Evaluation of different wood by-products for sustainable building biomaterial production using fungal mycelium
2022 - IRG/WP 22-50373
As human population increases, the demand for new innovative, sustainable, and low impact construction materials also grows. Mycelium-based composites have shown to be an excellent alternative for traditional products ranging from low-density objects to semi-structural applications. They also present the advantage of using the waste streams from other productive processes as feedstock, enabling th...
C Charpentier-Alfaro, M Poggerini, S Palanti, G Della Rocca, D Pellegrini, A Crisci
Enhanced durability of bio-based materials for green building
2023 - IRG/WP 23-50382
Wood protection technologies provide tools to enhance the durability of bio-based materials for green building. Both wood and related bio-based material are regarded as eminent for green building. It allows to underpin several of the United Nations sustainable development goals and is regarded critical for the Green Deal objectives of the EU. Nevertheless, to enhance the potential it needs to be b...
J Van Acker, L De Ligne, J Vand den Bulcke
Binder-free, fire-resistant, light-weight fiberboard materials encrusted with expandable graphite and borax
2024 - IRG/WP 24-20714
Despite abundant data on innovative fire protection technologies tailored for wood and lignocellulosic materials, the prevailing approach revolves around the formulation of fire retardant solutions employing water-soluble salts, e.g., phosphorus or boron compounds. On the other hand, additives fostering the formation of a char layer during the combustion of lignocellulosic materials as a non-leach...
W Perdoch, W Grześkowiak, B Mazela
Transformation of bamboo: From multiscale fibers to robust and degradable cellulose-based materials for plastic substitution
2025 - IRG/WP 25-41032
Bamboo is an ideal candidate to replace traditional plastics, reduce environmental pollution, and promote harmony between nature and humanity owing to its rapid growth and renewability. However, achieving arbitrary shape-shifting of bamboo while retaining its high strength and degradability remains challenging. This study used multiscale interface engineering to transform bamboo into a robust, bio...
J Hu, Y Zhang, Y He, Z Su, W Lao, S Zhang, Y Yu, W Yu, Y Huang
Biocomposites based on fungal mycelium and beech particles impregnated with BPCM (bio-phase change material) for thermal energy storage
2025 - IRG/WP 25-41034
The building sector is a major contributor to Europe's carbon emissions, and transition to a bio-based economy is essential for achieving long-term sustainability goals. The European Union has set ambitious targets for climate-neutral heating and cooling by 2050, which requires the widespread adoption of energy-efficient and environmentally friendly technologies. A key element in this transition i...
E Nigrone, F De Francesco, J Conti, M Jebrane, M Nazari, N Terziev, S Palanti
Recycling wood treated with copper-based preservatives to produce hard carbon materials for energy storage applications
2025 - IRG/WP 25-50401
In this study, we explored the possibility of recycling wood treated with copper-based preservatives to produce hard carbon materials for use in energy storage devices. We pyrolsed both untreated and copper-treated wood into hard carbon, conducted microstructural and physicochemical characterisation, prepared electrode materials, and evaluated their electrochemical performance in sodium-ion batter...
D Huo, J-P Bonnet, A Jamali
Penichroa fasciata (Stephens) (Col. Cerambycidae) a pest in wood materials
1988 - IRG/WP 1365
Penichroa fasciata (Stephens) (Col. Cerambycidae) is found to be a frequent pest occurring in hardwood in storage in Italy. This paper reports the characteristic for identification, biological features, distribution and timber liable to attack....
A Gambetta, E Orlandi.
How to Document the Performance of Super-Critical Treated Wood in above Ground Situations?
2005 - IRG/WP 05-20316
The paper presents practical experiences from the preparation of a new preservative treated wood product for introduction to the market. The product in question is Superwood™, which is treated with organic biocides using CO2 in a supercritical state as a solvent.
The question is how to evaluate the performance of a new product such as Superwood™ in order to get an acceptance on the market a...
N Morsing, A H H Wong, F Imsgard, O Henriksen
Summary of development of pile wrappings in Los Angeles Harbour
1987 - IRG/WP 4141
G Horeczko
Developments in the protection of wood and wood-based products
1980 - IRG/WP 340
Technology is playing an increasingly important role in the field of wood protection. This current review highlights how modern techniques have provided greater insight into the biological and physical processes affecting the durability of wood and wood-based products. Emphasis is also given to developments in preservative testing methodology and to the encouraging changes towards both the correct...
J M Baker
Leaching of the new boron based biocide from coated wood
2001 - IRG/WP 01-30267
We investigated leachability of the new boron based biocide - a complex of an amine and boric acid - from vacuum impregnated spruce wood samples. It was determined by the standard ENV 1250-2 procedure that the new biocide is susceptible to leaching so from the water borne as well as from the ethanol borne boron containing preservative treated wood. Leaching may be retarded by application of surfac...
M Petric, M Pavlic, F Cadez
Preliminary results of investigations on screening test of chemical compounds suitable for the preservation of lignocellulosic materials against biodeterioration
1976 - IRG/WP 262
This paper investigates the possibilities of reducing the time needed for the determination of the effectiveness of chemical compounds from the point of view of their eventual application to lignocellulosic materials for preservation against decay and soft-rot....
K Lutomski, S S Neyman
Mycological testing of plywood and board materials. Part 1: Review of information supplied by IRG members
1978 - IRG/WP 284
In December 1975 IRG members were asked for published information, information of current work in progress and views on mycological test methods for board materials. The object was to stimulate discussion and possibly establish a joint research effort within IRG in order to establish a meaningful test with reproducible results....
C R Coggins
Possibility of use of wood species per class of biological risks. Attempt to determine criteria based on Pr EN 350-1/2/3
1992 - IRG/WP 92-2409
M Rayzal
A new wood preservative based on polymerized complexes of aminotriazole with copper acetate
1998 - IRG/WP 98-30169
This paper presents the results of preliminary fungitoxicity tests as carried out on new polymerized complexes of aminotriazole with copper acetate (PCC) against Coniophora puteana and Trichoderma viride.
Laboratory tests on wood confirmed the findings arrived at in the screening test on agar medium. Deep penetration into pine wood of compounds studied was observed and particularly so at humidity...
K J Krajewski, A Lukasiewicz, J Wazny
Conforming to european standards for preservative-treated timber: Specifying with confidence
2000 - IRG/WP 00-20194
A four-year collaborative study between four industrial partners and BRE has assessed timber treated by current UK industrial practices in the light of current European Standards. Data were collected for CCA and creosote treated timber components, and compared with the requirements laid out in EN351-1 and -2. A number of difficulties were encountered that have been described in previous IRG papers...
E D Suttie, R J Orsler
Water-based wood preservatives for curative treatement of insect-infested spruce constructions
1998 - IRG/WP 98-30171
On laying down sanitation measures for wooden constructions infested by wood boring insects, we must take into account static risks for the construction - and, thus, for the security of the user - as well as risks for humans and environment due to the chemical preservative compounds of the treated wood.
Analyses on many roof constructions made with spruce (Picea abies L.) have revealed that Hylot...
E Graf, P Manser, B Lanz
The resistance of painting materials and consolidants against wood-destroying insects
1997 - IRG/WP 97-10239
Natural and synthetic adhesives, varnishes, painting materials and consolidants were used in investigations of bioresistance against newly hatched larvae and beetles of Hylotrupes bajulus (L.). Animal glues, casein, drying oils and natural resins such as dammar resin and shellac, were not resistant to attack by these larvae. Similarly, semi- and all-synthetic polymers tested including hydroxypropy...
W Unger, H Fritsche, A Unger
Volatile borates in the treatment of wood and wood based panel products against subterranean termites
1995 - IRG/WP 95-30094
Blocks of pine solid wood, oriented strand board and plywood were treated with trimethyl borate by vapour treatment. It was meant to obtain either a full impregnation of the specimens or a shell treatment of the outer three millimetres. The efficacy of the treatments against subterranean termites (Reticulitermes lucifugus) was evaluated using an European Standard method....
L Nunes, D J Dickinson, R J Murphy
A collaborative test to determine the efficacy of polyurethane coatings on wood samples exposed in the marine environment
1984 - IRG/WP 4113
Aims are: a) to determine the effectiveness of elastomeric polyurethane as a protective coating against marine wood boring animals in a range of tropical and tempreate sites; b) to compare the adhesion of polyurthane coatings on different wood species exposed in seawater; c) to record the severity of attack in failed samples and to identify the causal marine organisms....
R A Eaton
Evaluation of polystyrene as a protective of wood in sea-water
1986 - IRG/WP 4129
A test is described on the biological protection of wood by treatment with polystyrene. The results, obtained in marine trials, after 18 months, show that the treatment with polystyrene is not all that effective in preventing the attack of marine borers....
A Gambetta
Information from the COIPM Wood Group. Summary received via Mme Dr Anna Gambetta (Italy)
1987 - IRG/WP 4139
Two co-operative programmes were discussed: 1) The IRG/COIPM co-operative programme on the CCA/CCB wood treatments and 2) The IRG/COIPM co-operative programme for testing the resistance of plastic wrapping for wooden pilings. The following was reported: In the wood treatment programme, beech, pine and alstonia wood samples have been pressure treated with 3 retentions (3%, 6% and 10%) of CCA and CC...
J R DePalma
Draft Business Plan of CEN/TC 38 - Durability of wood and wood-based products - Introduction
2000 - IRG/WP 00-20207
CEN Technical Committees and Business Planning. The extension of formal business planning to CEN Technical Committees (CEN/TCs) is an important measure which forms part of a major review of business processes (known as 'Optimization'). The aim is to align the CEN work programme with expressed market needs and to ensure the adequate resourcing of projects through their development...
R Hüe
Evaluation of wood treated with copper-based preservatives for Cu loss during exposure to heat and copper-tolerant Bacillus licheniformis
1999 - IRG/WP 99-20155
Copper-based wood preservatives need to be effective against exposure to all types of microorganisms. Wood treated with six copper-based preservatives was exposed to 121°C and 20 psi pressure for 15 minutes under standard autoclave conditions and the copper-tolerant bacterium, Bacillus licheniformis CC01, for 10 d at 28°C and 150 rpm. Sixteen to 37 percent of the copper was released from the woo...
D M Crawford, C A Clausen
Reliability-based service life prediction methodology for assessment of water protection efficiency for coatings on wood
2003 - IRG/WP 03-20268
Assessment of water protection efficiency according to EN 927-5 has been shown to give significant differences in water absorption values for different types of coatings on wood. It is shown that the combination of EN 927-5 and an artificial weathering procedure gives more information regarding expected durability and long-term performance than a single measurement of water absorption on fresh, un...
J Ekstedt