Selecting fumigants for treatment of internal decay in wood
1986 - IRG/WP 3370
A number of potential fumigants were screened with respect to their toxicity to decay fungi, (Poria carbonica, and Lentinus lepideus) and their sorption characteristics on Douglas Fir (Pseudotsuga menziesii Mirb. Franco) wood. Wafers of infected wood were exposed to different fumigant concentrations for various times then cultured to determine viability. The lethal concentration X time (ct) factor...
P A Cooper


Analysis of tebuconazole in wood treated with Tanalith™ E
1999 - IRG/WP 99-20158
A simple gas chromatographic method for determining tebuconazole in Tanalith™ E treated wood is described. A two step sequential extraction procedure with methanol was used. Sample extracts were analysed without cleanup or concentration using capillary column GC with thermionic specific detection. The performance of the method was assessed using radiata pine (Pinus radiata) sapwood, radiata pine...
D E Ferlazzo


An investigation into the stability of TBTO in LOSP-treated radiata pine
1987 - IRG/WP 3459
Nuclear magnetic resonance (NMR) spectroscopy and reverse phase paper chromatography were used to characterise the organotin compounds found in radiata pine treated with bis (tri-n-butyl) tin oxide (TBTO). Preliminary results indicate that the preservative is remarkably unstable in wood after light organic solvent preservative (LOSP) treatment. Significant decomposition of TBTO occurs in a matter ...
K J Archer, R Meder


An evaluation of the potential of ion mobility spectrometry for detection of organic wood preservative components in solutions and treated wood
1994 - IRG/WP 94-20038
For the disposal of wood waste under ecological sound conditions information about its hazardous potential is required. Until now, no highly sensitive rapid analytical methods are available for the detection of wood preservatives under industrial process conditions. Preliminary experiments showed that Ion Mobility Spectrometry (IMS) could be a promising method for rapid detection of organic preser...
A Voss, J N R Ruddick, W J Homan, H Militz, H Willeitner


Biocidal screening method of wood extractives by a direct use of cellulose TLC plate
2001 - IRG/WP 01-20226
Most of the methods to evaluate the biological durability of woods have focused on decay fungi and termite as deteriorating organisms and it is well known that one of the most important factors affecting the biological characteristics of wood is extractives. Bioassays for evaluating the biological activities of wood extractives have been mainly conducted with treated filter papers for termites or ...
R Yusiasih, T Yoshimura, T Umezawa, Y Imamura


Gas chromatographic determination of 1,8-naphthalimide, N-Hydroxy-1,8-naphthalimide (N,N-naphthaloylhydroxylamine) and the sodium salt of N-Hydroxy-1,8-naphthalimide
2003 - IRG/WP 03-20259
A number of naphthalimide (NI) derivatives are used as efficient laser dyes, in medicine or in scanning electron microscopy. Only N,N-naphthaloylhydroxylamine (NHA) has been shown to be an effective wood preservative against wood decay fungi and termite damage. However, limited information is available concerning the analytical detection of NI-derivatives in treated timber. There is a clear need ...
E Melcher, F Green III


Volatile organic compounds (VOC) measured during drying of impregnated timber
2004 - IRG/WP 04-50216
Discussion about drying of impregnated timber has taken place in the Nordic countries under eighties and nineties and goes on nowadays. The drying increase the value of production and the customer gets fewer problems when handles the timber. This introduces a positive attitude to the impregnation as a process and its products. Beside the important information about the advantages of impregnated ti...
N Terziev, V Djokic


The detection of organic solvent preservatives in wood by thin-layer chromatography
1975 - IRG/WP 357
A simple and rapid method for the detection of common organic solvent wood preservative materials is described. The method uses thin-layer chromatography after leaching of the preservative from sections of timber with chloroform. RF values and the sensitivity of the method are discussed and a routine procedure for identification of the organic and organometallic preservatives is proposed. Methods ...
B G Henshaw, J W W Morgan, N Williams


Stability of bifenthrin in a commercial phenol-formaldehyde plywood glue
2003 - IRG/WP 03-30311
Liquid phenol formaldehyde (PF) glue mixes used for plywood manufacture are strongly alkaline. At this pH insecticidal additives may not be stable for long periods. In order to establish practical working life of the synthetic pyrethroid insecticide, bifenthrin, in liquid PF glues the concentration of bifenthrin in the glue mix was measured under laboratory conditions over a 24 hour period. Glu...
M J Kennedy, P A Collins, R D Vella


Moisture correction for ultrasonic MOE measurements above fibre saturation point in Scots pine sapwood
2006 - IRG/WP 06-20333
There is a high correlation between methods for dynamic modulus of elasticity (MOEdyn) and static modulus of elasticity (MOEstat). MOEdyn methods have been found sensitive to detect early stages of decay and may be seen as an option for non-destructive wood durability testing. As the MOEstat measurements do not change after reaching the fibre saturation point, the uncorrected MOEdyn data from ultr...
E Larnøy, G Alfredsen, H Militz


Interactions between wood and propiconazole in supercritical carbon dioxide
2009 - IRG/WP 09-40461
Understanding the movement and deposition of biocides in wood is a fundamental aspect of the supercritical wood impregnation process and a key issue in developing the process e.g. to handle wood of larger dimensions. Previous research on supercritical wood impregnation frequently reports of a biocide concentration gradient in impregnated samples i.e. a lower concentration of biocides in the core o...
A W Kjellow, O Henriksen


Profiling fungal community in wood decay ecosystem by Denaturing High-Performance Liquid Chromatography
2010 - IRG/WP 10-20443
A DNA-based fingerprinting technique, Denaturing High Performance Liquid Chromatography (DHPLC) was developed to profile fungal communities colonizing indoor timber. Molecular fungal diversity was assessed using amplification based on the Internal Transcribed Spacer (ITS1) rDNA of 74 wood samples collected from infected buildings in France. Due to its high sensitivity, the PCR-DHPLC technique was ...
S Maurice, G Le Floch, M Le Bras-Quéré, J P Rioult, G Barbier


Theoretic discussion on the way and driving forces of moisture migration in wood during vacuum drying
2011 - IRG/WP 10-40538
Most of parameters in conventional drying cannot explain a lot of phenomena appeared in vacuum condition, so it is necessary to further explore the moisture migration way and driving forces in wood under vacuum condition. For the water movement channel in wood is very narrow, the characteristic of heat and mass transfer in wood is similar to that in microscale. This article applies theory of liqui...
Zhengbin He, Xueli Yao, Liqiong Chen, Songlin Yi


Surface energy characterization of thermally modified wood using inverse gas chromatography
2013 - IRG/WP 13-20532
The objective of this work is to characterize surface energetics of thermally modified wood. Such information may be useful for a better understanding and predictions of adhesion properties between the modified wood and other material systems, e.g. coatings, adhesives or matrices in composites. Inverse gas chromatography (IGC) was used to study the surface energy characteristics of thermally modif...
S Källbom, K Segerholm, D Jones, M Wålinder


A review on prediction methods of wood natural durability
2017 - IRG/WP 17-10892
Natural durability of timber may be defined as “inherent ability of timber to attack by wood destroying organisms (bacteria, fungi, insects, marine borers) without preservative treatment. On the base of biological tests, EN-350-2 standard (Afnor, 1994), describe the classification of wood species according to their natural durability. But these specifications are not adapted in the case of wood ...
N Amusant, C Flora, J Beauchène, E Houël, C Duplais