Soluble nutrient content in wood and its susceptibility to fungal discoloration and decay in above ground and ground tests
2000 - IRG/WP 00-10336
The objective of this comprehensive study was to reveal the impact of soluble nutrients in wood on its susceptibility to fungal discoloration and decay in various tests, which is important for the test methodology and standardisation. Seven tests were carried out including pure culture above and ground contact tests, above ground field test and laboratory ground contact tests. The samples containi...
O M Caballero, N Terziev


Association of contents of nitrogen and sugars in rubberwood (Hevea brasiliensis) clones with susceptibility to sapstain by Botryodiplodia theobromae, Aureobasidium pullulans and Aspergillus niger
1999 - IRG/WP 99-10307
The purpose of this study was to determine if nitrogen and sugar contents in rubberwood from three selected varieties (clones) rubber trees would affect the rate of colonisation by Botryodiplodia theobromae (a tropical sapstain fungus), Aureobasidium pullulans (a temperate sapstain fungus) and Aspergillus niger (a common mould fungus). Sapstain growth was rated daily until at least 50% mycelial co...
A J Ashari, J W Palfreyman, A H H Wong


A technique for the rapid assessment of wood surface degradation during weathering
1987 - IRG/WP 2281
Radiate pine (Pinus radiata D. Don) sapwood samples taken from four trees were converted into thin strips 100 x 10 x 0.085 (85 µm) mm³, (longitudinal x radial x tangential) in size and exposed in preweighed hatches to the weather inclined at 45° facing equatorially for 10, 20, 40, 60, 80 and 100 days. Significant (P < 0.001) weight losses occurred with time over the exposure period. Differen...
P D Evans, D Abbott, S Thein


Aspects of leaching
1976 - IRG/WP 267
With respect to Document No: IRG/WP/246, and the recommendation that an economic leaching test can be based on a non-changing volume of water (500 ml/block), I would like to relate our experiences with this suggestion. Following 14 days of continuous immersion in de-ionized water it was found that blocks treated with moderate and above concentrations of a preservative gave no problems, but those b...
R S Smith


Blue stain in service on wood surface coatings. Part 1: The nutritional requirements of Aureobasidium pullulans
1992 - IRG/WP 92-1556
The nutritional requirements of Aureobasidium pullulans was examined with regard to nutrient sources that are potentially available in fresh and weathered wood. The study was designed to determine how far wood cell wall components need to be broken down during weathering before they provide a useful nutrient source for Aureobasidium pullulans. Various carbon sources were tested, with eight differe...
P R Sharpe, D J Dickinson


The importance of blue stain attack for the colonization by wood-rotting fungi of wood not in contact with the ground
1988 - IRG/WP 1349
When used in constructions not in contact with the ground, wood has been shown often to proceed from blue stain to moulds. The appearance of wood rotting fungi is normally delayed. Solid wood artificially inoculated with the blue stain fungus Pullularia pullulans was shown to permit germination of Pycnoporus cinnabarinus basidiospores. This was demonstrated by the use of an indirect and a direct b...
J Bjurman


An examination of the potential for the use of the Maillard reaction to modify wood
2018 - IRG/WP 18-40829
Finding efficient ways to decrease wood decay caused by fungi and increasing its dimensional stability is an important issue in the timber construction. A possible way to avoid wood decay by fungi is by reducing the water content of wood, since water is a primary condition for fungal growth. Bulking of the wood cell wall by chemical reagents occupies the space where water normally occurs. At the s...
K Peeters, E Larnøy, A Kutnar, Č Tavzes, C A S Hill