IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 138 documents. Displaying 25 entries per page.


Quality of timber impregnated with preservatives of class AB after three years in service
2002 - IRG/WP 02-20241
Quality of impregnated timber is most often expressed by penetration and retention of the preservative used. Relatively less information is available about the performance of the final product, e.g. decks, panels etc. regarding product’s surface checks, deformations and overall appearance. Together with the timber durability, the above mention features are of esthetical importance in the above g...
N Terziev


High-energy multiple impact (HEMI)-test – Part 1: A new tool for quality control of thermally modified timber
2006 - IRG/WP 06-20346
Thermal modification processes improve durability and dimensional stability of wood, but the strength properties, especially the dynamic ones, are compromised and need to be considered with respect to industrial quality control. Results from standard dynamic strength testing, such as impact bending tests, suffer from high variability, and therefore require a high number of replicates. To overcome ...
C Brischke, A O Rapp, C R Welzbacher


Estimating the heat treatment intensity through various properties of thermally modified timber (TMT)
2009 - IRG/WP 09-40459
The suitability of different measures for prediction of the heat treatment intensity was investigated. Therefore, the resistance to impact milling (RIM), the lightness L*, the equilibrium moisture content (EMC), the anti swelling efficiency (ASE) and the total amount of soluble carbohydrates (TSC) of heat treated specimens were correlated with corresponding fungal resistance achieved by heat treat...
C R Welzbacher, C Brischke, A O Rapp


Morphological and Impregnability Properties of Narrow-Leaved Ash (Fraxinus angustifolia Vahl.) Wood Taken From Plantations with Different Spacings
2009 - IRG/WP 09-40475
Narrow-Leaved Ash, an important hardwood in Turkey, (Fraxinus angustifolia) is one of the fast growing species. In Turkey, several plantations have been established for 40 years. Narrow-Leaved Ash grows very fast and produces 25 (m3/year) mean increment. Except for eucalyptus and poplar, this increment is the highest compared to the other imported fast growing wood species. Until 1980, the spacing...
C Güler, H Ibrahim Sahin, S Sen


Influence of heat treatment intensity on the structural integrity of 14 timber species
2012 - IRG/WP 12-40586
Thermally modified timber (TMT) is characterized by improved durability and dimensionally stability, but strength properties, especially the dynamic ones, are compromised at the same time. Because dynamic standard tests require high efforts and time, the high-energy multiple impact (HEMI) –test was developed for the fast and reliable characterisation of the structural integrity of TMT, showing a...
C R Welzbacher, C Brischke, G Maier


Problems caused by termites in buildings in the State of Sao Paulo
1976 - IRG/WP 150
Termites are the main insects attacking buildings in the State of Sao Paulo - Brazil. Their attack occurs in wood and wooden materials as well as paper, textile, leather and so on....
M S Cavalcante


Improved equipment and technique for high pressure sap displacement impregnation of natural round wood
1972 - IRG/WP 309
Hitherto the main problem in the practical application of high pressure sap displacement impregnation (HPSD) has been in devising a satisfactory cap. Such a cap must be easily fitted to different size log ends to give a leak proof seal. The present contribution describes a new type of cap and sealing system designed to meet these requirements....
C G W Mason, F B Shorland


A case study on quality control on telephone poles as a cost saving tool in Tanzania
1987 - IRG/WP 3418
A sample of 28 CCA treated Eucalyptus poles from a lot of 2,000 poles awaiting delivery to the field, was studied to reveal the quality of treatment. Results showed a product of very poor quality. Average figures for penetration and retention were 8.4 mm and 2.2 kg/m³; these results are 66% and 91% below the required standards, respectively. Consequences of such results are estimated to amount to...
K K Murira


Wood preservation in France. "Bois plus" chain of quality. Description of the scheme early 1989
1989 - IRG/WP 3519
1989 - description of the French "CTB-BOIS PLUS" homologation scheme
G Ozanne


Treatment of dried sawn spruce and redwood building timbers with water-borne preservatives under a scheme for the quality control of the preservation and preserved wood in the Netherlands
1978 - IRG/WP 3123
Treatment of dried sawn spruce and redwood Building Timbers with water-borne preservatives under a scheme for the quality control of the preservation and preserved wood in the Netherlands. The aim of this article is to give the reader a modest description of the evaluation of fundamental research in wood preservation into a practical application....
H F M Nijman, N Burgers


Changed susceptibility of the chemically and thermally degraded spruce wood to its attack by the dry rot fungus Serpula lacrymans
1999 - IRG/WP 99-10322
In buildings, some intentional or unintended situations can occur at which some wood products are exposed to aggressive chemicals and also to higher temperatures. Occasional activity of fungi on such pre-attacked wood products can be either higher or lower. This paper deals with changes in the susceptibility of spruce wood (Picea abies L. Karst.) to attack by the dry rot fungus Serpula lacrymans, ...
L Reinprecht


Wood Preservation in France. A statement of quality control early 1986
1986 - IRG/WP 3389
A statement of quality control in France early 1986 - Summary of new - Standards criteria for preservatives and treated wood - Aptitude of treated wood for use per class of biological hazard...
M Romeis, G Ozanne


A simple leaching procedure for in-plant monitoring of CCA fixation
1993 - IRG/WP 93-30023
A simple leaching test is described to quantitatively estimate the extent of fixation of chromated copper arsenate (CCA) preservative treated wood products. It is based on the reaction between diphenylcarbazide and unreacted hexavalent chromium leached from borings taken from treated wood during the fixation process. The test requires about 20 minutes to complete and can be set up in a treating pl...
P A Cooper, Y T Ung


New developments in wood preservation
1974 - IRG/WP 335
Most of the developments in wood preservation in recent years have been stimulated by changing circumstances, particularly the increasing interest in reducing hazards and environmental, pollution but also the serious difficulties that are now being encountered in obtaining economic supplies of established preservatives. There is perhaps a danger that new controls to reduce pollution dangers may be...
B A Richardson


Preservative treatment of Pinus elliottii
1987 - IRG/WP 3435
The treatment of Pinus elliottii with copper-chrome-arsenic preservative by four alternative seasoning and treatment methods is investigated. Steam conditioning followed by either alternating pressure method (APM) or 'Q' treatment resulted in inadequate preservative penetration. Air drying or high temperature drying followed by the Bethell process resulted in a high standard of t...
P Vinden, L Carter


Measurement of VOC emissions from curative treated wood: A new emission test chamber
2001 - IRG/WP 01-50166-13
A poor indoor air quality (IAQ) is now recognized as a potential factor affecting occupants health. There are three basic strategies to improve IAQ: source control, improvement of the ventilation and use of air cleaners. Usually, the most efficient way to improve IAQ is to eliminate the different pollutant sources or to reduce their emissions. In order to precisely measure emissions from building ...
F Maupetit, O Ramalho, C Yrieix


Decay resistance of high performance biocomposites based on chemically modified fibres
1998 - IRG/WP 98-40120
Different partners within the framework of a European research project produced high performance biocomposites aiming at the utilisation of board materials as durable products both in dimensional and biological degrading circumstances. This paper summarises test data, which indicate the potential of board materials produced with modified fibre material. The chemical modifications applied cover a r...
V Rijckaert, J Van Acker, M Stevens


The role of third party independent inspection agency for wood preservation industry in China
2009 - IRG/WP 09-20425
This presentation attempts to provide a brief historical background and a current status report on the wood preservation industry in China. In addition, it will briefly introduce the need for building the quality control procedures and China wood protection Quality Supervision and Testing Center, a third-party inspection agency. Besides, some suggestions of this industry are proposed for its furth...
Zhenzhong Tang, Changsheng Shen, Yujie Han, Changming Song


Quality assurance approach of the German TMT manufacturers
2010 - IRG/WP 10-40513
Due to an increasing number of TMT manufacturers in central Europe, an organisation of TMT manufacturers was founded in Germany in the beginning of 2010. Since the current level of product testing and property declaration is not satisfying, one of the first activities is the establishment of a quality assurance system. In this paper a concept for quality assurance (QA) will be outlined....
W Scheiding, C R Welzbacher, A O Rapp


Radio frequency heating times for sterilization radiata pine solid piles
2017 - IRG/WP 17-40815
In this work was sterilized wood packaging material of radiata pine, stacked as solid piles without stickers, for determining the heating times using radiofrequency treatment. The experiments were performed in a radio frequency semi-industrial equipment. The results showed that the radio frequency heating times increases with wood volume and that radio frequency treatments were faster than convent...
H Esquivel, V Sepúlveda, J Torres, L Salvo, R A Ananías


Quality control of microwave treatment of timber after dry rot attack
2001 - IRG/WP 01-40205
In Denmark microwave treatment of timber has been used during the last 15 years for eradication of dry rot (Serpula lacrymans). About 1500 microwave treatments have been employed in coorporation with Hussvamp Laboratoriet. Previously all the infected timber was removed plus an extra metre as a safety zone. This meant that all casting boards and plaster had to be removed as well and joists replaced...
J Bech-Andersen, J Andreasson, S A Elborne


Exterior wood stains
1980 - IRG/WP 3135
Experience has shown that conventional paints cannot now be relied upon to provide a complete seal against water entry, that in practice water can often circumvent the film and that the paint, far from serving to keep water out will seal it in. Moreover present-day paints are often subject to localised and premature failure out of doors and consequently entail high maintenance costs. Problems of w...
E R Miller


Resin bleed after light organic solvent preservative treatment - the effect of drying method and process type
1986 - IRG/WP 3378
The effects of drying method and treatment process type on resin bleed were investigated. High-temperature drying of resinous radiata pine (Pinus radiata D. Don) heartwood resulted in improved wood permeability, higher preservative uptake, and greater resin bleed when treated by the Rueping process. Resin bleed was reduced substantially when timber was treated by the Lowry process, and totally eli...
P Vinden


Observations on the uptake and penetration of various liquids in clear heartwood and sapwood of Pinus radiata D.Don
1983 - IRG/WP 3224
Volumetric uptake of water (aqueous copper-chrome-arsenic (CCA)) or methanol, applied by bulk hydrostatic pressure to air dried clear heartwood specimens of Pinus radiata D. Don, far exceeds that of a wide variety of polar and non-polar solvents. In air dried sapwood, the volumetric uptake of CCA tends to be less than that achieved for most solvents including methanol. No comprehensive explanation...
J E Barnacle


The effect of high temperature and long pressing time on the dimensional stability and decay resistance of OSB
2002 - IRG/WP 02-40237
The exterior use of OSB is restricted because when it is exposed to wet conditions swelling, loss of internal bond strength (IB) and decay occur. In this study an alternative process of pressing which results in the production of dimensionally stable and a more decay resistant strandboard was investigated. Boards were pressed at elevated temperatures for prolonged pressing cycles and their physi...
G J Goroyias, M D C Hale


Next Page