Your search resulted in 187 documents. Displaying 25 entries per page.
The influence of thermal modification and surface charring to different levels on wettability of Norway spruce wood
2022 - IRG/WP 22-40942
The wood can alternatively be protected from water absorption by thermal modification and charring. Both techniques cause certain chemical and physical changes in the wood, the extent of which depends on the level of temperature applied. The objective of this study was to determine how the combination of charring to different levels and thermal modification affects the chemical, morphological, and...
J Žigon, C Gerardin, M E P Wålinder, P Gerardin
Influence of weathering on the mechanical properties and performance of exterior wood coatings
2022 - IRG/WP 22-40951
Three commercial coatings were exposed to artificial (EN 927-6) and natural weathering (EN 927-3) on wood samples. Cracking was visually assessed as well as Persoz hardness. Free films of the same coatings were also exposed to the same weathering tests before their tensile properties were measured. Results show that artificial and natural weathering modified the overall mechanical properties of wo...
L Podgorski, J-D Lanvin
The influence of climate changes on Central European forests with an emphasis on Slovenia
2022 - IRG/WP 22-50368
When forests are managed sustainably, they play an essential role in protecting climate and biodiversity. They protect soils and water resources, provide livelihoods, and contribute to the well-being of rural and urban communities. European forests are multifunctional and provide a range of ecosystem services. These include the production of renewable materials that can replace materials with a la...
J Gričar, L Krajnc, M Westergren, S Rus, H Kraigher
Influence of weathering of wood surfaces before and after treatment with iron(II) sulphate
2023 - IRG/WP 23-30786
Outdoor wood is exposed to various factors that cause the wood to grey or age. The ageing processes can vary greatly depending on the exposure. Parts of the wood that are not exposed to external factors, e.g. under the eaves, are less exposed and the ageing process is therefore slower. This can be accelerated by solutions based on iron ions. In this way, the wood greys quickly and evenly. However,...
B Lesar, M Humar, F Osvald
The influence of chemical and thermal modification on homogeneity between sapwood, heartwood, and transition wood of short rotation teak
2023 - IRG/WP 23-40961
Short rotation teak wood has low quality especially in durability. Heartwood presents sufficient natural durability and poor impregnability; meanwhile, most sapwood requires special treatment to increase its durability. The objective of this work was to investigate the effect of thermal or chemical treatment on homogenization between sapwood, heartwood, and transition wood for some selected proper...
R Martha, B George, W Darmawan, P Gerardin
Influence of the substitution of phenol with lignin cleavage products in phenol-formaldehyde impregnation resins for wood modification on the fungal decay resistance and impregnation depth
2024 - IRG/WP 24-30805
The impregnation modification of wood with phenol-formaldehyde (PF) resins increases the woods dimensional stability and resistance against fungal decay. However, to decrease the usage of non-renewable resources, the substitution of phenol has been a topic of scientific interest. Lignin is a currently underutilized resource with a chemical structure that contains phenolic units. For adhesive appli...
J Karthäuser, L Tarentino, A Treu, H Militz, G Alfredsen
How personality traits influence the perception of fungal decay in a wooden cladding – A survey in three Modelling wood moisture content in outdoor conditions from measured data
2024 - IRG/WP 24-41002
This study examined perceptions of fungal decay damage on wooden cladding across Norway, Sweden, and Germany. The majority of respondents across all countries did not find the fungal decay damage in question acceptable, with the least acceptance in Norway. This could be due to Norway having the highest frequency of wooden residential buildings and the most experience with maintaining wooden claddi...
G W Gustavsen, G Alfredsen, P B van Niekerk, J Niklewski, C Brischke
Modelling the service life of wood in ground contact – Verification of remotely sensed soil data from the reanalysis dataset ERA5-Land using in-situ measurements at a test site of utility poles in Eastern Norway
2024 - IRG/WP 24-41003
This study compared soil moisture and temperature estimates from the 5th European reanalysis (ERA5-Land) dataset with in-situ measurements to assess the accuracy and applicability of ERA5-Land data for modelling the service life of wood in ground contact. The ERA5-Land soil temperature estimates showed a moderate correlation with the in-situ temperature measurements (Spearman’s ρ of 0.73) and a...
U Hundhausen, P B van Niekerk, B Marais
Influence of incising methods and wood moisture content on ‘deep penetration treatment’ in Japanese cedar and larch
2025 - IRG/WP 25-20749
To expand applicability of ‘deep penetration treatment’, a solvent-borne and non-pressure treatment that is commonly coupled with roller-type incising using a flat blade, we investigated drill and laser machining as alternative incising methods and examined the influence of wood moisture content on the preservative penetration. Various incising methods were applied to heartwood of Japanese ced...
S Taira, T Miyauchi, S Isaji, H Matsunaga
Chestnut tannin-furfurylic resins for wood preservation: influence of the proportion of tannins as a copolymer
2025 - IRG/WP 25-30816
Tannin, which is present in all plants, is the most abundant polyphenol globally and can be extracted using water or organic solvents such as acetone, ethanol and methanol. Tannins are classified into two categories: condensed tannins (catechin-based polymers) and hydrolysable tannins (sugar esters with galloyl units). Previous studies have demonstrated its potential as a raw material for modifyin...
J V Dorini-Falavinha, C Gerardin-Charbonnier, P Cademartori
Process Development in Continuous Wood Densification and the Influence of Ionic Liquids on Set-Recovery and Mechanical Properties
2025 - IRG/WP 25-30827
The densification of wood significantly enhances its mechanical properties, making low-density species more viable for high-performance applications. However, challenges such as set-recovery (SR) and production speed hinder large-scale adoption. This study investigates continuous surface densification using a custom-built belt press and examines the effect of chemical pre-treatment with ionic liqu...
D Jones, A Scharf, B Neyses, D Sandberg
Influence of plasma treatment on the coatability of wood primer with a topcoat for exterior use
2025 - IRG/WP 25-30828
The coatability of oil, or of solvent-borne alkyd resin wood primers with waterborne acrylic finish is the subject of much debate, but not much information can be found in the scientific literature on this topic. The aim of our study was therefore to evaluate the adhesion strength of the waterborne acrylic coating on oiled wood or wood with a solvent-based alkyd primer and to test the recoatabilit...
M Petrič, L Albreht, N B Štrus, E Keržič, M Pavlič, J Žigon, S Dahle