IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 306 documents. Displaying 25 entries per page.


Assessment of wood decay in small-scale unsterile soil-bed tests
1997 - IRG/WP 97-20111
This study is concerned with the investigation of wood decay in small-scale unsterile soil-bed tests. Tests were performed with untreated heartwood samples from five hardwood species of different natural durability classes ranging from highly perishable to very resistant. Our results confirmed the critical role of soil moisture content on wood decay. The highest decay rates were observed at moistu...
L Machek, A M Derksen, R Sierra-Alvarez


Statistical evaluation of 'micro-bending' samples for classification of wood attacking fungi
1992 - IRG/WP 92-1544
Micro-specimens from both hardwood and softwood were exposed to selected species of field isolated fungi. The strength reduction and weight loss caused by these fungi were determined. A statistical procedure was then developed to classify the fungi into brown-, white-rot, or non-decay fungal categories based on these data. The procedure reveals the extent of hazard a fungus poses to wood members. ...
B Goodell, Jing Liu, A Homola, J Jellison, J Shottafer


Fungal remediation of CCA-treated wood
2004 - IRG/WP 04-50210
This study evaluates oxalic acid accumulation and bioremediation chromated copper arsenate (CCA) treated wood by three brown-rot fungi, Fomitopsis palustris, Coniophora puteana, and Laetiporus sulphureus and ten mold and staining fungi, Aspergillus niger, Aureobasidium pullulans, Gliocladium virens, Penicillium funiculosum, Rhizopus javanicus, Ceratocystis pilifera, C. peceae, Alternaria alternata...
S N Kartal, Y Imamura


Oxalic acid quantification, oxaloacetase assay and ESI localization of P, C, and Fe from the brown rot fungus Postia placenta
1994 - IRG/WP 94-10063
The mechanism by which brown-rot fungi initiate depolymerization of holocellulose in wood remains unknown. Recently, oxalic acid (OA) has received considerable attention in cellulose breakdown by brown-rot fungi. The OA could serve as a proton donor for hydrolytic or an electron donor for oxidative (Fenton's reaction-H2O2/Fe2+) cleavages of cellulose. The acid may originate via oxaloaceta...
C R Jordan, W V Dashek, T L Highley


Early detection of brown-rot decay in southern yellow pine using immunodiagnostic procedures
1990 - IRG/WP 2356
Immunodiagnostic procedures have been used to detect incipient decay of southern yellow pine by six common brown-rot fungi. Rabbit polyclonal antibodies were raised to liquid culture fractions of the six fungi. The antibodies, after preadsorption to sawdust, were tested in particle agglutination assays, immuno-dot blot, and ELISA for their·ability to detect the decay organisms when they were grow...
C A Clausen, F Green III, T L Highley


Comparing the resistance of a number of lesser known species of tropical hardwoods to the marine borer Limnoria using a short term laboratory assay
2003 - IRG/WP 03-10500
Naturally durable species of timber are used as an alternative to preservative treated timber for marine structures, but many species have not been evaluated for their potential for use in this environment. EN 275 specifies a 5-year test period - too long a period for screening tests to be economically viable. In this study, durability was assessed by measuring the production of faecal pellets by ...
L M S Borges, S M Cragg, J R Williams


Termite and fungal resistance of in situ polymerized tributyltin acrylate and acetylated Indonesian and USA wood
2000 - IRG/WP 00-30219
Wood [Indonesian pine (IP), Indonesian Jabon (IJ) and USA southern yellow pine (USP)] was either in situ polymerized with tributyltin acrylate (TBTA) or acetylated and then exposed to termite and fungal degradation both in laboratory tests and field exposure. The TBTA woods had an average weight percent gain (WPG) of 11% for IP, 12% for IJ, and 10% for USP. The acetylated woods had a WPG of 15-27%...
R E Ibach, Y S Hadi, D Nandika, S Yusuf, Y Indrayani


Factors affecting resistance to sapstain infection in freshly felled softwood logs
2003 - IRG/WP 03-10467
Previous studies in the UK have shown a marked difference in the susceptibility of logs of five softwood species to infection by sapstain fungi over a 4 month field trial. Recently this result has been confirmed and the rank order of greatest to least susceptibility in these commercially important species is lodgepole pine > Scots pine > Norway spruce > Japanese larch > Sitka spruce. C...
E J Young, R A Eaton, J F Webber, M A W Hill


The WOODCARE project: Development of detection methods for Death watch beetle larvae and fungal decay
1999 - IRG/WP 99-20172
Woodcare was a European project coordinated by English Heritage. The aim of the research was to develop more targeted and more environmentally friendly treatment methods for Death watch beetle infections in Oak constructions of historical buildings. TNO has developed two new methods for fast and reliable detection of Death watch beetle larvae and related fungal decay in Oak. The problem with Death...
P Esser, P Van Staalduinen, A C Tas


Laboratory testing of wood natural durability - In soil-bed assays
1998 - IRG/WP 98-20141
Laboratory methods for assessing wood decay resistance are being investigated in the framework of an ongoing European research project. This paper summarizes the main results obtained for soil-bed tests based on the European prestandard ENV 807-Test 2. The data suggest that this testing methodology is suitable for evaluating the natural durability of timber species in soil-contact under conditions...
R Sierra-Alvarez, I Le Bayon, J K Carey, I Stephan, J Van Acker, M Grinda, G Kleist, H Militz, R-D Peek


Aspects of the fungal degradation of quaternary ammonium compounds in liquid culture
1997 - IRG/WP 97-30160
Didecyldimethylammonium chloride (DDAC) is a quaternary ammonium compound (QAC) that has found use as an anti-sapstain preservative for the transportation of softwood lumber from Canada to overseas markets. However, its use is limited by the knowledge that certain mould fungi seem capable of degrading it. The aim of this research was to gain knowledge about the fungal degradation of DDAC. The effe...
J W Dubois, J N R Ruddick


Laboratory trial to identify potential in-forest treatments to control fungal pre-infections of radiata pine logs
2000 - IRG/WP 00-30220
Development of fungal infections of radiata pine logs by wood degrading fungi commences immediately after tree felling. In general, subsequent antisapstain treatments are unable to control fungal degrade on logs where the pre-treatment log storage time exceeds 2-5 days. However, use of an in-forest treatment of logs may be advantageous to log exporters to control fungal pre-infections during the p...
D R Eden, B Kreber, R N Wakeling, J G Van der Waals, C M Chittenden


Fungal colonisation of the keelson and associated structures of a nineteenth century wooden frigate: Concepts of community structure and development
1994 - IRG/WP 94-10072
The early stages of microbial colonization and succession of wooden surfaces exposed to the sea have been extensively studied as have the community structures of archaeological timbers subjected to submergence and then retrieval from the sea. The frigate UNICORN, a largely intact 19th century wooden ship based in Dundee, Scotland, provides the microbial ecologist with a unique opportunity to study...
N A White, J W Palfreyman, G M Smith


Evaluating the resistance of wood-based panel products to fungal attack
1995 - IRG/WP 95-20071
At present there is considerable disagreement among national research institutes within Europe and panel product manufacturers on the most appropriate method of testing and indeed the need for specific biological durability testing. This paper seeks to place before a broader international audience, the issues related to development of a European standard for evaluating the resistance to fungal dec...
R G Lea, R W Berry


Mechanisms of Protection by NHA Against Fungal Decay
2002 - IRG/WP 02-10429
Treating wood with the water-borne sodium salt of N'-N-naphthaloylhydroxylamine (Na-NHA) protects wood against decay and termite damage. Initial testing indicated little or no inhibition of sapstain fungi, molds, or soft-rot fungi by Na-NHA, suggesting that the mechanism by which this compound protected wood was complex and not that of a broad-spectrum biocide. Previously, we (Green et...
F Green III, W Henry, T Schultz


The biological effectiveness of wood modified with heptadecenylsuccinic anhydride against two brown rot fungi: Coniophora puteana and Gloeophyllum trabeum
1992 - IRG/WP 92-3705
A modified soil block test was carried out using wood samples reacted with heptadecenylsuccinic anhydride (ASA). This modification gave good resistance to decay brought about by the brown rot fungi Coniophora puteana and Gloeophyllum trabeum during the twelve week exposure period. Results indicated that there was a good correlation between increased loading of modifying reagent and an increase in ...
C Codd, W B Banks, J A Cornfield, G R Williams


Screening of the efficacy of tall oils against wood decaying fungi
2004 - IRG/WP 04-30354
Tall oil is a by-product in pulping of resinous wood by the sulphate process. Tall oil contains a complex mixture of wood extractives. Some of these extractives act as natural protection against wood decaying fungi while other serve as nutrition for the fungi. This report describes a screening of the efficacy of four refined tall oils with different chemical composition on wood decaying fungi. ...
G Alfredsen, P O Flæte, A Temiz, M Eikenes, H Militz


Effect of some resin treatments on fungal degradation reactions
1999 - IRG/WP 99-10318
The effect of impregnation of wood with vegetable oil, tall oil and two water soluble on fungal degradation reactions was assessed by hydrolysis and enzyme activity measurements. The experiments were carried out by using isolated enzyme preparations and a living brown-rot fungus Poria placenta. The results indicate that the inhibitory effect of treatments was clearly directec towards the enzymatic...
A-C Ritschkoff, M Rättö, A J Nurmi, H Kokko, A O Rapp, H Militz


Some studies on fungal deterioration of rubber wood (Hevea brasiliensis)
1980 - IRG/WP 2140
For the sreening of anti-stain chemicals trials with selected agricultural fungicides and new chemicals were carried out. Botryodiplodia theobromae, Aspergillus sp. and Penicillium sp. were used at test organisms. For testing the durability of rubber wood (Hevea brasiliensis) suitable local rotting fungi (Basidiomycetes), based on high degrading power, which may later be employed in standard tests...
A Sujan, A G Tan, M Stevens


Fungal siderophores and their rôle in wood biodegradation
1990 - IRG/WP 1442
Iron and other metals such as manganese, play an important role in the metabolic functions of fungi that cause wood deterioration. These transition metals are also found in, or associated with, the extracellular fungal enzymes shown to be directly involved in the decay process. Recently our research group was able to show that siderophores (low molecular weight biological chelators) are produced b...
J Jellison, B Goodell, F Fekete, V Chandhoke


Preliminary evaluations of a small wafer assay for screening potential biological control agents
1989 - IRG/WP 2332
Screening potential biological agents for controlling wood decay fungi poses a dilemma. The ideal test would eliminate as many variables as possible. Most tests utilize pure cultures of the test organism on an artificial media which in no way resembles wood. The use of sawdust improves this approach, but the sawdust increases fungal access to the lignocellulose matrix, potentially inflating the im...
C M Freitag, J J Morrell


Sapstain development on Jack pine logs in Eastern Canada
2000 - IRG/WP 00-10358
During 1998-99, a study was initiated to investigate the influence of seasons, log types and storage time on the sapstain development on jack pine logs at two sites in Eastern Canada. Jack pine trees (Pinus banksiana) were harvested into whole-tree and cut-to-length logs in spring and in autumn. Sapstain development was examined in these logs at 2 to 4 week intervals after felling. The mean stain ...
Dian-Qing Yang, R Beauregard


Regulation of hyphal sheath formation iron-chelator production by the brown rot fungi Gloeophyllum trabeum and Postia placenta
1994 - IRG/WP 94-10074
Hyphal sheath formation and iron-chelator production by liquid cultures of the brown rot fungi Gloeophyllum trabeum and Postia placenta were monitored over time. The effects of incubation at various temperatures, pH's and concentrations of iron, manganese and nitrogen were determined. Hyphal sheath production was observed microscopically and quantified with JAVA video analysis. The hyphal...
Y Chen, J Jellison


Breakdown of cellulose derivatives by cellulolytic enzymes. I. Action of fungal ß-glucosidases toward substituted PNP ß-D-glucopyranosides
1998 - IRG/WP 98-10281
The action of fungal ß-glucosidases on the methyl derivatives of p-nitrophenyl (PNP) ß-D-glucopyranoside, which were regioselectively substituted at 0-2, 0-3, 0-4 and 0-6 positions was studied. Several ß-glucosidases from brown-rot, white-rot, and soft-rot fungi and almond were used for the study. These ß-glucosidases did not act on the 2, 3, and 4-0-methyl derivatives, while the 6-0-methyl on...
T Nishimura, I Momohara, M Ishihara


The suitability of isothiazolone microemulsions as long term wood preservatives
1997 - IRG/WP 97-30150
Microemulsion formulations of 4,5 dichloro-2-n-octyl-4-isothiazolin-3-one were investigated to determine the leaching potential of these formulation types as well as their efficacy against decay fungi. These patented low leaching formulations exhibited good anti fungal efficacy in standard tests combined with minimal leaching of the active ingredient from the wood. The data suggests that the excel...
B M Hegarty, Bing Yu, L E Leightley


Previous Page | Next Page