Your search resulted in 90 documents. Displaying 25 entries per page.
Contribution to the testing of wood based board material
1982 - IRG/WP 2176
R G Lea
Worldwide in-ground stake test of acetylated composite boards
1997 - IRG/WP 97-40088
Acetylated wood composite stakes are being tested in ground contact (graveyard test) in seven fields around the world. Three types of acetylated wood composites were prepared: spruce fiberboard in Sweden, aspen fiberboard in Madison and rubber wood particle board in Indonesia. Two levels of acetylation were used, a high level of ~20% acetyl content and a low level of 10% acetyl content. Control bo...
R M Rowell, B S Dawson, Y S Hadi, D D Nicholas, T Nilsson, D V Plackett, R Simonson, M Westin
Biological Protection of Composite Panel from Moulds and Decay
2007 - IRG/WP 07-10612
Composite panels, such as oriented strand board (OSB), are widely used in house construction in North America. These structural panels are normally made of non-durable wood species and are susceptible to moulds and decay when exposed to wet conditions. Building envelope failures due to moulds, decay or poor construction practices can negatively impact the image of wood. To ensure durability of com...
Dian-Qing Yang, Xiang-Ming Wang, Hui Wan
Effects of Nano-Zycosil on Liquid and Gas Permeability of MDF
2012 - IRG/WP 12-40578
Effects were studied of zycosil nanoparticles, with size range from 30 to 90 nm, on liquid and gas permeability of medium density fiberboard. 100 g of nanozycosil was added to each kg of dry fibers. Density was kept constant at 0.67 g/cm3. The obtained results indicated that addition of zycosil to the mat resulted in a significant increase in gas permeability due to the lower fiber-content in the ...
H Reza Taghiyari, K Heidarhaee, P Noori, A Karimi
Nano-Zycosil in MDF. Part I: Gas and Liquid Permeability
2014 - IRG/WP 14-40652
Effects were studied of zycosil nanoparticles, with size range from 20 to 80 nm, on liquid and gas permeability of medium density fiberboard. Nanozycosil was used at four consumption levels of 0, 50, 100, and 150 g/kg dry wood fibers. Density of all treatments was kept constant at 0.67 g/cm3. The obtained results indicated that the addition of zycosil to the mat resulted in a significant increase...
H Reza Taghiyari, A Karimi, P M D Tahir, O Schmidt, E Bari, P Nouri , A Jahangiri
Effect of silver nanoparticles on the rate of heat transfer to the core of the medium-density fiberboard mat
2014 - IRG/WP 14-40653
Effect of silver nanoparticles on the rate of heat transferred to the core section of medium-density fiberboard (MDF) mat was studied here. A 400 ppm aqueous nanosilver suspension was used at three consumption levels of 100, 150, and 200 mL/kg based on the weight of dry wood fibers; the results were then compared with the control MDF panels. The size range of silver nanoparticles was 30-80 nm. Res...
H Reza Taghiyari, O Schmidt, E Bari, P M Tahir, A Karimi, P Nouri, A Jahangiri
The resistance of composite boards protected with azole and inorganic nanoparticles to basidiomycetes and moulds
2015 - IRG/WP 15-40688
This paper presents a study on the resistance of wood composite boards, glued with silicone adhesive and obtained from chips of Scots pine Pinus silvestris L. and willow Salix viminalis L., to basidiomycetes and mould. The boards were protected in the production processes with fungicides based on metal nanoparticles, as well as on derivatives of 1,2,4-triazole, benzimidazole, and thiazole. The bio...
J Zabielska-Matejuk, I Frąckowiak, A Stangierska
Increasing the hardness of wood-composite panels by nanosilver
2016 - IRG/WP 16-40715
Effect of silver nanoparticles on hardness in medium-density fiberboard (MDF) was studied here. A 400 ppm aqueous nanosilver suspension was used at three consumption levels of 100, 150, and 200 mL/kg, based on the dry weight of wood fibers; the results were then compared with the control panels. The size range of silver nanoparticles was 30-80 nm. Composite mats were hot-pressed for 6, 8, and 10 m...
H R Taghiyari, J Norton, K Heidarhaee
Effect of Nano-Silane on Permeability in MDF as a Result of Susceptibility to Moulds and Fungi
2016 - IRG/WP 16-40716
Effects were studied of vapor chamber on specific gas permeability of nanosilane-treated medium-density fiberboards (MDF). Size range of nanoparticles was 20 – 80 nm. Nano-silane (NS) was used at four consumption levels of 0, 50, 100, and 150 g/kg dry wood fibers. Density of all treatments was kept constant at 0.67 g/cm3. Specimens were kept for 18 weeks in vaporized chamber; their specific gas ...
H R Taghiyari, J Norton, A Moradiyan, M Sadegh Taher Tolou Del, H Siahposht, B Moradi-Malek, M Noferesti
Nondestructive Evaluation of Oriented Strand Board Exposed to Decay Fungi
2002 - IRG/WP 02-20243
Stress wave nondestructive evaluation (NDE) technologies are being used in our laboratory to evaluate the performance properties of engineered wood. These techniques have proven useful in the inspection of timber structures to locate internal voids and decayed or deteriorated areas in large timbers. But no information exists concerning NDE and important properties of wood composites exposed to dec...
B Illman, V W Yang, R J Ross, W J Nelson
Mycological testing of plywood and board materials. Part 1: Review of information supplied by IRG members
1978 - IRG/WP 284
In December 1975 IRG members were asked for published information, information of current work in progress and views on mycological test methods for board materials. The object was to stimulate discussion and possibly establish a joint research effort within IRG in order to establish a meaningful test with reproducible results....
C R Coggins
Results on termite resistance of building materials against Coptotermes formosanus by choice test
1998 - IRG/WP 98-10275
Various building materials, included wood species, wooden board materials, thermal insulation materials and fire-protection materials, were tested for grading of termite resistance against Coptotermes formosanus. The dimension of most specimens were 2x2x2cm3. Ten repeats were prepared. The specimens were put between Akamatsu sapwood control specimens on a laboratory cultured mound colony of termit...
K Suzuki, K Hagio
The effect of storage or simulated internal use on the durability of wood based panels to decay fungi
1997 - IRG/WP 97-20106
Wood based panels such as particleboard and medium density fibreboard are experiencing a steady increase in use, in areas from structural to decorative applications. Understanding the "natural" durability of these panel products against basidiomycete fungal decay is therefore of great importance. Various methods have been proposed or are under development to test the durability/susceptibility of v...
S F Curling, R J Murphy, J K Carey
Field testing of soil insecticides as termiticides
1986 - IRG/WP 1294
This paper reviews field methods used to evaluate soil insecticides as termiticides by the U.S. Department of Agriculture, Forest Service, Gulfport, Mississippi. Field tests are conducted on a minimum of five "nationwide sites" in the United States to determine the efficacy of chemicals in various soil types and against different termite species. Test results of selected insecticides are presented...
R H Beal
Use of the Pilodyn to assess deterioration of treated aspen waferboard after 30 months of outdoor exposure
1986 - IRG/WP 2254
Samples of preservative treated aspen waferboard exposed outdoors for 30 mo. were compared using pin penetrations of the 6 Joule Pilodyn. These results correlated well with rankings of treatment performance based on more laborious standard mechanical tests, and demonstrate the potential for use of the Pilodyn as a tool to evaluate wood composites in test exposures with minimal destruction....
E L Schmidt, M G Dietz
Decay resistance of high performance biocomposites based on chemically modified fibres
1998 - IRG/WP 98-40120
Different partners within the framework of a European research project produced high performance biocomposites aiming at the utilisation of board materials as durable products both in dimensional and biological degrading circumstances. This paper summarises test data, which indicate the potential of board materials produced with modified fibre material. The chemical modifications applied cover a r...
V Rijckaert, J Van Acker, M Stevens
Biodegradation of acetylated southern pine and aspen composition boards
1994 - IRG/WP 94-40020
This objective of this study was to investigate the influence of the acetylation treated wood fiber, Phenol-formaldehyde resin content level, two wood fiber species, three fungi species on the dimensional stability and decay resistence of high density composition boards. A standard ASTM method was used to evaluate weight loss and thickness change. The linear shrinkage and expansion of each species...
P Chow, T Harp, R Meimban, J A Youngquist, R M Powell
The evaluation of the occurrence of soft rot in creosoted wooden poles
1988 - IRG/WP 1368
The occurrence of soft rot decay in creosoted wooden poles for overhead power lines was investigated by collection of field samples, their subsequent microscopic examination and statistical analysis of the data collected. Examination of samples collected from 296 poles revealed that approximately 15% of the pole population studied (Eastern Electricity Board) showed the presence of soft rot decay. ...
A Wylde, D J Dickinson
A Preliminary Report on the Properties of Engineered Wood Composite Panels Treated with Copper Naphthenate
2005 - IRG/WP 05-40294
This paper reports on our preliminary investigation of the properties of randomly oriented strandboard which had waterborne or powdered copper naphthenate (CuN) incorporated into the board during manufacture. When compared to zinc borate-treated controls (ZnB), the mechanical properties of strandboard (MOR, MOE, work-to-maximum load, internal bond strength) were not adversely affected by treatmen...
J W Kirkpatrick, H M Barnes
Health and safety aspects of the use of wood preservatives in Sweden
1977 - IRG/WP 396
The Act on products Hazardous to Health and to the Environment (Swedish Code of Statutes SFS 1973:329) came into force on 1st July 1973. The Act cancelled and superseded the Poison Act, the Pesticides Act and the PCB Act from 1962, 1962 and 1971 respectively. Regulations for the implementation of the Act are contained in the Ordinance on Products Hazardous to Health and to the Environment (SFS 197...
B Henningsson
Utilization of plasma treatments in the field of wood protection
2021 - IRG/WP 21-40912
Plasma treatments have been used for modification of surfaces of wood and wood-based materials for some decades and solutions were developed to apply it for wood protection. This contribution aims to present the background, introduce the available plasma technology, and to give an overview on the typical applications and benefits....
S Dahle, H Militz
Treatment of wood-based panel products with volatile borate
1990 - IRG/WP 3616
The paper presents recent developments in the use of volatile borate esters for the preservative treatment of wood based board materials. Several advances on previous reports are discussed. In laboratory studies, treatment times of approximately ten minutes at 20°C on boards at equilibrium moisture content provided full penetration and retentions of 1% wt/wt boric acid. Biological tests have been...
P Turner, R J Murphy, D J Dickinson
Properties of plywood and Oriented Strand Board manufactured with an organic insecticide incorporated in the adhesive formulation
2000 - IRG/WP 00-40174
The efficacy of Fipronil as an insecticide has been established by laboratory and field experiments and commercial use against a broad range of insect pests for various crops. It can be used by either foliar or soil application. Development is underway for the non-agricultural uses of fipronil. Research is ongoing for the control of ants, cockroaches, fleas, ticks, houseflies, mosquitoes, termites...
D P Kamdem, J H Hope, A Jermannaud
Durability of Wood Plastic Composites Relative to Natural Weathering and Preservative Treatment With Zinc Borate
2005 - IRG/WP 05-40316
Wood-Plastic Composites (WPCs) used for decking have experienced dramatic increases in North America, averaging 25% growth per annum since 1998. A key factor contributing to this growth has been the successfully communicated message that they are "virtually maintenance free". The common perception being that the wood fiber is completely encapsulated by the thermoplastic resin, minimizing the pot...
M E Mankowski, F M Ascherl, M J Manning
Soil bed studies of the dimensional stability of composite products
1999 - IRG/WP 99-40134
The influence of boron and isocyanate resin on the dimensional stability of high moisture resistant particleboard was assessed after burial in a soil bed for one month. The samples were treated with two levels of a boron compound and coated in isocyanate resin. The samples were randomly placed in a fungal cellar in soils of two different water holding capacities. Weight differences and dimensional...
K M Filcock, P Vinden