Your search resulted in 548 documents. Displaying 25 entries per page.
The influence of thermal modification and surface charring to different levels on wettability of Norway spruce wood
2022 - IRG/WP 22-40942
The wood can alternatively be protected from water absorption by thermal modification and charring. Both techniques cause certain chemical and physical changes in the wood, the extent of which depends on the level of temperature applied. The objective of this study was to determine how the combination of charring to different levels and thermal modification affects the chemical, morphological, and...
J Žigon, C Gerardin, M E P Wålinder, P Gerardin
Utilization of Pressure Treated Lumber in Cross Laminated Timber Manufacture and its Impact on Bondline
2022 - IRG/WP 22-40953
Mass timber building construction is increasing dramatically across North America which presents challenges to these structures not seen in Northern Europe. Large parts of the United States harbor termites and existing mass timber building technologies that rely solely on moisture exclusion to increase durability are insufficient in these areas. The successful expansion of mass timber construction...
G Presley, C Wainscott, J Valenti, S Noble
Assessment of the Material Durability and Structural Integrity of the Wooden Velodrome in Češča vas, Slovenia
2023 - IRG/WP 23-11012
Wood is a widely used material in the construction industry, and it has been utilized for thousands of years to create buildings and other structures. When wooden structures are designed, built, and maintained properly, they can be safe and long-lasting. Sports facilities, which provide athletes with a space to train, compete, and improve their abilities, are crucial in creating a strong and susta...
D Kržišnik, M Humar, B Lesar
Identifying compatible waterborne timber preservatives and fire retardants for use in a VPI system: a practical approach
2023 - IRG/WP 23-30796
To enhance the use and suitability of timber in all applications in both exterior and interior settings, timber typically needs to be treated with a preservative and/or a fire retardant chemical. Combining fire retardants with preservatives into a single treatment process has been a long-term aim of researchers in the timber preservative industry because of the significant logistic and economic ad...
R Robinson, S Meldrum
Biological durability and wood-water interactions of sorbitol and citric acid modified wood – Effects on the expected service life
2023 - IRG/WP 23-40960
A high level of research activities on sorbitol and citric acid (SorCA) modified wood has been recognized in Europe over the last few years. As this treatment is close to entering an industrial-scale production, it is of interest to investigate how such treated wood performs upon long-term outdoor exposure. Hence, in this study Scots pine (Pinus sylvestris L.) sapwood was modified with aqueous sol...
K Kurkowiak, L Emmerich, H Militz
Non-vacuum/pressure ACQ treatment
2023 - IRG/WP 23-40971
Many developing countries are located in sub-tropical or tropical regions where rapid wood deterioration results in early failure of many structures. Whilst preservative treatment would help to reduce these losses and extend the forest resource commercial vacuum pressure treatment systems are often too expensive. The use of lower technology treatment systems, while not as quick as vacuum pressure ...
J Norton
Short-term absorption of water and coatings on thermally modified blue-stained spruce wood
2023 - IRG/WP 23-40984
The importance of wood has been increasing in the last decades. Among conifers, predominantly spruce (Picea abies) wood is often used in building constructions in Europe. Namely for construction and facades of buildings, decking and fences. Due to the increased public concerns about biocides, alternative techniques for protection, such as thermal modification and protection by construction, are ga...
R Hasanagic, M Bahmani, M Humar, L Fathi, L Cai
Characterization of cell wall morphology and water-soluble extractives in Japanese larch decayed by white-pocket-rot fungi
2024 - IRG/WP 24-11034
Porodaedalea chrysoloma (Fr.) Fiasson & Niemelä is a basidiomycete that can cause white-rot decay in Japanese larch (Larix kaempferi) heartwood. P. chrysoloma is a white-rot fungus with a unique pattern that causes white-pocket-rot in the xylem of Japanese larch. However, the mechanism by which P. chrysoloma yields the pattern of white-pocket-rot in Japanese larch heartwood remains unclear. Thus,...
Y Mori, H Arai, T Ito, H Hashitani, K Yamashita, Y Ota, M Kiguchi
Intra-species variability of moisture dynamics in wood
2024 - IRG/WP 24-11040
Moisture dynamics of wood and wood-based materials play a major role in wood durability against different decay organisms. Their impact becomes particularly evident when wood is exposed, but not permanently wet. To date, however, this has only been taken into account indirectly and therefore inadequately when testing the durability of wood. While test methods are available, for example to determin...
C Brischke, H Purps, L Emmerich
Surface treatment of cross-laminated timber to improve water repellency and UV resistance
2024 - IRG/WP 24-20716
Cross-laminated timber (CLT) has emerged as a revolutionary building material, offering a sustainable alternative to traditional construction methods. By layering and bonding multiple layers of wood at right angles, CLT creates a robust and versatile structural element capable of supporting significant loads while promoting eco-friendliness and design flexibility. However, despite its numerous adv...
M Chen, S Uphill, J Hilsenbeck, A Hughes
Elevated pressure hybrid wood modification: Synergistic effects on durability performance
2024 - IRG/WP 24-20725
The combination of different wood modification technologies to obtain improved performance is increasingly receiving attention in research. In this study, Scots Pine was impregnated with furfuryl alcohol (FFA) in pure aqueous 20, 40 and 60% solution strength without adding any catalyst. In a second step, the FFA was polymerized while simultaneously performing thermal modification in a closed syste...
P Klaas, D Jones
International joint field trial on the moisture performance of wood – Set up and first results
2024 - IRG/WP 24-40996
Wood durability to decay stems from its inherent resistance to fungi resistance to fungi. In this regard, wood's ability to withstand moisture uptake plays an important role as the lower threshold for wood decay is a moisture content of 25%. However, the aspect of moisture resistance is not yet sufficiently emphasized as a durability factor, both in the assessment of durability as a material prope...
C Brischke, et al. (33 co-authors)
Evaluation of the water exclusion ability and inherent bioactivity of heartwood against decay in Japanese and European wood species via above-ground exposure and water absorption tests
2024 - IRG/WP 24-40998
The natural durability of wood has been thought to mainly depend on bioactive extractives and the water exclusion ability. To clarify the contribution of each factor to wood durability, above-ground exposure tests were conducted on Japanese and European wood species. A double-layer test was carried out using heartwood specimens of four wood species, i.e., Japanese cedar, Japanese cypress, Scots pi...
T Osawa, R Noda, K Yamamoto
Determining the minimum water vapor permeability of exterior wood coatings by means of hygrothermal and decay models
2024 - IRG/WP 24-20717
The objective of this study was to determine the minimum water vapor permeability of exterior wood coatings for log homes using hygrothermal and decay modeling. The approach is based on a worst-case scenario assumption, namely a moisture trap at a given wood moisture content in a coated wall log. The minimum limit of vapor permeability of the coating system was determined by simulating the time re...
U Hundhausen, S Ullah, D Kraniotis
The durability and mechanical properties of 40 years old Black locust poles
2024 - IRG/WP 24-11042
This study investigates the durability and mechanical properties of 40-year-old black locust (Robinia pseudoacacia) poles harvested from a vineyard in Slovenia. Wood from these poles was compared to recently harvested black locust wood to determine possible reuse options. Visual inspection, hyperspectral imaging, and laboratory tests were conducted to assess decay, density, mechanical properties, ...
M Humar, J Malik, J Levanic, D Krzisnik, E Kerzic, B Lesar
Multifactorial analysis of the reasons behind wood natural durability
2025 - IRG/WP 25-11065
Physical, chemical and biological properties of several wood species were investigated in order to highlight the main factors involved in wood natural durability and wood characteristic using a principal component analysis. Interaction of wood with water were evaluated using contact angle measurements to determinate wood wettability by water and wood impregnability tests with water allowing to cal...
L-F E Nkogo, M S M Mouendou, S Dumarçay, P E Engonga, F Zannini, E Gelhaye, P Gérardin
Improvement and practical application of dry-type pressure treatment method
2025 - IRG/WP 25-20734
In years, the need for environmental consideration has been reaffirmed worldwide, and in Japan too, there is a demand for the expansion of the uses of wood in order to achieve a decarbonised society. So, there is also a need to develop and improve wood preservation treatment methods that overcome the weaknesses of wood and enable it to be used in a wide range of applications. The authors have impr...
D Tezuka, C Igarashi
Evaluation of 'Deep Penetration Treatment' for wood preservation
2025 - IRG/WP 25-20746
‘Deep Penetration Treatment’ (DPT) is a recently developed wood preservation technique in Japan designed to meet the preservation standards required for residential foundations. This method involves spraying a specially formulated solvent-borne wood preservative onto properly incised dried lumber. Despite being a non-pressure treatment, DPT achieves penetration levels comparable to conventiona...
M Ikeda, T Shigeyama, Y Sugai
Influence of incising methods and wood moisture content on ‘deep penetration treatment’ in Japanese cedar and larch
2025 - IRG/WP 25-20749
To expand applicability of ‘deep penetration treatment’, a solvent-borne and non-pressure treatment that is commonly coupled with roller-type incising using a flat blade, we investigated drill and laser machining as alternative incising methods and examined the influence of wood moisture content on the preservative penetration. Various incising methods were applied to heartwood of Japanese ced...
S Taira, T Miyauchi, S Isaji, H Matsunaga
Performance Verification of Water-Based Outdoor Wood Protection Coatings Based on Weather Resistance Evaluation
2025 - IRG/WP 25-41015
Recent trends in wood protective coatings: Concerns over volatile organic compound (VOC) emissions and the need to reduce maintenance costs have increased demand for environmentally friendly and highly durable coatings. While conventional solvent-based paints are superior in durability, they have been associated with problems such as environmental impact and odour during application. As an alterna...
N Ikemoto
Experimental characterizing of liquid water uptake and release – key to understand moisture-induced decay risk analysis
2025 - IRG/WP 25-41020
Wood can absorb water vapour (sorption) or liquid water (capillarity). Moisture from liquid water (rain, spray water) is often a problem for the performance of wood products used in outdoor structures. Wood is prone to biodegradation when is it too moist for too long periods. Experimental studies that allow conclusions to be drawn about the practical use of wood water uptake are limited due to the...
M Nopens, J T Benthien, J Trautner, C Brischke
Validation of a measurement method for cyproconazole retention in pressure-treated wood through an interlaboratory study
2025 - IRG/WP 25-41037
The Japanese Agricultural standard (JAS) defines national regulations for preserved wood and wooden materials, in Japan. Traditionally the JAS focused on quality of product, however, the revision of the JAS Act in 2017 enabled standardisation of test or measurement method for the quality evaluation. The Japan Wood Protection Association (JWPA) has been working toward standardisation of methods for...
T Miyauchi, Y Itou, M Samejima
Investigation of Pressure-Treated Foundations with Wood Preservative and Termite Control in Existing Wooden Houses in Japan
2025 - IRG/WP 25-50402
Japan has extremely limited natural resources. Therefore, it is necessary to build a circular economy in which waste and other recyclable resources are effectively utilized in order to achieve sustainable development. This study aims to investigate the degradation of existing wooden houses and to contribute to the reuse of existing houses and the reuse of building materials during demolition. We i...
K Usami, T Kawada, H Ishiyama