An experimental method to simulate incipient decay of wood by basidiomycete fungi
2000 - IRG/WP 00-20200
At very early stages of decay of wood by basidiomycete fungi, strength loss can be measured from wood before any measurable weight loss. Therefore, strength loss is a more efficient measure of incipient decay than weight loss. However, common standard decay tests (e.g. EN 113 or ASTM D2017) use weight loss as the measure of decay. A method was developed that allowed progressive removal of samples ...
S F Curling, J E Winandy, C A Clausen


Ancillary properties of vapor boron-treated composites
2001 - IRG/WP 01-40210
This paper discusses the water absorption, thickness swelling, and internal bond strength of North American composites treated using a vapor boron treatment process. For oriented strandboard, high boron loadings led to lower internal bond strength and lower thickness swelling. Water absorption results were variable but no deleterious effect of treatment was noted. For medium density fiberboard, th...
W A Jones, H M Barnes, R J Murphy


Natural durability of eight tropical hardwoods species from Africa
2005 - IRG/WP 05-10563
Current forest inventory results reveal that there are more than 700 hundred-hardwood species in tropical forests, of which less than 10 percent are harvested and used for commercial purposes. The increased use of lesser-known species can decrease the pressure on current commercial species, increase the value of the forest and lead to better management practices. However basic information on physi...
P Nzokou, K Wehner, D P Kamdem


A short note on the subject of pretreatment decay in wood
1984 - IRG/WP 1245
The paper reviews five national standards for wood utility poles and some literature that concerns the problems of pretreatment decay. Finally it is proposed to form a new sub-group to study that problem....
J A Taylor


A deflection test for monitoring decay in miniature beams
1986 - IRG/WP 2269
A laboratory apparatus for assessing decay in small stakes is described. It involves the measurement of deflection in a static bending apparatus using a displacement transducer linked to a microcomputer. Measurements are non-destructive, rapid, accurate and automatic and decay can be assessed repeatedly over long time periods....
S M Gray


Dimensional stability, biological resistance, and mechanical properties of phenol-resin-treated particleboard
1990 - IRG/WP 3622
Particleboards were treated with a low molecular-weight phenol-formaldehyde (PF) resin and their enhanced properties were evaluated. Besides dipping of particles in aqeous solutions of resin, and spraying of resin solutions before spray of the conventional phenol-formaldehyde resin for adhesive binder, one step treatment by spraying of the mixture of the low molecular-weight resin and the adhesive...
Y Imamura, H Kajita


Acetylation of lignocellulosic materials
1989 - IRG/WP 3516
A simplified procedure for the acetylation of lignocellulosic materials has been developed. The acetylation is done with a limited amount of liquid acetic anhydride without the addition of a catalyst or an organic co-solvent. Dimensional stability and biological resistance are both much improved by the acetylation. Equilibrium moisture content in acetylated material is considerably lower than in u...
P Larsson, A-M Tillman


Development of an Australasian protocol for assessment of wood preservatives
1994 - IRG/WP 94-20043
The Australasian Wood Preservation Committee (AWPC) is currently developing a suite of assessment procedures (protocols) for the biocidal efficacy of wood preservatives for approval in Australasia (Australia, New Zealand, Papua New Guinea, Fiji). Protocols are being prepared for the six hazard levels recognised in the relevant standards of member countries and represent the minimum procedures requ...
W D Gardner, H Greaves, M E Hedley, K J McCarthy, J Norton


The present classification of wood degradation factors
1993 - IRG/WP 93-10031
Contemporary classification of biotic and abiotic wood degradation factors is presented in two aspects: etiological and simptomatical one....
J Wazny


An evaluation on durability of untreated mining timber support
1997 - IRG/WP 97-20121
Wedge blocks in dimension of 5 x 7 to 8 x 155 cm3 were cut from indigeneous scots pine pitprops. Each of wedge block pairs were numbered and half of them were placed as the test blocks between the steel arches and the strata in a hard coal pit. Controls in laboratory and test wedge blocks in the mine were then sawn into 20 by 20 by 300 mm standard test sticks. Impact bending, static bending and MO...
A Bobat


Methods of assessing decay in poles in service with the Pilodyn wood tester
1978 - IRG/WP 2107 A
H Friis-Hansen


A method of predicting the average life of field tests on preservative-treated stakes
1977 - IRG/WP 297
The paper presents an analysis of the results of completed field stake tests on untreated and preserved timber, and develops a method of predicting the average life of incomplete stake tests on wood preservatives from the failures that have occurred so far....
D F Purslow


Results of field tests on the natural durability of timber (1932-1975)
1976 - IRG/WP 3105
This paper describes a continuing field stake trial to determine the natural resistance of different species of timber to decay. Data are presented for about 180 timbers, covering over 6000 stakes, and the results are discussed in terms of a natural durability classification....
D W Purslow


Use of the Pilodyn to assess deterioration of treated aspen waferboard after 30 months of outdoor exposure
1986 - IRG/WP 2254
Samples of preservative treated aspen waferboard exposed outdoors for 30 mo. were compared using pin penetrations of the 6 Joule Pilodyn. These results correlated well with rankings of treatment performance based on more laborious standard mechanical tests, and demonstrate the potential for use of the Pilodyn as a tool to evaluate wood composites in test exposures with minimal destruction....
E L Schmidt, M G Dietz


Mechanical resistance of Pinus radiata CCA treated and face jointed with PVA adhesive
1999 - IRG/WP 99-40140
Due to the increased use of Pinus radiata timber composites (laminated structural members, panels, etc), its low natural durability and the toxicity of phenol-formaldehyde type adhesives, a PVA (polyvinyl acetate) adhesive was evaluated in machined and rough CCA treated and untreated face joint samples under DIN 68602 (EN 204-205) standard for groups of requirement 3 and 4. The results showed that...
M C Rose, L Reyes, P León


A Preliminary Report on the Properties of Engineered Wood Composite Panels Treated with Copper Naphthenate
2005 - IRG/WP 05-40294
This paper reports on our preliminary investigation of the properties of randomly oriented strandboard which had waterborne or powdered copper naphthenate (CuN) incorporated into the board during manufacture. When compared to zinc borate-treated controls (ZnB), the mechanical properties of strandboard (MOR, MOE, work-to-maximum load, internal bond strength) were not adversely affected by treatmen...
J W Kirkpatrick, H M Barnes


Decrease of the antidecay resistance of beech wood treated with organotin fungicides after its natural ageing
1998 - IRG/WP 98-30185
The antidecay resistance of beech-wood samples (120 x 8.5 x 8.5 (MM)) treated with tributyltin fungicides gradually decreased due to prolongation of their natural ageing: tributyltin fungicides (TBTO, TBTS, TBTCA, TBT-DEDTK were applied by pressure impregnation technique in ethanole solutions (c = 0. 1%, 0.33% or 1%); treated beech-wood samples were naturally aged without their contact with grou...
L Reinprecht


Effect of soft-rot decay on the static bending strength of wood
1991 - IRG/WP 2361
In this study, a modified static bending test has been developed as a method for measuring soft-rot decay in soil bed studies. A good correlation was found between the strength loss of the southern pine test specimens and extent of decay. This data suggests that it may be possible to develop a dynamic test based on stress relaxation that is more sensitive than static bending....
D D Nicholas, J A Wilson, R C Vasishth


A simple non-destructive means of testing poles in situ
1982 - IRG/WP 2167
Anonymous


Japanese Classification of Wooden Building Members for ISO Use Classes according to the Building Code in Japan.
2006 - IRG/WP 06-20337
Because of the international approve of use class system for the biological degradation of wood by ISO/DIS 21887 and ISO/DIS 21892, Japanese committee of ISO/TC165/SC1 asked to the JWPA for classify the wooden commodities by use class of these draft ISO. The JWPA was prepared a draft use class model in Japan. Japanese building code systems are described and Japanese draft use class system is also ...
K Suzuki


Natural Durability Classification Systems Used Around the World
2009 - IRG/WP 09-10694
Around the world natural durability is classified in different ways. The nature and rigor of the tests used to measure durability, the method of classification based on these data, and use of these classifications to specify end uses or predict service life all vary. This can lead to confusion among people not familiar with the various systems used. This review describes the methods used to classi...
R Stirling


Chapter 6 - Preservatives of bamboo
2007 - IRG/WP 07-10635-06
Almost all currently available oil-borne, water-borne and compound types of preservatives suitable for the preservation of bamboo or wood have been described along with their classifications, applications, formulations, merits and demerits, history of invention or discovery and development. The preservatives suitable for wood are also considered suitable for bamboo....
A K Lahiry


Relationship between bond strength and surface characteristics of CCA-treated Douglas-fir
1993 - IRG/WP 93-30008
Chromated-copper-arsenate (CCA) treated Douglas-fir was laminated using a commercial phenol-resorcinol resin. CCA treatment enhanced the water repelleney of wood espeeially in the presence of extractives. However, the shear strength of CCA treated wood was 12% lower in dry condition and 38% lower in wet condition after six cycles of vacuum-pressure test than that of untreated wood. Slight removal ...
K Yamamoto, J N R Ruddick


Accelerated laboratory soil contact decay test using soil amended with composted wood
2004 - IRG/WP 04-20284
The effect of amending soil with wood compost on the decay rate of wood wafers in contact with the unsterile soil, as measured by radial compression strength loss, was explored. It was found that the addition of composted wood to the soil significantly increased the wood decay rate. The reason for this acceleration in wood decay is not entirely clear, but appears to be at least partially associate...
D D Nicholas, H Borazjani, T Schultz


Treatment of wood with formaldehyde. Acid catalysis of the reaction between formaldehyde and wood
1980 - IRG/WP 3146
Formaldehyde reacts with the free OH-groups in wood forming cross-linking bonds. The reaction can be brought about without any catalyst but in that case the activation energy is very high and high temperatures and long reaction times are needed. Normally, the reaction is catalysed by different acids. Acid catalysts, however, tend to degrade the cellulose and the wood matrix causing reduction in th...
T Vihavainen, K Piispanen, P Mansikkamäki