Characterization of checks and cracks on the surface of weathered wood
2000 - IRG/WP 00-40153
The surface roughness of unweathered and untreated pine; unweathered copper chromium arsenate type C (CCA) - treated pine; weathered CCA-treated pine; and weathered CCA-plus-water-repellent (WR) - treated pine was evaluated by a stylus tracing method. Surface roughness parameters Ra, Rz, Rmax, Rk, Rpk, and Rvk were measured. Ra, Rpk, and Rvk were the most appropriate parameters for describing modi...
D P Kamdem, Jun Zhang


A novel solvent penetration assessment technique for wood preservativation treatments using waterborne systems
1990 - IRG/WP 2346
Solvent and hence solute (a.i.) penetration during any wood preservation treatment cycle and the flow pathways taken by the solvent in the wood are crucial elements in determining the adequacy of any treatment. Inadequate solvent penetration into specimens or an inappropriate tissue throughflow pattern during impregnation will markedly affect the distribution pattern achieved by many non-diffusibl...
A J Pendlebury, J Coetzee, E Sorfa, A Botha


New approaches to practical evaluation method of bio-degradation of wooden construction - Non-destructive detection of defects using radar technique
2000 - IRG/WP 00-20214
There have been a number of researches and developments on the techniques and apparatus for the nondestructive evaluation of the biological deterioration in wood and wooden constructions, such as decay or insect attack in house, public buildings or in historically important architectures. As for the detection of the decay in wood, techniques using sound in audible or in ultrasonic frequency ranges...
Y Fujii, Y Komatsu, Y Yanase, S Okumura, Y Imamura, M Tarumi, H Takiuchi, A Inai


On the occurrence of Phialophora species in preservative treated wood in ground contact
1977 - IRG/WP 163
Phialophora is a fairly large genus comprising about thirty described species. They are widespread in very diverse environments, such as soil, sea water, wood and wood pulps. Some species are known as parasites on plants and animals, including man. Phialophora species were early known for their ability to produce blue stain in timber. Later it was discovered that several species were able to produ...
T Nilsson, B Henningsson


The effectiveness of three tributyltin compounds in beech against soft rot fungi using a soil-bed technique: A preliminary report
1986 - IRG/WP 3390
The effectiveness, towards soft rot fungi, of bis (tributyltin) oxide, tributyltin ethanesulphonate (TBTES) and benzyltributylammonium tributyldichlorostannate in both leached and unleached beech stakes is compared to that of a CCA preservative (Tanalith CT 106), using a soilbed technique. In addition, the effect of test solvent (water or toluene) on the performance of TBTES is evaluated. Total ti...
R Hill, A H Chapman, B Patel, A Samuel, J K Carey


Patterns of decay in CCA-treated horticultural post populations - A fungus cellar simulation
1986 - IRG/WP 1286
The distribution of decayed posts in 10-, 14-, and 18-year-old vineyards supported a hypothesis to explain variability in intensity of decay found among posts in New Zealand horticultural properties. The development of decay patterns between samples in a simulated vineyard plot established in the Forest Research Institute fungus cellar gave additional support to the hypothesis that decay within la...
M E Hedley


Preservative technique of three commercially important timber species – Sissoo (Dalbergia sissoo), Akasmoni (Acacia auriculiformis) and Ghoraneem (Melia azedarach) of Bangladesh
2005 - IRG/WP 05-40299
Wood is renewable resource and is widely used as construction material in rural and urban areas of Bangladesh. Dalbergia sissoo, Acacia auriculiformis and Melia azedarach, locally known as Sissoo, Akasmoni and Ghoraneem respectively are three important timber species of Bangladesh. These are used for different purposes normally without preservative treatment. Heartwood of Sissoo, Akasmoni and Ghor...
M R Bulbul, M O Hannan, P K Sarker, A A Mahafuz, G N M Ilias


Mechanical properties of CCA-treated southern pine after post-treatment kiln drying
1989 - IRG/WP 3543
This report reviews current research dealing with the effects of waterborne preservative treatment and redrying on the mechanical properties of wood. In general, waterborne preservative treatments reduce average mechanical properties. This effect is exaggerated when treated wood is kiln-dried after treatment, especially at elevated temperatures. For lumber, recently completed research at the Missi...
H M Barnes, J E Winandy


Field study: Wood degradation pattern in buildings and utility poles in tropical climates of Nigeria
1992 - IRG/WP 92-1521
The paper is the result of five years field study of wood degradation patterns in three ecological forest zones (Guinea Savannah, Tropical rain forest and mangrove forest zones, respectively). It involved 800 residential buildings and 700 electric overhead transmission poles. The methodology used was a modified Eslyn (6) test. A high rate of Ascomycetes and Basidiomycetes attack especially on the ...
E O Onuorah


Effect of post-treatment drying schedule on the modulus of elasticity of CCA-treated southern pine dimension stock using nondestructive methods
1987 - IRG/WP 3413
This paper describes the results from the nondestructive testing for modulus of elasticity (MOE) of southern pine (Pinus sp.) 2 x 6's treated with chromated copper arsenate and redried using three commercial kiln schedules. The data indicate that redrying CCA-treated southern pine dimension stock treated to above-ground retentions (4 kg/m³) has no deleterious effect on the MOE, regardles...
H M Barnes, S Moore


Method of embedding and staining of wood after biological testing to support the identification of decay type
1998 - IRG/WP 98-20131
A method for preparing wood for microscopic analysis after decay testing is described, with special regard to a novel fast simultaneous staining, which helps to identify different types of decay. The novel staining process is explained as well as the embedding of heavily decayed samples in polyethylene glycol (PEG) and picking up of sections by transparent adhesive tape. Special feature of the int...
A O Rapp


Effect of post-treatment processing on leachability of ACZA-treated douglas-fir lumber
1998 - IRG/WP 98-50109
The effect of post-treatment procedures that more rapidly precipitate copper, zinc, and arsenic in douglas-fir treated with ammoniacal copper zinc arsenate (ACZA) on subsequent leaching resistance were investigated at two retentions (6.4 and 40 kg/m3). Total leaching was greater from boards treated to the higher retention. At both levels, copper was lost at the highest rate. Post-treatment process...
J J Morrell, C S Love, S Kumar, C M Freitag


Isolation and identification of the fungal flora in treated wood. Revised technique
1977 - IRG/WP 159
At the 8th Annual Meeting in Wildhaus a paper was presented for discussion on the isolation of fungi from treated wood.·Since then work of this nature has been undertaken at Imperial College and as a result a revision of that document has been made and is presented here. The main alterations are: 1) To streamline the isolation procedure 2) Modification of the benomyl agar 3) The inclusion of a st...
C P Clubbe, J F Levy


Biological control of internal decay in Scots pine poles: A seven year experiment
1992 - IRG/WP 92-1529
The interactions between key fungi were monitored, by non-destructive and destructive sampling methods, during the course of an experiment on the effectiveness of Scytalidium sp. and Trichoderma spp. for eliminating established infections of Lentinus lepideus (Fr. ex Fr.) Fr. in creosoted Pinus sylvestris poles. Although extensively isolated at the beginning and end of the experiment, Trichoderma ...
P I Morris, D J Dickinson, B Calver


The effect of synthetic pyrethroid insecticides on post-treatment emergence of Anobium punctatum
1992 - IRG/WP 92-1568
Data is presented from trials in which wood specimens, treated with a range of remedial insecticidal formulations, were aged in a roof void for 5 years and then tested for emergence of adult Anobium punctatum. The technique used followed that described in IRG/WP/2175. The results from formulations containing synthetic pyrethroids are compared with those from formulations containing the chlorinated...
R W Berry


Surface Barriers for Protection of Culture and Heritage Wooden Objects from Insect Attack
2004 - IRG/WP 04-40286
Anoxic treatment is an environment friendly procedure for eradication of wood boring insects in wooden objects of cultural and historical heritage. However, after the anoxic treatment, wooden antiques remain susceptible to further insect attacks. Possible protection against insects could be provided by the so-called post-repression protective barriers. Potential coating materials for such barriers...
M Petric, M Pavlic, B Kricej, M Humar, F Pohleven


A technique for measuring preservative loss or redistribution during leaching
1983 - IRG/WP 2199
Radiata pine sapwood stakes were treated with benzalkonium chloride (AAC) or copper-chrome-arsenate (CCA). After fixation and drying the outer 2 mm and 2-4 mm layers were removed from one radial longitudinal face. The planed face was coated with a waterproof coating and AAC-treated stakes were leached for 6, 12 or 18 weeks; 12 weeks for the CCA-treated stakes. After airdrying three 2 mm layers (0-...
J A Drysdale


Minthea rugicollis (Walk.) (Coleoptera: Lyctidae): A pest of rubberwood
1992 - IRG/WP 92-1570
Rubberwood (Hevea brasiliensis) has grown in prominence as a source of timber in recent years. One of the drawbacks in the utilization of this species is its susceptibility to attack by powder-post beetles belonging to the family Lyctidae. In Malaysia, Minthea rugicollis (Walk) is the, most commonly found species attacking seasoned rubberwood. In this paper, information available thus far on Minth...
F Abood, R W Berry, R J Murphy


A technique for determining the efficacy of water diffusible preservative plugs for implanting in joinery in service
1987 - IRG/WP 2291
A technique is described for determining the efficacy of soluble, diffusible preservative plugs for eradicating decay in joinery. It uses blocks of Scots pine sapwood or heartwood adjusted to known moisture contents prior to the establishment of the test fungus Coniophora puteana, from a single longitudinal dowel and the subsequent introduction of the preservative plugs. Prevention of decay, eradi...
J K Carey, A F Bravery


The development of a field testing technique using Coptotermes lacteus mounds in Australia
1985 - IRG/WP 1270
A method to rapidly screen potential bait substrates placed around Coptotermes lacteus mounds is described. A perforated P.V.C. conduit is buried in a shallow trench in a rectangular arrangement around an active mound. Seven P.V.C. holders containing cork baits are inserted vertically into the conduit around the mound. Within three weeks following installation of the baits around five mound coloni...
J R J French, P J Robinson


Characterization of wood decay enzymes by MALDI-MS for post-translational modification and gene identification
2002 - IRG/WP 02-10442
The recent sequencing of the Phanerochaete chrysosporium genome presents many opportunities, including the possibility of rapidly correlating specific wood decay proteins of the fungus with the corresponding gene sequences. Here we compare mass fragments of trypsin digests, determined by MALDI-MS (Matrix Assisted Laser Desorption Ionization-Mass Spectrometry), with predicted mass fragments derive...
T H de Koker, P J Kersten


A study of methanogenesis and sulphate-reduction: A possible source of explosive gas mixtures in a gold mine
1989 - IRG/WP 1399
Previous work isolated anaerobic bacteria from timbers and drainage water in a gold mine. The present work identifies the predominant methanogen in the mine ecosystem as Methanobacterium bryantii and sulphate-reducing isolates as Desulphovibrio desulphuricans and Desulphotomaculum antarcticum. Laboratory studies using model systems evaluate the activity of methanogenic and sulphate-reducing bacter...
L D Abraham, J F Putterill, A A W Baecker


A determination of the toxic level of ACQ2100 wood preservative for the powder post borer Lyctus brunneus (Stephens)
1994 - IRG/WP 94-20029
The sapwood of two Lyctus susceptible Australian hardwoods, messmate (Eucalyptus obliqua L'Herit.) and black bean (Castanospermum australe A. Cunn. et Fraser ex Hook) were pressure impregnated with ACQ2100, a wood preservative, to produce replicates of a range of retentions. Preservative retentions were determined by solution weight uptake at treatment and chemical analyses of selected sa...
A R Moffat


A non-destructive testing technique for wood poles
1987 - IRG/WP 2293
A method has been developed to evaluate the stiffness and condition of a wood pole based on structural dynamics. This paper describes the results of tests performed on nearly 200 wood utility poles across Western Canada. A high correlation exists between the dynamic non-destructive test and direct mechanical tests. The need for an accurate non-destructive testing technique is demonstrated by the f...
W M Murphy, D E Franklin, R A Palylyk


A novel technique for comparative toxicity studies of potential insecticidal wood preservatives
1983 - IRG/WP 2198
For some years now a device has been under development at the New Zealand Forest Research Institute, the purpose of which is to study the effects of sub-lethal amounts of stomach poisons (but also of fumigants and contact active materials) on the co-ordinative abilities of a cerambycid larva. This insect is Prionoplus reticularis - indigenous to New Zealand its larvae feed in decaying logs and are...
D J Cross