IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 348 documents. Displaying 25 entries per page.


Marine borers as wood degraders in Bangladesh and their protection
1996 - IRG/WP 96-10186
Field study on timber piles used in Bangladeshi brackish waters revealed that untreated and pentachlorophenol treated piles drastically degraded by the attack of molluscs and pholads (marine borers). Adequately CCA-C impregnated (30 kg/m³ or 6% W/W dry oxide retention) timber piles can protect the attack of molluscs. It is very difficult to protect pholads which can invade naturally very durable ...
A K Lahiry


Efficacy of some extractives from Pinus heartwood for protection of Pinus radiata sapwood against biodeterioration. Part 1: Fungal decay
1995 - IRG/WP 95-30072
Chemical compounds thought to contribute to the natural durability of heartwood of Pinus spp. were either chemically synthesised in the laboratory or extracted from the heartwood of Pinus elliottii or Pinus caribaea. These compounds included the stilbenes, pinosylvin and its mono- and di-methyl ethers, and the flavonoids, pinobanksin and pinocembrin. Small blocks of Pinus radiata sapwood were impr...
M J Kennedy, J A Drysdale, J Brown


Susceptibility of angiosperm sapwood to white-rot fungal colonization and subsequent degradation: a hypothesis
1997 - IRG/WP 97-10211
It has long been recognized that angiosperm sapwood in nature is relatively easily and preferentially degraded by white-rot fungi. This susceptibility to white-rot fungi is generally believed to be mainly caused by the structure and concentration of angiosperm lignin. However, an explicit explanation as to why lignin structure makes a particular wood vulnerable to white-rot colonisation and subseq...
T Schultz, D D Nicholas


United States Federal Committee on Wood Protection
1971 - IRG/WP 43
A C Jewett


Marine borers and marine wood protection - Some answers and some outstanding questions - A comment
1990 - IRG/WP 4163
A brief description of the nature of hazards encountered in different parts of the marine environment is given. An attempt is then made to assess what were the essential findings of selected areas of research in the marine wood protection field and what still needs to be done. That is, if we are to more adequately understand what we are attempting to do in this field of study!...
J E Barnacle


The role of communication in the field of environment protection: A case study "Wood Protection"
1990 - IRG/WP 3574
L Wöss


Wood preservation in China
1989 - IRG/WP 3546
Huiming Zhou, Zhongwei Jin


Quelques observations biologiques sur la conduite des essais de protection des bois immerges en milieu marin
1976 - IRG/WP 421
P Deschamps


Surface Barriers for Protection of Culture and Heritage Wooden Objects from Insect Attack
2004 - IRG/WP 04-40286
Anoxic treatment is an environment friendly procedure for eradication of wood boring insects in wooden objects of cultural and historical heritage. However, after the anoxic treatment, wooden antiques remain susceptible to further insect attacks. Possible protection against insects could be provided by the so-called post-repression protective barriers. Potential coating materials for such barriers...
M Petric, M Pavlic, B Kricej, M Humar, F Pohleven


Framework document for an international code of good practices for wood preservation and wood protection (anti-sapstain) facilities
1992 - IRG/WP 92-3683
At the Kyoto meeting, the Health & Safety committee agreed to form a task force to prepare a global plan for writing a code of good practices (Code) for wood protection and preservation facilities (Doc. No. IRG/WP/3681). The Canadian document had been presented to the IRG group earlier (Doc. No. IRG/WP/3447) and similar documents were solicited from other countries for preparing a framework do...
V N P Mathur, G Das


Protection of Ochroma pyramidale from fungal decay with N,N-napthaloylhyroxylamine
1998 - IRG/WP 98-30182
Fungal decay of wood in service results in billions of dollars (U.S.) in losses annually. Recent environmental restrictions, both U.S. and international, are limiting and eliminating the use of broad-spectrum, heavy metal biocides for wood preservation. Restrictions result primarily from problems with disposal. New wood preservatives need to be developed and tested which specifically target key el...
F Green III, T L Highley


Investigation of the fixation in wood of chromated zinc chloride and copperised chromated zinc chloride preservatives
1976 - IRG/WP 372
A biological method of evaluating the extent to which CZC and CCZC preparations are retained in wood in terms of the potential protection which they afford against destruction by Merulius lacrymans (dry rot) is given. CCZC is recommended for protection of wood under moderate leaching conditions, while the use of CZC under such conditions is not recommended....
V N Sozonova, D A Belenkov


Copper based water-borne preservatives: The use of a thin section technique to compare the protection of wood by copper based preservatives against soft-rot and bacterial decay
1987 - IRG/WP 2286
This paper describes the techniques developed and gives examples of results obtained for the performance of copper based wood preservatives against both the bacterial and fungal hazards....
A M Wyles, D J Dickinson


Biocide Treatments for Wood Composites - A Review
2006 - IRG/WP 06-40323
This paper reviews the biocidal treatment of wood composites. Included are in-process and post-process treatments. Various biocides are covered as are methods of application. Novel treatments and technologies are also presented....
J W Kirkpatrick, H M Barnes


The use of chlorothalonil for protection against mold and sapstain fungi. Part 1: Laboratory evaluation
1989 - IRG/WP 3515
Laboratory screening of chlorothalonil alone and in combination with other fungicides was conducted against six mold and sapstain fungi. The most promising treatments appear to be chlorothalonil supplemented with CCA or copper-8-quinolinolate. Field tests have been implemented....
J A Micales, T L Highley, A L Richter


The leachability and specificity of the biological protection of timber using Scytalidium sp. and Trichoderma spp
1986 - IRG/WP 1302
The results of field experiments, using biological control against internal decay of creosoted poles, are briefly reviewed and the evidence concerning the leachability of the antibiotics produced by these species is presented. A pure culture miniblock decay test on biological control treated pine sapwood is described and the results compared to previously published data. The protection against Len...
P I Morris, N A Summers, D J Dickinson


Correlation between a laboratory bioassay and field trial conducted to determine the termiticidal effectiveness of bifenthrin
2002 - IRG/WP 02-20248
Details are given of a laboratory bioassay and field trial undertaken to determine the termiticidal effectiveness of the synthetic pyrethroid bifenthrin, when impregnated into Pinus radiata D. Don sapwood specimens. Results show a strong correlation between the laboratory and field methods of evaluation. Protection threshold limits obtained were the same for the two test species of termite employe...
J W Creffield, K Watson


Protection of beech veneer for fruit and vegetable boxes
1981 - IRG/WP 3176
In Yugoslavia about 50,000 m³ of low quality beech logs annually are rotary cut into veneer from which boxes are made for transporting fruit and vegetables. Because of steaming before rotary cutting, beech veneer becomes extremely sensitive to mould attack which decreases the quality and commercial value of the final product. To avoid mould attack, veneer sheets are dried to 16% moisture content ...
N Vidovic


Less environmental impact of wood preservatives by considering the risk of attack in addition to the hazard class system
1995 - IRG/WP 95-50040-10
Hazard classes, which are standardized in Europe in EN 335, are most useful to direct chemical wood preservation towards the organisms which may attack wood in the various fields of utilisation. However, hazard only signifies the fact that an attack may occur without considering the actual risk to attack. To minimize the application of chemicals with respect of less environmental impact it is nece...
H Willeitner


Role of Global Cooperation in Wood Protection for Conserving Forest Resources
2007 - IRG/WP 07-50249
The current uses of treated wood are discussed along with the emerging concerns for continued use of these products. The issues of new chemicals, treatments for wood based composites, migration of chemicals from treated wood, and the disposal of these products at the end of their useful life are all outlined. The potential for the IRG to serve as the focus for research discussion as well as coll...
J J Morrell, G Deroubaix


Protection of OSB against termites by incorporation of different actives via glue line treatment
2008 - IRG/WP 08-30453
Different organic actives and zinc borate were incorporated into OSB during the manufacturing process to enhance the resistance against termites. Tests according to EN 117 revealed excellent performance of thiacloprid. Other organic actives such as permethrin might be effective when used in higher amounts. Zinc borate failed the test by far....
S Donath, P Spetmann, T Jaetsch, T Zahlmann


The effect of low molecular weight chelators on iron chelation and free radical generation as studied by ESR measurement
2000 - IRG/WP 00-10367
The focus of this work was to improve our current knowledge of the non-enzymatic mechanisms involved in brown-rot decay. Electron Spin Resonance (ESR), also known as Electron Paramagnetic Resonance (EPR), is an attractive technique for the identification and study of chemical species containing unpaired electrons (such as radicals and certain transition metal species). ESR spin-trapping techniques...
Yuhui Qian, B Goodell


The use of ESR spectroscopy to assess the photostabilising effects of wood preservatives
2000 - IRG/WP 00-20186
The degradation of wood surfaces exposed to UV light which leads to poor performance of clear coatings is understood to be due to delignification via a mechanism involving free radicals. Certain wood preservatives most notably CCA are able to photostabilise wood and therefore they may reduce the concentration of free radicals formed when treated wood is exposed to ultraviolet light. As a first ste...
S Schmid, R D Webster, P D Evans


Generic code of good practices for wood protection facilities. Part 1: Wood protection (antisapstain) facilities
1993 - IRG/WP 93-50003
In general, the potential of high toxicity (aquatic and human) of wood protection (antisapstain) chemicals dictates the need to protect the environment and humans from its harmful effects. This document is a compendium of recommendations for the design and operating practices of wood protection facilities. The suggested recommendations focus on achieving the objectives of protecting the environmen...
G Das, V N P Mathur


Laboratory evaluation of fipronil (a phenyl pyrazole) as a candidate termiticide in the protection of wood against the subterranean termite, Coptotermes acinaciformis (Froggatt) Rhinotermitidae
1997 - IRG/WP 97-10225
In this laboratory evaluation, radiata pine wood blocks (50 x 25 x 15 mm3) were impregnated with fipronil (a phenyl pyrazole) at various concentrations (0, 5, 10, 20, 40, 80, 100 and 200 ppm). Half the treated blocks underwent a leaching schedule for 5 days, while the remainder were unleached after treatment. Five replicates per treatment regime were presented to the test termite, Coptotermes acin...
B M Ahmed, J R J French, P Kwint, G Webb


Previous Page | Next Page