Natural durability of wood in ground contact - A correlation between field and laboratory tests
1985 - IRG/WP 2182
A field test is being carried out to evaluate the natural durability of 20 hardwoods. The resistance to decay and termite attack was evaluated in accelerated laboratory tests. The results of the field test after 6 years and 8 months indicate that there is not necessarily agreement between results from laboratory and field tests. It is pointed out that apart from the artificiality of the laboratory...
M S Cavalcante, G A C Lopez, R G Montagna, M E S Fosco Mucci


Laboratory determination of the natural decay resistance of some lesser-utilized timbers from Tanzania against wood decay fungi
2004 - IRG/WP 04-10517
Four lesser known/utilized timber species (sap and heartwoods) from Tanzania, namely Albizia lebbeck, Zanthoxylum gilletii, Faurea saligna and Parinari curatellifolia were exposed to the brown rot fungi (Gloeophyllum trabeum and Coniophora puteana) and the white rot fungus (Coriolus versicolor) to determine their natural decay resistance according to the EN 113 standard procedure. The timbers were...
P R Gillah, R C Ishengoma, E Julias, S A Amartey, D H Kitojo


The chemical analysis and biological evaluation of wood extractives as potential timber preservatives
1995 - IRG/WP 95-30090
Work involved the biological performance of water and organic solvent soluble extractives of four naturally durable wood species, namely; Matumi, Tamboti, Sneezewood and the Turpentine tree. These timber species are known to be naturally durable against termites and fungi (±25 to 35 years). The extractives were evaluated against termites and fungi using impregnated pine pencil stakes in field tes...
P Turner, D Conradie


Vapour boron treatment of wood based panels: Mechanism for effect upon impact resistance
1994 - IRG/WP 94-40036
Samples of medium density fibreboard, chipboard and oriented strandboard (OSB) were treated to two retentions of boric acid by a vapour phase treatment. The results of a range of mechanical tests were reported by Hashim et al. (1992, 1993) in which a small reduction in impact resistance was observed. Several investigations were carried out to study how and where this loss in impact resistance occu...
R Hashim, R J Murphy, D J Dickinson, J Dinwoodie


Decrease of the antidecay resistance of beech wood treated with organotin fungicides after its natural ageing
1998 - IRG/WP 98-30185
The antidecay resistance of beech-wood samples (120 x 8.5 x 8.5 (MM)) treated with tributyltin fungicides gradually decreased due to prolongation of their natural ageing: tributyltin fungicides (TBTO, TBTS, TBTCA, TBT-DEDTK were applied by pressure impregnation technique in ethanole solutions (c = 0. 1%, 0.33% or 1%); treated beech-wood samples were naturally aged without their contact with grou...
L Reinprecht


Effect of media composition on the antagonistic properties of Trichoderma spp. against wood decay fung
1992 - IRG/WP 92-1538
Most screening of potential biocontrol agents of wood decay fungi has previously been undertaken using artificial media. Similarly experiments designed to evaluate the mechanisms involved in antagonism between biological control agents and target fungi, have largely been carried out in conditions which do not accurately reflect the nutrient status of wood. This paper examines the influence of nutr...
U Srinivasan, A Bruce, H J Staines


An in-ground natural durability field test of Australian timbers and exotic reference species. Part 5: Extensive data from a site where both decay and termites are active. Results from a full-replicated set of heartwood specimens from each of ten myrtaceous hardwoods after 18, 19 and 20 years' exposure - A discussion paper
1988 - IRG/WP 2324
Extensive data are presented on the decay situation, the termite situation and the decay-termite associations; all gathered from a fully-replicated set of heartwood specimens of 10 hardwood timbers after 18, 19 and 20 years' exposure in the ground at a single test site, i.e. a semi-arid steppe site. Sixteen tables are presented in addition to the one table providing the rating data; the l...
J D Thornton, G C Johnson, J W Creffield


Assessment of dehydrogenase activity, fluoride content and total chromium content of soil profiles exposed to preservative treated wood within a model system
1993 - IRG/WP 93-10015
The development and prospective use of a closed model system to facilitate study of a number of indicators of environmental impact of wood preservatives laboratory conditions has been described (IRG/WP/2395-92). Chemical analysis of leachate samples collected from drained soil profiles containing creosoted pole sections remedially treated with a chromated fluoride preservative indicated small incr...
G M Smith, D C R Sinclair, A Bruce, H J Staines


Natural decay resistance of some lesser-used tropical hardwoods from Ghana
2002 - IRG/WP 02-10438
Ghana is a tropical African country that is rich in diverse timber species. In order to reduce over-exploitation of the popular timber species and increase the resource base for the wood industry, lesser-used or lesser-known timber species are being promoted locally and for export. To do this successfully, it is essential to determine the physical, mechanical and biological properties of these tim...
S A Amartey, F R Hanson


Investigation on different variation factors in the results of mycological test and means to reduce and avoid them
1986 - IRG/WP 2264
In order to clarify the causes of the dispersion observed in the results obtained with mycological tests made in accordance with standard EN-113, different factors assumed to be sources of the variations were studied. These included the moisture content of the test samples during the test, the influence of certain technological properties of the wood, the virulence of the fungus strains, the metho...
D Dirol


Improvement of wood decay resistance by tannin impregnation
1991 - IRG/WP 2380
The fungical effect of tannins is appraised after exposure of treated woods samples to wood rotting fungi. A screening-test is carried out with several solutions containing extracts of two kinds of tannins; a condensed tannin derived from Quebracho heartwood (Schinopsis sp.) and a hydrolyzable one extracted from chestnut heartwood (Castanea sativa Mill). If a fungicidal action was indeed found it ...
D Dirol, A Scalbert


Biological resistance of aldehyde-treated wood
1994 - IRG/WP 94-40018
Biological resistance of wood treated with aldehyde cross-linking agents such as glyoxal, glutaraldehyde and dimethylol dihydroxy ethyleneurea (DMDHEU) were investigated. Sapwood blocks of Japanese cedar and Japanese beech, measuring 20 x 20 x 10 mm³ (T x R x L), were vacuum-impregnated at room temperature with 5-25% of aldehyde solutions. Blocks were kept in the solution for 1 week to gain the o...
S Yusuf, Y Imamura, M Takahashi, K Minato


Preservation of robinia wood (Robinia pseudoacacia L.) stakes by vintners
1982 - IRG/WP 3194
This work discusses decay resistance of robinia wood to fungi Trametes versicolor (L.ex Fr.) Pil. and Coniophora puteana (Schum. ex Fr.) Karst., and also the possibility of influencing its resistance by means of chemical protection. The results showed that natural resistance of robinia wood to these two different agents of wood decay is not the same. It is much less resistant to the fungus Conioph...
R Benko


Comparing the resistance of a number of lesser known species of tropical hardwoods to the marine borer Limnoria using a short term laboratory assay
2003 - IRG/WP 03-10500
Naturally durable species of timber are used as an alternative to preservative treated timber for marine structures, but many species have not been evaluated for their potential for use in this environment. EN 275 specifies a 5-year test period - too long a period for screening tests to be economically viable. In this study, durability was assessed by measuring the production of faecal pellets by ...
L M S Borges, S M Cragg, J R Williams


Natural resistance of timbers to marine borer attack. A laboratory test with Limnoria tripunctata
1977 - IRG/WP 430
Attack of the timber specimens was much less severe in the laboratory than in some marine localities. This is not surprising. One reason is certainly that wood-boring molluscs (Teredinidae and Pholodidae) which were missing in the laboratory are the most important wood-destroying organisms in the open sea. Another reason is that it is not possible to offer the gribbles optimal environmental condit...
H Kühne


Efficacy of anhydrides as wood protection chemicals
1997 - IRG/WP 97-30162
Wood samples treated with anhydrides of various compositions have been examined for their decay resistance and moisture behaviour. For this purpose two brown rot fungi (Coniophora puteana and Gloeophyllum trabeum) and two white rot fungi (Trametes versicolor and Pycnoporus sanguineus) were used in conventional and modified soil block tests. The modified soil block tests conformed to the method as ...
S C Forster, M D C Hale, G R Williams


Evaluating the potential of amine chemicals for use as wood protecting agents. Part 1: Investigation of cation components of quaternary ammonium compounds
1994 - IRG/WP 94-30049
Quaternary ammonium compounds (quats) have shown a great potential as more environmentally acceptable wood preservatives. In order to identify chemicals possessing the wood protecting potential, an evaluation was carried out of a range of commercially available 'quats', using a modified soil block test. Ponderosa pine sapwood blocks were treated with selected 'quat&a...
Hang Tang, J N R Ruddick


Biological resistance of wood treated with waterbased resins and drying oils in a mini-block test
1998 - IRG/WP 98-40107
In recent years it was found that the resistance of wood against fungal degradation could be increased by impregnation with an etherificated melamine formaldehyde resin. Using this resin as a reference, a waterbased fatty acid modificated alkyd-resin and two drying-oils were assessed for their biological performance in a mini-block laboratory test. Although drying-oils, like linseed-oil, are often...
M Sailer, A O Rapp, R-D Peek


Comparative natural resistance of eighty-two timber species to damage by marine borers at Goa (India)
1996 - IRG/WP 96-10139
Natural bioresistance of eighty-two species of Indian timbers to attack by marine wood-borers has been presented based on data collected from test panels exposed in Goa waters (west coast of India) for periods ranging from five to thirteen months. All the timber species, except Artocarpus gomeziana and Pterocarpus santalinus, were completely destroyed within a short period of three to six months. ...
L N Santhakumaran


Resistance to decay of particle boards: Presentation of a test method
1986 - IRG/WP 2260
The experimentations were undertaken on particle boards 35 and 50 mm thick. The rot resistance tests were carried out on specimens whose dimensions were 600 x 75 x 35 mm³ for particle boards 35 mm thick and 800 x 75 x 50 mm³ for particle boards 50 mm thick according to a method derived from the one described in the documents IRG/WP/2214 and IRG/WP/2243. Two exposure periods were used: 12 and 16 ...
G R Y Déon, N Trong


Investigation of the suitability of silver fir (Abies alba Mill.) for thermal modification
2004 - IRG/WP 04-40275
In this study the suitability of silver fir (Abies alba Mill.) was examined for thermal modification. Comparative experimental investigations were performed with silver fir and Norway spruce (Picea abies Karst.) after thermal treatments. Besides properties, which characterize the quality of heat treatments, like dimensional stability and resistance against fungal attack, strength properties of the...
C Brischke, A O Rapp


The improvement of wood durability by retification process
1993 - IRG/WP 93-40015
A material with new properties is obtained by retification process. It consists of a light pyrolysis of wood which becomes more stable and especially more resistant to fungal attack with few decrease of mechanical properties. Tests were carried out on three susceptible wood species (Poplar, Spruce, Fir) that are used in construction and are difficult to treat with wood preservatives. Retified wood...
D Dirol, R Guyonnet


Resistance of acetylated wood to biological degradation. Evaluation of field test
1997 - IRG/WP 97-30139
Acetylated wood samples were tested in ground contact (stake test) at two test fields, one in Simlångsdalen, Sweden, and one in Viikki, Finland, according to European standard EN 252. The test samples were inspected annually and their condition was compared with that of untreated controls and of samples treated with two reference CCA preservatives. The use of untreated controls and preservative t...
P Larsson Brelid, R Simonson, Ö Bergman


The high decay resistance in the sapwood of the naturally durable Malaysian hardwood Belian (Eusideroxylon zwageri)
2001 - IRG/WP 01-10410
It has long been assumed that the observed natural durability of the heartwood in certain timbers is perhaps associated with a relatively lower decay susceptibility also of the sapwood of these species. While the heartwood of Belian is reputedly highly decay resistant among the tropical hardwoods of Southeast Asia, laboratory decay tests reported in this paper have also confirmed the high decay re...
A A H Wong, A P Singh


The Effect on Biological and Moisture Resistance of Epichlorohydrin Chemically Modified Wood
2002 - IRG/WP 02-40224
Southern pine solid wood and fiber were chemically modified with epichlorohydrin to help in understanding the role of moisture in the mechanism of biological effectiveness of chemically modified wood. The solid wood had weight gains from 11% to 34%, while the fiber had weight gains from 9% to 75%. After modification, part of the specimens were water leached for 2 weeks or extracted for 2 hours ...
R E Ibach, B-G Lee