Local preservation with difluoride pills: Life-time of preservative
1998 - IRG/WP 98-40127
A brief history of the situation in the Netherlands with respect to the preservation of joinery is given. Already in the eighties in the Netherlands many spruce window frames were treated with difluoride pills. One of the possible disadvantages of this kind of diffusing preservatives is the high leaching rate found in laboratory situations. The leaching rate in practice is influenced by many facto...
W J Homan, C Blom, B W Holleboom


Water-based wood preservatives for curative treatement of insect-infested spruce constructions
1998 - IRG/WP 98-30171
On laying down sanitation measures for wooden constructions infested by wood boring insects, we must take into account static risks for the construction - and, thus, for the security of the user - as well as risks for humans and environment due to the chemical preservative compounds of the treated wood. Analyses on many roof constructions made with spruce (Picea abies L.) have revealed that Hylot...
E Graf, P Manser, B Lanz


Inventory of the use of preservative-treated wood and wood preservatives in Sweden 1900-1997
1999 - IRG/WP 99-50137
The objective of this study was to present an overview of the use of wood preservatives and their active ingredients and industrially preservative-treated wood in Sweden since the beginning of the 20th century. The data presented in the report could for example be used as a basis for different waste management scenarios for preservative-treated wood. Before 1960 railway sleepers and utility poles ...
J Jermer, K Nilsson


An investigation of the effects of pre-steaming on the treatment of sawn spruce timber with Celcure A, a copper-chrome-arsenic preservative
1981 - IRG/WP 3150
Difficulties in the treatment of spruce using standard vacuum/pressure techniques with both water-borne and organic solvent preservatives are well known. We have evaluated the influence of steaming on treatability with a waterborne CCA preservative....
C R Coggins


Light organic solvent preservative treatment schedules for New Zealand-grown radiata pine
1986 - IRG/WP 3379
The influence of pressure differential and treatment time on preservative uptake and distribution in radiata pine heartwood and sapwood is investigated. Treatment schedules are defined which minimise solvent usage but ensure complete sapwood penetration and optimise heartwood penetration....
P Vinden


Preservative treatment of Eucalyptus saligna fence posts by the double-diffusion method
1982 - IRG/WP 3196
Eucalyptus saligna fence posts treated by the double-diffusion method with two chemical combinations showed average lives of 11.2 years (copper sulphate and potassium dichromate at 10.5 kg/m³ retention)and of 14.3 years (copper sulphate and sodium mono-H arsenate at 7.1 kg/m³ retention), as determined in five test sites in the State of Sao Paulo, Brazil. The exponential model was the best fit wh...
E S Lepage, A R De Freitas


Reticulitermes lucifugus Rossi, and its damages in Turkey
1982 - IRG/WP 1152
The moist-wood termite, Reticulitermes lucifugus Rossi, is generally observed on the wood material which has a direct contact with the soil as trunks and fence stakes. It was reported to be found in some provinces in Turkey. The termite has been seen in these areas so far at the endemic level, but any considerable damage or epidemy has not yet been reported. Considerable damages were observed on t...
O A Sekendiz


Options for accelerated boron treatment: A practical review of alternatives
1985 - IRG/WP 3329
Boron wood preservatives are almost exclusively applied by momentary immersion and block diffusion storage. Alternative techniques are described which can be used to accelerate boron treatment. Diffusion coefficients have been derived to define the acceleration of diffusion with increasing temperature. Schedules are described for pressure impregnation of green timber, involving steam conditioning,...
P Vinden, T Fenton, K Nasheri


Rates of emission from CCA-treated wood in the marine environment: measurement, modelling and requirements for further research
2001 - IRG/WP 01-50166-12
Accurate estimates of rates of emission of leachate from preservative treated wood are crucial for realistic predictions of the environmental impact of its use in maritime construction. Estimates are available for some commonly used preservatives, but these vary widely. Though variable, these measurements suggest that emission generally decreases exponentially with time. Part of the variation is d...
S M Cragg, C J Brown, R A Albuquerque, R A Eaton


Preliminary results of investigations on screening test of chemical compounds suitable for the preservation of lignocellulosic materials against biodeterioration
1976 - IRG/WP 262
This paper investigates the possibilities of reducing the time needed for the determination of the effectiveness of chemical compounds from the point of view of their eventual application to lignocellulosic materials for preservation against decay and soft-rot....
K Lutomski, S S Neyman


Mould resistance of lignocellulosic material treated with some protective chemicals
1984 - IRG/WP 3294
Effectiveness of preserving lignocellulosic material against moulding by treatement with water solutions of commercial wood preservatives and mixtures of various inorganic salts was investigated and compared with the effectivenes of sodium pentachlorophenoxide and boric acid....
K Lutomski


IRG test of preservative-treated hardwoods with particular reference to soft rot. Report on condition of specimens installed in Victoria, Australia
1982 - IRG/WP 3207
J Beesley


Factors affecting leaching of preservatives in practice
1978 - IRG/WP 3113
At the 7th Meeting of the IRG in Poland in May 1975, the findings of collaborative laboratory leaching techniques were discussed, and the dangers inherent in using such results to predict the behaviour of preservative-treated components in service were emphasised. In order to improve our understanding of the factors governing leaching of preservatives in practice, and to identify areas where furth...
R Cockcroft, R A Laidlaw


The identification and preservative tolerance of species aggregates of Trichoderma isolated from freshly felled timber
1992 - IRG/WP 92-1553
The surface disfigurement of antisapstain treated timber by preservative-tolerant fungi remains a major problem in stored timber. Identification of a range of isolates of Trichoderma based on microscopic morphological characteristics was found to be imprecise due to the variable nature of this organism. In addition, studies to compare visual (morphological) characteristics of these isolates with t...
R J Wallace, R A Eaton, M A Carter, G R Williams


An in-ground natural durability field test of Australian timbers and exotic reference species. Part 2: Progress report after approximately 13 years' exposure
1983 - IRG/WP 1189
The condition of heartwood specimens of Australian and exotic timber species after approximately 13 years' in-ground exposure is given. Four of the 5 test sites have a termite hazard in addition to the hazard from a range of decay fungi. Values for specimen life are given only where all replicates of a timber species have become unserviceable. Results give evidence leading to doubt about ...
J D Thornton, G C Johnson, I W Saunders


Some observations on causes of failure of preservative treated natural round transmission poles in Nigeria
1977 - IRG/WP 291
Treated natural round transmission poles in Nigeria have been discovered to be attacked underground as early as two years after planting. Termites and rot fungi attack the inner tissues and leave a pattern characteristic for the species of the pole. Tectona grandis, Nauclea diderrichii and Wide Pore pine, the major species for transmission poles in Nigeria show these attacks. A form of termite shi...
M A Odeyinde


Report on International Conference on Marine Biodeterioration, Goa, India, January 1986
1986 - IRG/WP 4127
At the International Conference on Marine Biodeterioration - Advanced Techniques Applicable to the Indian Ocean, there were a number of papers relevant to the aims of Working Group IV of IRG. Abstracts of these papers and a brief commentary on the conference are presented....
S M Cragg


Collaborative soft rot tests: Interim report on PRL tests of Cu/Cr/As preservative using method of Document No: IRG/WP/208
1972 - IRG/WP 211
Preservative: Tanalith CT.106 - Results obtained with beech are given in the table and indicate a toxic limit of 16.7-19.2 kg/m³ - The initial soil moisture content was adjusted to 27.8% (the water holding capacity). Noticeable drying out has occurred in some of the test bottles....
J G Savory


New technique for inoculation of wood wafers with fungi
1997 - IRG/WP 97-20113
A pilot study is described for determining the best possible method for inoculating fungi onto the surface of wood wafers for sapstain control studies. Direct inoculation and spray inoculation are compared on water soaked and malt extract broth soaked wood wafers. The best growth of fungal hyphae across the surface of the wood wafers was achieved following spray inoculation onto malt extract broth...
J Snow, P Vinden


Some physiological characteristics of a non-degradative strain of Postia (=Poria) placenta
1988 - IRG/WP 1341
The decay capacity of 14 strains of the brown-rot fungus Postia (= Poria) placenta was determined using soil-wood block tests. One isolate was identified as being unable to degrade wood and was determined to be monokaryotic. It retained the ability to produce extracellular carbohydrate-degrading enzymes, although regulation of certain enzymes was atypical under certain cultural conditions. It prod...
J A Micales, T L Highley


Movement of boron from fused boron rods implanted in Southern pine, Douglas fir, red oak, and white oak timbers
1995 - IRG/WP 95-30061
This paper reports the distribution of boron from fused boron rods installed into six-inch (15.2 cm) square timbers of Douglas-fir, Southern Pine, red oak and white oak exposed aboveground. The composition and size of rods was: sodium borate and sodium borate-copper oxide (8.5 x 100 mm²); sodium borate-copper, sodium borate and boric oxide-copper oxide (12 x 76 mm²). The boric acid equivalent wa...
T L Highley, L Ferge


Laboratory investigations about the mobility of some inorganic wood preservatives in soils
1998 - IRG/WP 98-50101-22
Wood preservatives and components of wood preservatives leached from impregnated wood can enter the soil and thus contribute to the pollution of the groundwater. However, there is lack of understanding concerning the interacting parameters of wood preservative, leachate, soil and soil solution. To characterise of the behaviour of active ingredients and for the assessment of their environmental imp...
E Melcher, R-D Peek


Fire resistance of Alder wood treated with some chemicals. Part II. Effect of Other Chemicals on the Combustion Properties
2002 - IRG/WP 02-40235
Samples from alder wood (Alnus glutinosa (L.) Gaertn. subsp. barbata (C.A.Mey) Yalt.) were impregnated according to ASTM D 1413-88 with boron compounds (boric acid, borax, sodium perborate), vinyl monomers (styrene, methyl methacrylate), Tanalith-CBC, Phosphoric acid, Vacsol, Immersol, Polyethylene glycole (PEG-400) and their mixed solutions of chemicals in order to determine their combustion pro...
A Temiz, Ü C Yildiz


Light organic solvent preservative treatment of glue-laminated radiata pine
1986 - IRG/WP 3380
The high permeability of radiata pine (Pinus radiata D. Don) is associated with ray-tissue and in particular the cross-field pits linking ray-tissue to tracheids. This pathway is absent in the tangential grain direction, leading to poor preservative penetration when treatment is restricted to the radial face - for example, timber fabricated into glue-laminated beams....
P Vinden


Finite element analysis of boron diffusion in wooden poles
2003 - IRG/WP 03-40263
The problem of describing the migration of dissolved boron in wood is treated with special reference to the commonly used remedial treatment of wooden poles. The governing equations are derived and discussed together with some of the material parameters required. The equations are solved by the finite element method and finally, results showing the effect of different treatment strategies are pres...
K Krabbenhøft, P Hoffmeyer, C G Bechgaard, L Damkilde