Performance of wood decking after 5 years of exposure: verification of the combined effect of wetting ability and durability
2019 - IRG/WP 19-20647
Wood is one of the most important construction materials and its use in building applications has further expanded in recent decades. In order to enable even more extensive and reliable use of wood, factors affecting wood’s service life need to be understood. More recently, a new concept to characterize the durability of wood-based materials and to predict the service lives of wood was proposed,...
M Humar, D Krzisnik, B Lesar, C Brischke


Performance of naturally durable decks after 15 years of field exposure
2020 - IRG/WP 20-10963
A decking test of Canadian species considered to be naturally durable was inspected after 15 years of exposure at test sites in Ontario and British Columbia. Based on the materials used in this experiment, Douglas-fir and yellow cypress had the greatest decay resistance, followed by eastern white cedar and western redcedar, and then by western larch and tamarack. All materials tested were more dur...
R Stirling, D Wong


Shelling of flat and profiled western larch deck-boards exposed to natural weathering
2024 - IRG/WP 24-40997
Shelling is a severe type of raised grain that occurs at the surface of deck-boards made from wood species that have growth rings with pronounced differences in density between earlywood and latewood, for example southern pine (Pinus spp.). Shelling is more severe in deck-boards fixed with their growth rings oriented pith-side-up (concave) rather than bark-side-up (convex). Far less is known about...
L H Leung, P D Evans


Evaluation of mass timber materials for military and commercial trailer decking
2024 - IRG/WP 24-41009
In this study, CLT trailer decking was manufactured to current military trailer decking specifications, verified using PRG320 performance criteria, and treated with either waterborne or oil borne wood preservatives. Preliminary results show adequate uptake of preservative solution and subsequent testing shows minimal effect due to treatment. Field durability tests are also being conducted of treat...
G Kirker, A Senalik, X Wang, K Ohno, R Arango, M Mankowski, X Xie, J Eskola, N Kamprath, S Karwaczynski, M Weaver


Copper migration from preservative-treated Douglas-fir decking: models vs laboratory leaching data
2024 - IRG/WP 24-50390
The ability of a model to predict copper migration from Douglas-fir treated with organic metallic substances into a freshwater slough was evaluated against data generated through simulated overhead leaching. The model predicted very high loadings of ammoniacal copper zinc arsenate, alkaline copper quaternary or copper azole that had the potential to impact water quality while data from the exper...
M J Konkler, G Presley, J J Morrell, T Singh


Previous Page