IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 1181 documents. Displaying 25 entries per page.


Determination of absorption, accumulation and transport of copper in mycelium of some wood decay fungi
1999 - IRG/WP 99-10323
Copper compounds are common wood preservatives. However, tolerance of some wood decay fungi to copper compounds has been observed recently. Therefore, we tried to elucidate possible causes of this phenomenon. We investigated uptake, accumulation and secretion of copper in the mycelium of potentially copper tolerant fungi (Antrodia sp.) and non tolerant fungus Trametes versicolor. We observed that ...
F Pohleven, S Breznikar, P Kalan, M Petric


Preliminary studies to assess the effects of aeration and lowered humidity on the decay capacity, growth and survival of the dry rot fungus Serpula lacrymans (Wulf ex. Fr.)
1997 - IRG/WP 97-10208
Novel microcosms were used to test separately the effects of aeration and humidity on the decay capacity, linear spread and survival of Serpula lacrymans. The application of a pumped air supply resulted in an effective cessation of fungal activity when all but the lowest of the air flow rates was used. Furthermore, the lowest air flow rate caused marked growth tropisms away from the stress. In sep...
G A Low, J W Palfreyman, N A White, H J Staines, A Bruce


Serpula lacrymans, The Dry Rot Fungus and its Tolerance towards Copper-based Wood Preservatives
2005 - IRG/WP 05-10555
Serpula lacrymans (Wulfen : Fries) Schröter, the dry rot fungus, is considered the most economically important wood decay fungus in temperate regions of the world i.e. northern Europe, Japan and Australia. Previously copper based wood preservatives were the most commonly used preservatives for pressure treatment of wood for building constructions. Because of a suspicion about tolerance toward cop...
A C Steenkjær Hastrup, F Green III, C A Clausen, B Jensen


L-joint trials: Part 2: The relationship between colonisation by decay fungi and long-term performance
2002 - IRG/WP 02-20251
Many of the L-joint trials conducted at BRE were assessed during the early stages to establish the rate of colonisation by fungi, principally basidiomycetes. At that time, a system of assessment incorporating colonisation studies was proposed for inclusion within the European Standard EN 330 but was rejected for the final version of the standard. The long-term trials associated with the colonisa...
J K Carey


Durability of Bamboos in India against termites and fungi and chemical treatments for its enhancement
2005 - IRG/WP 05-10553
Bamboo is a very important forest resource that benefits the life of people in a myriad ways including meeting the need for structural uses like posts, pole fencing, scaffoldings, house building, etc. Although it is one of the strongest structural material available, often succumbs to fungal decay and biodeterioration by insects (termites and powder post beetles) during storage and usage. Studies...
O K Remadevi, R Muthukrishnan, H C Nagaveni, R Sundararaj, G Vijayalakshmi


Ability of chitosans to limit wood decay under laboratory conditions.
2004 - IRG/WP 04-30339
Chitosans have recently been explored for controlling a number of plant pathogenic fungi and have shown some promise for controlling stain fungi on wood. The potential for using chitosans either alone or in combination with copper sulfate to protect wood from fungal decay was explored using maple veneers. Chitosan treatment reduce weight losses caused by two brown rot and one white rot fungi, howe...
M Maoz, J J Morrell


Resistance of painted wood to mould fungi. Part 3. The effect of weathering, wood substrate and fungicides on mould growth
1998 - IRG/WP 98-10284
The effect of 6 month outdoor weathering on the resistance of acrylate paint systems on different types of pine and spruce sapwood to mould fungi was studied. Dipping into the preservative prior to painting, a primer with and without a fungicide (propiconazole + IPBC 0.50 + 0.2%) and a topcoat with and without a fungicide (propiconazole + IPBC 0.25 + 0.12%) were combinations of the treatments stud...
H Viitanen, P Ahola


Generation of hydroxyl radical by the brown-rot fungus, Postia placenta
1988 - IRG/WP 1360
In an electron spin resonance (ESR) survey of various liquid cultures and wood slivers innoculated with the brown-rot fungus, Postia placenta, the spin trap dimethyl-l-pyrroline N-oxide (DMPO) was used to detect the presence of the hydroxyl radical. The ESR spectra for the paramagnetic DMPO- hydroxyl radical adduct was observed in (1) nitrogen-limited, liquid cultures having 1.0% glucose or 0.1% c...
B Illman, D C Meinholtz, T L Highley


Which fungi should be included in the laboratory evaluation of anti-stain chemicals?
2001 - IRG/WP 01-20236
Test fungi for efficacy tests of anti-stain formulations were selected based on the assumptions that test fungi should be fungicide-tolerant antagonists and fungi resistant to both fungicides and fungicide- tolerant antagonists, and such fungi should be re-isolated from treated samples with the highest fungicidal concentration used for laboratory evaluation of fungicides. This paper discusses the ...
Hyung-Jun Kim, Jae-Jin Kim, Gyu-Hyeok Kim


Accelerated laboratory testing of preservatives on 13 North American wood species
1999 - IRG/WP 99-30201
The ability of selected water and solvent based biocides to protect wood against fungal attack was evaluated on 13 North American wood species using 7 decay fungi in a modified soil block test. Most preservatives were capable of providing protection at their recommended above ground and soil contact use levels. Many decay fungi caused substantial weight losses on blocks treated with chlorothalonil...
J J Morrell, C M Freitag


Interim report on the use of borate rods for the in-situ treatment of joinery
1980 - IRG/WP 3159
In the U.K. in recent years, it has been recognised that there is a major need for in-situ treatment of joinery at risk from or showing the early signs of decay. Several techniques have been developed to provide such a treatment, one of which is based on the insertion of anhydrous borate glass rods. The tests in hand are long term and this report is confined to the mycological isolation data from ...
D J Dickinson


Use of wood-decay fungi for disposal of PCP-treated wood
1995 - IRG/WP 95-50040-33
Although PCP has been classified as a priority pollutant, PCP-treated wood products are currently allowed to be disposed of as ordinary solid (non-hazardous) wastes in the US. Non-regulated disposal of these materials is allowed because PCP concentrations in extracts from PCP-treated products such as utility poles and crossarms, determined by the Toxicity Characteristic Leaching Procedure (TCLP) h...
R T Lamar


Fenton's reagent as a modification tool in brown-rot decay
1996 - IRG/WP 96-10155
A biomimetic approach was used to clarify the role and importance of the Fenton-type reaction in the carbohydrate degradation by brown-rot fungi. Spruce sawdust and microcrystalline cellulose were modified in the H2O2/Fe(II) treatment. The degree of hydrolysis of the pretreated spruce sawdust was clearly increased with the complete cellulase (Econase), purified endoglucanase from Trichoderma reese...
M Rättö, A-C Ritschkoff, J Buchert, L Viikari


Effect of cyclic change of temperature on fungal growth and mass loss
1994 - IRG/WP 94-10065
For estimating the effect of cycling change of temparature on fungal growth, four Japanese species, sugi (Cryptomeria japonica), hinoki (Chamaecyparis obtusa), akamatsu (Pinus densiflora) and buna (Fagus crenata), four fungal species, Tyromyces palustris, Gloeophyllum trabeum, Coriolus versicolor, Pycnoporus coccineus, and five temperature conditions, 10, 20, 27, 35°C and cyclic temperature (20°...
K Suzuki, K Okada


On the effectiveness of fumigants against wood-destroying insects and fungi in wooden cultural property
1993 - IRG/WP 93-10030
Based on a survey of the history of the use of fumigants the actual agents are mentioned in relation to their biogenic effect on wood-destroying insects and fungi as well as their corrosive behavior on cultural property. Furthermore the conditions for the use of reactive fumigants in buildings are discussed. Trials to control wood-destroying insects and fungi by nitrogen and bromomethane are the m...
W Unger, A Unger


Unsuitability of the limiting dose as a criterion for assessing the toxicity of preservatives to wood-destroying fungi
1974 - IRG/WP 243
In the majority of methods for investigating preservatives for wood-destroying fungi their toxicity is assessed by determining what is called the "limiting dose". This normally denotes a range of preservative solution concentrations or retentions of dry preservative in the timber, the lower value serving to indicate the amount of preservative at which is observed the expected effect, e.g. the grow...
D A Belenkov


The probable mechanism of action of boric acid and borates as wood preservatives
1990 - IRG/WP 1450
The tetrahydroxyborate ion [B(OH)4-] acts by complexation with poly-ols and probably attacks decay fungi through extracellular substrate sequestration; intracellular substrate sequestration; enzyme inhibition; and change in membrane function. Work was carried out to investigate this further and to try to explain certain phenomena observed in the area of boron preservation. The effect of Na borate ...
J D Lloyd, D J Dickinson, R J Murphy


Biochemical relationships between biodegradation of cellulose and formation of oxalic acid in brown-rot wood decay
1991 - IRG/WP 1472
Non-enzymic hydrolysis of cellulose with low concentrations of oxalic acid was examined. The incubation of pine wood pulp with 1% oxalic acid (pH 1.3) at 35°C for 4 weeks reduced the original viscosity to 60%. Reducing sugars were liberated from various cellulosic samples by the oxalic acid treatment. However, crystallinities of cellulose in those samples did not change before and after the treat...
M Shimada, Y Akamatsu, A Ohta, M Takahashi


Poplar wood and its damages in Iran
1987 - IRG/WP 1332
In Iran poplar planting has been used for many centuries ago specially in regions without forests. It had rural uses in ancient time, but recently many fast growing poplar species have been planted and many hybrids also have been planted; the following species had been cultivated widely in Iran: Populus nigra L. var. italica, Populus alba L., Populus caspica Bornm, Populus deltoides L., Populus X....
D Parsapajouh, P Niloufari


Screening results of fungicides for sapstain control on Pinus radiata
1983 - IRG/WP 3236
Thirty-two compounds were tested to determine their ability to contain the growth of stain, mould and rot organisms on fresh Pinus radiata D Don. A screening technique was employed using 35 to 50 mm diameter biscuits of Pinus radiata stemwood 10 mm thick. No compound was found to be cost effective when compared against the standard treatments of NaPCP (0.5% a.i.) plus borax (1.5%) and Captafol (0....
P J Hayward, J Duff, W Rae


Laboratory screening to determine the preventive effectiveness against blue stain fungi and moulds
1991 - IRG/WP 3677
This paper reports results of preservative treatment and leaching experiments, using borax, polybor and boracol 20, on small wood blocks of English oak and American pitch pine heartwood. Earlier experiments on the performance of various biocides as possible additives to bilgewater to prevent fungal decay of shipping timbers had suggested that some formulations of boron might be associated with phy...
M T De Troya, A M Navarrete


Lethal temperature for some wood-destroying fungi with respect to eradication by heat treatment
1984 - IRG/WP 1229
The lethal heat dosis as a function of temperature and time of exposure has been tested for mycelium and for wood infested by three strains of Serpula lacrymans and by Coniophora puteana, Poria monticola, Paxillus panuoides, Gloeophyllum trabeum and Gloeophyllum sepiarium. Even for Serpula lacrymans, which is well known for its sensivity to heat treatment, 30 min at 55°C were necessary to kill th...
M Miric, H Willeitner


Analysis of D-glucose metabolism of wood decay fungi using 13C-NMR and 13C-labeled substrates
2003 - IRG/WP 03-10475
D-Glucose metabolism is thought to be important during wood decay by fungi, not only for anabolic and catabolic purposes of central metabolism, but also as a potential source of peroxide required by extracellular peroxidases. There has been some confusion in the literature as to whether this peroxide-generating activity is of the glucose 1-oxidase or pyranose 2-oxidase (glucose 2-oxidase) type wi...
T H de Koker, M D Mozuch, P J Kersten


The natural durability story
1997 - IRG/WP 97-20119
Wood species with superior natural durability were in use since the beginning of timber utilisation. Their importance decreased with increasing industrial timber impregnation. In recent time, however, they gained worldwide new interest due to environmental problems involved with treated timber. In Europe a special Standard (EN 350) has been published and a multinational research project on testing...
H Willeitner, R-D Peek


A technique for assessing the preventive efficacy against decay fungi of preservative treatments applied to wood
1988 - IRG/WP 2309
A method is described in which test blocks with envelope preservative treatments can be challenged by selected test fungi previously established on an untreated feeder block. The progress of the test fungus through the treated zone is monitored using novel baits or sensors inserted in holes drilled into blocks to within predetermined distances of the face being challenged. Preliminary results show...
J K Carey, A F Bravery


Previous Page | Next Page