IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 38 documents. Displaying 25 entries per page.


Micro-Distribution of Metals in Wood Treated with a Nano-Copper Wood Preservative
2007 - IRG/WP 07-40360
The microdistribution of copper in southern pine treated with a newly-developed nano-copper wood preservative was examined to determine if it differed from that reported for wood treated with conventional copper-based wood preservatives. Field Emission Scanning Electron Microscopy (FE-SEM) in combination with x-ray microanalysis (EDX) revealed the presence of nano-sized copper and iron particles i...
H Matsunaga, M Kiguchi, P Evans


Mechanical strength of wood from the Vasa shipwreck
2008 - IRG/WP 08-20381
Samples from three ancient ship wrecks (Vasa, Elefanten, and Gröne Jägaren) and recent oak samples as reference were examined with regard to mechanical strength using the high-energy multiple impact (HEMI) - test method, which delivers the resistance to impact milling (RIM) of a material. Adoption and optimisation of the test method for the particular sample size of the wooden drilling cores was...
A O Rapp, C Brischke, C R Welzbacher, T Nilsson, C Björdal


Serpula lacrymans – calcium, iron, and foundering wooden boats
2009 - IRG/WP 09-10691
Serpula lacrymans is one of the most destructive wood-degrading brown rot fungi in temperate environments. Its virulence has often been linked to its ability to grow over non-woody materials and extract calcium (Ca) or iron (Fe) to promote wood degradation in buildings. This fungus has also been a severe problem in historic wooden warships and in modern wooden vessels, sometimes leading to founder...
J S Schilling, S M Duncan


The Chelator Mediated Fenton System in the Brown Rot Fungi: Details of the Mechanism, and Reasons Why it has Been Ineffective as a Biomimetic Treatment in some Biomass Applications – a Review
2014 - IRG/WP 14-10828
The chelator-mediated Fenton (CMF) reaction requires the action of two types of chelating compounds. The first chelator, oxalate, solubilizes and then sequesters iron, and the second chelator reduces iron. Iron reduction must be controlled near the fungal hyphae to prevent damaging Fenton chemistry from occurring in that location. Similarly, iron reduction must be promoted within the wood/plant ce...
B S Goodell, M Nakamura, J Jellison


Fungal decay of archaeological waterlogged oak timber: role of the mineral content
2016 - IRG/WP 16-10873
In service, wood foundation poles are subjected to water level fluctuation in soil. While wood is saturated by water only bacterial decay occurs. When oxygen content increases and moisture content decreases, severe fungal attack may occur. To evaluate the long term fungal durability of wood foundation pole in the context of service, 300 years waterlogged archaeological wood poles were used. The oa...
A Besserer, M Letellier, E Fredon, Q Kleindienst, M-L Antoine, C Perrin, J Lallemand, C Rose, M-C Trouy


Study on Nailed Joint with Iron Contamination. Part1: Shear Performance of Nailed Joint with Iron Contamination
2019 - IRG/WP 19-50349
In Japan, The building standard law was amended in 2000.1) The use of metal joint was obligated by this law. Since then, metal joints have been largely used for wooden buildings. Also, Act on the Promotion of Popularization of Long-life Quality Housing was enacted in 2009 and leaving Long-life Quality Housing has been focused on2). However, leaving houses to posterity for a long time causes severa...
R Nakano, D Nakano, H Ishiyama


Study on Nailed Joint with Iron Contamination. Part2: Elucidation of the Occurrence Condition of Iron Contamination
2019 - IRG/WP 19-50350
In recent years, efforts towards wooden buildings are progressing in Japan. And many woods are used in various places. However, various problems have also occurred in wooden buildings. One of the problems is iron contamination which appears when wood and metal chemically react. At present, tree species that are prone to iron contamination and components that cause iron contamination are clarified....
D Nakano, R Nakano, H Ishiyama


The iron reduction by chemical components of wood blocks decayed by wood rotting fungi
2021 - IRG/WP 21-10979
Brown-rot fungi, a group of wood rotting fungi, is well known to be one of major microorganisms that cause the deterioration of wooden buildings in Japan and have been considered to use chelator-mediated Fenton (CMF) reaction in concert with hydrolytic and redox enzymes for degradation of wood cell wall. CMF can be described as a non-enzymatic degradation system that utilizes hydroxyl radicals pro...
R R Kondo, Y Horikawa, K Ando, B Goodell, M Yoshida


Properties of Iron (II) Sulphate treated Norway Spruce
2022 - IRG/WP 22-30765
Exterior wood is exposed to various environmental factors that cause weathering. Weathering is important primarily from an aesthetic standpoint. However, not all parts of the building are equally susceptible to weathering. Parts exposed to moisture will discolour faster than protected parts, such as wood under roof overhangs. To achieve fast and uniform artificial greying, a surface treatment with...
B Lesar, M Humar, M Škamlec


Comparative study of the properties of silicate coatings with different mineral pigments (titanium dioxide, iron (III) oxide, copper (II) oxide) on the surface of wood
2022 - IRG/WP 22-40936
Silicate coatings are attractive alternatives to conventional organic-based coatings for wood protection. In this work, silicate coatings were prepared with a potassium silicate binder modified with a methyl siliconate solution, and three types of mineral pigments titanium dioxide, iron (III) oxide and copper (II) oxide. The coatings were applied on beech wood and cured under ambient conditions. T...
A M Cheumani Yona, M Petrič


Optimized composition of alkyd emulsion with nanoparticles of iron oxide for enhancing protection of thermally modified wood
2022 - IRG/WP 22-40940
Thermal treatment is acknowledged as an environmentally friendly method to improve durability of wood and some of its properties, such as biological resistance, dimensional stability, reduced hygroscopy. Despite these improvements, when used outdoors, also thermally treated wood is subjected to the action of environmental factors, like solar radiation, moisture, precipitations, temperature, etc., ...
E Sansonetti, D Cīrule, I Andersone, B Andersons, E Kuka


Make do and mend: Re-using timber in Smithfield Market
2022 - IRG/WP 22-50371
Historic buildings are part of our built environment. They are a record of how construction and use of materials have evolved and provide excellent opportunities for regeneration of urban areas. Moreover, re-using these buildings and as much of the material within, contributes to the Green Revolution. Currently, there is tremendous growth in green construction and as Bob Dylan once said, “the t...
J R Williams


Influence of weathering of wood surfaces before and after treatment with iron(II) sulphate
2023 - IRG/WP 23-30786
Outdoor wood is exposed to various factors that cause the wood to grey or age. The ageing processes can vary greatly depending on the exposure. Parts of the wood that are not exposed to external factors, e.g. under the eaves, are less exposed and the ageing process is therefore slower. This can be accelerated by solutions based on iron ions. In this way, the wood greys quickly and evenly. However,...
B Lesar, M Humar, F Osvald


Previous Page