Your search resulted in 419 documents. Displaying 25 entries per page.
Development of accelerated decay test for CLT using a fungus grown on agar medium
2019 - IRG/WP 19-20664
CLT is a large-scale wooden board which consists of several layers of sawn lumber stacked in altering directions. Therefore, a lot of large cross sections appear on all narrow faces of CLT. As water penetrates easily into timber from cross section, wooden material whose cross section is exposed to water in in a usage environment is susceptible to deterioration by organisms. Wood deterioration orga...
T Miyauchi, K Kambara, W Ohmura, T Mori, H Matsunaga, N Hattori
Improvement of wood decay and termite durability resulting from combined treatments based on borax/phenol-formaldehyde impregnation followed by thermal modification
2019 - IRG/WP 19-40871
This study determined the factors influencing the boron content after leaching of pine blocks impregnated with aqueous solution of phenol-formaldehyde (PF) resin with or without borax and subjected to heat treatment by response surface methodology. An experimental design permits to analyze the effects of heat treatment temperature (150, 185 and 220°C), curing time (5, 12, 5 and 20 hours), resin c...
S Salman, M-F Thevenon, A Petrissans, S Dumarcay, P Gerardin
A new approach to wood protection: Potential of biologically synthesised CuO and ZnO nanoparticle formulation as a wood preservative
2022 - IRG/WP 22-30758
Even though metal nanoparticles are effective in protecting wood, they are less preferred, as they are synthesised using methods which are expensive and are not environmentally friendly. Biological synthesis of nanoparticles using plants, fungi, yeast, bacteria and viruses, has been accepted as an alternative approach and is referred to as green synthesis. Utilization of biologically synthesised n...
Shiny K S, R Sundararaj, N Mamatha
Properties of Iron (II) Sulphate treated Norway Spruce
2022 - IRG/WP 22-30765
Exterior wood is exposed to various environmental factors that cause weathering. Weathering is important primarily from an aesthetic standpoint. However, not all parts of the building are equally susceptible to weathering. Parts exposed to moisture will discolour faster than protected parts, such as wood under roof overhangs. To achieve fast and uniform artificial greying, a surface treatment with...
B Lesar, M Humar, M Škamlec
Environmentally Friendly Wood Modification based on Tannin-Furfuryl alcohol - Effect on stabilisation, mechanical properties and decay durability
2022 - IRG/WP 22-40929
Furfurylation is a well-known wood modification technology. This paper studied the effect of tannin addition on the wood furfurylation. Three kinds of dicarboxylic acids, adipic acid, succinic acid, and tartaric acid, as well as glyoxal as a comparing agent, were used to catalyse the polymerisation of furanic or tannin-furanic solutions during wood modification. Impregnation of furanic or tannin-f...
M Mubarok, E Azadeh, F O Akong, S Dumarçay, A Pizzi, C Charbonnier-Gérardin, P Gérardin
Accelerated surface mould testing for exterior wood treatment in Temperate, Tropical and Laboratory environments
2023 - IRG/WP 23-20699
Mould attack is a very common cause of discoloration on wooden surfaces and can subsequently promote development of wood decay by other organisms. Prevention of mould growth is relevant for both pigmented wood paints as well as more transparent systems with a high or low amount of binder. The use of commercial biocides has led to effective microbiological inhibition in many contexts, but the incre...
A Nazeri, J Stenbaek, T R Laursen, A H H Wong, B M Hasnul
Establishing the minimum effective penetration of wood preservatives in the refractory heartwood of E. nitens
2023 - IRG/WP 23-30780
Conventional pressure treatment of many Australian hardwoods results in little to no penetration of heartwood and a non-uniform envelope treatment of <5 mm surrounding a mostly untreated core. This is a major issue for many of the low durability plantation hardwood timbers that are grown in Tasmania, which contain high percentages of heartwood. Long term studies on softwoods such as spruce decking...
J R Vargas, J J Morrell, L Yermán, K C Wood
Optimization of furfurylic alcohol/tannin ratio to improve the performance of biosourced thermoset resins for wood protection
2023 - IRG/WP 23-40994
This study concerns the chemical modification of wood with different ratios of tannin and furfuryl alcohol (FA) in the presence of maleic acid as catalyst. Tannins were used not only as cross-linking agents, but also as co-monomers to improve wood durability, while reducing the amount of FA used. Different aqueous formulations were prepared containing decreasing amount of FA (from 45.45% to 0%) an...
E Azadeh, A Pizzi, P Gérardin, C Gérardin-Charbonnier
Exposure tests on railroad ties treated with DOT
2024 - IRG/WP 24-20705
Keruing railroad ties were treated with disodium octaborate tetrahydrate (DOT) to retentions of 0.7 to 1.7% boric acid equivalent (BAE) and selected borate treated ties were subsequently over treated with creosote/diesel fuel mixture. The treated ties were exposed in a simulated railway track test bed in Malaysia. The leaching of borate was measured over 5 years. BAE in the ties after 5 years of e...
L Arthur, J-W Kim
Comparison of copper leaching from alkaline copper quat and copper compound nanosol-based wood preservative treated wood
2024 - IRG/WP 24-20726
To improve the leaching resistance of copper ion-based wood preservatives, copper compound nanosol-based wood preservatives were developed and its copper leaching characteristics were evaluated. Three types of preservatives (DC1, DC2, DC3) were prepared with different crystallinity and dispersant types of copper compound nanosol, and the copper concentration was adjusted to be the same as that of ...
Y-S Choi, S-M Yoon, J O Kim, J-G Kang, J-G Park
Copper migration from preservative-treated Douglas-fir decking: models vs laboratory leaching data
2024 - IRG/WP 24-50390
The ability of a model to predict copper migration from Douglas-fir treated with organic metallic substances into a freshwater slough was evaluated against data generated through simulated overhead leaching. The model predicted very high loadings of ammoniacal copper zinc arsenate, alkaline copper quaternary or copper azole that had the potential to impact water quality while data from the exper...
M J Konkler, G Presley, J J Morrell, T Singh
Quantifying metal migration from a deck constructed with copper-azole-treated lumber
2024 - IRG/WP 24-50391
Soluble copper or micronized copper wood preservatives are the most common available wood preservative systems for residential applications in the United States. Copper containing wood preservatives have been scrutinized for their potential negative impacts on the environment, across many jurisdictions. Concerns arise from the potential for preservatives to migrate out of treated wood upon water e...
G Presley, M Konkler
Characterization of zinc borate synthesized in laboratory and scaled-up study
2025 - IRG/WP 25-20730
The organic nature of wood makes it vulnerable to both abiotic and biotic degradation. Impregnation with chemical products is a widely used method for wood protection. Inorganic borates exhibit a unique combination of properties that make them particularly effective for this purpose: they are insecticidal, fungicidal, and flame-retardant. In this study, ammoniacal zinc borate synthesized in labora...
Laffite, E Fernandez, C M Ibañez
Securing Flame Retardancy in Wood: Durability After Artificial and Natural Weathering Test
2025 - IRG/WP 25-20738
The outdoor use of wood is often limited by challenges such as dimensional instability, vulnerability to fungal decay, and high flammability. Traditional flame retardant treatments improve fire resistance but suffer from significant leaching under environmental exposure, reducing their long-term effectiveness. This study introduces an innovative solution by integrating flame retardants with DMDHEU...
M Wu, L Martin, H Militz
Curing Behaviour of Bio-based Phenol Formaldehyde Resin and the Durability Performance of Treated Wood
2025 - IRG/WP 25-20758
The aim of the study is to investigate the curing behaviours of bio-based PF resins treated Japanese Cedar (Cryptomeria japonica). Compared to conventional wood preservatives such as metal-based ACQ, bio-based PF resin was more environmentally-friendly and can store more plant-based carbon inside treated wood. However, all these preservatives have the risk of being leached out. This study conducte...
Y-S Lee, P-Y Kuo
Enhancing Wood Greying: A Study of Pre-Treatments and Iron(II) Sulphate Application
2025 - IRG/WP 25-41018
Recent trends in architecture and environmental policies have increased the demand for natural, unprotected wood in outdoor applications. However, wood exposed to the elements tends to grey unevenly, which can be problematic for visually important applications like timber façades. One solution is artificial greying with iron ions, providing a uniform colour that later transitions to natural greyi...
B Lesar, M Humar, A Kordiš
AI Models for Accelerating Wood Protection Testing: Development of Predictive Tools Based on Long-Term Field Test Data
2025 - IRG/WP 25-41023
In this study, we present the development of DecAI, an artificial intelligence (AI) model designed to optimise and accelerate performance evaluations of wood protection products in the European EN 330:2014 "Field test: L-joint method." The Danish Technological Institute (DTI) compiled a dataset of over 100,000 data points from approx.10,000 L-joint samples collected over +15 years at field sites i...
J Stenbaek, B Noufel, L Glade, P Bisgaard
Quantitative Prediction of Latent Deterioration in Wood Coatings Using Mid-Infrared Spectroscopy and Machine Learning
2025 - IRG/WP 25-41038
Wood coatings play a vital role in prolonging the lifespan of timber structures by protecting them from environmental degradation. However, conventional evaluation methods rely on visual inspections, which cannot detect latent deterioration before visible damage occurs. This study integrates attenuated total reflectance-Fourier transform infrared (ATR-FTIR) spectroscopy with partial least squares ...
Y Teramoto
Development of an Early Degradation Diagnosis Technology for Wood Coatings Using Mid-Infrared Spectroscopy and Machine Learning
2025 - IRG/WP 25-41047
Accurately predicting the degradation state of wood coatings is challenging, and as the coating deteriorates, it becomes a major factor accelerating the degradation of the wood itself. In this study, we aimed to develop a diagnostic technology that combines mid-infrared spectroscopy and machine learning to assess latent coating degradation, which cannot be detected visually, and to enable appropri...
K Nishimura, T Ito, S Isaji, T Takano, H Ohki, Y Teramoto