribution of their pure cultures,
- change of the treatment and control samples exposure procedure,
- application of mathematical estimation of toxic value results,
- shortening the duration of fungitoxic t...
J Wazny
Rapport sur l'activité du CEN/TC 38 "Méthodes d'essais des produits de préservation du bois"
1982 - IRG/WP 2188
M Pottevin
Towards a colour assay of wood degradation
1982 - IRG/WP 2180
A colour assay for the enzyme catalase is described. Since the activity of this enzyme has previously been shown to be correlated with degree of wood degradation as determined by other methods, this assay may provide a rapid quantitative indicator of superficial and internal wood decay....
M A Line
Leaching of inorganic wood preservatives – Investigating the relationship between leachability, dissociation characteristics and long-term leaching potential
2003 - IRG/WP 03-50199
Estimation of the leaching properties of preservative components is greatly affected by the leaching test method applied since not all methods equally consider the physical components responsible for leaching. These include: wetting of the wood and penetration of water (affected by dimensions, amount of end grain, permeability, duration and nature of water exposure); solution of preservative comp...
L Waldron, Y T Ung, P A Cooper
Laboratory experiments on aerial emissions from wood treated with wood stains
1993 - IRG/WP 93-50001-06
Due to the actual environmental interest in wood preservation, a series of experiments was carried out on the emission of biocides from treated wood. The research focussed on the volatilization of 5 biocides from boards treated with wood preservative finishes containing dichlofluanide (DCF) azaconazole (AZA), pentachlorphenol (PCP), iodopropynylbuthylcarbamate (IPCB) and tributhyltinoxide (TBTO). ...
G M F Van Eetvelde, M Stevens
Disposal of Pressure Treated Wood in Construction and Demolition Debris Landfill
2005 - IRG/WP 05-50235
Pressure treated wood is often disposed in landfills in the US, very frequently in construction and demolition (C&D) debris landfills. C&D debris disposal facilities in many states are not equipped with liner systems to protect underlying groundwater. In this paper, issues associated with the disposal of metal-containing treated wood in C&D debris landfills are discussed. C&D de...
T G Townsend, B Dubey, J Jambeck, H M Solo-Gabriele
Influence of variable lignin content on brown rot decay of wood
1987 - IRG/WP 1320
Compilation of published data and new experiments with brown-rotting fungi on different timber species suggest that their decay activity, in contrast to soft rot and white rot fungi, is not greatly influenced by the type or amount of lignin present....
T Nilsson, G F Daniel