Insect transmission of fungal sapstain to freshly sawn unseasoned softwood lumber
1994 - IRG/WP 94-20025
Chemical dip treatments were used to investigate micro-arthropod transmission of fungal sapstain to unseasoned pine sapwood boards. Saptain, mould and basidiomycete defacement of chemically treated sawn boards of Corsican pine was recorded during a 14 week field trial. Boards were treated with either a fungicide, an insecticide/acaricide, a combination of the fungicide with the insecticide/acarici...
M A Powell, R A Eaton, J F Webber


Migration of Metals from Douglas-fir Lumber Treated with ACZA or Pentachlorophenol Using Best Management Practices: Preliminary Tests
2005 - IRG/WP 05-50224-4
The potential for migration of preservative components from ammoniacal copper zinc arsenate (ACZA) and pentachlorophenol treated Douglas-fir lumber in non-soil contact exposure was assessed in a simulated rainfall device. Metal levels from ACZA treated wood were elevated for the first 30 minutes of rainfall and then declined sharply. Repeated cycles of rainfall led to declines in initial metal l...
J J Morrell, Hua Chen, J Simonsen


Ancillary properties of vapor boron-treated composites
2001 - IRG/WP 01-40210
This paper discusses the water absorption, thickness swelling, and internal bond strength of North American composites treated using a vapor boron treatment process. For oriented strandboard, high boron loadings led to lower internal bond strength and lower thickness swelling. Water absorption results were variable but no deleterious effect of treatment was noted. For medium density fiberboard, th...
W A Jones, H M Barnes, R J Murphy


Leachability of borate-modified oriented strandboard: A comparison of zinc and calcium borate
2002 - IRG/WP 02-40232
The leachability of boron in zinc and calcium borate-modified oriented strandboard (OSB) was investigated in this study. The leaching experiments were conducted by exposing edge-sealed OSB samples under running water for 8, 24, 72, and 216 hours. The results were compared with those from the unleached controls. Boron leaching of the modified OSB occurred upon the initial water exposure, and the le...
S Lee, Q Wu


Effect of incising depth and density on treatment of Douglas fir, hem fir and spruce-pine-fir lumber with CCA, ACZA or ACQ
1997 - IRG/WP 97-40093
Incising markedly improves both the depth and uniformity of preservative treatment of refractory wood species, but there are few studies directly comparing the effects of incising depth and density on penetration and retention of commonly used waterborne preservatives in wood species from the western United States. The effects of two incision densities (7300 and 8900 incisions/square meter) at two...
M Anderson, J J Morrell, J E Winandy


Long-term protection of stored lumber against mould, stain, and specifically decay: A comparative field test of fungicidal formulations
1984 - IRG/WP 3281
The problem of decay in packaged, unseasoned lumber stored for many months has become of major importance in recent years. Large financial claims have resulted from decay in Canadian lumber stored at length in seaports and storage yards of distributors. For decades acceptable protection from moulds and sapstain was readily achieved with chlorinated phenols applied at appropriate treating levels. H...
A J Cserjesi, A Byrne, E L Johnson


Comparative moisture uptake of Douglas fir and radiata pine structural lumber when exposed to rain wetting as an indicator of relative decay resistance
2004 - IRG/WP 04-20285
Trials were undertaken to determine the relative resistance of radiata pine and Douglas-fir to wetting when exposed to the weather. Douglas-fir samples were obtained from one Central North Island and three South Island sources and had a heartwood/sapwood mix typical for each resource. Radiata pine sapwood and heartwood samples were obtained from a Central North Island source. Material was exposed...
M E Hedley, G Durbin, L Wichmann-Hansen, L Knowles


A termite field test with diffusion treated lumber
1991 - IRG/WP 3648
Douglas fir lumber, diffusion treated with concentrated sodium octaborate solutions, was tested against Coptotermes formosanus in an above ground field test wherein the samples were not exposed to a direct leaching hazard during the test period. After 2.5 years exposure, the untreated control samples were almost completely destroyed while poorly treated controls pressure treated with chromated cop...
K J Archer, D A Fowlie, A F Preston, P J Walcheski


Decay and mold resistance of borate modified oriented strandboard
2003 - IRG/WP 03-40260
Decay and mold resistance of zinc borate (ZB) and calcium borate (CB) modified oriented strandboard (OSB) from southern mixed hardwoods and yellow pine was investigated in this study. Tests were done with brown rot, Gloeophyllum trabeum, and white-rot, Trametes versicolar, fungi for 8 and 12 weeks, respectively. Wood species and fungus type had significant influence on the decay resistance. Decay...
Q Wu, S Lee, J P Jones


A new technique for testing decay resistance of framing lumber
2002 - IRG/WP 02-20247
Model house frame units (two studs, top and bottom plates and a central “dwang”) were constructed using short (500-600 mm) lengths of framing timber. Constructed frames were impregnated with water using a mild pressure schedule to raise the initial moisture content to 35-40 % mc. The back face of each unit was then covered with black polyethylene. Two locations at the stud/dwang and stud/botto...
M E Hedley, D Page, B E Patterson


Treatment of lumber with preservative/water repellent emulsions - The significance of shear stability on penetration
1997 - IRG/WP 97-20124
Currently, the treatment of lumber with a water repellent emulsion and a wood preservative formulation in combination is the most cost effective way to prevent decay and to maintain the appearance of uncoated lumber in service. Water repellents influence the movement of moisture into and out of wood and, by so doing, can decrease checking and splitting significantly. Adequate penetration of the em...
F Cui, K J Archer


A prototypical needle-incisor for refractory timber
1995 - IRG/WP 95-40041
A needle-incisor was manufactured for trial. This machine has an incising mechanism that a set of needles held by a rotary plate incises timber which is moved toward the front simultaneously, and then another set of needles incises a new part of the timber. Timber is incised by recycling the process. Timber incised of 4400 incisons/m² with the depth of 56 mm by 2.8 mm-diameter needles on all the ...
A Yakuwa, H Endoh, M Mori, S Doi


Sentry®, a new antisapstain formulation for protecting logs and lumber. - Part 2: protection of lumber
1999 - IRG/WP 99-30189
Recent research conducted by Forest Research, Chemcolour Industries (NZ) Ltd. and Fletcher Challenge Forest Ltd. has resulted in the development of antisapstain formulations that meet the efficacy requirements of the New Zealand Forest industry for export logs. One treatment, called Sentry®, is now poised for commercial use in New Zealand for treating export logs, having undergone an extensive su...
R N Wakeling, D R Eden, C M Chittenden, J G Van der Waals, B Carpenter, I Dorset, R Kuluz, J Wakeman


Characterization of checks and cracks on the surface of weathered wood
2000 - IRG/WP 00-40153
The surface roughness of unweathered and untreated pine; unweathered copper chromium arsenate type C (CCA) - treated pine; weathered CCA-treated pine; and weathered CCA-plus-water-repellent (WR) - treated pine was evaluated by a stylus tracing method. Surface roughness parameters Ra, Rz, Rmax, Rk, Rpk, and Rvk were measured. Ra, Rpk, and Rvk were the most appropriate parameters for describing modi...
D P Kamdem, Jun Zhang


Termite attack on susceptible lumber above naturally durable support posts
2000 - IRG/WP 00-10370
A multi-year field study was designed to simulate the use of naturally durable sill plates (dodai) and floor support posts in Japanese housing construction and test whether Formosan subterranean termites (Coptotermes formosanus) would tunnel over or through these resistant timbers to attack susceptible Japanese red pine (Pinus densiflora) lumber placed above them. This test was intended to explici...
J K Grace


Oxine copper (NYTEK® GD) for the control of mould and sapstain on lumber in North America
1989 - IRG/WP 3517
NYTEK® GD is a new, water-based, micro-dispersible formulation of oxine copper registered in the United States and Canada for control of mold and sapstain-causing fungi. NYTEK GD is noncorrosive and of low hazard to applicators and people handling treated lumber, when used according to the label. The product is an effective wood protectant applied as a dip or spray treatment at concentrations of ...
D F Myers, J M Fyler, C H Palmer, G D Rosebery


Dimensional lumber model demonstrates the sensitivity of the particle capture immunoassay in early detection of brown-rot fungi
1995 - IRG/WP 95-20058
A dimensional lumber model was designed to test the sensitivity of the particle capture immunoassay (PCI) compared to traditional methods of culturing and microscopic examination for detection of brown-rot fungi. Southern yellow pine 2 x 4's (5.1x10.2 cm²), and 86.4 cm in length, were inoculated on one end with the brown-rot fungus, Postia placenta, and tested over the full length of the...
C A Clausen, L Ferge


Integrated protection of freshly sawn lumber using Bacillus subtilis and selected fungicide
1997 - IRG/WP 97-10235
Bioprotection against stain fungi has tremendous potential for reducing discoloration of freshly sawn wood while decreasing chemical consumption. Unfortunately, most bioprotectants appear to be unable to consistently perform under the array of conditions to which freshly sawn wood is exposed. While research is underway to understand the nature of the inconsistent performance, a more pragmatic appr...
M E Mankowski, M Anderson, J J Morrell


Effect of climate, species, preservative concentration and water repellent on leaching from CCA-treated lumber exposed above ground
2001 - IRG/WP 01-50178
Few studies have examined leaching of chromated copper arsenate (CCA) from treated wood in above ground exposures due to the assumption that leaching is less severe compared to wood in continuous contact with soil or water. However, a significant portion of CCA treated wood is used for above ground applications, exposing considerable volumes of the preservative to precipitation and potential leach...
J L Taylor, P A Cooper


Evaluation of chlorothalonil for stain and mould control on lumber
1992 - IRG/WP 92-3713
Chlorothalonil is a commercially important fungicide with many industrial and agricultural applications. It has a very low mammalian toxicity and is considered to be an environmentally benign material. This paper describes the laboratory evaluation of chlorothalonil as a wood antisapstain treatment. Chlorothalonil was tested as three formulation types - an emulsifiable concentrate (EC), a water-ba...
P E Laks, T L Woods, D L Richter


Resistance of borate-treated lumber to subterranean termites in the field
1998 - IRG/WP 98-10255
Borate-treated wood samples were tested for their resistance against subterranean termites in the field. Wood samples (10.5x10.5x40cm3) of western hemlock were pressure impregnated with disodium octaborate tetrahydrate (DOT) and didecyldimethylammonium chloride (DDAC), and assigned into two groups on the basis of boron contents:high retention (1.5-2.2%BAE) and low retention(O.7~1.3%BAE). Eight rep...
K Tsunoda, A Adachi, T Yoshimura, A Byrne, P I Morris, J K Grace


Comparative field performance of CCA and CCA-water repellent treated Southern pine lumber
1995 - IRG/WP 95-30089
This paper describes the field performance of end-matched southern pine boards treated with either CCA type C or CCA type C containing an emulsion water repellent (WR) additive. Boards were either kiln or air-dried after treatment, constructed into decks, and exposed for over 3 years at Harrisburg, NC. During this exposure, matched boards were monitored for internal moisture content, cupping at mi...
A R Zahora


Recent development in North American industrial wood preservation plants
1988 - IRG/WP 3467
After remaining static for many years there have been a number of changes in plant design and treating cycles in recent years. This has been particularly true in the USA where few restrictions are placed on plant treating cycles by specifications; since only results type specifications are used. It is also important to realize that the AWPA Specifications for Southern Yellow Pine only call for tre...
J F Bridges


A comparison between high and conventional incision densities for improving preservative treatment of Douglas-fir heartwood lumber
1993 - IRG/WP 93-40009
Incising is required for the preservative treatment of most wood species from the western United States; however, there is considerable debate about the density of incisions required to achieve adequate treatment. Previous studies have shown that the incision effect on treatment is relatively narrow, suggesting that incision densities should be significantly increased over current practices and st...
S T Lebow, J J Morrell


Sawn timber of fir (Abies alba Mill.) - Treatability and usability for the Hazard Classes 3 and 4
1999 - IRG/WP 99-40147
Within a national research project, tests on the treatability on sawn timber of fir (Abies alba Mill.) in oscillation pressure, vacuum pressure and double-vacuum processes have been worked out with 95 trunks taken from 3 different altitude levels (up to a height of 590 metres, 600 to 990 metres and over 1000 metres) and from 4 different regions of Switzerland. As the treatability of round wood can...
E Graf, T Bör