Comparison of the in-ground performance of pigment emulsified creosote (PEC) and high temperature creosote (HTC)
2000 - IRG/WP 00-30217
A long-term field trial was conducted in Australia to compare the in-ground performance of two oil-borne preservative formulations, conventional high temperature creosote (HTC) and a modified creosote formulation, pigment emulsified creosote (PEC). Three retentions (50, 100 and 200 kg/m³) were targeted for each formulation. An additional retention of PEC formulation (308 kg/m³), which contained ...
J W Creffield, H Greaves, N Chew, N K Nguyen


The loss of insecticidal action from synthetic pyrethroid-treated wood samples: The effect of high temperatures and relative humidities
1992 - IRG/WP 92-1569
This paper describes the results from bioassays using Hylotrupes bajulus, and chemical analyses, of pyrethroid-treated wood samples following storage for up to 3 years. A range of four storage environments was used consisting of combinations of two temperatures (20°C and 40°C) and two relative humidities (60% and 90%). It is concluded from the chemical analyses that, although losses at room temp...
R W Berry, S J Read


Wood durability in the light of recent trends and research on the durability of building materials and components
2000 - IRG/WP 00-20195
Building-related research of today demonstrates a clear shift in focus from the design and production phases to usage and to the entire life time. A consequence is that the performance criteria of materials, components and of the entire building must be regarded over the life time rather than at the time of production or delivery. As one example can be mentioned the Building Construction Directive...
K Ödeen


A real scale evaluation method and results on termite resistance of housing wall systems and floor framings
1999 - IRG/WP 99-10314
For evaluating the termite resistance of real scale houses especially housing wall systems and floor framings, a experimental building was prepared. After initial feeding of termite, this house was constructed. In this experimental building, several parts which were built by different wall systems and floor framing. The room temperature of these parts were controlled. Water can be provided in the ...
K Suzuki, K Okada, K Hagio, Y Tanaka


Tropical In-Ground Durability of Structural Sarawak Hardwoods Impregnated to High Retention with CCA-salts, CCA-oxide and FCAP after 20 Years Exposure
2005 - IRG/WP 05-30384
Statistical analysis (ANOVA) was conducted on durability (termite and decay combined) rating data collected over 20 years exposure period of over 140 species of Sarawak timbers with altogether 30,000 stake specimens, at the Forest Department’s Sibu “graveyard” stake test sites from 1977. About 20 replicated stakes were pressure-treated to refusal with 10% g/ml concentration of up to 3 CCA-sa...
Wang Choon Ling, A H H Wong


Accidental mold/termite testing of high density fiberboard (HDF) treated with borates and N’N-naphthaloylhydroxylamine (NHA)
2003 - IRG/WP 03-10462
High density fibreboard (HDF) was made from beech and pine furnish (50:50) and treated with boric acid (0.1-3%), borax (0.1-3%) or N'-N-(1,8-naphthalyl) hydroxylamine (NHA) (0.1-1%) prior to gluing with urea formaldehyde (UF) resin in order to determine resistance to Eastern subterranean termites (Reticulitermes flavipes Kollar), the most economically important termite species in North Am...
S N Kartal, H H Burdsall Jr, F Green III


Termite durability of sugi (Cryptomeria japonica) heartwood kiln-dried under high-temperature process in relation to wood extractives
2005 - IRG/WP 05-10547
Termite durability of sugi heartwood samples kiln-dried under a high-temperature process were evaluated by using Reticulitermes speratus (Kolbe) as a test termite sp. The n-hexane extractives of these samples were analysed by a GC technique. The less termite durability was shown on the wood samples dried under the high-temperature process, in comparison with that of the air-dried samples. No GC-p...
S Shibutani, E Obataya, K Hanata, S Doi


Long-term preservation technology for a large-scale timber structure building in Japan
2001 - IRG/WP 01-40203
Several 1.000-year-old Buddhist temples and shrines built of wood are surviving in Nara, some areas of which are inscribed on the World Heritage List. These old buildings are indicative of excellent timber construction technology having existed in ancient Japan, though it is thought that such technology has not been handed down. This paper introduces one of large-scale wood buildings built in rece...
Y Iimura


Major insects attacking timber used for building purposes and a practical approach for their control
1990 - IRG/WP 1449
Lignocellulosic materials like wood, bamboos, palmyra palms, reeds, leaves and grasses have been the oldest materials used by human beings. Although with the rapid pace of industrialisation, specially in several western countries, wood began to be replaced with alternative materials like cement, steel etc. yet its use has not vanished even in highly developed countries. Some of the reasons for thi...
V R Sonti, B Chatterjee


Gaseous preservative treatment of wood
1990 - IRG/WP 3631
A recent development in processing wood with a gaseous preservative means that dry, treated wood can be produced in under 30 hours with the benefits of product diversification, faster stock turnover and the ability to respond to short term demand. About 400,000 m³ of wood are treated each year in New Zealand with boron salts to protect from borer infestation. Traditionally this treatment is effec...
R Burton, A J Bergervoet, K Nasheri, P Vinden, D R Page


Serpula lacrymans the dry rot fungus. Revue on previous papers
1989 - IRG/WP 1393
It is found that the Dry rot fungus Serpula lacrymans grows in houses only because of its need for basic materials to neutralize the oxalic acid production or heavy metals which celate the oxalic acid. The average distance from the mycelium to the basic materials is found in average to be 14.2 cm with a variation from 0-100 cm. In contrast to Serpula lacrymans the Coniophora puteana and the Rigido...
J Bech-Andersen


Compatibility of deltamethrin with wood-finishing and construction materials
1993 - IRG/WP 93-30010
Under normal use conditions, treated wood comes to close contact with the structural components of a buiLding, and/or receives finishing, forming a new interface, which can affect the performance of a new product such as deltamethrin. To study this possibility, block-tests of Parana-Pine (Araucaria angustifolia), measuring 12 x 24 x 0.5 cm³ (with the largest dimension parallel to the wood-grain),...
E S Lepage


Durability of Sugi (Cryptomeria japonica D.DoN ) wood treated in high temperature liquid paraffin
2002 - IRG/WP 02-40221
Sugi(Cryptomeria japonica D.DoN )wood was subject to a heat treatment in high-temperature liquid paraffin for the purpose of improving the resistance against fungi and termites without chemicals. The bath of paraffin liquid, which can provide a uniform heat transfer (±2?), was used at temperatures of 90?,120?and 150?.?ecay resistance according to JIS K 15711) was evaluated using a brown rot fungu...
Y Matsuoka, W Ohmura, S Fujiwara, Y Kanagawa


Permeability measurements on surface layers for detecting wood with abnormally high permeability
1988 - IRG/WP 2298
Wet storage of timber during the warm period of the year may lead to an increased permeability of the wood, an undesirable phenomenon for several wood industries and also for many end-uses. Neither before nor after drying, such wood with "wet storage damage" can be visually distinguished from wood with a normal permeability. A non-destructive method for inspecting the permeability of surface layer...
J B Boutelje, G Hägglund


Termite physical barriers: update on retrofitting Granitgard™ around 'mock-up' buildings after five years
1997 - IRG/WP 97-10226
This field experiment was installed five years ago (March 1992) to evaluate the effectiveness of graded crushed granite stone, commercially marketed under the name Granitgard™, as a physical barrier when retrofitted around 'mock-up' buildings. The field site is located at Walpeup in the semi-arid mallee region of north-west Victoria (360 km from Melbourne), and there are eight ...
J R J French, B M Ahmed


Water transfer in wood in relation to fungal attack in building - Effect of condensation and diffusion
1992 - IRG/WP 92-1543
Wood is continuously exchanging moisture with the surrounding atmosphere, the temperature and relative humidity are important factors. Wood moisture in this case is not enough to provoque decay by fungi. However, when, during the night, condensation appears cyclically, wood absorbs water and moisture content may be sufficiently high to allow development if drying does not take place. The water tra...
D Dirol, J-M Vergnaud


The potential of high pressure pulsation processes to treat white spruce lumber with water-borne preservatives
1988 - IRG/WP 3471
Laboratory work using end sealed 4x8x46 cm³ white spruce samples has been done to explore the suitability of three variants of a 2.1 MPa pulsation process for the impregnation of white spruce with CCA. The results showed that the process improved significantly the penetration of the preservatives and reduced significantly cell collapse, when compared with the results of treatment using a 2.1 MPa ...
J P Hösli, J N R Ruddick


Factors affecting the resistance of fibre building boards to fungal attack
1975 - IRG/WP 252
Fungal decay is initiated at lower moisture contents in standard and tempered hardboards (18%) than in pine sapwood (26%). In contrast, in a saturated atmosphere, the equilibrium moisture contents of standard hardboard (14%) and of tempered hardboard (12.5%) are much lower than the moisture content permitting decay initiation whilst the equilibrium moisture content of pine sapwood (25.1%) approach...
C Grant, J G Savory


Evaluation of decay fungi in Norwegian buildings
2005 - IRG/WP 05-10562
During a period of 2 years and 3 months (1 January 2001 - 20 March 2003) Mycoteam had 3161 consultations in buildings in southern Norway, 1428 revealing damage from decay fungi. One consultation often revealed several occurrences of fungi, and the total number of occurrences of decay fungi was 3434. Thirty-five different species/genera/groups of decay fungi were recorded. During this period brown ...
G Alfredsen, H Solheim, K Mohn Jenssen


Social and economocal impact of an extension of service life resulting of an adequate preventive treatment. Application to wooden components used in urban areas with a high density of population
1993 - IRG/WP 93-50001-15
Le document évalue les problèmes rencontrés en zone urbaine pour le sauvetage des constructions: coordination de la lutte, délimination des chantieres et des périmètres d'investigation, nuisances causées par les interventions, risques pour la santé, risques pour l'environnement. Coûts. Comparaison socio-économique du traitement préventif et des interventions à posteri...
A T De Lelis, G A C Lopez


The effect of high and low boron soils on foraging termite behaviour and their metabolic systems
2007 - IRG/WP 07-10602
The highest concentrations of boron are found in ground water and soils of some of the driest climate areas (arid and semi arid regions) in the world. This present study examined the various concentrations of boron levels on filter papers against the subterranean termite species Coptotermes from different provenances and different boron soil levels. The termites were presented with no-choice bioas...
B M Ahmed, J R J French, P Vinden


High-energy multiple impact (HEMI)-test – Part 2: A mechanical test for the detection of fungal decay
2006 - IRG/WP 06-20339
The suitability of the high-energy multiple impact (HEMI)-test for detection of early fungal decay was examined. The HEMI – test characterizes the treatment quality of thermally modified wood by stressing the treated material by thousands of impacts of pounding steel balls. This method differentiates between heat treatment intensities, which are expressed by structural changes of the wood. Simil...
C R Welzbacher, C Brischke, A O Rapp


High-energy multiple impact (HEMI)-test – Part 1: A new tool for quality control of thermally modified timber
2006 - IRG/WP 06-20346
Thermal modification processes improve durability and dimensional stability of wood, but the strength properties, especially the dynamic ones, are compromised and need to be considered with respect to industrial quality control. Results from standard dynamic strength testing, such as impact bending tests, suffer from high variability, and therefore require a high number of replicates. To overcome ...
C Brischke, A O Rapp, C R Welzbacher


A roadmap for performance-based specification of wooden components based on service life prediction
2007 - IRG/WP 07-20351
The need for an unified and harmonised system for performance classification and specification of wood and wood-based products in Europe emanates from requirements of users and the European Construction Products Directive, CPD. A road to a feasible specification system is outlined. Exposure-related performance prediction was worked out as a key task on the way to product specification. Therefore s...
C Brischke, A O Rapp


Effect of fiber type and content on the natural durability of wood flour/high density polyethylene composites against rainbow fungus (Coriolus versicolor)
2007 - IRG/WP 07-40387
In order to evaluate the effect of fiber type and content on the natural durability of wood flour/high density polyethylene (HDPE) composites against Coriolus versicolor, samples containing 25% and 50% by weight of various natural fibers and HDPE were selected. Natural fibers included in the study were wood flour, rice hulls, hemp fibers and newsprint. Samples containing 25% and 50% natural fiber ...
A Karimi, M Tajvidi, S Pourabbasi