Your search resulted in 932 documents. Displaying 25 entries per page.
Fluorine compounds for wood preservation
1971 - IRG/WP 304
Fluoride compounds have gained a considerable importance in wood preservation, especially in Germany and some other countries of Europe. They are used as single compounde or in mixtures of different compounds. In the International Research Group on Wood Preservation which continues the activities of a former OECD-Group, it was moved to prepare a survey on fluorides in wood preservation together wi...
G Becker
Decay fungi in Finnish houses on the basis of inspection samples from 1978 to 1988
1989 - IRG/WP 1401
A summary of the causes and sources of fungal damages was made on the basis of decay samples and sample information sent to the Forest Products Laboratory of the Technical Research Centre of Finland (VTT) between 1978 and 1988. About 50-130 decay cases in wood structures were studied annually. In almost 50% of all fungusdamage cases the cause was Serpula lacrymans. The proportion of Coniophora put...
L Paajanen, H Viitanen
Detection of brown rot decay in wood by ion mobility spectrometry
1991 - IRG/WP 2377
A test method for the detection of brown rot decay in wood is described and involves a two-step procedure: thermal release of vapours from wood samples followed by analysis using Ion Mobility Spectrometry (IMS), with results being obtained in 5-10 seconds. The advantages, limitations as well as the detection limit of the technique are presented....
A H Lawrence, T Nilsson
Decay in external joinery in the United Kingdom
1978 - IRG/WP 3116
no abstract available...
J G Savory, J K Carey
Contribution to study of the degradation caused in Pinus spp. poles used in field test
1989 - IRG/WP 1417
The study of the degradation produced by soil natural microflora on wood in contact with it in the field, has been going on for several years now. Our contribution to this aim in the present work has dealt with the possible relationship of the microorganisms in the soil. The microscopic visualization of wood colonization by the microorganisms, and the chemical analysis of the degraded wood compare...
M T De Troya, A Garcia, M J Pozuelo, A M Navarrete, A Cabanas
Efficacy of anhydrides as wood protection chemicals - II. Performance against soft rot fungi
1998 - IRG/WP 98-30174
Pine sapwood modified with various anhydrides and with butyl isocyanate was tested for its resistance to soft rot decay. Small stakes were exposed for 20 months in unsterile soil in a fungal cellar test.
Wood modified with butyl isocyanate performed better than any of the anhydrides tested, with a threshold level of protection (less than 3% weight loss) at 12% weight percent gain (WPG). Stakes ac...
S C Forster, M D C Hale, G R Williams
An in-ground natural durability field test of Australian timbers and exotic reference species. Part 2: Progress report after approximately 13 years' exposure
1983 - IRG/WP 1189
The condition of heartwood specimens of Australian and exotic timber species after approximately 13 years' in-ground exposure is given. Four of the 5 test sites have a termite hazard in addition to the hazard from a range of decay fungi. Values for specimen life are given only where all replicates of a timber species have become unserviceable. Results give evidence leading to doubt about ...
J D Thornton, G C Johnson, I W Saunders
Elimination of alternative explanations for the effect of iron on treated wood
1993 - IRG/WP 93-30006
Amounts of iron which had previously been found in stakes removed from ground contact reduced decay of untreated wood by four brown-rot fungi. This suggested that the effect of iron may be on the preservative. Analysis of the leachates from CCA- and ACA-treated wood blocks first exposed to rusting iron, then to a brown-rot fungus, showed that the increased decay found in the laboratory for wood ex...
P I Morris, J K Ingram, D L Gent
Proposed test procedure to determine the effect of timber substrate on the effectiveness of a copper/chrome/arsenic preservative in seawater
1975 - IRG/WP 411
R A Eaton
Recent names for some common decay fungi
1976 - IRG/WP 143
A Käärik
Model questionnaire for preparation of monographic cards for wood-destroying fungi
1972 - IRG/WP 103
C Jacquiot
Some observations on causes of failure of preservative treated natural round transmission poles in Nigeria
1977 - IRG/WP 291
Treated natural round transmission poles in Nigeria have been discovered to be attacked underground as early as two years after planting. Termites and rot fungi attack the inner tissues and leave a pattern characteristic for the species of the pole. Tectona grandis, Nauclea diderrichii and Wide Pore pine, the major species for transmission poles in Nigeria show these attacks. A form of termite shi...
M A Odeyinde
Blue-stain fungi (Ceratocystis spp.) found in Spain on pine woods
1989 - IRG/WP 1410
So far, there is only a very limited reported description of the different Ceratocystis spp. present on fresh wood in Spain. So, the main goal of this work has been the identification of species of this genus causing blue-stain on Pinus pinaster A. Ait. and Pinus sylvestris L. woods. We have also investigated the relationship between the species found and their propagation vectors (insects and win...
M T De Troya, A M Navarrete
Collaborative experiments in testing the toxicity of wood preservatives to soft rot fungi
1970 - IRG/WP 25
Eight Institutes from seven countries, Austria, England, France, Germany, Holland, Sweden and Switzerland have collaborated in an attempt to assess the suitability of various laboratory test procedures for acceptance as standard methods of determining the toxicity of wood preservatives to the cellulose-attacking micro-fungi which cause 'soft rot' of wood. Pure culture methods wit...
J G Savory, A F Bravery
Relationship between stacking, location and antisapstain preservatives on visible degrade of Eucalyptus regnans and Pinus radiata boards
1999 - IRG/WP 99-20162
An antisapstain trial was established at a Eucalyptus hardwood sawmill in Victoria, Australia. The trial incorporated two commercial formulations of antisapstain preservatives, used at four different concentrations on both hardwood (Eucalyptus regnans F. Muell) and softwood (Pinus radiata D. Don) boards. The trial also utilised different stacking methods (block-stacked, sticker-stacked, and block-...
J Snow, P Vinden, S M Read
An insight into brown rot decay of timber as revealed by 13C CP/MAS NMR
1985 - IRG/WP 1259
L E Leightley
A preliminary report on lignicolous marine fungi in the Java Sea, Indonesia
1982 - IRG/WP 488
This report is part of a study on the natural durability of Indonesian timbers against marine borers conducted in Pari Island waters, Java Sea (Suhirman and Eaton, 1981), and contains preliminary information which has not yet been published....
Suhirman, R A Eaton
Tentative method of testing wood preservatives against blue staining
1977 - IRG/WP 259
The blue stain of sawn wood is still a real problem in Poland. Although a preservative based on sodium orthophenylphenoxide has been introduced into sawmill practice, and the technology of wood protection developed with it, new information has been obtained concerning blue stain in wood material destined for export. In order to select new chemicals or to improve the effectiveness of the ones in cu...
E Tarocinski, O Lewandowski, M H Zielinski
Natural durability and basic physical and mechanical properties of secondary commercially less accepted wood species from Brazil
2002 - IRG/WP 02-10451
The natural durability towards basidiomycete fungi and termites of several secondary timber from Brazil (Vatairea sp., Hymenolobium sp., Inga sp., Manilkara sp., Caryocar sp., Terminalia sp., Apuleia sp.) has been evaluated according to the EN 350-1. Some basic physical and mechanical properties (density, shrinkage, hardness, colour, static strength in flexion and compression) were also measured a...
M-F Thévenon, A Thibaut
Some wood-destroying Basidiomycetes. Volume 1 of a collection of monographs
1981 - IRG/WP 1121
One of the first tasks of the International Research Group on Wood Preservation, when it began its work in 1969, was to compile a series of reports on the common decay fungi which can attack wood. This volume, which contains the first of these reports, has been compiled with the help of mycologists and wood preservation specialists in France, Ghana, the Federal Republic of Germany, the Netherlands...
R Cockcroft
Efficacy of some extractives from Pinus heartwood for protection of Pinus radiata sapwood against biodeterioration. Part 1: Fungal decay
1995 - IRG/WP 95-30072
Chemical compounds thought to contribute to the natural durability of heartwood of Pinus spp. were either chemically synthesised in the laboratory or extracted from the heartwood of Pinus elliottii or Pinus caribaea. These compounds included the stilbenes, pinosylvin and its mono- and di-methyl ethers, and the flavonoids, pinobanksin and pinocembrin. Small blocks of Pinus radiata sapwood were impr...
M J Kennedy, J A Drysdale, J Brown
A new approach to the maintenance of wooden railway sleepers. (Second report)
1988 - IRG/WP 3492
The microenvironment and micro-ecology of wooden railway sleepers was investigated to assess their condition to determine the necessary treatment, repair and replacement criteria. In this report the efficacy of the secondary preservative treatment with solid boron rods is discussed and the development of an in-situ, nondestructive test method based on the creation and assessment of structural dyna...
W Beauford, P I Morris, A M Brown, D J Dickinson
Detection of incipient brown rot decay in wood by fourier transform infrared spectrometry
1987 - IRG/WP 2275
Fourier transform infrared spectrometry was evaluated as a possible method for detecting different levels of brown-rot decay in pine sapwood. By using first derivative spectra and regression analysis, an equation based on 4 absorption peaks, normalized with an internal standard peak, was developed. The correlation between weight loss and absorption was highly significant indicating that this is a ...
D D Nicholas, T Schultz
Prevention of brown-rot decay by chelators
1992 - IRG/WP 92-1540
In this work the brown-rot decay was shown to be prevented by chelating the endogenous metals existing in wood by using organic or inorganic chelators or iron-binding siderophores. The fungal growth and decaying ability were significantly decreased by the chelating treatments of the solid wood-based culture medium and pine wood pieces, respectively. The transition metals existing in native wood ar...
L Viikari, A-C Ritschkoff
The effect of storage or simulated internal use on the durability of wood based panels to decay fungi
1997 - IRG/WP 97-20106
Wood based panels such as particleboard and medium density fibreboard are experiencing a steady increase in use, in areas from structural to decorative applications. Understanding the "natural" durability of these panel products against basidiomycete fungal decay is therefore of great importance. Various methods have been proposed or are under development to test the durability/susceptibility of v...
S F Curling, R J Murphy, J K Carey