Your search resulted in 789 documents. Displaying 25 entries per page.
Evaluation of the permeability of fast grown wood species
1995 - IRG/WP 95-40042
The low natural durability of certain species of wood, implies the need for applying a protecting treatment to increase its life in service. Because of this, a knowledge of the permeability properties of the wood is desired. In this work, a simple and reliable method to evaluate the wood permeability is presented. For that, we have been used fast grown species, with low natural durability, Poplar ...
M T De Troya, A M Navarrete, E Sanchez, J E Garcia de los Rios, E L Rodríguez Trobajo
Deltamethrin effectiveness against subterranean termite attack on wood under natural conditions
1989 - IRG/WP 1407
On fighting subterranean termites on wood, out of ground contact, the synthetic pyrethroid Deltamethrin shows positive aspects such as its efficiency and low mammalian toxicity. To evaluate its performance in conditions very similar to those in service use, specimens of Pinus sp were treated with solutions of Deltamethrin diluted in "white spirits" at 0.005% (w/w) and 0.01% (w/w) and exposed in a ...
P A Zanotto
Chemical and biological investigations of double-vacuum treated windows after 7½ years in service
1985 - IRG/WP 3339
Earlier investigations of double-vacuum treated windows after five years in service have shown that tributyltin oxide (TBTO) degrades to di- and monobutyltin compounds and that the resistance of the wood against decay decreases. An investigation 2.5 years later of the same windows shows that the degradation of TBTO proceeds fast. After 7.5 years in service only 15-35% of the remaining organotin co...
M-L Edlund, J Jermer, B Henningsson, W Hintze
Multiple-Phase Pressure (MPP) Process: One-stage CCA treatment and accelerated fixation process. 4. MPP compared with other processes for achieving acceptable treatment of radiata pine heartwood
1998 - IRG/WP 98-40115
Although radiata pine sapwood is very amenable to preservative treatment, it is often difficult to achieve the required standard for heartwood treatment.
A preliminary investigation showed that to achieve the NZ Timber Preservation Council minimum penetration requirements for radiata pine heartwood using the Multiple-Phase Pressure (MPP) Process, a hydraulic pressure of at least 1250 kPa for 20 m...
K Nasheri, J A Drysdale, G Durbin, M E Hedley
Exposure of preservative treated wood to terrestrial microcosms, pure cultures of fungi and in the field
1997 - IRG/WP 97-20114
Small stakes (5x10x100 mm3) of treated and untreated Pinus sylvestris sapwood were exposed in terrestrial microcosms with different soils, two taken from test fields in Sweden, one soil from a conifer forest and one garden compost soil. Stakes of the same size were also exposed to pure cultures of the brown and white rot fungi, Postia placenta and Phanerochaete chrysosporium. After exposure, weigh...
M-L Edlund
Changes in some important mechanical and physical properties of untreated and treated mining timber after exposure to the conditions of a colliery
1996 - IRG/WP 96-20082
Each of salt treated and untreated mining timber (wedge) pairs with 5x15 cm² cross-section and 155 cm length prepared from Scots pine, Bornmüller's fir and oriental beech was cut in the small standard test specimens to determine changes in some important mechanical and physical properties, 13 month after exposure to the conditions of Kozlu Hard Coal Mines in the depth of 52 m. Thus, the...
A Bobat
Surface checking of CCA-treated radiata pine decking timber exposed to natural weathering
2000 - IRG/WP 00-40165
A field trial was established at four locations in Australia to assess the effect of CCA and CCA-wax treatment on the checking (cracking) of radiata pine decking timber exposed to natural weathering. Untreated decking timber and timber that had been pressure treated with water acted as controls. After 1 year's exposure the number and sizes of checks occurring in treated timber and control...
P D Evans, P J Beutel, C F Donnelly, R B Cunningham
Potential toxicants for controlling soft rot in preservative treated hardwoods. Part 2: Laboratory screening tests using sawdust
1977 - IRG/WP 2101
A technique is described for the rapid screening of toxicants against microorganisms, represented by the brown rot, Gloeophyllum trabeum, and a natural inoculum from soft rotted wood. Sawdust, in this case from sapwood of Eucalyptus maculata, is pretreated with the candidate formulation and moistened before inoculation. Visual scoring of growth can be used to discriminate suitable candidates as ea...
J D Thornton
Differential retention and leaching of CCA (C) in sapwood and heartwood of Kenyan-grown blue gum (Eucalyptus saligna) and black wattle (Acacia mearnsii)
2005 - IRG/WP 05-30371
Retention and leaching of CCA(C) in small samples of sapwood and heartwood of Kenyan-grown blue gum (Eucalyptus saligna) and black wattle (Acacia mearnsii) were tested under laboratory conditions. Clear samples (100mm x 30mm x 40mm) were removed from the sapwood and heartwood of sampled defect-free and sound plantation trees of the two species. These were separately air-dried to 15% MC, end-seal...
R Venkatasamy
Micromorphological and chemical changes of archaeological woods from wrecked ship's timbers
1987 - IRG/WP 4136
Micromorphological and chemical alterations of sea-waterlogged woods obtained from the ship-wrecked materials which had been submerged in Yellow Sea for over 700 years were investigated. The woods were deteriorated in varying degrees by marine organisms depending on species and parts of the woods. Under the light and scanning electron microscope the morphological characteristics of deteriorated wo...
Y S Kim
The degradation of wood surfaces by dilute acids
1985 - IRG/WP 3326
Thin radial/longitudinal sections(~100 µ) of Corsican Pine (Pinus nigra) and Lime (Tilia vulgaris), were exposed to Sulphuric, Sulphurous, nitric, acetic, and formic acid at 40°C in the pH range 2-6. After about 3 months exposure to Sulphuric, nitric, acetic and formic acid at pH 2.0 Pine lost some 20-25% of its tensile strength. Losses in tensile strength due to sulphurous acid were greater bei...
P D Evans, W B Banks
An analysis of the effects of some factors on the natural durability of pine (Pinus sylvestris L.) and spruce (Picea abies Karst.)
1986 - IRG/WP 1279
The effects of some factors on the natural resistance of pine and spruce sapwood against fungal decay and against attack of house-longhorn beetle larvae have been studied in laboratory tests and the results are evaluated by analysis of variance and regression analysis. Following conclusions were reached: Wood from summer-felled trees did not have a lower inherent natural durability against fungal ...
J B Boutelje, T Nilsson, S Rasmussen
Effect of aqueous polymer treatments on wood properties. Part 1: Treatability and dimensional stability
1990 - IRG/WP 3610
Partially air-dried sapwood of sweetgum (Liquidambar styraciflua) and southern pine (Pinus spp.) was treated with either aqueous polyacrylate or aqueous dimethyloldihydroxyethyleneurea (DMDHEU) solutions. Tests for dimensional stability were conducted on matched treated and untreated pieces. Measurement of the antishrink efficiency indicated that DMDHEU was a better stabilizer than the polyacrylat...
Z Ashaari, H M Barnes, R C Vasishth, D D Nicholas, D E Lyon
The fixation of copper in Pinus sylvestris using the sodium salts of two polyhydroxycarboxylic acids
1992 - IRG/WP 92-3706
As part of the research concerned with the development of fixed, copper based preservatives, the salts of polyhydroxycarboxyIic acids, have been used in copper sequestration studies and fixation trials in Pinus sylvestris splinters. Selected compounds have been shown to be effective sequestrants at low concentrations allowing alkaline solutions to be formulated. Leaching trials following a 48 hour...
M Bacon, J A Cornfield
Le pin: Matériau à contact alimentaire [Pine wood as a material for food contact]
1995 - IRG/WP 95-50040-01
Monoterpenes emitted to air from woods of pine (Pinus nigra, Pinus laricio, Pinus pinaster and Pinus sylvestris) were determined on the one hand by static analysis and by other hand by sampling on the Tenax adsorbent, followed by analysis using thermal desorption, both being combined with gas chromatography coupled with mass spectrometric detection. The major monoterpenes were alpha-pinene and 3-c...
A Waymel, M Lamour, G Labat
Permatek IM 30 as a termiticide treatment for veneer-based wood products
2003 - IRG/WP 03-30325
Permatek IM 30 is a termiticide designed for incorporation into wood products during manufacture.
Whereas existing approved products in Australia are based predominantly on synthetic pyrethroids carried in solvents, Permatek IM 30 is based on imidacloprid, a neonicotinoid insecticide. The formulation has very low mammalian toxicity, is free of VOCs, and has been successfully tested as a glueline ...
J Doyle, K Webb, W R Rae, A F Siraa, J Malcolm-Black
Termite resistance of treated wood in an above-ground field test
1986 - IRG/WP 1300
This paper provides an update on the results from an above ground field test evaluating the effectiveness of wood preservatives against subterranean termites. Results for the one and two year inspections of treated southern pine sapwood exposed in Hawaii to Coptotermes formosanus are presented. Chromated copper arsenate is providing excellent protection as is the pyrethroid deltamethrin. Borate an...
A F Preston, P A McKaig, P J Walcheski
Examination of preservative-treated Pinus sylvestris using electron paramagnetic resonance
1992 - IRG/WP 92-3710
EPR is currently being used to help elucidate the nature and extent of the chemical reactions occurring between wood and copper based timber preservatives. In the work reported here treated Scots pine samples were examined at room temperature and in the frozen state. Plots of the electronic parameters A|| vs. g|| were found to be a useful index of the electronic properties of the various formulati...
A S Hughes, R J Murphy, J F Gibson, A J Cornfield
Penetration and absorption of water-borne preservatives in conifers from the Western United States: A preliminary report
1988 - IRG/WP 3475
The treatment of most softwoods from the western United States with waterborne chemicals poses a major challenge. Although many of these species are commercially treated with waterbornes, there is considerable debate about their treatability. At present, there is little or no information on the treatability of western wood species with waterborne chemicals. The lack of accurate treatability inform...
S Kumar, J J Morrell
The effect of moisture content on the electrical resistance of timber as detected by a pulsed current reistance meter (Shigometer)
1984 - IRG/WP 2212
The literature concerning the use of the Shigometer® for detecting decay in standing trees and wood poles is reviewed and the differences of opinion over the effect of timber moisture content on electrical resistance are highlighted. A simple experiment designed to test this effect is described and the implications of the results for testing poles in service are discussed. There was a large diffe...
P I Morris, D J Dickinson
Shorter-term biological control of wood decay in pre-seasoning pine roundwood as an alternative to chemical methods
1992 - IRG/WP 92-1555
Previous studies on the long-term control of decay in creosoted transmission poles, using Trichoderma and other antagonistic moulds, have met with limited success. However, it is possible biological control is more suited to control of decay on shorter time scales. An earlier study, focusing on pre-seasoning treatment of transmission poles showed that favourable porosity increases could be brought...
M W Schoeman, D J Dickinson
Depletion of preservatives from treated wood: Results from laboratory, fungus cellar and field test
1993 - IRG/WP 93-50001-07
This paper compares results of preservative component losses using a range of test procedures with several different water-borne preservatives. The data shows that laboratory leaching tests are in some cases comparable to, but in other cases significantly underestimate preservative component losses when compared with field or fungus cellar depletion tests. The results also suggest that preservativ...
L Jin, A F Preston
Influence of the content of organic matter of soil on the degradation of wood by soft rot fungi
1970 - IRG/WP 27
The degradation of wood specimen burried in the soil by soft rot fungi is influenced by a number of factors. These are in particular the water holding capacity, water content, content of organic matter, pH, content of mineral nutritive substances etc. The results of the interlaboratory tests, carried out within the IRG/WP let presume that the intensity of wood degradation occurs proportionally inv...
O Wälchli
An investigation of the nutritional physiology of the wood-boring weevil Euophryum confine Broun
1994 - IRG/WP 94-10082
The digestion of Picea abies Karst and Pinus sylvestris L. by Euophryum confine, at two sites is reported in this study. The composition of sound wood, wood from the heads of the weevil tunnels and the frass egested has been determined by gravimetric analysis. A comparison of sound wood and wood ingested showed that weevils tunnelled in microbially decayed wood, while a comparison of the wood inge...
A J Pitman, S M Cragg, G S Sawyer
Factors affecting decay rates in a fungus cellar
1985 - IRG/WP 2242
Birch and pine stakes treated with chromated copper arsenate and didecyldimethylammonium chloride were incubated in two soils in a "Fungus Cellar" test. At three month intervals, sets of stakes were inspected and assigned visual ratings or removed from the soil beds for weight loss determination. Preliminary results after nine months exposure have shown differences in the decay rates between birch...
P A McKaig