Studies on the preservation of structrual plywood - Part 1: Decay resistance of structural plywood
1974 - IRG/WP 238
The weight loss and the decreases in the compression strength and in the modulus of elasticity were measured to determine the decay resistance of structural plywood (lauan). Test pieces (50x25xA mm³) were exposed to the wood destroying fungi (Coriolus versicolor and Coriolellus palustris) for 2-3 or 2-4 months. After exposure, the measurement of the compression strength was carried out on the pie...
K Minami, Y Kenjo, S Sugiyama


Preliminary study of the fungicidal and structural variability in copper naphthenates and naphthenic acids
1996 - IRG/WP 96-30114
Copper naphthenates, an oil-borne wood preservative listed by the American Wood-Preservers' Association (AWPA), is manufactured by complexing copper(II) with naphthenic acids. Prior to AWPA listing as a wood preservative, field experiments showed that copper naphthenates generally had good stability and were active against wood-destroying organisms. Recently, however, there have been reports ...
T Schultz, D D Nicholas, L L Ingram Jr, T H Fisher


Ultra-structural observations on the degradation of wood surfaces during weathering
1987 - IRG/WP 2280
Radiata pine (Pinus radiata D. Don) sapwood was converted into blocks with a transverse face about 5 mm square and measuring 8 mm longitudinally. Transverse (T.S.), Radial (R.L.S.) and Tangential (T.L.S.) surfaces were prepared and specimens exposed to the weather inclined at 45° facing equatorially for periods of between 20-60 days. After 30 days exposure erosion of the middle lamella was observ...
P D Evans, S Thein


Evidence supporting the use of termite baiting systems for long-term structural protection
2000 - IRG/WP 00-10377
The efficacy of the Sentricon Colony Elimination System containing Recruit II termite bait (0.5% hexaflumuron) in controlling active subterranean termite infestations has been demonstrated in numerous studies. This baiting system and other termite baiting systems are now widely used, and generally accepted, tools for remedial termite control in North America, Hawaii, and other parts of the world. ...
J K Grace, N-Y Su


Insect resistance of preservative treated tropical plywood against Lyctus
1990 - IRG/WP 1453
Seven plywood types composed of tropical wood species, vulnerable to Lyctus, were treated with various commercial water-borne and oil-borne preservatives. A wide range of preservative retentions was obtained by treating boards with dip treatment, steeping, double-vacuum and vacuum-pressure impregnations. Selected samples were subsequently tested for their insect resistance against Lyctus africanus...
J Van Acker, M Stevens, M Pallaske


Non-pressure treatability of plywood by CCA, CCB and boron
2005 - IRG/WP 05-40295
Study on diffusibility and absorbability of CCA, CCB and boric acid in 3 mm thick 3-ply hardwood plywood at water saturated and air-dry conditions and dipped at same concentration (5%) and same duration of time (12 hours) revealed complete diffusion of all the preservatives at water saturated condition. Only the CCA-C was found absorbed by the plywood at air-dry condition. The rate of absorption a...
A K Lahiry


Effects of various preservative treatments on the mechanical and physical properties of plywood
1993 - IRG/WP 93-40007
The technical properties of plywood are related to both the intrinsic characteristics of its composing wood species and the quality and performance of the glue bond which acts as an interface between veneer sheets. Consequently mechanical and physical testing and glue bond strength analysis offer an appropriate means for studying the effect of preservative treatments on the overall quality of plyw...
J Van Acker, M Stevens


Treatability of plywood containing intermountain Douglas fir veneers
1982 - IRG/WP 3203
Eighteen sheets of plywood were obtained which contained intermountain Douglas-fir veneers from two regions of British Columbia. Following pressure treatment with chromated copper arsenate (CCA type C) and ammoniacal copper arsenate (ACA) the preservative penetration and retention in individual veneers was assessed. It was concluded from the study that the intermountain Douglas-fir veneer could no...
J N R Ruddick, A Walsh


On the occurrence of the Australian Lyctus parallelocollis Blackburn in Israel and how to distinguish from Lyctus brunneus (Steph.)
1978 - IRG/WP 194
In June 1976 attacked plywood was sent from Tel Aviv for determination of the insects concerned. An unknown Lyctus species and the asiatic Heterobostrychus aequalis (Waterhouse) were responsible for the damage. Further material sent by Dr. J. Halperin, Forestry Division, Ilanoth, in September 1976 and beetles of his field collection in 1977 revealed this Lyctus sp. to be a rather widely distribute...
S Cymorek


A direct method for testing plywood and particle boards against fungal decay
1984 - IRG/WP 2214
A method directly inspired from the French standard testing method of the resistance of particle boards against fungal decay (AFNOR N° 51.295 May 1980) is described. But in that experimentation, the infestation is localized and realized in non sterile conditions. Small blocks of Fagus sylvatica (60 x 20 x 10 mm³) used as " inoculates " are infested with basidiomycetes, in Kolle flask for 4 to 6 ...
L N Trong


Mycological testing of plywood and board materials. Part 1: Review of information supplied by IRG members
1978 - IRG/WP 284
In December 1975 IRG members were asked for published information, information of current work in progress and views on mycological test methods for board materials. The object was to stimulate discussion and possibly establish a joint research effort within IRG in order to establish a meaningful test with reproducible results....
C R Coggins


Resistance to soft rot of hardwood plywood treated with CCA salt
1983 - IRG/WP 3258
Plywood made from indigenous hardwoods was treated at an average loading of 34 kg Celcure A per m³ and was installed in a field test. After 20 years the samples were only slightly attacked by soft rot and the glue bonds were still intact....
R S Johnstone


Volatile borates in the treatment of wood and wood based panel products against subterranean termites
1995 - IRG/WP 95-30094
Blocks of pine solid wood, oriented strand board and plywood were treated with trimethyl borate by vapour treatment. It was meant to obtain either a full impregnation of the specimens or a shell treatment of the outer three millimetres. The efficacy of the treatments against subterranean termites (Reticulitermes lucifugus) was evaluated using an European Standard method....
L Nunes, D J Dickinson, R J Murphy


A laboratory soil-block decay evaluation of plywoods edge-treated with preservatives
1982 - IRG/WP 2174
Preservative-treated plywood used under conditions or severe decay hazard frequently has its original, or cut edges, protected by the application of a field-cut preservative. This study uses a laboratory test method to compare the efficacy of four commercial preservative treatments against two commonly occurring brown-rot fungi. The results are not meant to indicate the service life of such treate...
R S Smith, A Byrne


Étude in vitro de la colonisation et de la dégradation structural du bois de hêtre par Coriolus versicolor (L.) Quélet
1976 - IRG/WP 158
L'attaque du bois de Hêtre par Coriolus versicolor (L.) Quélet, agent de pourriture fibreuse blanche est étudiée après des périodes d'exposition à ce champignon variant de 15 jours à trois mois. L'observation des premiers stades, c'est à dire de la colonisation du bois par les filaments de champignon est faite en microscopie optique, puis au fur et à m...
D Dirol


Thirty-four year test of on-site preservative treatments to control decay in wood above ground
1993 - IRG/WP 93-30015
This research was initiated in 1958 to investigate efficacy of various preservatives and treating methods for new lumber going into exterior structures of buildings. Post-rail units (2x4 inches) constructed of Southern Pine sapwood, Douglas-fir heartwood, and mill run western hemlock were dip- or brush-treated before or after assembly. Units were trested with pentachlorophenol in various petroleum...
T L Highley, T C Scheffer


Performance of treated spruce in Canadian field test sites
1989 - IRG/WP 3506
Spruce material under test in Canadian field test sites is performing better than anticipated. From the comparison of the performance of spruce treated with various preservatives, it appears that penetration may be far more important on durability performance than the preservative itself or the retention of preservatives in the wood. However, there is still insufficient data on the influence of pe...
J P Hösli, E E Doyle


The development of a screening method for the activity of pyrethroids against wood boring marine crustaceans, Limnoria spp
1978 - IRG/WP 443
The present work is concerned with the develepment of a suitable bio-assay technique to determine the biological activity (contact action) of pyrethroids against Limnoria spp. Estimates of the toxicity of three pyrethroids, permethrin, cypermethrin and decamethrin (the structures of which are shown in Fig. 1.) to the marine borer have been obtained....
D Rutherford, R C Reay, M G Ford


Biocide Treatments for Wood Composites - A Review
2006 - IRG/WP 06-40323
This paper reviews the biocidal treatment of wood composites. Included are in-process and post-process treatments. Various biocides are covered as are methods of application. Novel treatments and technologies are also presented....
J W Kirkpatrick, H M Barnes


Laboratory evaluation of phoxim in plywood
2001 - IRG/WP 01-30264
Two types of phoxim treated plywood bonded by phenolic resin glue and urea resin glue were challenged with termites of Coptotermes formosanus Shiraki in laboratory. It was found that the sawdust of phoxim treated plywood bonded by phenolic resin glue was not active or did not kill termites of Coptotermes formosanus Shiraki within the test period. Moreover, the phoxim treated plywood bonded by phen...
Zhong Junhong, Lin Liling, Huang Hong


Natural durability of some common Indian timbers and marine plywood against biodeterioration in Kochi waters (India)
1992 - IRG/WP 92-4177
Panels of thirty-eight timber species and marine plywood were tested in Kochi harbour (South-west India) for periods ranging from 3 to 21 months, so as to evaluate their natural resistance against marine borers. Results indicate that all the timber species studied are non-durable, 6 of them having undergone more than 50% internal destruction within 3 months; 14 species in 6 months, 13 species and ...
L N Santhakumaran, M V Rao


Bending properties of treated western hemlock plywood
1996 - IRG/WP 96-40064
This study investigated the mechanical properties of western hemlock plywood after treatment with waterborne preservatives and redrying. Unlike previously reported results for southern pine plywood, western hemlock plywood was more sensitive to redrying temperature than to preservative treatment. Generally, western hemlock plywood was affected by temperature and other variables. Losses in mechanic...
H M Barnes, A Khouadja, D E Lyon


A Soil Bed Test of the Effect of CCA Penetration on the Performance of Hem-fir Plywood
2004 - IRG/WP 04-30332
An accelerated decay test was set up to compare the performance of CCA-treated Western hemlock/amabilis fir plywood treated to meet the preserved wood foundation (PWF) retention standard with various patterns of preservative penetration. Short lengths of treated plywood and comparable untreated material were installed in a soil bed. After eleven years of exposure, the CCA treatments were all sou...
P I Morris, J K Ingram


Bending creep test of plywoods under long term exposure to fungal attack
1981 - IRG/WP 2163
Bending creep test and decay test were coupled in order to evaluate the durability of structural plywoods and preservative efficacy. Experimental blocks, 5.0 x 1.2 cm² section x 35.0 cm length, were impregnated with distilled water and inoculated with mycelial fragments of test fungus. Polyethylene bags stretched with metal frame were used as decay chambers. The chambers containing inoculated blo...
M Takahashi


Decay Resistance and Bonding Properties of Structural Flakeboard
2002 - IRG/WP 02-40233
Experimental structural flakeboard panels consisting of differing furnishes and resins were produced and tested for internal bond, linear expansion, thickness swell, and decay resistance. One group of panels was produced with recycled CCA-treated wood as the furnish and commercial phenol formaldehyde (PF) resin as the binder. Other groups of panels were produced with either mixed hardwoods or so...
T F Shupe, Chung-Yun Hse


Next Page