IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 1630 documents. Displaying 25 entries per page.


Studies on accelerated ageing procedures with TBTO-treated wood
1985 - IRG/WP 2244
The efficacy of various procedures for accelerated ageing of organotin based wood preservatives in treated wood has been investigated. It was found that leaching of the treated wood samples in water according to the European Standard EN 84 was not satisfactory for organotin based preservatives and is probably also unsuitable even for other types of organic solvent preservatives. Keeping tributylti...
J Jermer, M-L Edlund, B Henningsson, W Hintze


Additions and corrections to recent names for some common decay fungi
1977 - IRG/WP 167
A Käärik


A summary of current information on actinomycetes and wood
1978 - IRG/WP 177
B King, R A Eaton, A A W Baecker


The dry rot fungus and other fungi in houses. Part 2
1993 - IRG/WP 93-10001
J Bech-Andersen


Valid names for some common decay fungi, their synonyms and vernacular names
1978 - IRG/WP 172
A Käärik


Resistance of Alstonia scholaris vestures to degradation by tunnelling bacteria
1992 - IRG/WP 92-1547
Electron microscopic examination of vessels and fibre-tracheids in the wood of Alstonia scholaris exposed to tunnelling bacteria (TB) in a liquid culture showed degradation of all areas of the secondary wall. The highly lignified middle lamella was also degraded in advanced stages of TB attack. However, vestured pit membranes and vestures appeared to be resistant to degradation by TB even when oth...
A P Singh, T Nilsson, G F Daniel


Successive collections of Basidiospores from wood decay fungi (in vitro) show variation in germination levels on common media
1978 - IRG/WP 191
In the course of various preliminary experiments in which spore germination levels of 6 decay fungi on malt and water agar were recorded as controls, it was noted that one could not reliably obtain an expected level of spore germination for any particular fungus. Inconsistent 'control' spore germination levels of a fungus greatly complicates large scale experiments in which compa...
E L Schmidt, D W French


Durability of larch (Larix spp.) wood against brown-rot fungi
1997 - IRG/WP 97-10228
Durability of the heartwood of Larix decidua, L. sibirica, L. gmelinii, L. gmelinii var japonica, L. gmelinii var olgensis and L. sibirica x decidua against brown rot fungi Coniophora puteana, Poria placenta and Gloeophyllum trabeum was tested according to EN 113 test method. Parallel samples were used to study the amount and composition of wood extractives. The sample trees originated from the re...
H Viitanen, L Paajanen, P Saranpää, P Viitaniemi


The biostatic effect of copper on decay of fire retardant-treated mining timber
1991 - IRG/WP 1507
Blocks of Eucalyptus grandis were treated with 20kg/m³ ammonium sulphate as fire retardant and challenged with Coriolus versicolor. Replicates were soil buried. A second set of blocks was treated with retardant and copper at 6.6 kg/m³ (ie 1% w/w), and challenged similarly. After 8 weeks weight losses produced by Coriolus versicolor in untreated, retardant treated and copper supplemented blocks w...
G D Shelver, E A Shelver, A A W Baecker


Termite standards questionnaire survey. Second Report
1989 - IRG/WP 1395
Information contained in replies received from IRG members responding to the survey continue to be summarised. Again, highlighted in this second report are the major termite species in the various zoogeographical regions, their damage ranking to timber-in-service, the chemicals used in control methods, and the status of the termite standards in the respondent countries....
J R J French, J P La Fage


Trials on the field control of the Formosan subterranean termite with Amdro® bait
1982 - IRG/WP 1163
Amdro® - treated paper towels were introduced into two field colonies of the Formosan subterranean termite in Hawaii. At the concentration of 180 ppm, the toxicant bait was ineffective one month after the introduction. At higher concentrations (> 6,400 ppm), the baits were eaten initially; however, one week after introduction, termites avoided or covered the baits. The 15,000 ppm baits supress...
N-Y Su, M Tamashiro, J R Yates III


Respiration methods used to follow the decay of wood and the toximetric evaluation of wood preservatives
1975 - IRG/WP 249
When wood is attacked and decayed by fungi, wood substance and oxygen (02) are consumed, while carbon dioxide (CO2), water and heat are liberated. Early in the 1960's workers from England, Canada and Sweden began studying CO2 evolution, with respect to decay and its control using chemical preservatives, while in Germany and the USA O2 utilization was being similarly examined. Oxygen consu...
R S Smith


Soft-rot ultrastructure
1981 - IRG/WP 1138 (+ Addendum)
The stages of growth of soft-rot fungal hyphae in birch cell walls has been studied using transmission electron microscopy. These observations are compared with time-lapsed cinemicrographic studies on infection and cavity development within wood cell walls which show a start-stop hyphal growth pattern. The fine structure of hyphae during each stage of the decay process shows that hyphae penetratin...
M D C Hale, R A Eaton


Some characteristics of Pinus radiata wood from trees subjected to resin extraction
1987 - IRG/WP 3403
35 year old Pinus radiata trees growing in La Puntilla (lat. 37° south, long. 72,4° west), Chile, were subjected to resin extraction 5 years ago. After harvesting them simultaneously with control trees of the same place and age, probes were taken from the bottom of each pole, at 3.4 m, 7.8 m and 11.4 m height. Analysis of ethanol/benzene extract, CCA salt penetration tests and sapstain and brown-rot development rate were performed. The extract content differed in both groups. In the ascendent sense it decreases in unextracted trees and increases in extracted. CCA salt penetration was deeper in treated trees than in untreated. Wood subjectect to resin extraction was less susceptible to sapstain development. No significant difference was detected in both groups in relation to the development of brown-rot.
M C Rose, J Navarrete, G Sandoval, A Bedoya, L Ortega, R Zurita


In-ground performance of two formulations of chlorothalonil after five years of exposure at three test sites in Australia
1996 - IRG/WP 96-30101
Sapwood specimens of Pinus radiata D. Don and Eucalyptus regnans F. Muell. were each treated to three retentions of each of two preservative formulations (chlorothalonil in oil; chlorothalonil plus chlorpyrifos in oil) and installed in-ground at three field test sites in Australia. Specimens were treated with each formulation to achieve 3.2, 6.4 and 12.8 kg/m³ of chlorothalonil a.i. and 3.2 + 0.2...
J W Creffield, T L Woods, N Chew


A method of isolating actinomycetes from decayed wood
1974 - IRG/WP 126
This paper deals with a tentative method of isolating Actinomycetes from dacayed wood....
T Haraguchi


A laboratory method for assessing the effectiveness of fungicides in preventing the spread of decay fungi within packages of unseasoned lumber
1983 - IRG/WP 2202
To study the deterioration caused by decay fungi in the laboratory, a method for testing fungicides for their effectiveness in preventing spread of decay was devised. Some experiments using this method are reported here....
A J Cserjesi, E L Johnson, A Byrne


Screening-method for the examination of the resistance against contact-insecticides of Lyctus brunneus Steph. beetles
1981 - IRG/WP 2148
A serie of filter-paper rondelles is treated with different concentrations of an organic insecticide dissolved in aceton. Beetles of Lyctus brunneus are put onto the dry surfaces. During the impact of the poison the knock-down is observed and after a following poisonfree holding, the knock-down and mortality are registred....
E Graf, B Lanz


Laboratory evaluation of chemicals as termiticides
1986 - IRG/WP 1293
Laboratory procedures are described for screening chemicals against subterranean termites. Fast-acting compounds with persistent termiticidal activity are identified in tests using a soil substrate, and slower-acting bait toxicants are evaluated in a series of tests using cellulose substrates....
S C Jones


Influence of aliphatic acids on spore germination of wood decay fungi
1984 - IRG/WP 2224
Influences of eight saturated fatty acids (C5-C10, C12 and C16) on spores of four isolates of wood decaying basidiomycetes (white rot fungi: Poria tenuis and Trametes hispida; brown rot fungus: Gloeophyllum trabeum [two isolates]) were observed in-vitro. Spore response after 24 hr on malt extract agar containing 10, 10² , or 10³ ppm of each fatty acid included: no effect on normal germination, d...
E L Schmidt


Resistance of the wood of Eucalyptus saligna and Paulownia tomentosa against some wood rotting fungi
1997 - IRG/WP 97-10238
Paulownia tomentosa and Eucalyptus saligna are not autochthonous species in Slovenia and we determined the resistance of their wood against our most common wood rotting fungi. The resistance against Coniophora puteana, Gloeophyllum trabeum and Trametes versicolor was determined according to EN 113 and compared to the resistance of beech (Fagus sylvatica) wood. It was stated, that both paulownia an...
F Pohleven, M Petric


Discussion of diiodomethyl p-tolyl sulfone (Amical® 48) as a fungicide for wood preservatio
1987 - IRG/WP 3425
The effectiveness of diiodomethyl-p-tolyl sulfone (Amical® 48) as a fungicide for preservation of wood is supported by a discussion of results from the literature and current research programs....
J M Stamm, K J Littel, F M H Casati, M B Friedman


Biological control of the Formosan subterranean termite Coptotermes formosanus Shiraki
1971 - IRG/WP 100
M Tamashiro, J K Fujii, P Lai, T E Richardson


Quantitative assessment of the condition of field specimens
1981 - IRG/WP 2154
Suggestions for a discussion on the desirability of an extension to the existing procedure of assessment of the condition of field specimens by adding more objective, reproducible methods in order to obtain earlier and more specific information than at present on the effect of biological attack on strength and other properties of the specimens as well as the time aspect....
H Friis-Hansen


Mould resistance of lignocellulosic material treated with some protective chemicals
1984 - IRG/WP 3294
Effectiveness of preserving lignocellulosic material against moulding by treatement with water solutions of commercial wood preservatives and mixtures of various inorganic salts was investigated and compared with the effectivenes of sodium pentachlorophenoxide and boric acid....
K Lutomski