Your search resulted in 892 documents. Displaying 25 entries per page.
Problems of fixation of CCA-preservatives in palm-wood
1985 - IRG/WP 3338
Palm-wood may be used for posts and poles where it needs proper treatment for long time use. Based on observations by W. Killmann on low CCA-fixation in palm-wood, samples of Jubaea-palm grown in a Greenhouse at Hamburg, have been treated in two different series with a 4% solution of CCA-type B. After 1-16 weeks of storage the blocks were split into sticks of 1-2 mm² and leached. In all series 50...
H Willeitner, K Brandt
Problem of the treatment of dried sawn spruce building timbers with water-borne preservatives. Interim reports for discussion at the 4th Annual Meeting in West Berlin on 27 October 1972
1972 - IRG/WP 311
One of the most difficult technical problems facing the preservation industry is how to improve the treatment of refractory species of timber such as spruce. Its resistance to penetration, even under pressure' precludes its use for more hazardous service situations, and even in less severe conditions a higher level of treatment would be desirable. The importance of this subject led us to ...
W Liese, J W W Morgan, T Hof, R O Ullevålseter
A new concept of oxalic acid biosynthesis in physiology of copper-tolerant brown-rot fungi
2001 - IRG/WP 01-10394
Recently, a wide variety of roles of oxalic acid (oxalate) in wood decay systems have been receiving much attention. Copper tolerance of wood-rotting basidiomycetes has been believed to be due to the detoxification of copper wood preservatives by oxalate produced by these fungi. However, biochemical mechanism of oxalate biosynthesis in relation to physiology of wood-rotting fungi has not been eluc...
E Munir, T Hattori, M Shimada
Principles and procedure of the planeing test
1981 - IRG/WP 2162
Small end-sealed samples of pine-sapwood (1.5 x 2.5 x 5 cm³) are treated by brushing and afterwards different parts of the treated surface are removed. The remaining part of the sample is tested against either insects or fungi. If no attack occurs sufficient amounts of biocides have been penetrated at least beyond the zone which has been removed. In spite of some problems the test seems the only ...
H Willeitner, M Gersonde
The registration of wood preservatives under the Pesticides Act of 1962 in the Netherlands
1976 - IRG/WP 364
J Van der Kolk
IRG/COIPM INTERNATIONAL MARINE TEST - to determine the effect of timber substrate on the effectiveness of water-borne salt preservatives in sea-water. Progress Report 8: Panama test results
1980 - IRG/WP 458
Summary of damage to ITRG test stakes by pholadidae and teredinidae at the Panama test site - 8 Mar. '78 to 11 Oct. '79...
J R De Palma
Soil blocks versus field test for evaluating and standardizing wood preservatives: A commercial view
1994 - IRG/WP 94-20024
On the basis of technical considerations, experience, costs and applicability, the author concludes that the soil block test and other laboratory tests have little meaning in a wood preservative standardization process and almost no merit in the commercialization of a wood preservative system. Field tests at sites known to be aggressive to preservative treated wood are strongly recommended....
W S McNamara
AAC preservatives: Recent New Zealand and Australian experience
1982 - IRG/WP 3188
This paper outlines the present commercial situation in New Zealand, presents results of current research undertaken at FRI and CSIRO, Division of Building Research (DBR), and comments on parallel research carried out elsewhere. Finally, some general comments are made on the limitations of present technology....
J A Butcher, H Greaves
Copper naphthenate performance: A new way to look at old data
2000 - IRG/WP 00-30215
Although copper naphthenate has over a 50-year test history, it is still considered as a "new" preservative in the United States when it is used for utility poles. It has also been extensively used in remedial treatments for poles and has considerable retail or over-the-counter sales. The test history includes a number of different tests and a rationale for evaluating this data and comparing the p...
C R McIntyre
Spruce lumber treatments with ammoniacal solutions of inorganic preservatives
1977 - IRG/WP 391
As a part of our work in the Wood Preservation group at the Eastern Forest Products Laboratory in Ottawa to facilitate exploitation of spruce, which is a large timber resource in Canada, we have been studying the treatability of spruce roundwood. A report on this subject was presented to this group last year. More recently, another commodity - spruce timber - has been rapidly gaining the interest ...
R Rak
Use of vermiculite as substrate in assays on phytotoxicity of treated wood
1989 - IRG/WP 3547
It is considered the possibility of using vermiculite instead of soil as substrate in assays on phytotoxicity of wood treated with preservatives for agricultural use. Three organic preservatives were used. It had been tested the behaviour of both, vermiculite and soil in case of preservative leaking due to a leach. So that, assays of germination with cucurbitaceous were carried out, mixing a dose ...
M V Baonza Merino, D Franco
CEN Draft (38 N 460E) Standard: Test method for determining the protective effectiveness of a preservative in the marine environment
1986 - IRG/WP 4132
This European Standard describes a marine test method which provides a basis for asseasing the effectiveness of a wood preservative used to prevent attack of timber in sea-water by marine borers. The method is only suitable for testing preservatives which are intended to prevent attack by marine wood boring organisms of treated timber for use in more or less permanent contact with sea-water. It is...
G Castan
Supplement to Document No: IRG/WP/56. Health and safety aspects of the use of wood preservatives
1975 - IRG/WP 356
H Willeitner
Wood preservation in France. "Bois plus" chain of quality. Description of the scheme early 1989
1989 - IRG/WP 3519
1989 - description of the French "CTB-BOIS PLUS" homologation scheme
G Ozanne
Effects of various preservative treatments on the mechanical and physical properties of plywood
1993 - IRG/WP 93-40007
The technical properties of plywood are related to both the intrinsic characteristics of its composing wood species and the quality and performance of the glue bond which acts as an interface between veneer sheets. Consequently mechanical and physical testing and glue bond strength analysis offer an appropriate means for studying the effect of preservative treatments on the overall quality of plyw...
J Van Acker, M Stevens
Exposure trial at tropical marine sites of pyrethroid/creosote mixtures as wood preservatives: Preliminary results
1989 - IRG/WP 4155
Pinus sylvestris sapwood blocks measuring 25 x 25 x 200 mm³, impregnated using a Lowry or Rüping pressure treatment cycle with solutions of permethrin, cypermethrin or deltamethrin in BS144 creosote, have been exposed at marine sites in Australia, Papua New Guinea, the U.K. and Singapore. The effectiveness of these solutions in preventing marine borer attack is being compared with the efficacy o...
S M Cragg
A new wood preservative based on polymerized complexes of aminotriazole with copper acetate
1998 - IRG/WP 98-30169
This paper presents the results of preliminary fungitoxicity tests as carried out on new polymerized complexes of aminotriazole with copper acetate (PCC) against Coniophora puteana and Trichoderma viride.
Laboratory tests on wood confirmed the findings arrived at in the screening test on agar medium. Deep penetration into pine wood of compounds studied was observed and particularly so at humidity...
K J Krajewski, A Lukasiewicz, J Wazny
Conforming to european standards for preservative-treated timber: Specifying with confidence
2000 - IRG/WP 00-20194
A four-year collaborative study between four industrial partners and BRE has assessed timber treated by current UK industrial practices in the light of current European Standards. Data were collected for CCA and creosote treated timber components, and compared with the requirements laid out in EN351-1 and -2. A number of difficulties were encountered that have been described in previous IRG papers...
E D Suttie, R J Orsler
Point sur la réglementation et contraintes administratives
1990 - IRG/WP 3575
J H Moneger
Some aspects of laboratory and field testing methods of antitermite wood preservatives
1973 - IRG/WP 235
Various methods for laboratory testing of antitermite activity of wood preservatives are described. The results of simultaneous tests of three water-borne preservatives, according to the various methods are discussed, and comparison is made with results of field tests on the same three preservatives, showing a fairly good accordance between laboratory results and field results....
M Fougerousse
Determination of the preventive efficacy against wood destroying basidiomycetes fungi, EN V 839 - CEN/TC 38 WG 9
1993 - IRG/WP 93-20015
The WG 9 of CEN TC/38 has presented to EC a mycological test to assess efficacy of preservatives applied by surface process. This method is now an experimental standard (EN V 839) which has to be approved by the different european delegations. The following paper is not the standard as it has been proposed but is a presentation of the principle of the method. The experimental standard specifies a ...
D Dirol
Inventory of the use of preservative-treated wood and wood preservatives in Sweden 1900-1997
1999 - IRG/WP 99-50137
The objective of this study was to present an overview of the use of wood preservatives and their active ingredients and industrially preservative-treated wood in Sweden since the beginning of the 20th century. The data presented in the report could for example be used as a basis for different waste management scenarios for preservative-treated wood. Before 1960 railway sleepers and utility poles ...
J Jermer, K Nilsson
Assessing the risks from the use of wood preservatives
2001 - IRG/WP 01-50166-07
PPT-Presentation...
C B Welch
Monographic card on Antrodia serialis
1984 - IRG/WP 1145
G Seehan
Test procedure to determine the effect of timber substrate on the effectiveness of different preservatives in sea-wate
1975 - IRG/WP 414
R A Eaton