IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 437 documents. Displaying 25 entries per page.


Laboratory decay test of Burmese in and kanyin treated with three wood preservatives
1982 - IRG/WP 3210
Laboratory decay tests were performed on samples of In (Dipterocarpus tuberculatus Roxb.) and Kanyin (Dipterocarpus alatus Roxb. and Dipterocarpus turbinatus Gaertn f.) pressure treated with three wood preservatives - copper arsenic additive (CAA - a variation of ammoniacal copper arsenate), Arquad C-33 (a waterborne quaternary ammonium formulation), and tributyltin acetate (TBTA) dissolved in eth...
J N R Ruddick, R S Smith, A Byrne


Über den Nagekäfer Oligomerus ptilinoides (Wollaston), Col., Anobiidae: Verbreitung und Einschleppung, Bestimmung, Lebens- beziehungen und Befallsmerkmale mit Vergleichen zu Nicobium
1980 - IRG/WP 1102
Oligomerus ptilinoides occurs in the Mediterranian and Black-sea area, in North-Africa and Asia minor as an important pest causing severe damage to dry wood. By travelling, by the immigration of people from south to north, and by accidental introductions the species tends to establish itself north of the Alps. Severe damage has recently been observed in two museums. An account is given of aspects ...
S Cymorek


Principles and procedure of the planeing test
1981 - IRG/WP 2162
Small end-sealed samples of pine-sapwood (1.5 x 2.5 x 5 cm³) are treated by brushing and afterwards different parts of the treated surface are removed. The remaining part of the sample is tested against either insects or fungi. If no attack occurs sufficient amounts of biocides have been penetrated at least beyond the zone which has been removed. In spite of some problems the test seems the only ...
H Willeitner, M Gersonde


Laboratory evaluation of chemicals as termiticides
1986 - IRG/WP 1293
Laboratory procedures are described for screening chemicals against subterranean termites. Fast-acting compounds with persistent termiticidal activity are identified in tests using a soil substrate, and slower-acting bait toxicants are evaluated in a series of tests using cellulose substrates....
S C Jones


Light organic solvent preservative treatment schedules for New Zealand-grown radiata pine
1986 - IRG/WP 3379
The influence of pressure differential and treatment time on preservative uptake and distribution in radiata pine heartwood and sapwood is investigated. Treatment schedules are defined which minimise solvent usage but ensure complete sapwood penetration and optimise heartwood penetration....
P Vinden


Discussion of diiodomethyl p-tolyl sulfone (Amical® 48) as a fungicide for wood preservatio
1987 - IRG/WP 3425
The effectiveness of diiodomethyl-p-tolyl sulfone (Amical® 48) as a fungicide for preservation of wood is supported by a discussion of results from the literature and current research programs....
J M Stamm, K J Littel, F M H Casati, M B Friedman


Annotated check-list of the Limnoriidae
1990 - IRG/WP 4160
The crustacean isopod family Limnoriidae comprises 51 species of marine borers. A list of species is provided, together with notes on the species known distributions, depth ranges, and habitats. There is also a brief account of the phylogeny of the group....
L J Cookson


Use of vermiculite as substrate in assays on phytotoxicity of treated wood
1989 - IRG/WP 3547
It is considered the possibility of using vermiculite instead of soil as substrate in assays on phytotoxicity of wood treated with preservatives for agricultural use. Three organic preservatives were used. It had been tested the behaviour of both, vermiculite and soil in case of preservative leaking due to a leach. So that, assays of germination with cucurbitaceous were carried out, mixing a dose ...
M V Baonza Merino, D Franco


Vertical distribution of fouling and wood-boring organisms in the Trondheimsfjord (Western Norway)
1981 - IRG/WP 467
Results of a detailed study on the vertical distribution of fouling and wood-boring organisms of Trondheimsfjord at an interval of 3 m from intertidal level to a depth of 30 m, has been presented, based on data collected from two series of panels, exposed from 15 March 1977 to 15 July 1977 (Series I) and from 22 July 1977 to 13 March 1978 (Series II). The intensity of fouling generally decreased w...
L N Santhakumaran


Establishment of a laboratory method to characterise the ecotoxicity of a polluted soil
1998 - IRG/WP 98-50101-23
This method consists in using the underground grub of the Oxythyrea funesta beetle as a bioindicator of the soils pollution. Due to the significant tolerance of the organism, a large type of substrate of different nature and grain size could have been studied. We have tested substances and preparations such as wood preservation products even under powder or liquid form but also some wastes of di...
P Martinet


Soil blocks versus field test for evaluating and standardizing wood preservatives: A commercial view
1994 - IRG/WP 94-20024
On the basis of technical considerations, experience, costs and applicability, the author concludes that the soil block test and other laboratory tests have little meaning in a wood preservative standardization process and almost no merit in the commercialization of a wood preservative system. Field tests at sites known to be aggressive to preservative treated wood are strongly recommended....
W S McNamara


Collaborative soft rot tests: Proposals for a standardized soil burial test
1971 - IRG/WP 201
A F Bravery


Some aspects of laboratory and field testing methods of antitermite wood preservatives
1973 - IRG/WP 235
Various methods for laboratory testing of antitermite activity of wood preservatives are described. The results of simultaneous tests of three water-borne preservatives, according to the various methods are discussed, and comparison is made with results of field tests on the same three preservatives, showing a fairly good accordance between laboratory results and field results....
M Fougerousse


Some observations on Chlorophora pilosus Forst. var. glabromaculatus Goeze (Coleoptera, Cerambycidae)
1980 - IRG/WP 1119
A Gambetta


Collaborative soft rot tests: Interim report on PRL tests of Cu/Cr/As preservative using method of Document No: IRG/WP/208
1972 - IRG/WP 211
Preservative: Tanalith CT.106 - Results obtained with beech are given in the table and indicate a toxic limit of 16.7-19.2 kg/m³ - The initial soil moisture content was adjusted to 27.8% (the water holding capacity). Noticeable drying out has occurred in some of the test bottles....
J G Savory


Microcapsule formulation of fenitrothion as a soil termiticide
1991 - IRG/WP 1478
The efficacy and the mode of action of a microcapsule formulation of fenitrothion against Coptotermes formosanus Shiraki were investigated. The physicochemical property that this formulation does not allow the active ingredient to diffuse through the capsule wall contributed to a long lasting efficacy and safety for the men spraying. The residual effect of the fenitrothion microcapsule in soil was...
H Teshima, T Itoh, Y Abe


Selective adsorption of antisapstain actives from two aqueous suspensions, and movement of actives into wood
1996 - IRG/WP 96-30103
Green-off-saw rough sawn Pinus elliottii (slash pine) boards were dipped in aqueous suspensions of two antisapstain formulations, NeXgenâ and Busanâ Sap Stain Preventative (Busan 1009), at three product concentration levels. Concentrations of active ingredients (NeXgen: CTL (chloro-thalonil) and MTC (methylene bisthiocyanate); Busan 1009: TCMTB (2(thiocyanomethylthio)-benzothiazole) and MTC) wer...
M J Kennedy, T L Woods


Studies of the distribution and degradation of tributyltin naphthenate in double-vacuum treated wood
1983 - IRG/WP 3230
The effects of forced solvent evaporation by kilning redwood (Pinus sylvestris) that has been double-vacuum treated with tributyltin naphthenate (TBTN) have been investigated. Contrary to previous studies reported, it has been shown that forced evaporation can have a considerable influence on the losses of the fungicide. It has been found that, whether the solvent is allowed to evaporate slowly or...
J Jermer, M-L Edlund, W Hintze, S V Ohlsson


Factors affecting leaching of preservatives in practice
1978 - IRG/WP 3113
At the 7th Meeting of the IRG in Poland in May 1975, the findings of collaborative laboratory leaching techniques were discussed, and the dangers inherent in using such results to predict the behaviour of preservative-treated components in service were emphasised. In order to improve our understanding of the factors governing leaching of preservatives in practice, and to identify areas where furth...
R Cockcroft, R A Laidlaw


A preliminary study on the feasibility of substituting the soil culture medium in soil block tests
1984 - IRG/WP 2209
In this work the possibility was studied of substituting the soil culture medium in preservative screening methods. The conclusions are that another type of material, Sphagnum moss, can be used with advantages, but that some more information is still needed to give a real idea regarding the differences caused by the substrate tested....
J C Moreschi


Contribution to the testing of wood based board material
1982 - IRG/WP 2176
R G Lea


An investigation concerning Camponotus spp. distribution and damage in buildings in Sweden
1985 - IRG/WP 1248
This is a report of an investigation by a Swedish insurance company on the occurrences of damage by Carpenter ants during 1974 to 1981. The distribution of damage in walls, roofs and floors of both permanent homes and summer-houses has been assessed. It is concluded that the increased frequency of attack is becoming economically serious....
V Butovitsch, K-J Hedqvist, C Tornberg


Contribution to study of the degradation caused in Pinus spp. poles used in field test
1989 - IRG/WP 1417
The study of the degradation produced by soil natural microflora on wood in contact with it in the field, has been going on for several years now. Our contribution to this aim in the present work has dealt with the possible relationship of the microorganisms in the soil. The microscopic visualization of wood colonization by the microorganisms, and the chemical analysis of the degraded wood compare...
M T De Troya, A Garcia, M J Pozuelo, A M Navarrete, A Cabanas


Assessment of losses of wood preservatives from treated wood by leaching into the environment
1993 - IRG/WP 93-50001-13
Wood preservative chemicals may be lost from treated timber by leaching into water or soil. The degree to which this might occur and its effect on the environment is difficult to assess quantitatively due to the absence of appropriate test methods. This paper describes work to assess test methodology capable of allowing the rates of loss of wood preservative from treated timber to be quantified. T...
R J Orsler, G E Holland


The effectiveness test of chemicals against Serpula lacrymans
1984 - IRG/WP 2222
The effectiveness tests of wood preservatives against Serpula lacrymans were conducted in accordance with Japan Industrial Standard A 9302 and Japanese Wood Preserving Association Standard No. 1. Also, the soil treatment test against this fungus was carried out with two chemicals. The preservatives tested without Creosote oil (out of JIS) had sufficient preservative effect against Serpula lacryman...
S Doi


Previous Page | Next Page