Efficacy of commercial wood preservatives against Bursaphelenchus xylophilus, a quarantine organism in Europe
2014 - IRG/WP 14-30638
Bursaphelenchus xylophilus (Steiner and Buhrer 1934) Nickle, 1970, pine wilt nematode (PWN), is a quarantine organism with a high potential to damage Conifer forests in Europe. This has driven the European Union to protect forest stands from the propagation and dispersion of this pathogen. Since the nematode was detected in Europe, eradication measures were taken. However, these measures were unsu...
C S Arcos, A Navas, L Robertson, M T Troya, M Conde, F Llinares
Study of the effectiveness of wood products for permanent protection against Fusarium circinatum
2014 - IRG/WP 14-30655
In Europe there exist a number of quarantine organisms that affect conifer forests, including Fusarium circinatum Nirenberg et O'Donnell (telemorph: Gibberella circinata Nirenberg et O'Donnell), a quarantine organism in Europe producing the disease known as pitch canker of pines. For a decade, the European Union has taken steps to locate and eradicate the pathogen with the aim of elimina...
M T Troya, M Conde, R Raposo, F Llinares, M Elvira-Recuenco
Wood protectors to control Bursaphelenchus xylophilus
2015 - IRG/WP 15-30661
Bursaphelenchus xylophilus, the pine wilt nematode (PWN), is a quarantine organism with a high potential to damage Conifer forests in Europe. The European Union is concerned in the protection of forest stands from the propagation and dispersion of this pathogen. In this line, the current control measures have been unsuccessful in preventing the dispersion of this organism, as it continues to be de...
M T Troya, C S Arcos, A Navas, L Robertson, M Conde, F Llinares
Indentation and pendulum hardness tests: two convenient assessment methods of the performance of exterior wood coatings
2015 - IRG/WP 15-40689
Developing formulations of exterior wood coatings with long service life is a big challenge. For many years in Europe the performances have been mainly evaluated through weathering tests (within the EN 927 series) followed by visual assessment (blistering, flaking, mould growth, chalking and cracking), colour and gloss measurements, and adhesion tests. Very recently the importance of the mechanica...
L Malassenet, L Podgorski, M Truskaller, G Grüll
Activity of wood preservatives against mould fungi
2016 - IRG/WP 16-30695
The resistance of experimental and commercial wood preservatives to mould fungi was determined using a method recommended by the Building Research Institute Instruction. The research of the inhibiting actions of the growth of fungi was carried out on the Scots pine wood Pinus sylvestris L. and beech Fagus sylvatica L. The most active compounds against mould were experimental herbicidal ionic li...
J Zabielska-Matejuk, A Stangierska
Response of the symbiotic flagellate protists community of subterranean termites to sublethal amounts of biocides
2018 - IRG/WP 18-10911
Subterranean termites are quite efficient at extracting nutrients from lignocellulose. Their ability relies not only on the digestive tract physiology but also on symbiotic relationships established with flagellate protists and bacteria. This work aimed to screen the response of the flagellate protists community of the subterranean termite Reticulitermes grassei Clément to the ingestion of differ...
S Duarte, T Nobre, P Borges, L Nunes
Rapid Screening test of potential antimicrobial agents for wood coatings
2018 - RG/WP 18-20644
A two-part screening test has been developed to evaluate additives for wood coatings. First, an additive is tested in the microbial laboratory and evaluated based on its inhibitory properties against selected test organisms, directly on agar plates. A microbial growth analysis is prepared and evaluated. If the additive is considered effective, it will be tested in a standard top coating (acrylic o...
J Stenbæk, E Morsing, T Østergaard Jensen
In-line quality control of the film thickness in industrial coating processes for exterior cladding
2018 - IRG/WP 18-40835
The production of industrially coated wood cladding has been strongly increasing in Scandinavia during the last years. In the beginning of this development, industrial coating processes included solely the application of pigmented primers; these however provide only a short protection of the wood surface and the application of a top coat is required during the first 6 to 12 months after mounting t...
U Hundhausen, M Slabohm
Influence of different triazoles as co-biocides in wood preservatives on efficacy and the environmental impact
2018 - IRG/WP 18-50333
In this study we investigated the efficacy and impact on the environment of different co-biocide triazoles in wood preservatives. Four different formulations (all containing 9.5% Copper) contained individual and combinations of cyproconazole, tebuconazole, propiconazole as co-biocides. Four formulations were tested according to EN 113 and EN 84 (ageing) to determine the brv for each formulation. T...
M Klamer, T Jensen, S Bang-Achton, E Morsing
Exemplary aboveground hardwood protection from Coptotermes curvignathus under weathered conditions conferred by proprietary microemulsion-based cypermethrin (SARPECO®) and permethrin (AXIL®) biocides
2019 - IRG/WP 19-30749
SARPECO® (with cypermethrin) and AXIL® (with permethrin) solutions are water-based wood preservatives approved for dipping treatment providing 25 years of termite protection for solid wood and wood-based products in Europe and for more than 10 years in Indonesia. SARPECO® and AXIL® solutions are patented formulations based on concentrated microemulsions (ME) diluted with water as a dipping tre...
D Messaoudi, A H H Wong, C A D Tawi, N Bourguiba, O Fahy
Monitoring of wood preservatives exposed to weathering: Extraction and analysis methods of organic biocides from treated wood and collected rain runoff
2020 - IRG/WP 20-30753
Weathering is the cause of numerous damages for outdoor joineries. Protection of wood using a preservative treatment covered with a coating is a process widely used to limit these damages. However, biocides from preservative treated wood are prone to degradation and leaching, having a direct influence on the joinery service life. This document deals with extraction and analytical methods for bioci...
O Ouali, K Le Ménach, E Raphalen, L Podgorski, S Legay, H Budzinski
Hyperspectral imaging in qualitative and quantitative assessment of biocide treated timber
2025 - IRG/WP 25-50407
A hyperspectral camera operating in the shortwave infrared light range between 1000 – 2500 nm was used to collect spectral profiles of timber treated with different biocides and varying concentrations of a copper-ethanolamine based wood preservative. The spectra were analysed using statistical methods like principal component analysis, linear discriminant analysis, and partial least squares to a...