Recent development in North American industrial wood preservation plants
1988 - IRG/WP 3467
After remaining static for many years there have been a number of changes in plant design and treating cycles in recent years. This has been particularly true in the USA where few restrictions are placed on plant treating cycles by specifications; since only results type specifications are used. It is also important to realize that the AWPA Specifications for Southern Yellow Pine only call for tre...
J F Bridges


A comparison between high and conventional incision densities for improving preservative treatment of Douglas-fir heartwood lumber
1993 - IRG/WP 93-40009
Incising is required for the preservative treatment of most wood species from the western United States; however, there is considerable debate about the density of incisions required to achieve adequate treatment. Previous studies have shown that the incision effect on treatment is relatively narrow, suggesting that incision densities should be significantly increased over current practices and st...
S T Lebow, J J Morrell


Accelerated diffusion treatment of sawn Sitka spruce grown in the UK
1986 - IRG/WP 3395
The treatment of 'green' sapwood and heartwood of Sitka spruce by diffusion methods was investigated. Steam/dip treatment processes gave increased solution uptakes and depths of penetration of copper in comparison with a simple dip treatment. Further investigation is required to reduce diffusion gradients with copper based formulations and to improve the penetration of '...
R J Murphy, D J Dickinson


Performance of Tuff Brite C™ and other formulations against blue-stain, mold and brown-stain in freshly-sawn rubberwood (Hevea brasiliensis) in the humid tropics of Peninsular Malaysia
1997 - IRG/WP 97-30163
The relative anti-sapstain and anti-mold efficacies, including brown-stain development in freshly-sawn rubberwood (Hevea brasiliensis) in the Malaysian tropics, between selected water-based product concentrations of formulations Tuff Brite CTM without/with added Borax (at 1.5/0, 1/1.5, 1.5/1.5 and 2%/1.5%), PQ8TM without/with added Borax (at 2.5/0, 1.5/1.5, 2/1.5 and 2.5%/1.5%) and NeXgenTM/NeX-Br...
A H H Wong, T L Woods


A field test with anti-stain chemicals on sawn pine timber in Brazil
1989 - IRG/WP 3513
Field tests were carried out in São Paulo State - Brazil, to evaluate pre-treatment formulations of O-Phenyl-Phenol (OPP) based products. The Sodium Pentachlorophenate solution was used as a reference formulation. The treated test blocks were stacked in a covered shed, and in an uncovered place for air drying. The evaluation was done by measuring the percentage of stained surface on each test blo...
M B B Monteiro, S Brazolin


Reduction of kiln brown stain in radiata pine lumber after log fumigation with methyl bromide
1997 - IRG/WP 97-30129
Methyl bromide fumigation of freshly felled radiata pine log sections effectively killed living cells in parenchyma to at least 75mm into sapwood. Lumber cut from logs (fumigated and control) stored 1 month outdoors (dry) showed slightly reduced brown stain when kiln dried at conventional temperatures. A more dramatic reduction and elimination of brown stain was noted in lumber cut from fumigated ...
E Schmidt, M E Hedley, D R Page, D Cross


Evaluation of the insecticidal efficacy of deltamethrin and the fungicidal efficacy of its association with TCMTB + MBT in the field of wood preservation
1986 - IRG/WP 1289 E
Deltamethrin possesses many advantages for the insecticidal protection of wood: relatively low toxicity, very reduced evaporation, very prolonged retention in the wood, very slight leaching after having penetrated the wood, and absence of odour. Its association with other active agents or solvents is being studied with regard to chemical compatibility. Compatibility studies have proved positive fo...
J S Duguet


Performance of Borate-treated lumber in a four-year, above-ground termite field test in Hawaii
2001 - IRG/WP 01-30265
We report the fourth year of field study results from a protected above-ground field test in Hawaii simulating the sill plate (dodai) used in conventional Japanese housing construction. Field tests were established in both Hawaii and Japan to examine the efficacy of disodium octaborate tetrahydrate (DOT, 2% and 3% shell and through) wood treatments. In Hawaii, chromated copper arsenate (CCA, 4 kg/...
J K Grace, R J Oshiro, A Byrne, P I Morris, K Tsunoda


Targeted inhibition of wood decay fungi: degradation of cotton cellulose
1999 - IRG/WP 99-10321
Brown-rot decay is responsible for 80% of the damage and replacement of wood in service. For nearly thirty years, researchers have postulated a one-electron oxidase system combining Fe+2 oxalic acid, and H2O2 in the production of hydroxy radicals which ultimately oxidize cellulose in situ. Recently, researchers have been investigating antioxicants, in combination with biocides (Schultz, et al.,199...
F Green III, T A Kuster


Six-year Report on the Performance of Borate-treated Lumber in an Above-ground Termite Field Test in Hawaii
2004 - IRG/WP 04-30343
We report the fifth and sixth years of field study results from a protected above-ground field test in Hawaii simulating the sill plate (dodai) used in conventional Japanese housing construction. Field tests were established in both Hawaii and Japan to examine the efficacy of disodium octaborate tetrahydrate (DOT, 2% and 3% BAE shell and through) wood treatments. In Hawaii, chromated copper arsen...
J K Grace, A Byrne, P I Morris, K Tsunoda


Fluoride movement through Douglas-fir and hem-fir lumber following dipping in potassium/ammonium bifluoride
1995 - IRG/WP 95-40040
The ability of ammonium and potassium fluoride to diffuse through Douglas-fir and hem-fir lumber was evaluated over a 90 day period. Boards were dipped in a solution containing 10% (by weight) of ammonium and potassium bifluoride, then stored under cover for 90 days. Samples removed 30, 60 and 90 days after treatment indicated that the fluoride was unable to completely penetrate the wood. Penetrat...
J J Morrell, C S Love


Sentry®), a new antisapstain formulation for protecting logs and lumber. - Part 1: advances in protection of New Zealand radiata pine logs
1999 - IRG/WP 99-30188
Until recently antisapstain formulations gave approximately 10 weeks protection to radiata pine logs and even within this time frame protection was often not consistent. Industry requires 20 weeks protection. The degree of protection sought by industry is in the order of 90-95%. For example, this equates to a maximum of 5 - 10% surface cover of sapstain in the first whole veneer produced from a pe...
R N Wakeling, D R Eden, C M Chittenden, J G Van der Waals, B Carpenter, I Dorset, R Kuluz, J Wakeman, T Price, B Nairn


Mould growth at lumber surfaces of pine after kiln and air drying
1994 - IRG/WP 94-40033
Distribution of water soluble substances in green wood and later redistribution during drying is of importance for the colonisation of wood by microorganisms. According to literature the availability of nitrogenous materials is probably a major limiting factor to the microbial colonisation of wood. King et al. (1974) and Oxley et al. (1976) have shown correlation between surface nutrient concentra...
N Terziev, J Bjurman, J B Boutelje


Evaluation of the effectiveness of defence anti-stain in the control of sapstain in laboratory and field tests
1990 - IRG/WP 3593
The anti-sapstain product Defence Anti-stain (DAS) has been evaluated internationally in laboratory and field tests during the years 1988 and 1989. Results of tests carried out by institutes and by own companies in countries like Indonesia, Ivory Coast, Japan, Portugal, Belgium, The Netherlands and Spain will be presented. In the several tests Defence Anti-stain showed a high fungicidal activity t...
G Rustenburg, C J Klaver


New experiences with Dry Rot in Danish buildings, heat treatment and viability tests
1989 - IRG/WP 1423
An increasing number of concealed dry rot attacks, especially in older multi-storey houses under renovation, have been detected during the last few years. A necessary consequence is a demand for cheaper methods of repair, compared to the standard method used in Denmark for many years otherwise severely attacked houses will by pulled down. A heat-treatment has been developed and tested in practice....
A P Koch, C Kjerulf-Jensen, B Madsen


Resistance of borate-treated lumber to subterranean termites under protected, above-ground conditions
2000 - IRG/WP 00-30239
An experiment to simulate the dodai (sill plate) of the Japanese houses was conducted at the termite field test site of Wood Research Institute in Kagoshima, Japan where two economically important subterranean termite species [Coptotermes formosanus Shiraki and Reticulitermes speratus (Kolbe)] are established. DOT(disodium octaborate tetrahydrate)-treated hem-fir samples [Tsuga heterophylla (Raf.)...
K Tsunoda, A Adachi, T Yoshimura, A Byrne, P I Morris, J K Grace


The potential for reuse of treated wood poles removed from service
1993 - IRG/WP 93-50001-18
Poles removed from service in Ontario and Quebec, Canada were characterized by age, wood species, preservative type, residual preservative, dimensions and condition. Based on this charactarization, the potential for reuse as round poles or posts, sawn posts, timbers and lumber, cedar roof shingles and firewood was assessed. A pilot study was conducted to evaluate the recovery and grade of lumber p...
P A Cooper


Database of sapstain fungi affecting lumber, logs and trees
2004 - IRG/WP 04-10534
Sapstain fungi discolour lumber, logs and tree sapwood and are often mistaken for moulds, which cause a superficial discoloration. Stained wood has a lower market value. Further, because stained wood products can potentially carry pathogenic fungi, such products may be refused by importing countries. Addressing these issues involves developing ways for accurately identifying staining fungi, docume...
S Lee, F de Giuli Vallverdu, S Alamouti, Jae-Jin Kim, A Uzunovic, C Breuil


Preservative treatment of green timber by soaking in ammoniacal copper borate
1984 - IRG/WP 3292
Freshly sawn boards of radiata pine sapwood were preservative treated by soaking in ammoniacal copper borate. Optimum schedules were obtained by partially seasoning the boards for one week prior to treatment. This aided the absorption of preservative and reduced the required soaking time to approximately 2 hours. Complete boron penetration was obtained after one week of block storage under cover a...
P Vinden, A J McQuire


Detection of increased metal cations after wood decay using Chromeazurol-S
1997 - IRG/WP 97-20112
Chromeazurol-S (CAS) is a dye used for the spectrophotometric determination of metals, mainly aluminum (Al), berillium (Be) and copper (Cu). CAS has been widely used for determining the penetration of copper containing preservatives like CCA (AWPA A3-96). Additional uses include: i) detection of utility pole decay (Esyln, 1979), ii) a chemical spot test for aluminum in wood (Kukachka and Miller, 1...
F Green III, U Srinivasan, R B Miller


Mechanical properties of CCA-treated southern pine after post-treatment kiln drying
1989 - IRG/WP 3543
This report reviews current research dealing with the effects of waterborne preservative treatment and redrying on the mechanical properties of wood. In general, waterborne preservative treatments reduce average mechanical properties. This effect is exaggerated when treated wood is kiln-dried after treatment, especially at elevated temperatures. For lumber, recently completed research at the Missi...
H M Barnes, J E Winandy


Prevention of non-microbial sapwood discolorations in hardwood lumber: chemical and mechanical treatments
1997 - IRG/WP 97-30137
Sapwood discolorations in hardwood lumber that are non-microbial in origin result from the formation of pigmented starch-like granules in ray parenchyma cells. These discolorations can be prevented by treating unseasoned lumber with an antioxidant (sodium bisulfite). Exposing unseasoned lumber to microwaves or treating logs with fumigants also will prevent these discolorations. Subjecting unseason...
T L Amburgey, S Kitchens


A study of fungal biodeterioration in unseasoned, packaged hem-fir lumber
1978 - IRG/WP 2116
This study was undertaken to determine the extent of biodeterioration that could occur within British Columbia (BC) prior to the export of packaged Canadian Lumber Standard Hem-Fir (Tsuga heterophylla, Abies amabilis and small amounts of Abies grandis). By examining the anti-stain treatments received by the lumber and identifying and characterizing the organisms responsible for the biodeterioratio...
P W Perrin, A J Cserjesi


A biochemical explanation for the observed patterns of fungal decay in timber
1980 - IRG/WP 1111
Experiments designed to compare the degree of localization of the cellulase enzymes of some white, brown and soft rot organisms are described. The site and nature of binding of the enzymes is discussed. The technique is ellution of mycelium grown in liquid culture with a variety: of agents including acetate buffer, carboxymethyl cellulose solution, borate/glycerol buffer and urea. The mycelium was...
N B Green, D J Dickinson, J F Levy


The effect of aqueous leaching on moisture uptake by CCA-treated blocks during soil burial
1987 - IRG/WP 2283
Mass loss, moisture content and nitrogen data from two soil burial experiments with untreated and CCA-treated Scots pine (Pinus sylvestris L.), Sitka spruce (Picea sitchensis Carr) and lime (Tilia vulgaris Hayne) are presented. These show that aqueous leaching of CCA-treated wood prior to burial significantly reduces its subsequent moisture uptake from soil. In the case of lime, a reduction in the...
C A Green, G M Smith, B King