The Effects of Industrial-Scale Heat Treatment and Impregnation with Boron Compounds on Water Uptake and Tangential Swelling of Some Wood Species
2012 - IRG/WP 12-40599
This study evaluated the effects of boron impregnation and heat treatment on water uptake and tangential swelling of spruce (Picea orientalis), pine (Pinus nigra), beech (Fagus orientalis) and poplar (Populus deltoides) wood species. The samples (10 x 5 x 40 - tangential x radial x longitudinal cm) were impregnated with 4 % boric acid and 4 % borax according to the ASTM D-1413 standard method. Aft...
A Can, S Yildiz, Ü C Yildiz


Effect of double-vacuum and vacuum-pressure impregnation with water-borne preservatives on the dimensional characteristics of spruce
1990 - IRG/WP 3613
Air-dried planed spruce (Picea abies) samples were treated with a water-borne preservative (micro-emulsion) and one oil-borne type both containing azaconazole and deltamethrin. Each set of samples contained equal number of specimens with different growth ring orientation, heartwood content and density. In addition to the preservative retention and the penetration of a.i., the swelling of the sampl...
J Van Acker, M Stevens, G Rustenburg


End grain sealing by polymer impregnation
1992 - IRG/WP 92-3708
The solution and dispersion characteristics of several hydrophobic derivatives of cellulose have been studied and the abilities of these polymers to afford effective end grain sealing of Corsican pine have been examined. Both solution and dispersion treatments with ethyl cellulose imparted good water repellency and end grain sealing to wood samples, however, the disperse systems possessed lower vi...
J M Lawther, W B Banks, D G Anderson, J A Cornfield


Influence of water-borne preservatives on water repellency and the impact of addition of water repellent additives
1992 - IRG/WP 92-3704
The primary goal of a desirable wood preservative system is to effectively control decay fungi and other biodeteriogens in service. The water repellent nature of a given system may play an important role in the protection of wood. In this study, the water repellency of several water-borne preservative systems has been evaluated by measurements of tangential swelling during immersion. The systems i...
L Jin, D M Roberts, A F Preston


Effects of nano-wollastonite impregnation on fire resistance and dimensional stability of Poplar wood
2012 - IRG/WP 12-40595
The fire-retardant properties of Nano-Wollastonite (NW) in poplar wood (Populus nigra) were determined in this study. Some physical properties such as water absorption, volumetric swelling and Anti-Swelling Efficiency (ASE) were also measured. Specimens were prepared according to the ISO 11925 standard for the fire-retarding properties, and ASTM D4446-2002 standard for the physical properties. Imp...
A Karimi, A Haghighi Poshtir, H Reza Taghiyari, Y Hamzeh, A Akbar Enayati


Hygroscopicity of wood after polyethylene glycol (PEG) impregnation and/or heat treatment
2013 - IRG/WP 13-40623
The hygroscopicity of wood after polyethylene glycol (PEG) impregnation and/or heat treatment was investigated by testing the water uptake, equilibrium moisture content (EMC) at various relative humidity levels, and contact angle of the poplar wood surface. The results showed that: (1) At the first moment, the heat treatment at temperatures lower than 160 ℃ did not reduce the water uptake be...
Weiyue Xu Yuan Zhu, Jinzhen Cao


Superhydrophobic treatment of Norway spruce wood for improvement of its resistance against brown rot and moulds
2016 - IRG/WP 16-40734
Water repellence of wood can be increased and its some other properties influenced by introduction of hydrophobic chemicals into and on cell walls without affecting the wood’s bulk density due to lumen filling. Herein, a simple dipping method to insert octadecyltrichlorosilane (OTS) into cell walls and to deposit the self-assembled hydrophobic monolayers (SAMs) of OTS is reported. It was found o...
A Kumar, P Ryparová, P Hajek, B Kričej, M Pavlič, A S Škapin, M Šernek, J Tywoniak, J Žigon, M Petrič


A practical method to evaluate the dimensional stability of wood and wood products
1990 - IRG/WP 2342
This paper presents a new simple method to evaluate wood and wood products for their resistance to swelling and to assess wood preservatives for their ability to dimensionally stabilize treated wood exposed to water. Permeable wood of various dimensions and treated with different preserving chemicals have been measured for swelling in the radial and tangential direction during immersion in liquid ...
J P Hösli


Water-based water repellents for treatment of wood
1987 - IRG/WP 3446
The water uptake by wood can be reduced by treatment with a water repellent. The water repellents most commonly used are solvent based. In the present work a new type of water repellent that is water-based has been investigated. Two different treatments have shown an effect of the same order as a commercial solvent based product. The cellular distribution of the water repellents has been investiga...
I G Svensson, G Hägglund, I Johansson, W B Banks


Treatment of particleboard with isocyanate resin to impart improved dimensional stability and water repellency
2000 - IRG/WP 00-40178
Standard particleboard panels (for interior use) of 16 mm nominal thickness were cut into samples measuring 6.4 mm x 78 mm2. The samples were divided into 4 end matched batches. Two batches were treated with isocyanate resin and cured. The other 2 batches were left untreated. One of the treated batched and 1 of the untreated batches were edge sealed with epoxy resin prior to isocyanate resin appli...
K M Filcock, P Vinden


Technique for monitoring absorption during a vacuum pressure process
1992 - IRG/WP 92-3696
A laboratory technique was developed and an apparatus constructed which allowed for the direct and continuous measurement and observation of volumetric uptake of water-borne preservative into wood samples throughout a controlled vacuum-pressure treatment process. Fractional filling of void space was calculated. Graphing (fractional saturation) against time allows prediction of optimum cycle length...
A J Pendlebury, J A Petty


Assessment of contamination of soil and water at a CCA treatment plant: A demonstration project
1996 - IRG/WP 96-50067
Soil, sludge, dust and water samples were collected at a copper/chromium/arsenic wood preservation plant. Contamination of soil, sludge, dust and surface water with copper, chromium and arsenic was detected. Levels of contamination were sufficiently high to require remediation. Contamination originated from preservative solution dripping from recently treated wood. Migration of contaminants was vi...
P N Durrant, D C R Sinclair, G M Smith


Washboard effect: A surface deformation of spruce resulting from vacuum-pressure impregnation with water-borne preservatives
1987 - IRG/WP 3450
The washboard effect has been observed in sawn spruce after both commercial and laboratory based preservative treatments and is of increasing economic importance. The effect is defined as a specific phenomenon at the wood surface. It is distinct from internal collapse in the wood, but it may occur in association with internal collapse damage. Experimental investigations on the causes of washboardi...
H Willeitner, R J Murphy


Ancillary properties of vapor boron-treated composites
2001 - IRG/WP 01-40210
This paper discusses the water absorption, thickness swelling, and internal bond strength of North American composites treated using a vapor boron treatment process. For oriented strandboard, high boron loadings led to lower internal bond strength and lower thickness swelling. Water absorption results were variable but no deleterious effect of treatment was noted. For medium density fiberboard, th...
W A Jones, H M Barnes, R J Murphy


Observations on the uptake and penetration of various liquids in clear heartwood and sapwood of Pinus radiata D.Don
1983 - IRG/WP 3224
Volumetric uptake of water (aqueous copper-chrome-arsenic (CCA)) or methanol, applied by bulk hydrostatic pressure to air dried clear heartwood specimens of Pinus radiata D. Don, far exceeds that of a wide variety of polar and non-polar solvents. In air dried sapwood, the volumetric uptake of CCA tends to be less than that achieved for most solvents including methanol. No comprehensive explanation...
J E Barnacle


Dynamics of pressure changes in wood during impregnation
1990 - IRG/WP 3615
Conventional methods of impregnation have to be improved for achieving better penetration of refractory wood species. Basic requirements for an adjustment of treatment schedules are, amoung others, a profound knowledge of the course of pressure changes in the wood during treatment. A new method of pressure measurement was developed which supplies exact and reproducible data. The results show that ...
R D Peek, S Goetsch


Effects of heat treatment on water repellence and anti-swelling efficiency of beech wood
2002 - IRG/WP 02-40223
The heating of solid wood to higher temperatures is the simplest and the cheapest means for stabilizing its dimensions. For the investigation of the effect of thermal treatment on water repellency effectiveness and anti-swelling efficiency of beech wood (Fagus orientalis Lipsky), air-seasoned samples of beech wood were heated in presence of air at temperatures of 130 C, 150 C, 180 C and 200 C for ...
S Yildiz


A Preliminary Report on the Properties of Engineered Wood Composite Panels Treated with Copper Naphthenate
2005 - IRG/WP 05-40294
This paper reports on our preliminary investigation of the properties of randomly oriented strandboard which had waterborne or powdered copper naphthenate (CuN) incorporated into the board during manufacture. When compared to zinc borate-treated controls (ZnB), the mechanical properties of strandboard (MOR, MOE, work-to-maximum load, internal bond strength) were not adversely affected by treatmen...
J W Kirkpatrick, H M Barnes


Determination of fixation properties by bioassays - A proposal for the assessment of safety indexes in wood protection
1990 - IRG/WP 3566
In the determination of environmental effects of chemicals tests with fishes, daphnia and algae have proved to be practicable. With respect to wood protection such bioassays are suitable to control effects of treated timber against aquatic organisms. By using the fish-acute-toxicity-test the development of a laboratory test method is described for the checking of the fixation rate of a copper-chro...
H-W Wegen


Recent developments in the treatment of sawn spruce by double vacuum impregnation
1978 - IRG/WP 3114
The timbers used for building purposes in the U.K. and on the Continent of Europe are mainly softwoods. The two types of wood most used are redwood (Pinus sylvestris) and whitewood (Picea abies or Picea sitchensis). Other species are used to a lesser extent when considerations such as a long length requirement or width requirement demand the use of, for example, hemlock, Douglas fir or Parana pine...
C T Kyte, L D A Saunders


Moisture uptake and volumetric swelling as probable factors also affecting leaching in CCA-treated wood. A preliminary study of treated Eucalyptus saligna sapwood
2003 - IRG/WP 03-30318 IRG/WP 03-30318
A number of factors affecting leaching of CCA from treated wood have been variously investigated and discussed. However, the possible effects of moisture movement in treated timbers on leaching have not received attention yet. The present study examines and compares moisture uptake and volumetric swelling in CCA-treated and untreated sapwood of Eucalyptus saligna, and tries to establish a correl...
R Venkatasamy


Influence of pre-swelling conditioning on swellometer results for CCA and water repellent additive treated wood
1997 - IRG/WP 97-20125
The pre-test moisture content and conditioning history of wafers cut from wood treated with CCA and an emulsion water repellent additive can dramatically influence swelling curves generated using a standard swellometer apparatus. The rate of water uptake and swelling increased significantly as wafers were dried to lower moisture contents prior to immersion swelling. The pre-swelling conditioning h...
A R Zahora


Improvement of some technological and biological properties of poplar wood by impregnation with aqueous macromolecular compounds
1992 - IRG/WP 92-3721
Poplars (Populus spp) belong to the most important tree species in afforestation programs of the Netherlands. Due to their rapid growth, the wood quality is usually low. Therefore, studies were performed to elucidate whether some technological properties and the resistance against fungal attack could be improved by impregnation with water-soluble resins. The results showed that swelling and shrink...
R D Peek, H Militz, J J Kettenis


Properties of hot oil treated wood and the possible chemical reactions between wood and soybean oil during heat treatment
2005 - IRG/WP 05-40304
Thermal treatment with hot oil as the heating media based on the original idea from oil-heat treatment in Germany was investigated. The treatment was mainly carried out at 200ºC and 220ºC for 2 hours and 4 hours, and the wood species were mainly spruce and fir. This paper focuses on the difference between soybean oil and palm oil and the possible chemical reactions between wood and soybean oil. ...
Jieying Wang, P A Cooper


Probing red maple pit membrane pore size at FSP and OD using polystyrene macromolecules
2001 - IRG/WP 01-40217
A modified solute exclusion technique was used to pressure impregnate a polystyrene molecular weight (MW) series dissolved in styrene into red maple samples at approximately the fiber saturation point (FSP) and oven dry (OD). Radial penetration was less than tangential and FSP less than OD. There was a marked penetration change with MW in the tangential direction, although there appeared to be a ...