Your search resulted in 121 documents. Displaying 25 entries per page.


SEM-EDXA of CCA-treated Rubberwood (Hevea brasiliensis)
2009 - IRG/WP 09-20399
The microdistribution of chromated copper arsenate (CCA) preservative in rubberwood was studied using scanning electron microscope in conjunction with energy dispersive X-ray analyzer (SEM-EDXA). Bulk X-ray analysis showed that there was a high accumulation of chromium, copper, and arsenic in the vessels and lower concentration of the three preservative elements in fibres. Chromium appeared to rec...
I Jusoh, D P Kamdem


Ultra-structural observations on the degradation of wood surfaces during weathering
1987 - IRG/WP 2280
Radiata pine (Pinus radiata D. Don) sapwood was converted into blocks with a transverse face about 5 mm square and measuring 8 mm longitudinally. Transverse (T.S.), Radial (R.L.S.) and Tangential (T.L.S.) surfaces were prepared and specimens exposed to the weather inclined at 45° facing equatorially for periods of between 20-60 days. After 30 days exposure erosion of the middle lamella was observ...
P D Evans, S Thein


Degradation of the normal fibre walls of rubberwood (Hevea brasiliensis) by the tropical blue-stain fungus Botryodiplodia theobromae
1998 - IRG/WP 98-10286
Rubberwood was examined by light microscopy and transmission electron microscopy (TEM) after exposure to the common tropical sapstain fungus Botryodiplodia theobromae for four weeks to study hyphal colonisation of wood cells and to determine if this fungus also degraded lignified normal fibre cell walls in addition to the walls of non-lignified elements. Light microscopy revealed relatively large ...
A A H Wong, A P Singh


Formation of soft rot cavities in relation to concentric layers in wood fibre walls
1983 - IRG/WP 1185
A large number of timber species attacked by soft rot have been examined using light microscopy. The S2 layers in a large number of the timbers exhibited special structural features in the form of thin concentric layers. Several observations indicate that these layers may be characterised as "weak" zones by being more easily degradable than the surrounding wall layers. The chemical structure of th...
T Nilsson, G F Daniel


Soft rot
1978 - IRG/WP 179
Soft rot decay of treated wood is examined with special reference to hardwoods treated with CCA. Factors which adversely affect the chances of protection of hardwoods against soft rot are discussed. The ratio of the volume of the fibre cell wall to the volume of the fibre lumen is presented as a major factor influencing final preservative concentration in the fibre cell wall, the major strength co...
C R Levy


The development of soft rot decay in bamboo fibres
1992 - IRG/WP 92-1572
The development of decay by soft rot fungus Chaetomium globosum was investigated in young and mature culms of bamboo Phyllostachys virideglaucescens. Soft rot decay was influenced both quantitatively and qualitatively by the differing levels of lignification in the material. Weight loss was significantly greater in the younger culm compared with the older, more heavily lignified culm. The distribu...
O Sulaiman, R J Murphy


Comparison of cubic and plug samples for preparation and data assembly in permeability study
2000 - IRG/WP 00-20197
In order to determine if plug experimental samples (PES: 30 x 15 mm2 diameter) could be used for inspection of wood permeability characteristics, radial and longitudinal flow directions were prepared according to either PES or cubic experimental samples (CES: 100 x 20 x 20 mm3) from the sapwood zone of Sitka spruce and treated by tanalith-C according to full-cell process. Results from the two prep...
I Usta


Resistance of Alstonia scholaris vestures to degradation by tunnelling bacteria
1992 - IRG/WP 92-1547
Electron microscopic examination of vessels and fibre-tracheids in the wood of Alstonia scholaris exposed to tunnelling bacteria (TB) in a liquid culture showed degradation of all areas of the secondary wall. The highly lignified middle lamella was also degraded in advanced stages of TB attack. However, vestured pit membranes and vestures appeared to be resistant to degradation by TB even when oth...
A P Singh, T Nilsson, G F Daniel


Analysing the characteristic role of moisture content for drying and fluid flow in Sitka spruce. - Part 1: The drying process of sapwood and heartwood of two different thickness of Sitka spruce using a kiln. - Part 2: Effects of moisture content on longitudinal permeability of Sitka spruce in vertical variation of the tree
2000 - IRG/WP 00-40173
The characteristic role of the moisture content in Sitka spruce (Picea sitchensis (Bong.) Carr.) that grown in the United Kingdom was examined by this study on the basis of (1) the reduction of moisture content in two different thickness of sapwood and heartwood by kiln drying process, and (2) the effects of moisture content to the longitudinal void volume filled of tanalith-C by the full-cell pro...
I Usta


An effective preservative treatment of borak bamboo (Bambusa balcoona Roxb.)
1996 - IRG/WP 96-40070
Adequate penetration and retention of CCA and CCB has been obtained in predried Borak Bamboo (Bambusa balcooa Roxb.), aboundantly grown in Bangladesh, with Full Cell Pressure Process. The treated bamboo can be used as building materials, the sufficient treatability ensured its long term best utilization at ground contact and indoors. Which will keep the environmental & socio economical conditi...
A K Lahiry, S Begum, G N M Ilias, M A Matin Sheikh, M A B Fakir, M I Hossain


A summary of tests and practical experiences with the Pilodyn wood testing instrument
1980 - IRG/WP 282
This paper presents a summary of the reports, tests and practical experiences with the Pilodyn wood tester not only, however, concerning poles but also in other fields such as standing trees, sawn timber etc. The principle of the Pilodyn is a spring-loaded pin which is fired into the object and the depth to which the pin penetrates is correlated to physical and mechanical properties of the object....
H Friis-Hansen


Water-based water repellents for treatment of wood
1987 - IRG/WP 3446
The water uptake by wood can be reduced by treatment with a water repellent. The water repellents most commonly used are solvent based. In the present work a new type of water repellent that is water-based has been investigated. Two different treatments have shown an effect of the same order as a commercial solvent based product. The cellular distribution of the water repellents has been investiga...
I G Svensson, G Hägglund, I Johansson, W B Banks


The effects of density on vertical variation of permeability of Sitka spruce within tree
2000 - IRG/WP 00-40156
Tree improvement of Sitka spruce is a combination of silviculture and tree breeding aimed at producing higher quality products including increased growth rate and timber yield, and wood density. It is useful to know annual ring structure and density distribution when studying the quality of wood, grading it, or determining how the wood structure affects residual flow in softwoods. Since density is...
I Usta.


TBTO absorption and penetration in pine joinery treated by various processes
1989 - IRG/WP 3523
Matched sections of several White pine (Pinus strobus) and Ponderosa pine (Pinus ponderosa) mouldings were treated with TBTO by Double vacuum, modified empty-cell, 15 second dip and several preheating treatments followed by a 15 s dip treatments. As expected the double vacuum and empty-cell (batch) treatments resulted in much greater retentions and penetrations than the dip treatments. The absorpt...
P A Cooper, Y T Ung


Ultrastructural aspects of bacterial attacks on an archaeological wood
1993 - IRG/WP 93-10007
Transmission electron microscopy of wood from a Chinese ship submerged in the mud for over 900 years showed bacteria to be the main factor for its deterioration. The micromorphology of degraded wood cell walls was similar to that observed during the attacks of wood by erosion bacteria. Other bacterial forms, previously considered lo be scavenging bacteria, were also abundant in degraded areas of t...
Yoon Soo Kim, A P Singh


Ultrastructural observations on wood-degrading erosion bacteria
1986 - IRG/WP 1283
G F Daniel, T Nilsson


Decay, decayed wood and the Shigometer
1980 - IRG/WP 281
A L Shigo


A behaviour of CCA penetration of fir (Abies bornmulleriana Mattf.) at different ramp times and constant vacuum/pressure applications
2006 - IRG/WP 06-40346
A behaviour of CCA penetration of Bornmulleriana fir (Abies bornmulleriana Mattf.) at different ramp times and constant vacuum/pressure applications was illustrated for the main flow directions by the experimental pictures....
I Usta, R Despot, M Hasan


Durable fibre for durable MDF – testing Tricoya®
2015 - IRG/WP 15-40704
The chemical modification of wood has been a commercial reality for a decade on release of technologies for the modification of solid wood including Accoya®. A challenge and an opportunity for the modification technologies which typically impart dimensional stability, water stability and enhanced biological durability was the adaptation of the technology to wood based panels. This paper presents ...
E Suttie, J Alexander, M Maes


The Relationship of Fiber Cell Wall Ultrastructure to Soft Rot Decay in Kempas (Koompassia malaccensis) Heartwoo
2004 - IRG/WP 04-10541
The ultrastructure of fiber walls in kempas (koompassia malaccensis) heartwood was examined in relation to soft rot cavity formation. The fibers consisted of middle lamella and thick secondary wall. The secondary wall was differentiated in to a S1 layer, and a unique multi-lamellar S2 layer. Two distinct forms of lamellae were recognisable, one type being considerably thicker than the other. They ...
A P Singh, A H H Wong, Yoon Soo Kim, Seung-Gon Wi


Sustainability Through New Technologies for Enhanced Wood Durability. COST Action E37 – A New Action in the Forestry Domain
2004 - IRG/WP 04-40293
The main overall objective of the action is to concentrate on the contribution of wood durability on the sustainability through the development of systems for quality assurance and perfoamance of modified wood and wood products as alternatives to wood treated with traditional preservatives. By this means it seeks to improve and consequently increase the cost-effective use of sustainably produced E...
R-D Peek


Leaching of copper, chromium and arsenic from CCA-treated slash pine heartwood
1994 - IRG/WP 94-50020
Drying green slash pine with any of three high temperature drying schedules produced a product in which both the sapwood and the heartwood could be penetrated with CCA using a modified Bethell treatment schedule. Required H3 retentions were achieved in both sapwood and heartwood, from 200 litres per m³ charge uptake. Post-treatment fixation/drying was accomplished by three different regimes, incl...
M J Kennedy, G Palmer


Estimation of effective diffusion path lengths in wood by swelling studies
1989 - IRG/WP 3524
The effective average distance that a solute must diffuse to penetrate the cell wall matrix following pressure treatment is estimated from the rate of swelling of wood, vacuum treated with water. It is assumed that the diffusion paths are similar for water and a solute such as a wood preservative component. Since bound water diffusion coefficients for water in wood have been estimated by others, t...
P A Cooper, R Churma


The attack of naturally durable and creosote treated timbers by Limnoria tripunctata Menzies
1995 - IRG/WP 95-10132
Limnoria tripunctata was found tunnelling in creosote treated Douglas fir (Pseudotsuga menziesii) pilings and naturally durable greenheart (Ocotea rodiaei) gate seals at two sites on the south coast of the United Kingdom. Examination of thc creosote-treated wood showed that Limnoria tunnels were concentrated at a depth of 2-3 cm from the timber surface, where creosote loading was lower. Fewer tunn...
A J Pitman, G S Sawyer, G F Daniel


Role of cell wall structure in soft rot decay of bamboo
1995 - IRG/WP 95-10133
Models of soft rot hyphal penetration of bamboo cell walls are proposed. Soft rot hyphae show an interesting capability of penetrating the bamboo cell wall in different forms; typical longitudinal penetrating hyphae and tangentially orientated penetrating hyphae. The second form of penetration was found to be different from that normally associated with wood cell walls. The differences can be attr...
O Sulaiman, R J Murphy


Next Page