Hydrothermal modification for upgrading the durability properties of soft deciduous wood
2010 - IRG/WP 10-40494
To extend the application potentialities of soft deciduous wood, upgrading the durability properties, hydrothermal modification (HTM) of aspen alder and birch wood was investigated. The treatment was conducted in a multifunctional laboratory device WTT. In the previous cases it has been found that the treatment at 160oC improves the durability insufficiently. The modification at 180oC ensured a hi...
B Andersons, I Andersone, V Biziks, I Irbe, J Chirkova, E Sansonetti, J Grinins, H Militz


Effect of acetylation on decay resistance of wood against brown-rot, white-rot and soft-rot fungi
1989 - IRG/WP 3540
Effect of acetylation on decay resistance of wood was investigated using wood blocks of Cryptomeria japonica, Pinus densiflora, Albizia falcata and Fagus crenata. Blocks were treated with uncatalyzed acetic anhydride for different lengths of time and exposed to Tyromyces palustris, Serpula lacrymans, Coriolus versicolor and unsterilized soil. The action of OH-radical on acetylated wood was also ex...
M Takahashi, Y Imamura, M Tanahashi


Efficacy of anhydrides as wood protection chemicals - II. Performance against soft rot fungi
1998 - IRG/WP 98-30174
Pine sapwood modified with various anhydrides and with butyl isocyanate was tested for its resistance to soft rot decay. Small stakes were exposed for 20 months in unsterile soil in a fungal cellar test. Wood modified with butyl isocyanate performed better than any of the anhydrides tested, with a threshold level of protection (less than 3% weight loss) at 12% weight percent gain (WPG). Stakes ac...
S C Forster, M D C Hale, G R Williams


Collaborative experiments in testing the toxicity of wood preservatives to soft rot fungi
1970 - IRG/WP 25
Eight Institutes from seven countries, Austria, England, France, Germany, Holland, Sweden and Switzerland have collaborated in an attempt to assess the suitability of various laboratory test procedures for acceptance as standard methods of determining the toxicity of wood preservatives to the cellulose-attacking micro-fungi which cause 'soft rot' of wood. Pure culture methods wit...
J G Savory, A F Bravery


Short term preconditioning of preservative-treated wood in soil contact in relation to performance in field trials
2000 - IRG/WP 00-20185
The effect of pre-exposure to primary colonising micro-organisms on preservative-treated wood, prior to a basidiomycete decay test, was determined by preconditioning in two soil types. Scots pine EN 113 blocks treated with 3 model systems (a triazole, a copper quaternary compound and a copper boron triazole) were leached according to EN 84 and subjected to 6 weeks and 8 weeks burial in either John...
S Molnar, D J Dickinson


Extracellular layers of wood decay fungi and copper tolerance
1983 - IRG/WP 1180
Extracellular layers around the hyphae of brown, white and soft rot fungi have been examined using electron microscopy. These layers were isolated for identification. Particular interest was directed towards the extracellular layers of copper-tolerant soft rot fungi....
D M Francis, L E Leightley


Wood in concrete. Summary of discussion at IRG 14, Surfers Paradise, Australia
1984 - IRG/WP 3264
The performance of untreated and preservative treated wood when placed in direct contact with concrete was considered in a discussion session at IRG 14. While published reports in this area are scarce, research is in progress internationally and a variety of practices are currently available to minimize any additional hazard posed by contact with concrete. This report summarizes the points raised ...
R J Murphy


The performance of wood preservatives in soil-bed soft rot tests
1993 - IRG/WP 93-20007
Testing the efficacy of wood preservatives in soil is recognised as a fundamental part of the assessment of long-term wood protection in ground contact. Laboratory based tests can provide a hazardous environment in which a preservative can be challenged by a range of micro-organisms. This paper presents the results of tests carried out to investigate the performance of wood preservatives in a wet ...
G R Williams, S Caswell


Collaborative soft rot test: Amended test method
1972 - IRG/WP 208
The initial draft of a standard test method (Document IRG/WP/201) was discussed at the meeting in Brussels in 1971. It was agreed that a revised draft should be prepared and that the Princes Risborough Laboratory (formerly FPRL) should conduct a trial test using the method as a preliminary to the main collaborative test....
J G Savory


Copper based water-borne preservatives: The biological performance of wood treated with various formulations
1987 - IRG/WP 3451
Wood samples treated with the various components of CCA preservative singly and in combination were tested against a soft rot organism, a copper tolerant brown rot organism and in soil burial both unleached and after leaching. The results suggest that, of the elements tested, fixed copper is essential for preventing soft rot attack and fixed arsenic is essential for preventing attack by a copper t...
S M Gray, D J Dickinson


A summary of tests and practical experiences with the Pilodyn wood testing instrument
1980 - IRG/WP 282
This paper presents a summary of the reports, tests and practical experiences with the Pilodyn wood tester not only, however, concerning poles but also in other fields such as standing trees, sawn timber etc. The principle of the Pilodyn is a spring-loaded pin which is fired into the object and the depth to which the pin penetrates is correlated to physical and mechanical properties of the object....
H Friis-Hansen


Ultrastructural observations on wood-degrading erosion bacteria
1986 - IRG/WP 1283
G F Daniel, T Nilsson


Development of a method for testing wood preservatives with soft rot fungi
1975 - IRG/WP 250
Although the first publications on experimental soft rot attack date back 20 years ago, so far no test method for evaluating the efficacy of wood preservatives against soft rot attack (Ascomycetes and Fungi Imperfecti) has been generally accepted. The reasons are diverse and the shortcomings and the disadvantages of the methods described are well known and have repeatedly been discussed. The soil ...
M Gersonde, W Kerner-Gang


Characterization of glycopeptide from white-, brown- and soft rot fungi
2002 - IRG/WP 02-10424
Extracellular low-molecular-weight substances that catalyze a redox reaction between O2 and electron donors to produce hydroxyl radicals have been isolated from wood degrading cultures of white-rot, brown-rot, and soft-rot fungi. They contained protein, neutral carbohydrate, and Fe(II). These substances were glycosylated (glycated) peptides and suggested to form Amadori product (ketoamine). The...
H Tanaka, S Itakura, A Enoki


Soil chemistry and wood decay
1978 - IRG/WP 2109
Soil is a most complex biological, chemical and physical material; its study is effectively a separate branch of science but almost entirely in relation to ist ability to grow plants - this paper is intendet just to note some known facets that might have relevance to the decay of wood and the performance of wood preservatives....
E A Hilditch


Effect of soft-rot decay on the static bending strength of wood
1991 - IRG/WP 2361
In this study, a modified static bending test has been developed as a method for measuring soft-rot decay in soil bed studies. A good correlation was found between the strength loss of the southern pine test specimens and extent of decay. This data suggests that it may be possible to develop a dynamic test based on stress relaxation that is more sensitive than static bending....
D D Nicholas, J A Wilson, R C Vasishth


The effect of treatment temperature on the biological performance of CCA treated wood
1990 - IRG/WP 3624
Birch and Scots pine sapwood blocks were treated with several concentrations of CCA at three different temperatures: 5, 20 and 35°C. The treated wood was maintained at the appropriate temperature for the fixation period. Leached and unleached samples were then exposed in a soft rot monoculture test using Chaetomium globosum and a brown rot monoculture test using Coniophora puteana. The treatment ...
S M Gray


Copper based water-borne preservatives: The use of a thin section technique to compare the protection of wood by copper based preservatives against soft-rot and bacterial decay
1987 - IRG/WP 2286
This paper describes the techniques developed and gives examples of results obtained for the performance of copper based wood preservatives against both the bacterial and fungal hazards....
A M Wyles, D J Dickinson


Preliminary screening of diffusion formulations for the control of soft rot
1978 - IRG/WP 2104
We have an urgent need in Australia to develop in situ remedial treatments for the present population of in-service transmission poles. For various reasons we have opted for formulations which can be applied as bandage treatments and thus we are primarily concerned with assaying diffusable toxicants. Two basic approaches have been made: an assay of the formulation's toxicity; and a combin...
H Greaves


Analysis of degradation observed on ancient wooden objects buried underground
2001 - IRG/WP 01-10403
Ancient wooden objects were sometimes excavated from the moat of mounded tombs in Japan. Such wooden objects were in the shape of a sunshade, bird, shield, pole, yugi(a bag that holds arrows) among others. Archaeologists discussed the usage of such shaped objects, but no one could clearly explain their use. Some objects were observed using an ordinary microscope. Deterioration by bacteria was foun...
H Sakai


Effects of artificial UV weathering and soft rot decay on heat treated wood
2005 - IRG/WP 05-40302
Oil and inert gas oven heat treated pine wood strips 100 µm thick were mildly heat treated (200°C, 30 mins linseed oil, 120 mins oven). Following treatment, specimens were exposed to UV weathering (300 hours) and decay by the soft rot fungus, Chaetomium globosum. The effects of each treatment were assessed by zero span tensile testing, microscopy and by FTIR. Tensile testing of heat treated s...
M D C Hale, S C Ghosh, M J Spear


Relative performances of DNBP and CCA wood preservatives in accelerated decay tests
1988 - IRG/WP 3496
The effectiveness of 2-sec-butyl-4,6-dinitrophenol (DNBP) was compared with that of CCA. Test blocks of Pinus patula and Eucalyptus grandis were impregnated to precisely known retentions of approximately 3, 6, and 10 kg/m³ CCA and solvent-borne DNBP respectively. They were then challenged in decay tests comprising soil burial and exposure to monocultures of Chaetomium globosum, Coriolus versicolo...
W H Schnippenkoetter, L D Abraham, A A W Baecker


Soft rot decay of Eucalyptus maculata Hook. in different soils from Queensland, Australia
1980 - IRG/WP 1113
In the present work, different Queensland soils were chosen and their gross effects on the decay of treated and untreated Eucalyptus maculata examined. The soils were also amended with various levels of phosphate to study the response of the wood decay mycota to an increasing supply of this nutrient. Phosphate amendment was chosen because of the wide-scale use of superphosphate on Queensland soils...
L E Leightley, I W Russell


Soft rot fungi as possible sources of odor in impregnated wood in buildings
1993 - IRG/WP 93-20013
Wood preservatives are frequently used inside houses. In several cases impregnated wood, particularly when used in crawlspaces or other near-ground constructions, has been found to be a source of odor. Mold fungi, soft rot fungi actinomycetes or bacteria growing on impregnated wood are possible producers of the odor. Analyses of volatile emissions from impregnated wood with odor and pure cultures ...
J Bjurman, J Kristensson


Ultrastructure of degraded, CCA-treated Pinus radiata wood from a marine pile
1990 - IRG/WP 1461
During an inspection of marine piles, 12 years after installation, severe degradation was noted on one of them in the vicinity of a corroded eye-bolt. The wood was dark brown in colour and tended to crumble easily. Wood fragments were examined by light microscopy and scanning and transmission electron microscopy and were also analysed for carbohydrates and lignin. Light microscopy showed numerous ...
A P Singh, M E Hedley


Next Page