IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 64 documents. Displaying 25 entries per page.


Decay resistance of beech wood and plywood treated with different type of phenol-formaldehyde (PF) resins
2016 - IRG/WP 16-40717
In this study treatment of beech and poplar wood veneers with (PF) resin industrial scale and screening tests of nine different phenol-formaldehyde (PF) resins were made. Specifically, the effect of different phenol-formaldehyde (PF) resin types on the resistance of beech wood against brown- and white-rot fungi was evaluated. Criteria for selection of optimal (PF) resin were based on minimum WPG ...
V Biziks, S Bicke, H Militz


Marine Borer Resistance of Acetylated and Furfurylated Wood – Results from up to 16 years of Field Exposure
2016 - IRG/WP 16-40756
Furfurylated and acetylated Scots pine sapwood has been tested since 1999 in a marine field with high marine borer activity. In 2004, two test groups with acetylated southern yellow pine (product later known as Perennial Wood™) were put out and over the whole test period differently furfurylated wood (later marketed as Kebony®) test groups have been started. Furthermore, some combinations of mo...
M Westin, P Larsson Brelid, T Nilsson, A O Rapp, J P Dickerson, S Lande, S Cragg


Lignin-Based Adhesive for Engineered Wood Products
2016 - IRG/WP 16-50319
Lignin as a naturally occurring polyphenolic compound has an excellent potential to replace petroleum-based phenol in formulation of phenol-formaldehyde adhesive that are used in manufacturing of engineered wood products. However, there are three major obstacles in application of polymeric lignin as phenol replacement: 1) low reactivity toward phenol, 2) high molecular weight, and 3) high polydisp...
I Kalami, M Arefmanesh, E Master, M Nejad


Weathering protection of European hardwoods through double modification
2017 - IRG/WP 17-30715
Beech and poplar were thermally modified, treated with melamine resin and both treatments were combined. The weathering performance (cracks and general appearance) of modified beech and poplar was assessed in natural weathering and correlated to material properties such as work in bending (WB) and Brinell hardness. In addition, the equilibrium moisture content after exposure of 12 months and subse...
G Behr, A Gellerich, S Bollmus, H Militz


Properties and potential use of Irvingia gabonensis and Irvingia wombolu kernel extracts as natural wood adhesives: Towards formaldehyde free wood composite products
2018 - IRG/WP 18-40832
Irvingia species are widely distributed in central and West Africa as well as parts of Asia and are earmarked for domestication due to the multitude of potential products that can be obtained from them. With renewed interest in renewable sources, the current study establishes the feasibility of utilizing extracts from Irvingia gabonensis and Irvingia wombolu kernels as wood adhesives. Proximate an...
A O Alawode, S O Amiandamhen, M Meincken, L Tyhoda


Improvement of wood decay and termite durability resulting from combined treatments based on borax/phenol-formaldehyde impregnation followed by thermal modification
2019 - IRG/WP 19-40871
This study determined the factors influencing the boron content after leaching of pine blocks impregnated with aqueous solution of phenol-formaldehyde (PF) resin with or without borax and subjected to heat treatment by response surface methodology. An experimental design permits to analyze the effects of heat treatment temperature (150, 185 and 220°C), curing time (5, 12, 5 and 20 hours), resin c...
S Salman, M-F Thevenon, A Petrissans, S Dumarcay, P Gerardin


Longterm Performance of Treated Timbers in Marine Exposures
2020 - IRG/WP 20-10969
The performance of preservative-treated or modified woods in marine exposures was evaluated at test sites in Newport, Oregon, USA and Brisbane, Queensland, Australia. All samples have exhibited excellent performance at the Newport, Oregon site, while attack was more aggressive at the sub-tropical Brisbane site. Acetylated wood as well as samples treated with 7.3% chromated copper arsenate (CCA-T...
M Konkler, A R Zahora, J Norton, J J Morrell


Performance of resin-treated solid wood and laminated veneer lumber (LVL) under marine conditions
2021 - IRG/WP 21-10973
Wood is a traditional building material in the marine environment, where it is exposed to extremely harsh conditions. Most of the indigenous softwood and hardwood species in Europe are not durable against attack by marine organisms. Recently, wood modification has been considered as an alternative to protect non-durable wood species under use class (UC) 5 (EN 335, 2013) conditions. The present stu...
L Emmerich, C Brischke, S Bicke, H Militz


Experience Experience from over 20 years of field trials of resin treated wood – Marine borer resistance of MMF and DMDHEU modified wood
2021 - IRG/WP 21-10976
In 1999 a field test of Scots pine treated with MMF (Methylated Melamine Formaldehyde) resin and acetylated Scots pine post treated with MMF resin was started. Six years later a commissioned full NWPC test for BASF of Belmadur® (DMDHEU resin treated wood) was started at the same site. The testing, according to European Standard EN 275, was done in a bay by Kristineberg Marine Research Station o...
M Westin, P Larsson Brelid, A O Rapp, J Habicht


Phenol formaldehyde modification and termite resistance under laboratory testing
2022 - IRG/WP 22-40952
The development of phenol formaldehyde (PF) resins as a means of impregnating solid wood is one that has been explored for several decades, both in terms of conventional impregnation processing (Impreg) or compressional impregnation (Compreg). However, it is only recently with advances in processing conditions that the method truly affords a means of achieving conventional modification for solid t...
L Nunes, A Pitman, M Duarte, B Stefanowski, D Jones


Long-term Performance of Treated Timbers in a Sub-tropical Marine Exposure
2023 - IRG/WP 23-11015
The long-term performance of preservative-treated and modified wood in marine exposures was assessed in Brisbane, Queensland, Australia. This report describes the final destructive assessment of the surviving Australian panels after 11 years of exposure. This site presents the potential for attack by shipworms (likely Bankia spp.), pholads (Martesia striata), Limnoria and Sphaeroma terebrans. Mos...
E L Galore, J Norton, A Zahora


Resistance of phenol formaldehyde impregnated beech (Fagus sylvativa L.) LVL against biodegradation in soil contact
2023 - IRG/WP 23-40965
Alternatives to preservative impregnation are emphasized in Germany and other European countries. Even though these treatments significantly improve wood's resistance to decay, they often do not have a beneficial impact on the dimensional stability. One alternative product, which may be used in ground contact for items like poles and railway sleepers, could be beech (Fagus sylvatica L.) laminated ...
M Slabohm, C Brischke, S Bicke, H Militz


Influence of the substitution of phenol with lignin cleavage products in phenol-formaldehyde impregnation resins for wood modification on the fungal decay resistance and impregnation depth
2024 - IRG/WP 24-30805
The impregnation modification of wood with phenol-formaldehyde (PF) resins increases the woods dimensional stability and resistance against fungal decay. However, to decrease the usage of non-renewable resources, the substitution of phenol has been a topic of scientific interest. Lignin is a currently underutilized resource with a chemical structure that contains phenolic units. For adhesive appli...
J Karthäuser, L Tarentino, A Treu, H Militz, G Alfredsen


A novel treatment for increasing UV stabuility of wood based on citric acid and urea
2024 - IRG/WP 24-30811
Wood, a fundamental material in the Built Environment, faces challenges related to durability and weathering, notably UV degradation leading to colour changes. This study explored a novel treatment method utilising citric acid and urea to enhance the UV stability of wood. The reaction between these compounds forms fluorescent species and insoluble nanoparticles upon thermal treatment. Two treatmen...
S Jué, A Scharf, C-F Lin, R Moutou Pitti, D Sandberg, D Jones