Your search resulted in 2 documents.


Cell wall properties of softwood deteriorated by fungi: combined chemical analyses, FT-IR spectroscopy, nanoindentation and micromechanical modelling
2013 - IRG/WP 13-20527
Mechanical properties of wood are determined by its inherent hierarchical microstructure, starting at the nanometer scale, where the elementary components cellulose, hemicelluloses, and lignin build up the wood cell wall material. Fungi cause degradation and decomposition of these components and, thus, alter the mechanical properties of wood. The aim of this study is to gain new insight into these...
L Wagner, T K Bader, K de Borst, T Ters, K Fackler


Assessing changes in hardness of furfurylated wood on a nano-scale to mimic levels experienced by the marine wood-boring crustacean, Limnoria
2023 - IRG/WP 23-11016
Wood-boring crustaceans and bivalves can cause severe damage to wooden structures in the marine environment, warranting the need for novel protection systems, such as chemical modifications. Furfurylation increases mechanical properties and resistance of timber species that would usually be susceptible to biodegradation by these borers, such as pine. In rapid laboratory and field testing, furfuryl...
L Martin, J Zekonyte, S Lande, M Westin, S Cragg