Your search resulted in 744 documents. Displaying 25 entries per page.
Durability of surface preserved wood particle boards submitted to atmospherical influence
1995 - IRG/WP 95-40039
The worldwide problem of the continuously growing deficit of high quality natural wood material has caused the attempts of many research workers to find effective composites such as wood particle boards (WPBs) for replacing the massive wood for constructive purposes, depending on where the boards are exploited - in the open or under a shed, they are submitted to various climatic factors such as he...
L Valcheva
Durability of surface coating systems. Mycologg - an accelerated mycological test.
2004 - IRG/WP 04-20301
Field testing and natural aging/degradation of test sample, e.g. coated wooden surfaces is a slow process. Accelerated tests focus on mechanical properties, water uptake or sometimes stain fungi.
Artificially weathered coated panels are not easily compared with naturally aged panels, and show the importance of involving the biological component among the degrading facors. It is a need for acce...
L Ross Gobakken, J Mattsson, B Jacobsen, F G Evans
Resistance of pine and spruce heartwood against decay - The effect of wood chemical composition and coating with water-borne wood oil product
2006 - IRG/WP 06-10597
Natural durability of wood has been widely studied, but the combination of the natural durability and different treatments has not been the focus of many studies. The durability of wooden products is mainly based on the water permeability and the resistance against organisms. In this study, the water absorption and decay resistance of sapwood and heartwood of Scots pine and Norway spruce were exam...
H Viitanen, S Metsä-Kortelainen, T Laakso
Bi-oleothermal treatment of wood at atmospheric pressure: resistance to fungi and insects, resistance to weathering and reaction to fire results
2008 - IRG/WP 08-40418
Bi-oleothermal process is a simple treatment which has been developped by CIRAD in cooperation with FCBA. It allows a deep impregnation of wood with hydrophobic products using cheap facilities. The process includes two steps at atmospheric pressure. The first one is a dipping of wood samples in a hot oil bath (between 110 °C and 200°C) which creates an overpressure inside the wood. The second on...
L Podgorski, I Le Bayon, I Paulmier, J-D Lanvin, V Georges, D Grenier, H Baillères, J-M Méot
Moisture protection and performance during 5 years exposure of 19 wood coating systems on a cladding in Vienna
2011 - IRG/WP 11-40561
A cladding with vertical boards of Norway spruce (Picea abies) comprising different coating systems had been exposed to natural weathering oriented south west in Vienna for 5 years. Weathering behaviour of the boards was assessed in intervals and wood moisture content was measured over the first 22 months of exposure. The moisture protective properties of the coating systems were assessed using la...
G Grüll, I Spitaler, M Truskaller
How to Increase the Lifespan of Exterior Wood Coatings
2015 - IRG/WP 15-40700
In addition to aesthetic appeal, coatings are designed to protect the wood from weathering degradation in outdoor conditions. This paper gives an overview of the effects of main components of coating, coating properties, and wood treatments on coating performance. Understanding how different type of resins (alkyd, acrylic or polyurethane), amount of pigments, type of solvents (organic or water), a...
M Nejad
Improvement of short rotation teak wood properties through thermal modification
2018 - IRG/WP 18-40842
Teak (Tectona grandis L.f) is one of the most popular tropical timber species. Nowadays, the source of long rotation teak is limited in the availability. Many wood processing industries use short rotation teak, which has lower quality especially in durability and dimensional stability. Heat treatment is an eco-friendly method improving dimensional stability and durability of wood. The objectives o...
L A Pratiwi, I W Darmawan, B George, A Merlin, C Gérardin, S Dumarçay, T Priadi, P Gérardin
Wood protection with cement – Part 1: Coating matters and durability of cement coated wood
2020 - IRG/WP 20-40911
The use of wood in geotechnical applications has seen renewed interest. However, concerns related to the durability and service life of wood in ground contact applications remain. Wood has the potential to substitute commonly used steel and concrete in the geotechnical engineering sector, but solutions to extending the service life and maintenance intervals require long-lasting wood protection sys...
S Hirschmüller, B Marais, C Brischke, A Krey, J Bösing
Quantitative Prediction of Latent Deterioration in Wood Coatings Using Mid-Infrared Spectroscopy and Machine Learning
2025 - IRG/WP 25-41038
Wood coatings play a vital role in prolonging the lifespan of timber structures by protecting them from environmental degradation. However, conventional evaluation methods rely on visual inspections, which cannot detect latent deterioration before visible damage occurs. This study integrates attenuated total reflectance-Fourier transform infrared (ATR-FTIR) spectroscopy with partial least squares ...
Y Teramoto
Development of an Early Degradation Diagnosis Technology for Wood Coatings Using Mid-Infrared Spectroscopy and Machine Learning
2025 - IRG/WP 25-41047
Accurately predicting the degradation state of wood coatings is challenging, and as the coating deteriorates, it becomes a major factor accelerating the degradation of the wood itself. In this study, we aimed to develop a diagnostic technology that combines mid-infrared spectroscopy and machine learning to assess latent coating degradation, which cannot be detected visually, and to enable appropri...
K Nishimura, T Ito, S Isaji, T Takano, H Ohki, Y Teramoto
Management of the wood and additives wastes in the wood processing industries: Problematics and technical answers review
1996 - IRG/WP 96-50073
Management pathways for pure wood subproducts are well known and used; but as soon as additives like preservatives, glues, varnishes or coatings are present within the wood wastes, their disposal or valorization becomes more tricky. The different kinds of mixed wood wastes of the wood processing industries, from the sawmill to the furniture manufacture, are identified herewith and their diversity ...
S Mouras, G Labat, G Deroubaix
JWPA method for testing effectiveness of surface coatings with preservatives against decay fungi
1981 - IRG/WP 2164
In 1979 JWPA established a new method for testing effectiveness of surface coatings in accordance with practical use of preservative-treated lumber. Comparing the new testing method with JIS A 9302, a few new trials - size of wood specimen, weathering procedure, and decay-test procedure - are incorporated....
K Tsunoda
Summary of development of pile wrappings in Los Angeles Harbour
1987 - IRG/WP 4141
G Horeczko
Effects of acetylation on the dimensional stability and decay resistance of kenaf (Hibiscus cannabinus L.) fiberboard
1996 - IRG/WP 96-40059
The objective of this study was to investigate the influence of the acetylation treated kenaf fiber, Phenol formaldehyde resin content level, and three fungi species on the dimensional stability and decay resistance of high density non wood composition boards. A standard ASTM method was used to evaluate weight loss and thickness change. The linear shrinkage and expansion of each species were also ...
P Chow, T Harp, R Meimban, J A Youngquist, R M Rowell
Wood preservation in Lithuania
2004 - IRG/WP 04-30363
This article is intended to give basic information on wood preservation activities in Lithuania and the main actors in wood preservations practice and research. Currently the main actors in practical Lithuanian wood preservation activity are enterprises of wood preservation industry united by the Lithuanian Wood Preservation Association. The most intensive activity in wood preservation practice an...
J Saladis
European standardization for wood preservation
1988 - IRG/WP 2321
G Castan
European standardization for wood preservation
1989 - IRG/WP 2335
G Castan
The susceptibility of 35 Amazon wood species to Cryptotermes brevis (Walker)
1982 - IRG/WP 1160
Laboratory tests were carried to evaluate the susceptibility of 35 Amazon hardwoods to Cryptotermes brevis (Walker). The results were analysed statistically and showed that five wood species were non resistant, nine were resistant and the other twenty-one in between those classes of resistance....
M D Canedo
Possibility of use of wood species per class of biological risks. Attempt to determine criteria based on Pr EN 350-1/2/3
1992 - IRG/WP 92-2409
M Rayzal
Development of marine borers research in Sao Paulo State, Brazil
1985 - IRG/WP 4117
This paper describes some field tests which have been carried on marine sites in Sao Paulo State mainly to investigate the natural resistance of Brazilian woods and the occurrence of marine borers. Some laboratory breeding tests which are being developed are also describe...
G A C Lopez
Natural Resistance of timbers to marine borer attack. COIPM/IRG CO-OPERATION. Final report concerning panels exposed in the sea at Sekondi, Ghana
1979 - IRG/WP 449
The test was carried out according to Document COIPM/72.044, Revised procedure for the testing of naturally durable timbers against marine borers. The panels of the three species remaining in the test at the end of 1978 were removed and assessed visually. An average rating was given to the panels of each species....
F F K Ampong
Natural durability transfer from sawmill residues of white cypress (Callitris glaucophylla). - Part 3: Full penetration of the refractory sapwood of white cypress
2000 - IRG/WP 00-40167
The heartwood of white cypress, Callitris glaucophylla, is renowned for its termite resistance and durability against decay. The sapwood, which can represent up to 30% of log volume, is non-durable and refractory to conventional preservative treatment. Previous work ascribes the lack of permeability to oily deposits within tracheids and ray cells. Environmental scanning electron microscopy was use...
M J Kennedy, L M Stephens, M A Powell
Interspecific variability of European oak durability against white rot fungi (Coriolus versicolor): Comparison between sessile oak and peduncle oak (Quercus petraea and Quercus robur)
2001 - IRG/WP 01-10393
The knowledge of wood natural durability against biologic predators enable its external use. The resistance of European oak wood was reported like durable according to the EN 350-2. However, some individuals may contain high durable wood. Our research was focused to understand this variability in oak population that represent the first french species (4.1 millions of ha). Natural durability of Eur...
N Ayadi, B Charrier, M Irmouli, J P Charpentier, C J Allemand, F Feuillat, R Keller
Durability of larch (Larix spp.) wood against brown-rot fungi
1997 - IRG/WP 97-10228
Durability of the heartwood of Larix decidua, L. sibirica, L. gmelinii, L. gmelinii var japonica, L. gmelinii var olgensis and L. sibirica x decidua against brown rot fungi Coniophora puteana, Poria placenta and Gloeophyllum trabeum was tested according to EN 113 test method. Parallel samples were used to study the amount and composition of wood extractives. The sample trees originated from the re...
H Viitanen, L Paajanen, P Saranpää, P Viitaniemi
The effect of sapwood on the rate of deterioration of fence posts
1986 - IRG/WP 1277
In order to evaluate the effect of the presence of sapwood on the rate of deterioration of fence posts, 30 specimens with and without sapwood of Eucalyptus citriodora, Eucalyptus paniculata, Eucalyptus saligna and Eucalyptus tereticornis were exposed in three test sites in the State of São Paulo, Brazil. The results of the inspection carried out in 1985, after 5 years of exposure, are reported in...
M S Cavalcante, G A C Lopez, E S F Mucci, R G Montagna