IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 158 documents. Displaying 25 entries per page.


Summary of development of pile wrappings in Los Angeles Harbour
1987 - IRG/WP 4141
G Horeczko


Moisture content levels and decay of hemlock
1986 - IRG/WP 1287
As a model of decay conditions of wooden members in wooden houses, a decay test was set up in which samples of western hemlock (Tsuga heterophylla) under 4 moisture levels were examined. Each week the samples were weighed and if the weights indicated that their moisture contents were lower than the expected levels, distilled water was added. Every 8 weeks 3 samples from each condition were oven dr...
K Suzuki


Loss of preservatives from treated wood during service
1992 - IRG/WP 92-3734
During the 23rd IRG conference in Harrogate the matter of preservative losses from treated wood during service was raised. We were asked to collect information in this field and ask now for help from you. Many tests have been carried out at a laboratory scale to study fixation and leaching from wood treated with different preservatives. Very little, however, is reported on losses of preservatives ...
M-L Edlund, D Rudolph


Effects of acetylation on the dimensional stability and decay resistance of kenaf (Hibiscus cannabinus L.) fiberboard
1996 - IRG/WP 96-40059
The objective of this study was to investigate the influence of the acetylation treated kenaf fiber, Phenol formaldehyde resin content level, and three fungi species on the dimensional stability and decay resistance of high density non wood composition boards. A standard ASTM method was used to evaluate weight loss and thickness change. The linear shrinkage and expansion of each species were also ...
P Chow, T Harp, R Meimban, J A Youngquist, R M Rowell


Strength loss associated with steam conditioning and boron treatment of radiata pine framing
1987 - IRG/WP 3438
The combined effect of included defects and wood moisture content on the strength loss of second rotation radiata pine framing following conventional steam conditioning is investigated. The green Modulus of Elasticity (MOE) is reduced by approximately 13% after steaming. When dried after steaming, however, neither the MOE nor MOR is significantly different from unsteamed dried controls....
M J Collins, P Vinden


Collaborative soft rot tests: PRL tests of Cu/Cr/As preservative using method of Document No: IRG/WP/208
1973 - IRG/WP 223
These tests were undertaken as a preliminary to the next series of collaborative soft rot tests. An interim report has already been presented at Berlin in 1972 as Document No: IRG/WP/211...
J K Carey, J G Savory


On Donkioporia expansa (Desm.) Kotl. & Pouzar
1986 - IRG/WP 1285
Donkioporia expansa is found more often in houses than realised until now. Virulence tests according to EN 113 show not only an attack of oak, but also of other hardwoods and even soft-woods....
G Buchwald


Soil virulence tests using Scots pine sapwood
1973 - IRG/WP 222
Following the tests reported in Document No: IRG/WP/210, in which soils from different laboratories were investigated for virulence, supplementary tests have been carried out using Scots pine sapwood and an extended incubation period....
J K Carey, J G Savory


Comparison of the agar-block and soil-block methods used for evaluation of fungitoxic value of QAC and CCA wood preservatives
1994 - IRG/WP 94-20039
The modyfied agar-block and soil-block methods were used for comparing the fungitoxic value of QAC and CCA type preservatives against Coniophora puteana and Coniophora olivacea The mass loss and moisture contents of wood were analysed....
J Wazny, L J Cookson


The biostatic effect of copper on decay of fire retardant-treated mining timber
1991 - IRG/WP 1507
Blocks of Eucalyptus grandis were treated with 20kg/m³ ammonium sulphate as fire retardant and challenged with Coriolus versicolor. Replicates were soil buried. A second set of blocks was treated with retardant and copper at 6.6 kg/m³ (ie 1% w/w), and challenged similarly. After 8 weeks weight losses produced by Coriolus versicolor in untreated, retardant treated and copper supplemented blocks w...
G D Shelver, E A Shelver, A A W Baecker


Temperature influence on the growing velocity and cellulolytic activities of Poria placenta strains from several locations
1986 - IRG/WP 2263
The differences observed on the FPRL 280 Poria Placenta strain at several Research European Laboratories for determining up the fungicide effectiveness of wood preservative has carry us to do a comparative study about the cellulolytic activity and growth velocity of each of this strains at different temperatures (22, 24 and 28°C). The results show significative differences when the temperature is...
A M Navarrete, M T De Troya


Evaluation of wood treated with copper-based preservatives for Cu loss during exposure to heat and copper-tolerant Bacillus licheniformis
1999 - IRG/WP 99-20155
Copper-based wood preservatives need to be effective against exposure to all types of microorganisms. Wood treated with six copper-based preservatives was exposed to 121°C and 20 psi pressure for 15 minutes under standard autoclave conditions and the copper-tolerant bacterium, Bacillus licheniformis CC01, for 10 d at 28°C and 150 rpm. Sixteen to 37 percent of the copper was released from the woo...
D M Crawford, C A Clausen


Collaborative soft rot tests: Interim report on PRL tests of Cu/Cr/As preservative using method of Document No: IRG/WP/208
1972 - IRG/WP 211
Preservative: Tanalith CT.106 - Results obtained with beech are given in the table and indicate a toxic limit of 16.7-19.2 kg/m³ - The initial soil moisture content was adjusted to 27.8% (the water holding capacity). Noticeable drying out has occurred in some of the test bottles....
J G Savory


Contribution to the testing of wood based board material
1982 - IRG/WP 2176
R G Lea


Evaluation of the decay caused by Chaetomium globosum Kunze, in the course of time
1987 - IRG/WP 2288
The main research done on soft rot has been directed to determining, by microscopic study, the different stages of penetration into the wood of the fungi that cause it. On the basis of the information furnished by this research, in this work we have tried to quantify its effect, by evaluating the weight loss caused by Chaetomium globosum Kunce in wood of Pinus sylvestris L. and Fagus sylvatica L. ...
M T De Troya, A M Navarrete


Proposals for a vermiculite burial soft rot test method
1980 - IRG/WP 283
J G Savory, J K Carey


Collaborative soft rot tests: 2nd interim report
1975 - IRG/WP 258
J G Savory, J K Carey


Virulence testing of cultures of different origins of the test fungus Coriolus versicolor strain CTB 863 A
1986 - IRG/WP 2267
The virulence of cultures of different origins of Coriolus versicolor CTB 863 A - a strain which is mentioned in EN 113 - was tested. Standard blocks of beech wood were used at temperatures of 20-22°C and 26-28°C and particleboard was tested at 26-28°C. The decay capacity of the different inoculations varied widely, as could be expected it was greatest at the higher temperature level....
W Kerner


Airborne algae as a wood degradation factor
1992 - IRG/WP 92-1549
The occurrence of airborne (aerophytic) algae on wood is a very frequent phenomenon. However, there is currently a lack of information concerning their effect on the wood tissue. Some important genus of algae infesting wood under natural conditions are listed, as well as the results of experimental studies in the "in vitro" culture concerning the effect of two selected algal species on some physic...
K J Krajewski, J Wazny


The rate of redistribution and loss of leachable preservatives under service conditions
1993 - IRG/WP 93-30026
This paper describes experiments carried out to determine patterns of preservative redistribution and any associated losses which occur when wood containing unfixed water-soluble wood preservatives is exposed to service conditions where leaching is possible. Scots pine sapwood treated with disodium octaborate was used as a model system. Results are recorded and discussed for trials representing pa...
R J Orsler, G E Holland


The performance of wood preservatives in soil-bed soft rot tests
1993 - IRG/WP 93-20007
Testing the efficacy of wood preservatives in soil is recognised as a fundamental part of the assessment of long-term wood protection in ground contact. Laboratory based tests can provide a hazardous environment in which a preservative can be challenged by a range of micro-organisms. This paper presents the results of tests carried out to investigate the performance of wood preservatives in a wet ...
G R Williams, S Caswell


On the use of % weight loss as a measure for expressing results of laboratory decay experiments
1992 - IRG/WP 92-2394
It is suggested that careful consideration should be given for the presentation of data from laboratory decay experiments, especially when comparisons are being made from experiments involving wood blocks of varying densities. Percent weight loss can be used for comparisons of durability even if wood blocks vary in density. It is suggested that the absolute weight loss for a given volume (g/cm³) ...
T Nilsson, G F Daniel


Termiticidal effectiveness of synthetic pyrethroids, carbaryl and chlordane in wood-block test
1985 - IRG/WP 3356
The results of some wood-block tests with allethrin, permethrin, fenvalerate, carbaryl and chlordane against Coptotermes formosanus are tabled and compared against some organophosphates, chlorpyrifos, fenitrothion, phoxim, tetrachlorvinphos and acephate. The treatment of the wood blocks was exactly as described in Document No: IRG/WP/3330. Among the pyrethroids tested, permethrin was the most effe...
K Tsunoda


Effect of leaching temperature and water acidity on the loss of metal elements from CCA treated timber in aquatic conditions. Part 2: Semi-industrial investigation
1995 - IRG/WP 95-50040-13
In continuation of previous leaching research on the quantification and modelling of metal elements released from CCA treated timber, a series of experiments has been carried out dealing with the influence of temperature and pH of the relative aquatic environment. The leaching method used is the Dutch prestandard for building materials, a long term static leaching test simulating practical bank-sh...
G M F Van Eetvelde, W J Homan, H Militz, M Stevens


Detection of incipient brown rot decay in wood by fourier transform infrared spectrometry
1987 - IRG/WP 2275
Fourier transform infrared spectrometry was evaluated as a possible method for detecting different levels of brown-rot decay in pine sapwood. By using first derivative spectra and regression analysis, an equation based on 4 absorption peaks, normalized with an internal standard peak, was developed. The correlation between weight loss and absorption was highly significant indicating that this is a ...
D D Nicholas, T Schultz


Next Page