Recent developments in the treatment of sawn spruce by double vacuum impregnation
1978 - IRG/WP 3114
The timbers used for building purposes in the U.K. and on the Continent of Europe are mainly softwoods. The two types of wood most used are redwood (Pinus sylvestris) and whitewood (Picea abies or Picea sitchensis). Other species are used to a lesser extent when considerations such as a long length requirement or width requirement demand the use of, for example, hemlock, Douglas fir or Parana pine...
C T Kyte, L D A Saunders


Changed permeability and surface properties of hornbeam wood due to its degradation by erosive strain of Phanerochaete chrysosporium
2004 - IRG/WP 04-40290
Specimens of hornbeam wood were submitted to a medium-term degradations by erosive fungus Phanerochaete chrysosporium. Biodegradations of specimens resulted in their apparent structural alterations, changes in permeability and increased intensity of interactions with polar liquids. Modified physical properties of biodegraded wood may significantly influence its penetration with polar media and che...
R Solár, S Kurjatko, L Reinprecht, M Mamon, V Vacek


Natural weathering of wood in a sunny climate effects on surface chemistry and paint adhesion
1997 - IRG/WP 97-20109
Radiata pine veneers and blocks were exposed to natural weathering under Australian summer conditions over a period of 30 days. Infrared spectroscopy revealed that there was perceptible surface delignification after 4 hours exposure, substantial surface delignification after 3 days exposure and almost complete surface delignification after 6 days. Viscometry determinations on holocellulose samples...
P D Evans, P D Thay, K J Schmalzl


Some experiences with attack of microorganisms on wooden constructions supporting foundations of houses and bridges
1997 - IRG/WP 97-10232
Reconstructions of bridges and public buildings or damage of houses during the construction of subway lines in Berlin have led to a number of inspections of wooden foundations, mostly pine or spruce piles, representing service lives of between ca. 70 and 140 years. In all cases bacterial attack was found both in wood submerged in ground water and in surface water. The extent of deterioration diffe...
M Grinda


Surface Barriers for Protection of Culture and Heritage Wooden Objects from Insect Attack
2004 - IRG/WP 04-20286
Anoxic treatment is an environment friendly procedure for eradication of wood boring insects in wooden objects of cultural and historical heritage. However, after the anoxic treatment, wooden antiques remain susceptible to further insect attacks. Possible protection against insects could be provided by the so-called post-repression protective barriers. Potential coating materials for such barriers...
M Petric, M Pavlic, B Kricej, M Humar, F Pohleven


Wood protection by surface treatment of two borate preservatives, TIM-BOR® and BORA-CARE®, for the formosan subterranean termite and eastern subterrean termite
1993 - IRG/WP 93-10044
TIM-BOR® (disodium octaborate tetrahydrate: DOT, Na2B8O134H2O) and BORA-CARE® (40% DOT in ethylene glycol) are two borate products marketed for treating wood in use by brushing or spraying onto the wood surface. The active ingredients presumably diffuse into wood by the 10-15% existing wood moisture. Few data, however, are available to demonstrate the diffusion rate. Su & Scheffrahn (1991) s...
M Toroko, N-Y Su


Improving the weather resistance of glue-laminated jarrah and karri
1994 - IRG/WP 94-40017
Surface modification and dimensional stabilisation significantly increased the dry and wet shear strength of karri and jarrah lap-shear specimens (laminates) bonded with resorcinol formaldehyde. The combination of surface modification (sanding/sodium hydroxide treatment), and furfurylation produced the highest dry and wet shear strengths. Acetylated laminates had the lowest dry bond strength, but ...
J Balfas, P D Evans


An inclination incising technique for the preservative treatment of refractory timbers
1991 - IRG/WP 3664
An inclination incising technique for preservative treatment of refractory timbers was examined by changing cutting angle to the longitudinal direction of test specimen and by using different types of knife edge. Incised wood were impregnated locally into incisions with CCA solution by the specified local pressure process. Width and length of penetration areas of CCA solution were measured on long...
Y Nakamura, K Nishimoto


Paper for discussion - Incising of spruce to improve preservative penetration
1973 - IRG/WP 318
Large quantities of whitewood or Norway spruce (Picea abies) are regularly imported into the United Kingdom from continental Europe. In addition, increasing amounts of Sitka spruce (Picea sitchensis) are likely to become available over the next decade from the Forestry Commission. In many ways spruce is a good structural timber, eg it is relatively cheap and easily available, it has adequate stren...
W B Banks


Improvement of some technological and biological properties of poplar wood by impregnation with aqueous macromolecular compounds
1992 - IRG/WP 92-3721
Poplars (Populus spp) belong to the most important tree species in afforestation programs of the Netherlands. Due to their rapid growth, the wood quality is usually low. Therefore, studies were performed to elucidate whether some technological properties and the resistance against fungal attack could be improved by impregnation with water-soluble resins. The results showed that swelling and shrink...
R D Peek, H Militz, J J Kettenis


Improvement of wood decay resistance by tannin impregnation
1991 - IRG/WP 2380
The fungical effect of tannins is appraised after exposure of treated woods samples to wood rotting fungi. A screening-test is carried out with several solutions containing extracts of two kinds of tannins; a condensed tannin derived from Quebracho heartwood (Schinopsis sp.) and a hydrolyzable one extracted from chestnut heartwood (Castanea sativa Mill). If a fungicidal action was indeed found it ...
D Dirol, A Scalbert


A study on the pressure impregnation of Eucalyptus globulus fence posts with CCA preservatives. Part 1
1988 - IRG/WP 3470
This paper describes the impregnation with CCA preservatives by full-cell process of Eucalyptus globulus fence-posts. Several treatments were made for different times of initial vacuum and treating pressure, with fence-posts from two coppice plantations (1st and 2nd rotations), assembled into three diameter classes: small, medium, large. The results concerning the absorption and lateral penetratio...
D De Sousa Castro Reimão, L Nunes


Probing red maple pit membrane pore size at FSP and OD using polystyrene macromolecules
2001 - IRG/WP 01-40217
A modified solute exclusion technique was used to pressure impregnate a polystyrene molecular weight (MW) series dissolved in styrene into red maple samples at approximately the fiber saturation point (FSP) and oven dry (OD). Radial penetration was less than tangential and FSP less than OD. There was a marked penetration change with MW in the tangential direction, although there appeared to be a ...
A Omidvar, M H Schneider, A R P Van Heiningen


Commercial potential of the four-cycle method for the impregnation of green beech sleepers in Yugoslavia
1975 - IRG/WP 347
This paper was presented to the Conference on Wood Protection held in Sarajevo (Yugoslavia) in 1973. The paper was based partially on the report prepared by J. Struhar and G. F. Franciosi, who were appointed in 1972 as FAO consultants to demonstrate the new impregnation process for green beech sleepers in Yugoslavia. The so-called 4-cycle method was developed at the State Forest Research Institute...
N Vidovic


Influencia de la impregnación con soluciones tánicas en la estabilidad dimensional de la madera de Pinus pinaster Ait. procedente de España
1992 - IRG/WP 92-3686
En virtud de la importancia que presenta la madera de Pinus pinaster Ait. en el sector constructivo español, se ha sometido a esta a tratamientos en autoclave con distintas soluciones tánicas naturales y artificiales a fin de estudiar su incidencia en la estabilidad dimensional frente a exposiciones exteriores. En el estudio se pone de manifiesto el efecto creado por el tratamiento protector en ...
J A Rodríguez Barreal, J Cubillo Jordan de Urries, L Garcia Esteban


Application of roller-pressing method to the novel liquid impregnation treatment of green timber
2001 - IRG/WP 01-40198
A transverse compression technique enabled us to impregnate liquid into green timber through replacement of the free water in the timber with a treatment liquid without any critical physical damage to the timber by the roller-pressing method. The roller-pressing is supposed to remove free water the cell cavities and to concurrently introduce the treatment solution into green timber in the treatmen...
M Inoue, K Adachi, K Tsunoda, Y Imamura, S Kawai


In situ timber treatments by spraying. Distribution of preservative in wood
1991 - IRG/WP 3678
This study was carried out in order to make the Pest Control Operators able to achieve correct treatments and enhance their efficacy. It was carried out in two steps: 1) in laboratory, to learn the influence of various parameters like spraying pressure, use of repeated applications, distance from nozzle to wood; 2) in situ on roof timber of five buildings. In this case, the applications of the pre...
C Defoin, G Dupont, M Lamour, H Sageot, M-M Serment


An investigation of the effects of pre-steaming on the treatment of sawn spruce timber with Celcure A, a copper/chrome/arsenic preservative
1981 - IRG/WP 3180
Difficulties in the treatment of spruce using standard vacuum/pressure techniques with both water-borne and organic solvent preservatives are well known. The growth characteristics of spruces (Picea spp) make them attractive candidates for forestry schemes. In 1975 the UK Forestry Commission had about 400 000 hectares, about 20% of total UK forest area, planted with Sitka spruce (Picea sitchensis)...
C R Coggins


Selective chromate elimination from the storage-drainage-water of a wood impregnation plant
1980 - IRG/WP 3153
With the Enviro-Chrom-Ex process it is possible to eliminate ecologically and economically hexavalent chromium (chromate) from water selectively. The process which is based on the principle of selective ion exchange works with different chromate concentrations and under the presence of other ions, irrespective of the water hardness. The values of water-offtake reach 0.1 mg CrVI at maximum, causing...
O Wälchli, R Ott, R Hugener, E Graf, B Lieberherr


Termite-tunnels formation on the surface of termite-resistant wood species in field sites
2001 - IRG/WP 01-10400
In this report, termite-tunnels formation by the subterranean termite, Coptotermes formosanus Shiraki on the surface of termite-resistant wood species, namely, Hinoki (Chamaecyparis abtsu), Yoshino Hinoki (Chamaecyparis abtsu), Miyazaki Hinoki (Chamaecyparis abtsu), Hiba (Chamaecyparis abtsu) and Japanese cedar (Cryptomeria japonica) was conducted in field sites. Westernhemlock (Tsuga heterophylla...
Y Kadekaru, K Kinjo, S Yaga


Efficiency of wood impregnation processes
1980 - IRG/WP 3151
Many wood impregnation processes have been in use for a very long time, up to 150 years, but they have not been progressively modified. This paper considers impregnation processes in relation to current requirements, particularly impregnation efficiency and energy consumption. The term 'pore' is used throughout in its physical sense and is not confined to botanical 'pore...
B A Richardson


Possibilities of improving the oscillating pressure method
1991 - IRG/WP 3668
Studies on the dynamics of pressure changes in wood during impregnation revealed no significant effect of fast pressure changes for green spruce as used by OPM (IRG/WP/3615). The following experiments were carried out on several hundreds of spruce palisades to examine the modification of single procedure parameters of common use OPM and to record the effects on the impregnation result with the aim...
S Goetsch, R-D Peek


Penetration of surface applied deltamethrin micro-emulsion formulations in four European timber species
1994 - IRG/WP 94-20030
The Netherland's Government, in line with many other European Governments initiated a programme (KWS2000) aimed at significantly reducing the emission of volatile organic compounds by the year 2000. As part of this programme a research project is currently underway to evaluate the potential for replacing organic solvent based remedial treatments with micro-emulsion formulations of the sam...
P Esser, W L D Suitela, A J Pendlebury


Quality of timber impregnated with preservatives of class AB after three years in service
2002 - IRG/WP 02-20241
Quality of impregnated timber is most often expressed by penetration and retention of the preservative used. Relatively less information is available about the performance of the final product, e.g. decks, panels etc. regarding product’s surface checks, deformations and overall appearance. Together with the timber durability, the above mention features are of esthetical importance in the above g...
N Terziev


Termite Field Tests of Various Timber Species Treated with permethrin using supercritical carbon dioxide
2005 - IRG/WP 05-10560
Termite field tests were conducted on permethrin-treated Eucalyptus obliqua heartwood, Pinus radiata sapwood and P. radiata LVL. The permethrin was impregnated using either supercritical carbon dioxide (scCO2) or light organic solvent preservative (LOSP) systems. Comparative permethrin retentions were most accurately achieved in P. radiata sapwood, where no difference between impregnation systems ...
A Qader, L J Cookson, J W Creffield, D Scown