Durability of timber products –Part 1: Inventory and evaluation of above ground data
2012 - IRG/WP12-20498
The material-inherent resistance of wood is one of the most important qualities influencing the durability of timber. Hence, it has also a major effect on the service life to be expected from a timber construction. In addition, design details and the respective climatic conditions determine durability and make it impossible to treat wood durability as an absolute value. Moreover, the reference mag...
C Brischke, L Meyer, G Alfredsen, M Humar, L Francis, P O Flæte, P Larsson Brelid
Testing service life for use class 3: accelerated L-joint performance of commodities
2012 - IRG/WP 12-20500
Above ground testing is considered important for the assessment of treated wood intended for use class 3. Laboratory testing of efficacy of biocides as well as of natural durability focussing on such applications has to be linked to performance and service life. An accelerated L-joint test was some 15 years ago developed at the Ghent University to allow worst case assessment under semi-controlled ...
J Van Acker, J Van den Bulcke, I De Windt, L De Vetter
Biological performance of wood- and bamboo-polypropylene composites: Effects of particle content, particle size and Zn borate
2012 - IRG/WP 12-40577
Particle content and size of wood material in wood plastic composites (WPCs) can affect efficacy of WPCs against fungi and termites. This study evaluated fungal and termite resistance of WPCs manufactured by using two different levels of particle content (50 and 70%) and three different particle sizes (30, 60, and 100 mesh). In fungal resistance tests, Tyromyces palustris, a standardized test fung...
S N Kartal, S Aysal, E Terzi, T Yoshimura, K Tsunoda
Relationships between heat treatment intensity and some conferred properties of different European softwood and hardwood species
2012 - IRG/WP 12-40593
Effect of treatment intensity on conferred properties like elemental composition, durability, anti swelling efficiency (ASE) and equilibrium moisture content (EMC) of different European softwood and hardwood species subjected to mild pyrolysis at 230°C under nitrogen for different durations has been investigated. Independently of the wood species studied, elemental composition is strongly correl...
M Chaouch, S Dumarçay, A Pétrissans, M Pétrissans, P Gérardin
Durability of Furfurylated Wood – Results from Laboratory and Field Tests in the Ecobinders project
2012 - IRG/WP 12-40602
Within the EU project Ecobinders, laboratory tests were performed with furfurylated wood produced in semi-industrial scale in the factory of Kebony ASA. Field trials in Horizontal double layer decks and in-ground of transmission poles were also started. Four wood species, Southern yellow pine (SYP), maple, beech and aspen were treated to two treatment levels by using two impregnating liquids with ...
M Westin
KERUING and APITONG: A Timely Review of the Perfect Choice Wood Species for Crossarms and Brace Arms, Including Data on Copper Naphthenate Treatments
2012 - IRG/WP 12-40603
Apitong or the wood species more commonly known as Keruing is an important tropical hardwood known for its high strength to weight ratio and its reasonable durability and preservative treatability. This wood has been exported from managed permanent forest estates in Malaysia into the United States for over 4 decades for its widespread use in wooden utility industry brace arms and crossarms, yet cu...
A Wong, M Freeman
Biodegration of treated wood waste by native fungal communities of tropical soil in French Guiana
2012 - IRG/WP 12-50285
Woods have been protected with fungicides for a long time, and the effects of these fungicides on soil after being leached into the ground have turned out to be a true environmental issue. It is in this perspective that we are proposing to study fungal communities of these contaminated woods in a purpose of bioremediation. Most of precedent studies have focused on ability of some Basidiomycetes an...
A Zaremski, L Gastonguay, C Zaremski, F Chaffannel, J Beauchêne, G LeFloch
Tar-oil uptake vs time in immersion treatment of short pine posts: A simple technique applicable to rural communities of Papua New Guinea
2012 - IRG/WP 12-40608
Pinus caribaea and Araucaria cunninghamii logs ca. 100 mm in diameter were shortened to lengths 25-30 cm, conditioned to at/below fibre saturation point (FSP) for immersion/dip treatment using a hot- and- cold bath open- tank process. Before oven-drying and subsequent treatment, individual test specimens were numbered, their green weights and volumes, and dry weights recorded for basic density, vo...
B K Gusamo, R Tulo
Classifying white rot decay resistance of some hardwoods from Sarawak and Peninsular Malaysia and correlations with their tropical in-ground durability
2012 - IRG/WP 12-10788
White rot wood decay under Malaysian (humid tropical) terrestrial conditions pose more serious threats to the in-ground service life of hardwoods than other common fungal decay types. A study is made on decay resistance variation for a total combined list of 30 Peninsular Malaysian and Sarawak timber species (plus 6 exotic reference temperate commercial woods for comparison) using the laboratory s...
A H H Wong, J M E Jem, Lai Jiew Kok
Succession after Fire of Fungal Fruiting Bodies in Mediterranean Pinus pinaster Stands in Spain
2012 - IRG/WP 12-10789
In this study we present the results of a 4-year survey aimed at describing the succession of fungal communities following fire in a Mediterranean ecosystem in Northwest Spain, dominated by Pinus pinaster Ait. After a large wildfire in 2002, six 2 x 50 m study plots were established in burned and unburned areas corresponding to early and late succession stages. During the autumn seasons from 2003 ...
P Vásquez Gassibe, M Hernández-Rodriguez, R Fraile Fabero, J A Oria-De-Rueda, P Martín-Pinto
Effect of growth rate and radial position on the natural durability of Douglas-fir
2012 - IRG/WP 12-10791
In terms of natural durability, Douglas-fir (Pseudotsuga menziesii (Mirb.) Franco) fame owns to the favourable characteristics of centuries-old trees harvested in old-growth North American forests. The properties of wood coming from plantations harvested between 50 and 100 years-old are likely to be different. In such stands, plantation density and thinning intensity may have a large impact on the...
C Pollet, J-M Henin, B Jourez, J Hébert
Triazole – based ionic liquids to protect of lignocellulosic materials against fungi
2012 - IRG/WP 12-30601
In presented paper we examined on biotic properties of novel structure of tebuconazole derivatieves: tebuconazole hydrochloride, allyltebuconazole chloride, methyltebuconazole iodide, tebuconazole dihydrocitrate. Our investigation against wood-degrading fungi were contained also the didecyldimethylammonium 3-aminotriazolate as well as didecyldime-thylammonium nitrate(V) with tebuconazole or wit...
J Zabielska-Matejuk, J Pernak, I Frąckowiak, A Stangierska, W Przybylska, M Kot
Effectiveness of CCA-C and CCB preservatives after a 30 years stake test
2012 - IRG/WP 12-30606
The objective of this experiment was to assess the durability of four pine species treated with waterborne preservatives. In order to determinate this, a stake field test, following the IUFRO (International Union of Forestry Research Organizations) recommendations, was installed at Experimental Station of Luiz Antonio (21º 32’ S and 47º 42’ W), State of São Paulo, Brazil.
Species under t...
I PJankowsky, E S Lepage, C Salvela, J M Vidal, S Takeshita
Development of a quality control assessment method to predict properties of heat treated wood
2012 - IRG/WP 12-40611
Heat treatment has been used to improve properties of non durable European species. Chemical modification of some of the wood components provides improved dimensional stability and biological performance against decay fungi while mechanical properties such as modulus of rupture are reduced. Quality control of commercially made thermally treated wood is one of the major challenges to allow its indu...
M Chaouch, K Candelier, S Dumarcay, A Pétrissans, M Pétrissans, P Gérardin
The effect on moisture content of water trapped in wood joints
2012 - IRG/WP 12-40613
To predict the service life of a structure, a model where the exposure of a structure is compared to its resistance can be used. Which exposure and resistance parameters that are relevant depend on which materials the structure consist of. This approach, with an exposure and a resistance parameter, is similar to the one used in structural engineering where a load (exposure) is compared to the bear...
M Fredriksson, L Wadsö, P Johansson
Differences between heat treated Pinus pinaster heartwood and sapwood
2012 - IRG/WP 12-40617
Heat treatment is a well known process to improve the durability and dimensional stability of less noble woods. The treatment can be applied for heartwood unlike the traditional treatments based on impregnation due to the difficulty of impregnating heartwood.
Pure sapwood and pure heartwood samples were treated in an oven at 190ºC and 200ºC for 2h, 4h and 6h. Dimensional stability, measured a...
B Esteves, L Nunes, I Domingos, H Pereira
Activities of moulds on wood as a function of relative humidity during desorption and absorption processes
2013 - IRG/WP 13-10794
Three different types of indoor moulds: Penicillium brevicompactum, primary colonizer; Alternaria tenuissima, secondary colonizer and Trichoderma harzianum, tertiary colonizer, grown on wood were measured for their activities under different relative humidity levels. The activities were measured by isothermal calorimetry. The activities of the moulds changed with the change of the relative humidit...
Yujing Li, L Wadsö
High-throughput sequencing highlighted contrasted pioneer fungal communities associated to coniferous and deciduous wood preservation assays
2013 - IRG/WP 13-10800
Studying the fungal communities in the wood, in particular during the first events of the colonization, and the factors that underlie the dynamics of fungal species assemblages remain a challenge in ecology, because of the absence of fructification during the pioneer steps of wood degradation. The use of Next-generation DNA sequencing methods, which produce massive volumes of data, provided new pe...
Y Mathieu, A Dassé, I Le Bayon, M Kutnik, L Harvengt, E Gelhaye, M Buée
The chemistry of wood degradation by Basidiomycetes studied in a van Krevelen diagram
2013 - IRG/WP 13-10805
The atomic composition ratios of decayed wood by Basidiomycetes are mapped in a van Krevelen diagram. It is shown that the wood residue after decay is chemically reduced, rather than oxidized. A previously developed and verified theoretical model for thermal wood modification, relating atomic composition ratios to moisture sorption and fungal resistance properties has tentatively been applied to w...
W Willems, H Militz
Transferable Durability: Enhancing decay resistance of non-durable species with extractives from durable wood species
2013 - IRG/WP 13-10808
Extractive content and composition is a vital component of naturally durable woods; however, variability in extractives can limit their usefulness in the field. Two extractive-free, non-durable wood species were pressure treated with ethanol-toluene extractives from 8 durable wood species. Extracted Southern pine, Paulownia and unextracted Southern pine blocks were treated and challenged in soil b...
G T Kirker, A B Blodgett, S Lebow, C A Clausen
Grading UK Grown Larch for Durability
2013 - IRG/WP 13-10809
This paper reports on a joint study by BRE, the Forest Products Research Institute and TRADA Technology into the feasibility of grading UK grown larch to maximise its natural durability. The research was undertaken to assist sawmills and timber specifiers in the selection of larch timber suitable for external cladding. The findings indicate that the heartwood of larch has variable durability due t...
D Jones, I Davies, P Sharphouse, E Suttie
Focus on the European standardization - Towards a revision of the EN 350 natural durability standard: a different approach to the inherent resistance and performance of wood and wood-based materials
2013 - IRG 13-10811
The European standard EN 350 “Natural durability of solid wood”, Parts 1 and 2, is one of the fundamental standards developed by the CEN/TC 38 “Durability of wood and wood-based products”. This standard is widely used by wood industries as the reference document which provides information on the resistance of wood species used in mainly the construction sector against decay fungi, wood-bor...
M Kutnik
Statistical analysis of durability tests - Part 1: Principles of distribution fitting and application on laboratory tests
2013 - IRG/WP 13-20504
Service life prediction is an important topic in wood research, especially with regard to the Construction Products Regulation (CPR). Both laboratory tests as well as in-service performance testing are therefore essential in combination with proper monitoring and analysis tools. A crucial concept is variability in testing and analysis, especially for a biological material such as wood. The larger ...
I De Windt, J Van den Bulcke, C Brischke, C R Welzbacher, A Gellerich, S Bollmus, M Humar,
Characterization of test fields
2013 - IRG/WP 13-20508
Test field characteristics and impact of test fields on wood degradation is important when testing wood protection. The current EN 252 standard has no requirement for knowledge of decay hazards, but most commonly a test field is known as a “brown”,- “white”,- or “soft rot” field. To understand which decay hazard wood preservatives are tested against, each test field should be character...
U Råberg, N Terziev, G Daniel
Determination of the natural durability of solid wood against wood-destroying fungi - a European round-robin test
2013 - IRG/WP 13-20511
In Europe the durability of wood against wood-destroying basidiomycetes is tested according to CEN/TS 15083-1 (2005). Hitherto existing experience with this standard is quite heterogeneous and results from previous round-robin tests have stayed unreported or have been reported incompletely. In particular the need for natural pre-weathering of the test specimens to allow potential detoxification of...
C Brischke, C R Welzbacher, A Gellerich, S Bollmus, M Humar, K Plaschkies, W Scheiding, G Alfredsen, J Van Acker, I De Windt